Lattice parameters variation with temperature of Ti2O3 and (Ti0.98V0.02)2O3 from single crystal X-ray data |
| |
Authors: | J.J. Capponi M. Marezio J. Dumas C. Schlenker |
| |
Affiliation: | Laboratoire des Rayons X, CNRS, BP 166X, 38042 Grenoble Cedex, France;Groupe des Transitions de Phases, CNRS, BP 166X, 38042 Grenoble Cedex, France |
| |
Abstract: | The lattice parameters of Ti2O3 and (Ti0.98V0.02)2O3 have been measured as a function of temperature (24–670°C for Ti2O3 and 24–440°C for V-doped Ti2O3) from single crystal X-ray data. The high temperatures were attained by blowing hot argon directly on the crystal mounted on an automatic Philips diffractometer. This experimental set-up gives standard deviations which are at least 10 times better than those of the previous measurements and allows to keep Ti2O3 as such well above the transition. The variations of a, c, (hexagonal axes) for pure Ti2O3 are in agreement with the previous results. On the contrary we did not observe any transition in the unit cell volume. The V-doping seems to attenuate the transition which is visible only on the a vs T curve |
| |
Keywords: | |
本文献已被 ScienceDirect 等数据库收录! |
|