A series of 2-cyano-3-methylthio-3-substituted methylaminoacrylates were synthesized as herbicidal inhibitors of photosystem Ⅱ (PSⅡ) electron transport, in order to estimate the effect of fluorine atom, pyridyl group, chirality and ester chain on activity. The important intermediate 2-fluoro-5-aminomethylpyridine was synthesized with high yield. The bioassay results showed that most of rifle compounds had high herbicidal activity in postemergence treatment. The introduction of an a-methyl into the 3-substituted methylamino could improve the activity notably. The replacement of hydrogen by chlorine or fluorine group and phenyl by pyridyl group showed different effects, and at the same time, the ester chain affected the activity too. 相似文献
2.
水溶性负性光致抗蚀剂的研制 总被引:1,自引:0,他引:1
以自制丙烯酰胺-双丙酮丙烯酰胺共聚物和聚乙烯吡咯烷酮(PVP)为成膜基体物质,芳香族叠氮化合物为感光剂,研制出水溶性负性光致抗蚀剂配方.通过正交试验确定了最优配方.即共聚物中AM与DAAM质量比为1:1;P(AM-DAAM)与PVP质量比为1:2;感光剂用量为占成膜基体物质质量的1/6;偶联剂用量占成膜基体物质质量的1/60;表面活性剂G-18用量占成膜基体物质质量的1/40.在该配方下配制的光致抗蚀剂达到商品规格要求.通过与国外同类商品的比较得出自制光致抗蚀剂具有同国外商品相当的感光性能. 相似文献
3.
5.
制备了导电高分子聚苯胺与活性炭的复合载体(PAnC),用PAnC作为载体制备的钯催化剂性能优于单独活性炭作为载体制备的催化剂。此外掺杂十二烷基磺酸钠制备的聚苯胺碳载体(PAnC-S)具有比PAnC更低的电荷传递电阻,10~25 nm的介孔数量明显增加,比表面积增大到94.9 m2/g。PAnC-S与PAnC粒径均匀,粒径均在30 nm左右。以PAnC-S和 PAnC为载体制备的钯催化剂比活性炭作载体制备的钯催化剂具有更大的电化学比表面积,分别为84.7和62.6 m2/g。对甲酸的氧化具有更高的电化学活性和稳定性。 相似文献
6.
7.
通过低温氧化法在活性碳表面修饰聚吡咯(PPy-C), 并以PPy-C为载体制备了纳米Pd催化剂(Pd/PPy-C). 采用X射线衍射、扫描电镜、透射电镜等手段对载体PPy-C及催化剂Pd/PPy-C进行了表征, 电化学测试结果表明, Pd/PPy-C催化剂电极不但能够增强催化剂对甲酸催化氧化的活性, 而且还能够大幅度提高催化剂的稳定性, 因此以PPy-C为载体的Pd/PPy-C催化剂是一类具有潜在应用前景的直接甲酸燃料电池阳极催化剂. 通过分析电化学比表面随循环伏安次数的变化及多电势阶跃实验结果表明, 催化剂电极活性衰减的主要原因是载体被氧化及电极表面积累强吸附物种的结果. 相似文献
8.
本文制备了二氧化锰和聚苯胺碳的复合电级材料(MnO2-PAnC),测试结果表明MnO2-PAnC材料为松散结构组成的纳米颗粒. MnO2-PAnC 材料的比电容最大可达459 F•g-1,MnO2-PAnC电极在较高的扫速下循环伏安曲线变形较小,表现出良好的可逆性. 交流阻抗测试结果表明,MnO2-PAnC 电极电荷传递电阻小,表面离子扩散速度快. 充放电500个循环后,MnO2-PAnC 电容的保持率仍高于60%. 以上实验结果表明,MnO2-PAnC 是很好的超级电容器的电极材料. 相似文献