首页 | 本学科首页   官方微博 | 高级检索  
     


Drying dissipative structures of aqueous solution of poly(ethylene glycol) on a cover glass, a watch glass, and a glass dish
Authors:Tsuneo Okubo  Junichi Okamoto  Shinya Takahashi  Akira Tsuchida
Affiliation:(1) Institute for Colloidal Organization, Hatoyama 3-1-112, Uji, Kyoto 611-0012, Japan;(2) Department of Applied Chemistry, Gifu University, Yanagido 1, Gifu 501-1193, Japan
Abstract:Drying dissipative structures of aqueous solution of poly(ethylene glycol) (PEG) of molecular weights ranging from 200 to 3,500,000 were studied on a cover glass, a watch glass, and a glass dish on macroscopic and microscopic scales. Any convectional and sedimentation patterns did not appear during the course of drying the PEG solutions. Several important findings on the drying patterns are reported. Firstly, the crystalline structures of the dried film changed from hedrites to spherulites as the molecular weight and/or concentration of PEG increased. Secondly, lamellae were formed along the ring patterns especially at high concentrations and high molecular weights. The coupled crystalline patterns of the spherulites and the lamellae were observed in a watch glass along the ring structures, supporting the important role of the convection by the gravity during the course of dryness. The coupled patterns were difficult to be formed on a cover glass and a glass dish, except at the outside edge of the dried film. Thirdly, the size of the broad ring at the outside edge of the dried film especially on a cover glass and a watch glass increased sharply as the molecular weight increased and also as the polymer concentration increased. Electronic supplementary material  The online version of this article (doi:) contains supplementary material, which is available to authorized users.
Keywords:Poly(ethylene glycol)  Poly(ethylene oxide)  Dissipative structure  Drying pattern  Spherulite  Hedrite  Lamellae
本文献已被 SpringerLink 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏