Micrometer-sized MoO2 hollow spheres were synthesized hydrothermally with ammonium heptamolybdate tetrahydrate as molybdenum source, Cetyltrimethylammonium bromide as structure-directing agent and C2H5OH as reducing agent, respectively. The products were investigated by X-ray diffraction, thermo- gravimetry and differential thermal analysis, scanning electron microscopy, transmission electron microscopy and X-ray photoelectron spectroscopy. A morphology transition of "blocks-solid spheres-hollow spheres" during the growth process was observed and the possible mechanism for the formation of MoO2 samples was proposed to be through a microscale Kirkendall effect. 相似文献
2.
3.
4.
以拟薄水铝石作为铝源,正磷酸为磷源,正三丙胺(TPA)作模板剂,采用水热法合成了AIPO4-5分子筛.在不同的反应物配比、温度以及晶化时间条件下,得到了不同尺寸的AIPO4-5分子筛单晶.实验表明,反应物质的摩尔比为Al2O3:P2O5:TPA:C2H5OH:H2O:HF=1:1.2:2.66:80:1000:0.7,反应温度为457K,晶化时间48h是生成六方AIPO4-5分子筛大单晶较适宜的条件;在该反应条件下合成出纵向尺度最大达到2.0mm、具有完整六方棱柱形态的MPO4-5分子筛单晶;部分晶体的横向尺度达到0.31mm.用扫描电镜观察晶体的形貌:AlPO4-5分子筛晶体结构通过SMART1000单晶衍射仪鉴定. 相似文献
5.
高质量AlPO4-5分子筛大单晶的合成与表征 总被引:2,自引:0,他引:2
以拟薄水铝石作为铝源,正磷酸为磷源,正三丙胺(TPA)作模板剂,采用水热法合成了AlPO4 5分子筛.在不同的反应物配比、温度以及晶化时间条件下,得到了不同尺寸的AlPO4 5分子筛单晶.实验表明,反应物质的摩尔比为Al2O3∶P2O5∶TPA∶C2H5OH∶H2O∶HF=1∶1. 2∶2. 66∶80∶1000∶0. 7,反应温度为457K,晶化时间48h是生成六方AlPO4 5分子筛大单晶较适宜的条件;在该反应条件下合成出纵向尺度最大达到2. 0mm、具有完整六方棱柱形态的AlPO4 5分子筛单晶;部分晶体的横向尺度达到0. 31mm.用扫描电镜观察晶体的形貌;AlPO4 5分子筛晶体结构通过SMART1000单晶衍射仪鉴定. 相似文献
1