Abstract: | (o-Methylphenyl)acetylene polymerized with high yields in the presence of W and Mo catalysts. W catalysts were more active than the corresponding Mo catalysts. The weight-average molecular weight of the polymer formed with W(CO)6–CCl4–hv reached 8 × 105, being higher than the maximum value (ca. 2 × 105) for poly(phenylacetylene). The polymer had the structure $rlap{--} [{rm CH} hbox{=hskip-1pt=} {rm C}(o - {rm CH}_3 {rm C}_6 {rm H}_4 )rlap{--} ]_n $. The stereochemical structure of the main chain could be determined by 13C-NMR; the cis content varied in a range of 41–61% depending on the polymerization conditions. The present polymer was thermally more stable than poly(phenylacetylene) according to thermogravimetric analysis. Interestingly, this polymer possessed deeper color than poly(phenylacetylene), and showed a fairly strong absorption in the visible region. |