排序方式: 共有3条查询结果,搜索用时 0 毫秒
1
1.
采用飞秒激光改性-化学腐蚀的方法, 分别研究了3种典型玻璃的化学腐蚀性能. 通过测试材料的微观结构, 分析了不同材料的腐蚀速率与脉冲能量及腐蚀时间的关系, 从材料组成、显微结构及化学键特征讨论了玻璃改性-腐蚀机理. 结果表明, 飞秒激光改性后的碲酸盐和PbO硅酸盐玻璃不具有选择性腐蚀特性, 而石英玻璃的选择性腐蚀比高于40; 飞秒激光改性玻璃的选择性腐蚀特性与材料结构有关, 分子体积大、网络结构不紧密的材料不具有选择腐蚀特性. 相似文献
2.
A double-cladding ytterbium-doped photonic crystal fibre (PCF) with a 350-μm^2 effective area is fabricated. The measurement results show that the PCF has high absorption peak at 915 nm. Its fluorescence lifetime is 840μs. Laser experiments with all-fibre configurations are carried out with this fibre. A continuous-wave output power of 3.96 W is achieved with a 5.2 W launched pump power. The central wavelength of the output spectrum is 1080.22nm. The results show that the PCF laser has a high slope efficiency of 79.6% and light conversion efficiency of 76.2%. 相似文献
3.
1