Abstract: | Improved reaction conditions for the preparation of poly(p‐phenylene sulfide) (PPS) directly from bis(4‐bromophenyl) disulfide (BBD) have been established. Heating BBD with magnesium metal afforded only a low molecular weight polymer. PPS with a melting temperature around 280 °C was obtained from BBD in the presence of sodium carbonate or zinc metal. The best results were obtained with the addition of a catalytic amount of KI to the zinc–BBD mixture. Polymers prepared by the above methods are semicrystalline and dissolve in 1‐chloronaphthalene and have properties comparable to commercial PPS. © 2005 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 44: 900–904, 2006 |