Abstract: | Mn substituted ZnO nanocrystals synthesized by a co‐precipitation method. X‐ray diffraction (XRD) studies confirms the presence of wurtzite (hexagonal) crystal structure similar to un doped ZnO, suggesting that doped Mn ions go at the regular Zn sites. The lattice parameters a and c are increasing with increasing Mn content. The unit cell volume increases with increasing Mn concentration, indicating the homogeneous substitution of Mn2+ for the Zn2+. The lattice distortion parameter (εv) is evaluated from XRD data and found that it enhances as Mn content increases. Transmission electron microscopy photographs show that the size of the ZnO crystals is in the range of 20‐50 nm. The SAED pattern confirms the hexagonal and crystalline nature of the samples which are in agreement with X‐ray analysis. The chemical groups of the samples have been identified by FTIR studies (© 2011 WILEY‐VCH Verlag GmbH & Co. KGaA, Weinheim) |