1
1.
The thermal decomposition of natural iowaite of formula Mg6Fe2(Cl,(CO3)0.5)(OH)16·4H2O was studied by using a combination of thermogravimetry and evolved gas mass spectrometry. Thermal decomposition occurs over a number of mass loss steps at 60°C attributed to dehydration, 266 and 308°C assigned to dehydroxylation of ferric ions, at 551°C attributed to decarbonation and dehydroxylation, and 644, 703 and 761°C attributed to further dehydroxylation. The mass spectrum of carbon dioxide exhibits a maximum at 523°C. The use of TG coupled to MS shows the complexity of the thermal decomposition of iowaite. This revised version was published online in July 2006 with corrections to the Cover Date.  相似文献   
2.
Hydrotalcites of formula Mg6(Al,Fe)2(OH)16(CO3)·4H2O formed by intercalation with the carbonate anion as a function of divalent/trivalent cationic ratio have been successfully synthesised. The XRD patterns show variation in the d‐spacing attributed to the size of the cation. Raman and infrared bands in the OH stretching region are assigned to (1) brucite layer OH stretching vibrations, (2) water stretching bands and (3) water strongly hydrogen bonded to the carbonate anion. Multiple (CO3)2− symmetric stretching bands suggest that different types of (CO3)2− exist in the hydrotalcite interlayer. Increasing the cation ratio (Mg/Al,Fe) resulted in an increase in the combined intensity of the two Raman bands at around 3600 cm−1, attributed to Mg OH stretching modes, and a shift of the overall band profile to higher wavenumbers. These observations are believed to be a result of the increase in magnesium in the structure. Raman spectroscopy shows a reduction in the symmetry of the carbonate, leading to the conclusion that the anions are bonded to the brucite‐like hydroxyl surface and to the water in the interlayer. Water bending modes are identified in the infrared spectra at positions greater than 1630 cm−1, indicating that water is strongly hydrogen bonded to both interlayer anions and the brucite‐like surface. Copyright © 2009 John Wiley & Sons, Ltd.  相似文献   
3.
The thermal decompositions of hydrotalcites with hexacyanoferrate(II) and hexacyanoferrate(III) in the interlayer have been studied using thermogravimetry combined with mass spectrometry. X-ray diffraction shows the hydrotalcites have a d(003) spacing of 11.1 and 10.9 Å which compares with a d-spacing of 7.9 and 7.98 Å for the hydrotalcite with carbonate or sulphate in the interlayer. XRD was also used to determine the products of the thermal decomposition. For the hydrotalcite decomposition the products were MgO, Fe2O3 and a spinel MgAl2O4. Dehydration and dehydroxylation take place in three steps each and the loss of cyanide ions in two steps.  相似文献   
4.
The mineral stichtite was synthesised and its thermal decomposition measured using thermogravimetry coupled to an evolved gas mass spectrometer. Mass loss steps were observed at 52, 294, 550 and 670°C attributed to dehydration, dehydroxylation and loss of carbonate. The loss of carbonate occurred at higher temperatures than dehydroxylation.  相似文献   
5.
A combination of high resolution thermogravimetric analysis coupled to a gas evolution mass spectrometer has been used to study the thermal decomposition of synthetic hydrotalcites reevesite (Ni6Fe2(CO3)(OH)16·4H2O) and pyroaurite (Mg6Fe2(SO4,CO3)(OH)16·4H2O) and the cationic mixtures of the two minerals. XRD patterns show the hydrotalcites are layered structures with interspacing distances of around 8.0. Å. A linear relationship is observed for the d(001) spacing as Ni is replaced by Mg in the progression from reevesite to pyroaurite. The significance of this result means the interlayer spacing in these hydrotalcites is cation dependent. High resolution thermal analysis shows the decomposition takes place in 3 steps. A mechanism for the thermal decomposition is proposed based upon the loss of water, hydroxyl units, oxygen and carbon dioxide.  相似文献   
6.
Refait  Ph.  Drissi  S.  Abdelmoula  M.  Génin  J.-M. R. 《Hyperfine Interactions》2002,139(1-4):651-655
Green rust-like compounds (GRs) were discovered as natural minerals in various hydromorphic soils, where anoxic conditions allow their stability. They may control some redox processes in aquifers and participate to the transformation of various pollutants. Since Mg(II) cations are present in the fields where GRs were discovered, a partial substitution of Mg(II) to Fe(II) leading to intermediate compounds between GRs and usual Mg(II)–Fe(III) hydroxysalts is suspected. Mg(II)–Fe(II)–Fe(II) hydroxycarbonates can be obtained as intermediate oxidation products of (Mg, Fe)(OH)2 in carbonate-containing aqueous media obeying to [FeII 4(1–x)MgII 4x FeIII 2(OH)12]2+ [CO3 2– nH2O]–2. TMS spectra at 12 K are similar to those of GRs, i.e., two quadrupole doublets, one due to Fe(II) with a large isomer shift =1.29 mms–1 (with respect to -iron at room temperature) and quadrupole splitting E Q=2.76 mms–1, the other one due to Fe(III) with smaller hyperfine parameters =0.49 mms–1 and E Q=0.44 mms–1. Fe(II) ions oxidise rapidly into Fe(III) with dissolved O2. The reactivity is similar to that of Fe(II)–Fe(III) hydroxysalts GR, and thus the potential of Mg(II)–Fe(II)–Fe(III) compounds for reducing pollutants.  相似文献   
7.
Hydrotalcites containing carbonate, vanadate and molybdate were prepared by coprecipitation. The resulting materials were characterized by XRD, and TG/DTA to determine the stability of the hydrotalcites synthesized. The thermal decomposition of carbonate hydrotalcites consist of two decomposition steps between 300 and 400°C, attributed to the simultaneous dehydroxylation and decarbonation of the hydrotalcite lattice. Water loss ascribed to dehydroxylation occurs in two decomposition steps, where the first step is due to the partial dehydroxylation of the lattice, while the second step is due to the loss of water interacting with the interlayer anions. Dehydroxylation results in the collapse of the hydrotalcite structure to that of its corresponding metal oxides, including MgO, Al2O3, MgAl2O4, NaMg4(VO4)3 and Na2Mg4(MoO4)5. The presence of oxy-anions proved to be beneficial in the stability of the hydrotalcite structure, shown by the delay in dehydroxylation of oxy-anion containing hydrotalcites compared to the carbonate hydrotalcite. This is due to the substantial amount of hydroxyl groups involved in a network of hydrogen bonds involving the intercalated anions. Therefore, the stability of the hydrotalcite structure appears to be dependent on the type of anion present in the interlayer. The order of thermal stability for the synthesized hydrotalcites in this study is Syn-HT-V>Syn-HT-Mo> Syn-HT-CO3-V>Syn-HT-CO3-Mo>Syn-HT-CO3. Carbonate containing hydrotalcites prove to be less stable than oxy-anion only hydrotalcites.  相似文献   
8.
Layered hydroxides crystallize in a hexagonal structure and incorporate a number of different types of structural disorders as an exigency of anisotropic bonding. Structural disorder contributes to the non-uniform broadening of lines in the powder X-ray diffraction pattern. Common among the disorders are stacking faults, which broaden theh0ℓ/0kℓ reflections. Interstratification selectively broadens the 00l reflections and turbostratic disorder broadens the 0kℓ reflections. The line broadening caused by structural disorder has to be discounted before estimates of particle size are made by applying the Scherrer formula. Dedicated to Prof J Gopalakrishnan on his 62nd birthday.  相似文献   
9.
Thermal analysis complimented with evolved gas mass spectrometry has been applied to hydrotalcites containing carbonate prepared by coprecipitation and with varying divalent/trivalent cation ratios. The resulting materials were characterised by XRD, and TG/DTG to determine the stability of the hydrotalcites synthesised. Hydrotalcites of formula Mg4(Fe,Al)2(OH)12(CO3)·4H2O, Mg6(Fe,Al)2(OH)16(CO3)·5H2O, and Mg8(Fe,Al)2(OH)20(CO3)·8H2O were formed by intercalation with the carbonate anion as a function of the divalent/trivalent cationic ratio. XRD showed slight variations in the d-spacing between the hydrotalcites. The thermal decomposition of carbonate hydrotalcites consists of two decomposition steps between 300 and 400°C, attributed to the simultaneous dehydroxylation and decarbonation of the hydrotalcite lattice. Water loss ascribed to dehydroxylation occurs in two decomposition steps, where the first step is due to the partial dehydroxylation of the lattice, while the second step is due to the loss of water interacting with the interlayer anions. Dehydroxylation results in the collapse of the hydrotalcite structure to that of its corresponding metal oxides and spinels, including MgO, MgAl2O4, and MgFeAlO4.  相似文献   