Polyimide/diamond nanocomposites have been synthesized from 4,4′‐diaminodiphenyl ether (ODA) and 3,3′,4,4′‐benzophenonetetracarboxylic dianhydride (BTDA). All the polyimides show non‐crystalline X‐ray diffraction. The frequent occurrence of particular interatomic distances (R) denoted by the non‐crystalline X‐ray diffraction maxima are determined. An ultramicro‐indentation technique is employed to evaluate the effects of nano‐diamond particles on the indentation behavior of polyimides. Indentation size effect is observed and discussed.