Abstract: | Acrylamide coordinated to Cr(III), Bi(III), Pb(II), and Ca(II) nitrates polymerizes spontaneously in concentrated aqueous solutions at 20°C with formation of glass-like polymers containing water. The process takes from several hours to several days, depending on reaction conditions and the nature of the metal nitrate. The product contains water-soluble and water-insoluble fractions. The insoluble fraction is polyacrylamide containing no metal compound. The possibility of spontaneous copolymerization of acrylamide complexes of metal nitrates with other water-soluble monomers was established.Institute of Energy Problems in Chemical Physics, Chernogolovka Branch, Russian Academy of Sciences, 142432 Chernogolovka. Institute of Chemical Physics, Chernogolovka Branch, Russian Academy of Sciences, 142432 Chernogolovka. Translated from Izvestiya Akademii Nauk, Seriya Khimicheskaya, No. 9, pp. 2073–2080, September, 1992. |