Abstract: | Catalytic oxidative coupling of methane over perovskite CaTiO3 prepared by modified ceramic method has been studied. The C2 yield was 13% at 830 °C and promotion with Na4P2O7 did not improve considerably the catalyst peformance. Regarding reactor test and mechanism studies it is believed that charge deficient, oxygen O– generated by transforming oxygen adsorbed on surface defects and dissolved into bulk vacancies is responsible for activating methane (active site). Adsorbed oxygen generates the oxidizing sites for actived methane. Strict conditions are required for generation and regeneration of the activating sites in lattice. |
| |