首页 | 本学科首页   官方微博 | 高级检索  
文章检索
  按 检索   检索词:      
出版年份:   被引次数:   他引次数: 提示:输入*表示无穷大
  收费全文   145篇
  免费   0篇
  国内免费   9篇
化学   116篇
晶体学   6篇
力学   5篇
物理学   27篇
  2022年   3篇
  2021年   2篇
  2020年   1篇
  2019年   4篇
  2018年   3篇
  2017年   6篇
  2016年   4篇
  2015年   1篇
  2014年   2篇
  2013年   5篇
  2012年   8篇
  2011年   9篇
  2010年   10篇
  2009年   8篇
  2008年   16篇
  2007年   12篇
  2006年   12篇
  2005年   10篇
  2004年   7篇
  2003年   12篇
  2002年   2篇
  2001年   1篇
  2000年   4篇
  1999年   2篇
  1998年   3篇
  1997年   2篇
  1996年   1篇
  1995年   2篇
  1994年   1篇
  1992年   1篇
排序方式: 共有154条查询结果,搜索用时 671 毫秒
61.
The transport of Na through the polycrystalline ceramic arc tube of high intensity discharge lamps has been investigated. This complex process consists of several steps: solution in the ceramics, diffusion through the ceramics, leaving the bulk phase, evaporation from the surface. Among the listed processes the kinetics of the diffusion was examined in the temperature range 400-1200 °C, separately from other disturbing effects. X-ray photoelectron spectroscopy (XPS) and secondary ion mass spectroscopy (SIMS) were used to determine the concentration depth profiles. The obtained results confirmed that the grain boundary diffusion plays an important role in the transport process of sodium through the ceramic wall. The bulk and the grain boundary diffusion coefficients and the temperature dependencies of these transport processes have been determined. The activation energy of Na bulk diffusion is 56.5 ± 6.7 kJ/mol at 900-1200 °C, respectively the activation energies of Na grain boundary diffusion amount to 97.5 ± 21.6 kJ/mol in the temperature range 700-1100 °C and 7.7 ± 4.0 × 10−2 kJ/mol at 400-700 °C. The preexponential factor of the bulk diffusion was found to be Do = 5.1 × 10−15 ± 9.5 × 10−17 cm2/s in the temperature range 900-1200°C, whereas the preexponential factors of grain boundary diffusion are Do = 1.1 × 10−10 ± 1.1 × 10−11 cm2/s at 700-1100 °C and Do = 7.5 × 10-15 ± 1.5 × 10−17 cm2/s at 400-700 °C.  相似文献   
62.
We have successfully synthesized a high-purity polycrystalline sample of tetragonal Li7La3Zr2O12. Single crystals have been also grown by a flux method. The single-crystal X-ray diffraction analysis verifies that tetragonal Li7La3Zr2O12 has the garnet-related type structure with a space group of I41/acd (no. 142). The lattice constants are a=13.134(4) Å and c=12.663(8) Å. The garnet-type framework structure is composed of two types of dodecahedral LaO8 and octahedral ZrO6. Li atoms occupy three crystallographic sites in the interstices of this framework structure, where Li(1), Li(2), and Li(3) atoms are located at the tetrahedral 8a site and the distorted octahedral 16f and 32g sites, respectively. The structure is also investigated by the Rietveld method with X-ray and neutron powder diffraction data. These diffraction patterns are identified as the tetragonal Li7La3Zr2O12 structure determined from the single-crystal data. The present tetragonal Li7La3Zr2O12 sample exhibits a bulk Li-ion conductivity of σb=1.63×10−6 S cm−1 and grain-boundary Li-ion conductivity of σgb=5.59×10−7 S cm−1 at 300 K. The activation energy is estimated to be Ea=0.54 eV in the temperature range of 300–560 K.  相似文献   
63.
Single crystals of iron(II) pyroborate, Fe2B2O5, were prepared at 1000–1050 °C under an argon atmosphere. The crystals were transparent, yellowish in color and needle-like or columnar. The crystal structure of Fe2B2O5 was analyzed by single-crystal X-ray diffraction. Refined triclinic unit cell parameters were a=3.2388(2), b=6.1684(5), c=9.3866(8) Å, α=104.613(3)°, β=90.799(2)° and γ=91.731(2)°. The final reliability factors of refinement were R1=0.020 and wR2=0.059 [I > 2σ(I)]. Transmittance over 50% in the visible light region from 500 to 750 nm was observed for a single crystal of Fe2B2O5 with a thickness of about 0.3 mm. The light absorption edge estimated from a diffuse reflectance spectrum was at around 350 nm (3.6 eV). Magnetic susceptibility was measured for single crystals at 4–300 K. Fe2B2O5 showed antiferromagnetic behavior below the Néel temperature, TN≈70 K, and the Weiss temperature was TW=36 K. The effective magnetic moment of Fe was 5.3μB.  相似文献   
64.
Various important processes, such as electron transfer reactions, adsorption/desorption, solvation/desolvation, and formation/cleavage of chemical bonds, take place at electrolyte/electrode interfaces during electrocatalytic reactions. Those processes have been understood on the basis of changes in the surface composition, atomic arrangement, and molecular and electronic structures of the interfaces by using various in situ analysis techniques. To date, in situ analysis and observation of those interfacial processes at an ideal single-crystal surface are indispensable not only for fundamental understanding of the reaction mechanism but also for rational design of the highly efficient and durable electrocatalytic materials. Here, historical and recent progress of in situ studies on electrocatalytic reactions is briefly reviewed with a focus on two major techniques, X-ray absorption fine structure and surface X-ray scattering.  相似文献   
65.
《Comptes Rendus Physique》2019,20(6):583-592
During the growth of a single-crystal diamond by MPCVD, polycrystalline diamonds are prone to grow in the edge regions. This substantially reduces the usable area of the grown diamond film. In addition, the inhomogeneous distribution of internal stress causes diamond to crack during continuous growth. In recent years, a series of experimental studies have been carried out to solve these problems and some achievements have been obtained. However, in order to understand fundamentally the growth mechanism of diamond, the relationship between growth quality and various influencing factors still needs to be quantitatively studied through integrated simulations and experiments. Electron number density and substrate temperature are important factors affecting diamond crystallization quality. In this paper, the growth conditions of the diamond were simulated and analyzed. Simulation results were compared with the experimental results. This evidences that the surface temperature distribution is relatively homogeneous, and that the significant electron number density gradient in the axial direction is the main reason for the formation of polycrystals in the edge regions. Therefore, substrate holders with different cavity depths were designed and the substrates grew in the same temperature range. The surface morphologies, crystalline qualities, and internal stress distributions of the grown diamonds were measured, and it was found that the quality of growth increased first and then decreased with the depth of the cavity, while the growth rate decreased with increasing the latter. These results are in good agreement with the simulation results. Finally, suggestions on the selection of the substrate holder for film growth with different thicknesses are proposed.  相似文献   
66.
In this study, single-crystal γ-MnO2 nanowires have been successfully synthesized at room temperature in the absence of catalysts or templates, the diameter was found to be ca. 10–20 nm and the characteristic lengths up to several micrometers. The crystal phase of nanowires was confirmed by XRD and TEM measurements. Further, a dissolution– condensation–recrystallization process was proposed for the formation of nanowires under the room temperature condition.  相似文献   
67.
68.
The solid solutions of barium containing Type I clathrate, Ba8−δSi46−xGex (0?x?23) were prepared under high-pressure and high-temperature conditions of 3 GPa at 800°C. All the solid solutions showed superconductivity, and the transition temperature (Tc) decreased from 8.0 to 2.0 K as the germanium content increased from x=0 to 23 in Ba8−δSi46−xGex. The single crystals with five different compositions were obtained and the structures, compositions, and site occupancies were determined from X-ray single-crystal analysis. A slight barium deficiency was observed at Ba1 (2a) sites for all the clathrates. The Ge atoms replaced the Si atoms at the Si3 (24k) site in the composition range of x<8, and then at the Si2 (16i) site. The crystals had a slight deficiency in the covalent (Si, Ge) network and the deficiency increased with the increase of the Ge content.  相似文献   
69.
A lattice-gas model is described for the adsorption of halides on single-crystal electrodes. The lateral interactions between the adsorbed halides include a short-range nearest-neighbor interaction and a long-range electrostatic interaction. By Monte Carlo simulations the model is used to fit the experimental isotherm of bromide adsorption on Ag(100), giving information about the relative importance of the long-range and short-range interactions. The model reproduces the order–disorder transition observed experimentally, and the way in which the long-ranged interactions influence the properties of this phase transition is discussed. The Monte Carlo simulations are also compared to analytical mean-field and quasi-chemical approximations to the isotherm. Finally, the kinetics of the disorder–order transition are studied by dynamic Monte Carlo simulations, and some results on isotherms and ordered phases on (110) and (111) surfaces are described.  相似文献   
70.
Single crystals of Li0.68CoO2, Li0.48CoO2, and Li0.35CoO2 were successfully synthesized for the first time by means of electrochemical and chemical delithiation processes using LiCoO2 single crystals as a parent compound. A single-crystal X-ray diffraction study confirmed the trigonal R3¯m space group and the hexagonal lattice parameters a=2.8107(5) Å, c=14.2235(6) Å, and c/a=5.060 for Li0.68CoO2; a=2.8090(15) Å, c=14.3890(17) Å, and c/a=5.122 for Li0.48CoO2; and a=2.8070(12) Å, c=14.4359(14) Å, and c/a=5.143 for Li0.35CoO2. The crystal structures were refined to the conventional values R=1.99% and wR=1.88% for Li0.68CoO2; R=2.40% and wR=2.58% for Li0.48CoO2; and R=2.63% and wR=2.56% for Li0.35CoO2. The oxygen-oxygen contact distance in the CoO6 octahedron was determined to be shortened by the delithiation from 2.6180(9) Å in LiCoO2 to 2.5385(15) Å in Li0.35CoO2. The electron density distributions of these LixCoO2 crystals were analyzed by the maximum entropy method (MEM) using the present single-crystal X-ray diffraction data at 300 K. From the results of the single-crystal MEM, strong covalent bonding was clearly visible between the Co and O atoms, while no bonding was found around the Li atoms in these compounds. The gradual decrease in the electron density at the Li site upon delithiation could be precisely analyzed.  相似文献   