An investigation was made into the effect of doping with the elemental crystal Ge or/and GeO2 on the TiO2-V2O5-Y2O3 varistor ceramics. The result shows that as the doping contents of V2O5 and Y2O3 are 0.5 mol%, respectively, co-doping with 0.3 mol% Ge and 0.9 mol% GeO2 makes the highest α value (α = 12.8), the lowest breakdown voltage V1mA (V1mA = 15.8 V/mm) and the highest grain boundary barrier ΦB (ΦB = 1.48 eV), which is remarkably superior to the TiO2-V2O5-Y2O3 varistor ceramics undoped with Ge and GeO2 and mono-doped with Ge or GeO2. The TiO2-V2O5-Y2O3-Ge-GeO2 ceramic has the prospect of becoming a novel varistor ceramic with excellent electrical properties. 相似文献
2.
3.
影响金刚石合成的粉末触媒形态因素 总被引:2,自引:0,他引:2
采用相同成分体系的片状、球状Ni-Mn-Cu粉末触媒体为原料,在六面顶压机上进行人造金刚石高温、超高压合成的对比实验.结果表明:具有片状等不规则形状的NiMnCu粉末触媒合成工艺较球状同类粉末触媒合成工艺更稳定、易于掌握.针对上述结果,结合金刚石成核、生长过程中合成腔体内温度变化对上述实验结果进行了讨论. 相似文献
4.
5.
选用Ni-Mn-C粉末触媒,在国产DS6×800A型铰链式六面顶压机上实现了高石墨转化率的金刚石合成,其石墨转化率可达90%以上。高石墨转化率金刚石的合成,不仅有助于提高金刚石的效率,而且还可以减化提纯后处理工序。 相似文献