首页 | 本学科首页   官方微博 | 高级检索  
     


Redox behavior of V/MgO catalyst in H2S wet oxidation at room temperature
Authors:Eun-Ku Lee   Kwang-Deog Jung   Oh-Shim Joo  Yong-Gun Shul
Affiliation:(1) Department of Chemical Engineering, Yonsei University, Seoul, 120-749, Korea;(2) Eco-Nano Center, Korea Institute of Science and Technology, P.O. Box 131, Cheongryang, Seoul, Korea
Abstract:The room temperature wet catalytic oxidation was conducted in a batch reactor with V/MgO catalyst. The XRD study of the catalyst used indicated that V/MgO could not only oxidize H2S to sulfur selectively, but also prevent the sulfidation of metal oxide effectively at the room temperature. The XPS study indicated that the H2S oxidation with V/MgO could proceed by a redox mechanism (V5+↔ V4+) and that V3+ formation (V4+→ V3+), was responsible for the deactivation of V/MgO. This revised version was published online in June 2006 with corrections to the Cover Date.
Keywords:H2S  Wet catalytic oxidation  V/MgO catalyst  redox mechanism
本文献已被 SpringerLink 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号