采用一种简单的溶剂热法成功的合成了花朵状的钴磁性粉体。通过X射线粉末衍射(XRD),扫描电子显微镜(SEM)等对样品进行物相与形貌的表征。结果表明样品为六排堆积(hcp)和面心立方结构(fcc)混合结构的钴单质,形貌为由很多个厚度约为50~150 nm的菱形花瓣构成的花朵状结构,每个花朵的尺寸约为2μm左右。采用振动样品磁强计(VSM)测试了样品的磁性能,测试表明样品在室温下表现出铁磁性,饱和磁化强度(Ms)为140 emu.g-1,剩磁(Mr)为9.4 emu.g-1,矫顽力(Hc)为280 Oe。 相似文献
3.
The effects of Al_2O_3, Yb_2O_3, Er_2O_3 and OH~- on spectral properties of P_2O_5.Na_2O.SrO.Al_2O_3.Yb_2O_3.Er_2O_3 erbium phosphate glass were studied. 5, 8, and 13 mol% Al_2O_3, 4, 5, 6, 7 and 8 mol% Yb_2O_3 and0.05, 0.2, and 0.4 mol% Er_2O_3 were used. It was found that Al_2O_3 can improve fluorescent lifetime ofEr~(3+)ions, but the integrated absorption cross section of Er~(3+)ions decreases with the increase of Al_2O_3concentration. Evaluating from energy transfer efficiency of Yb~(3+)to Er~(3+)and spectral parameters ofYb~(3+)and Er~(3+),we conclude that 6 mol% Yb_2O_3 and 0.4 mol% Er_2O_3 are needed for LD pumped 相似文献
4.
Er~(3+)激活玻璃是继钕玻璃后的一种具有实用意义的激光玻璃。输出波长为1.54μm,处于大气窗口,便于传输,尤其是在战场硝烟下的透过率高,故特别适用于测距和军事模拟。鉴于Er~(3+)吸收带少、振子率小,故使用Cr~(3+)-Yb~(3+)-Er~(3+)系统来实现能量转移敏化发光;选择磷酸盐玻璃基质,以增加能量转移的效率;1.54μm激光产生跃迁是三能级系统,选用低的激活离子浓度(3×10~(10)cm~(-3)),以降低激光阈值并减少自吸收;增大Yb~(3+)浓度以提高能量转移几率;控制Cr~(3+)浓度以 相似文献
5.
氟磷玻璃作为光学玻璃及激光工作物质,正在获得应用。在研究Al(PO_3)_3系统玻璃的生成及结构的基础上,本文研究了光学及其它物理性质。Al(PO_3)_3含量低的氟磷玻璃,网络结构受到极大的破坏,处于破坏区,性质变化及各种氟化物对性质的影响与处于破坏区的氧化物玻璃相似。LiF、MgF_2和AlF_3等氟化物的特殊作用在物理性质变化方面也得到反映。同时,与硅酸盐和硼酸盐等玻璃生成体含量高的玻璃比较,静电吸引力对Al(PO_3)_3含量低的氟磷玻璃的性质变化起着更大的作用。文中表示所研究玻璃在n_d~v_d图中的位置,给出低Al(PO_3)_3含量玻璃中的部分性质,与文献数据进行比较,并把部分性质的变化与Al(PO_3)_3含量相联系. 相似文献
6.
7.
8.
9.
在概述国内外高功率激光钕玻璃的发展及其主要性质的基础上,重点论述了上海光学精密机械研究所在大口径N31高功率激光钕玻璃半连续熔炼工艺、连续熔炼工艺、包边工艺等方面的研究进展。报道了半连续熔炼工艺制备的不同Nd2O3浓度N31钕玻璃的光吸收损耗和荧光寿命及小信号增益系数,并给出了这些钕玻璃坯片小信号增益系数的波动范围。通过对半连续熔炼和连续熔炼工艺制备的N31激光钕玻璃主要性能的比较,证明连续熔炼工艺制备的N31钕玻璃的主要性能指标与半连续熔炼的性能相当。对于400 mm大口径N31钕玻璃坯片的包边进行了模拟考核,结果表明,采用现有包边工艺的钕玻璃可以承受1 000次高功率氙灯辐射。 相似文献