用水热法在ZnO薄膜上制备了直径、密度及取向可控的ZnO纳米线阵列。ZnO薄膜是通过原子层沉积(ALD)方法制备并在不同温度下退火处理得到的,退火温度对ZnO薄膜的晶粒尺寸、结晶质量和缺陷性质有很大的影响。而ZnO薄膜的性质对随后生长的ZnO纳米线的直径、密度及取向能起到调节控制的作用。通过扫描电子显微镜(SEM)、X射线衍射(XRD)仪和光致发光(PL)测试对ZnO薄膜和ZnO纳米线进行了表征。最后得到的垂直取向的ZnO纳米线阵列适合在发光二极管和太阳能电池等领域使用。 相似文献
3.
Biofunctional europium(Ⅲ)-doped ZnS(ZnS:Eu) nanocrystals are prepared by a sol–gel method. The characteristic luminescence of ZnS:Eu is used as a probe signal to realize sensitive immunoassay. The luminescence intensity of the Eu~(3+) in the ZnS matrix shows strong concentration dependence, and the optimal doping concentration is 4%. However,the emission wavelengths of the ZnS:Eu nanocrystals are not dependent on doping concentration nor the temperature(from 100 K to 300 K). Our results show that these features allow for reliable immunoassay. Human immunoglobulin, used as a target analyte, is captured by antibody modified ZnS:Eu probe and is finally enriched on gold substrate for detection.High specificity of the assay is demonstrated by control experiments. The linear detection range is 10 nM –800 nM, and the detection limit is about 9.6 nM. 相似文献
4.
本研究在SBA-15分子筛孔道中制备了纳米ZnS。Zn2+首先通过离子交换交换到SBA-15中,通过水热法在SBA-15分子筛孔道中制备了纳米ZnS。(SBA-15)-ZnS复合物由粉末X-线衍射,傅立叶变换红外光谱,低温氮气吸附-解析附技术,固体扩散漫反射光谱以及发光研究进行了表征。粉末X-线衍射研究说明在制备主-客体纳米复合材料中分子筛骨架未被制备过程所破坏,保持完整且结晶度仍很高。傅立叶变换红外光谱表明制备的材料骨架完好。77 K低温氮气吸附-解析附研究表明所制备的复合材料孔体积,孔尺寸以及表面积相对于SBA-15分子筛降低,证明客体ZnS已成功地组装入分子筛孔道中。所制备的纳米复合材料固体扩散漫反射吸收光谱相对于体相ZnS显示出蓝移表明,ZnS已限制在分子筛的孔道中且复合材料中分子筛的孔道对ZnS具有明显的立体限域效应,ZnS成功地组装在SBA-15分子筛的孔道中。发光研究表明,(SBA-15)-ZnS样品出现明显发光现象。主-客体复合材料具有良好的发光性能,有望在发光材料领域中获得应用。 相似文献
5.
6.
用一种低成本的方法制备出了树形结构Si/ZnO纳米线阵列。首先在室温条件下用金属辅助化学腐蚀法在Si(100)衬底上制备了Si纳米线阵列,Si纳米线的直径尺寸及分布都很均匀,通过改变腐蚀时间,能够得到高度不同的Si纳米线阵列。利用磁控溅射在Si纳米线表面制备一层ZnO薄膜,然后利用水热法在Si纳米线阵列上生长了ZnO纳米线。通过扫描电子显微镜(SEM)、能谱分析仪(EDS)和光致发光(PL)测试对样品进行了表征。通过这种方法制备的Si/ZnO复合结构在太阳能电池、光催化等领域有潜在应用价值。 相似文献
1