排序方式: 共有5条查询结果,搜索用时 15 毫秒
1
1.
为了提高熔石英元件表面抗激光损伤阈值,利用超声波辅助HF酸研究平滑光学元件表面缺陷形貌和去除刻蚀后残留物效果,通过扫描电子显微镜电镜和原子力显微镜记录表面形貌结构,以及单脉冲激光辐照测试抗损伤阈值确定实验参数。研究表明,超声波场的引入能催化HF酸的刻蚀速率、提高钝化效果并且更易剥离嵌入的亚μm级杂质粒子。经过实验测试,获得了熔石英类元件相匹配的超声辅助HF酸刻蚀实验参数,研究结果对应用超声波辅助HF酸研究熔石英表面抗激光损伤有重要意义。 相似文献
2.
The experimental performance of beam smoothing by combined one-dimensional (1D) spectral dispersion and lens array (LA) technology is presented, as applied in the ninth beam of SG-II. Using 3w spectral dispersion with a bandwidth of 270 GHz and a line dispersion that is 24.9 times the beam's diffraction- limited width decreases the focal spot non-uniformity of 80% energy concentration from 46% to 17%. The multiple-beam interference properties of the LA are theoretically and experimentally validated by spatial power spectral density analysis. Peak-spectra suppression ratios of 20 and 10 dB are achieved in the dispersion and orthogonal directions, respectively. 相似文献
3.
4.
5.
当前高功率激光装置系统中, 国内使用透射式衍射光栅进行光束采样, 国外甚至使用光栅聚焦并同时结合谐波分离和采样功能. 高功率激光辐照下, 除了0级透射打靶光以及目标取样光外, 其他级次衍射光的影响也不可忽视, 可能造成诸如鬼像聚焦破坏、时间脉宽测量不稳定、近远场测量噪声等问题. 尤其是透射衍射光栅内部全反射级次会导致光栅出射一系列规律的衍射花样, 造成上述干扰和危害. 首先理论上针对透射式光栅(包括取样光栅和聚焦光栅)进行了相应的计算和分析, 然后从实验上观察并测量了取样光栅内部全反射级次的现象, 并且结合镀减反膜前后的衍射现象进行了讨论, 最后分析并给出了如何消除或规避全反射级次和其他冗余级次影响的方法. 相似文献
1