Affiliation: | 1.Department of Physics,National Institute of Technology,Tiruchirappalli,India;2.Advanced Ceramics and Nanotechnology Laboratory, Department of Materials Engineering,University of Concepcion,Concepcion,Chile |
Abstract: | ZnO nanoparticles and Cu-doped ZnO nanoparticles were prepared by co-precipitation method. Also, a part of the pure ZnO nanoparticles were annealed at 750 °C for 3, 6, and 9 h. X-ray diffraction studies were carried out and the lattice parameters, unit cell volume, interplanar spacing, and Young’s modulus were calculated for all the samples, and also the crystallite size was found using the Scherrer method. X-ray peak broadening analysis was used to estimate the crystallite sizes and the strain using the Williamson–Hall (W–H) method and the size–strain plot (SSP) method. Stress and the energy density were calculated using the W–H method assuming different models such as uniform deformation model, uniform strain deformation model, uniform deformation energy density model, and the SSP method. Optical absorption properties of the samples were understood from their UV–visible spectra. Photocatalytic activities of ZnO and 5 % Cu-doped ZnO were observed by the degradation of methylene blue dye in aqueous medium under the irradiation of 20-W compact fluorescent lamp for an hour. |