排序方式: 共有2条查询结果,搜索用时 0 毫秒
1
1.
To meet the processing requirements of resin transfer moulding(RTM)technology,reactive diluent containing m-phenylene moiety was synthesized to physically mixed with phenylethynyl terminated cooligoimides with well-designed molecular weights of 1500-2500 g/mol derived from 4,4’-(hexafluoroisopropylidene)diphthalic anhydride(6 FDA),3,4’-oxydianiline(3,4’-ODA)and m-phenylenediamine(m-PDA).This blend shows low minimum melting viscosity(<1 Pa·s)and enlarged processing temperature window(260–361℃).FPI-R-1 stays below 1 Pa·s for2 h at 270℃.The relationship between the molecular weight of the blend and its melting stability was first explored.Blending oligoimides with lower molecular weights exhibit better melting stability.Upon curing at 380℃for 2 h,the thermosetting polyimide resin demonstrates superior heat resistance(Tg=420-426℃). 相似文献
2.
1