In this paper, the dynamic propagation problem of a mixed-mode crack was studied by means of the experimental method of caustics. The initial curve and caustic equations were derived under the mixed-mode dynamic condition. A multi-point measurement method for determining the dynamic stress intensity factors,K I d , andK II d , and the position of the crack tip was developed. Several other methods were adopted to check this method, and showed that it has a good precision. Finally, the dynamic propagating process of a mixed-mode crack in the three-point bending beam specimen was investigated with our method.  相似文献   

2.
Experimental results suggest that the interfacial fracture resistance is minimal for approximate near tip Mode I accompanied by positive and negative near tip Mode II. Finite-strain FE analysis is made for an elastic–plastic medium bonded to an ideally elastic medium with an interface crack. Small-scale plasticity conditions are invoked and examined in relation to the elastic–plastic stress distribution along the bond line. Plasticity engenders a tendency to turn near tip biaxiality towards pure Mode I regardless of the mixed-mode loading. High levels of hydrostatic stress are attained. For different mode mixities of the applied load, the dependence of the elastic–plastic normal bond stress on load level is examined. It is found that under positive Mode II loading, the normal bond stress σyy tends to saturate as the load level rises. This does not occur for Mode I and negative Mode II loading. In addition, deformation patterns inside the plastic zone are examined for mixed-mode situations. A displacement criterion based on the normal bond crack opening suggests a dependence of the critical load level on the extent of mixed mode. Under positive mode II fracture, traces of the ductile material are found at the top of the elastic substrate. Some of these conclusions appear to be consistent with the fracture patterns observed for LD-polyethylene/glass interfacial mixed-mode fracture.  相似文献   

3.
The mixed-mode, elastodynamic state of stress in the neighborhood of a constant-velocity crack tip is used to generate numerically unsymmetric isochromatics. Unsymmetry associated with the third-order terms of a mixed-mode stress field, with and without the Mode II singular stress term, is also investigated. In extractingK I from an unsymmetric isochromatic pattern, errors in the Mode I fracture parameters due to the assumed presence ofK II in aK I stress field were found to be significant when data are taken more than 4 mm from the crack tip. Paper was presented at V International Congress on Experimental Mechanics held in Montreal, Quebec, Canada on June 10–15, 1984.  相似文献   

4.
The present paper discusses the results of an investigation into the effects of test rate and the mode of loading on the fracture energy, Gc, of adhesively-bonded fibre-composite joints. Various carbon-fibre reinforced-polymer (CFRP) matrix composite substrates have been bonded using two different types of automotive structural epoxy-adhesives. They have been tested via loading the bonded joints in mode I (tensile), mode II (in-plane shear) and mixed-mode I/II from slow rates (i.e., of about 10?5 m/s) up to relatively high rates of test of about 15 m/s. The high-rate tests were photographed using a high-speed digital video camera to record the deformation of the joint and the fracture behaviour. An analysis strategy has been developed for the various modes of loading (i) to account for the observed fracture behaviour, (ii) to circumvent the problems posed by oscillations in the load traces due to the presence of dynamic effects in the faster tests, and (iii) to account for the kinetic energy associated with the moving specimen arms in the faster tests. Based on the analysis strategy developed, the effect of the test rate on the fracture energy, Gc, for the different loading modes for the joints has been ascertained. Furthermore, various different fracture paths were observed in the tests. They were either cohesive, in the adhesive layer, or interlaminar in the composite substrates. The exact fracture path observed was a function of (i) the type of composite substrate, (ii) the type of adhesive, and (iii) the mode of loading employed. However, the nature of the fracture path was found to be quite insensitive to the test rate. Essentially, it was found that joints subjected to mixed-mode I/II loading were more likely to exhibit an interlaminar fracture path in the composite substrates than when loaded in either pure modes I or II. The propensity for a given joint to exhibit such a fracture path via delamination of the composite substrate has been explained by calculating the transverse tensile stresses induced in the loaded composite arms, and comparing this value to the measured transverse tensile strength of the composite. Following this approach, the underlying reasons for the observed fracture path were identified and could be predicted. Also, the proposed scheme provides a route to design against delamination failure occurring in adhesively-bonded fibre-composite test specimens.  相似文献   

5.
For a crack subjected to combined mode I and III loading the influence of a T-stress is analyzed, with focus on crack growth. The solid is a ductile metal modelled as elastic–plastic, and the fracture process is represented in terms of a cohesive zone model. The analyzes are carried out for conditions of small scale yielding, with the elastic solution applied as boundary conditions on the outer edge of the region analyzed. For several combinations of the stress intensity factors KI and KIII and the T-stress crack growth resistance curves are calculated numerically in order to determine the fracture toughness. In all situations it is found that a negative T-stress adds to the fracture toughness, whereas a positive T-stress has rather little effect. For given values of KI and T the minimum fracture toughness corresponds to KIII = 0.  相似文献   

6.
The direct identification of the cohesive law in pure mode I of Pinus pinaster is addressed in this work. The approach couples the double cantilever beam (DCB) test with digital image correlation (DIC). Wooden beam specimens loaded in the radial-longitudinal (RL) fracture propagation system are used. The strain energy release rate in mode I (G I) is uniquely determined from the load–displacement curve by means of the compliance-based beam method (CBBM). This method relies on the concept of equivalent elastic crack length (a eq) and therefore does not require the monitoring of crack propagation during test. DIC measurements are processed with two different purposes. Firstly, the physical evidence of a eq is discussed with regard to actual estimation of the crack length based on post-processing full-field displacement measurements. Secondly, the crack tip opening displacement in mode I (w I) is determined from the displacements near the initial crack tip. The cohesive law in mode I (σ I???w I) is then identified by numerical differentiation of the G I???w I relationship. The methodology and accuracy on this reconstruction are addressed. Moreover, the proposed procedure is validated by finite element analyses including cohesive zone modelling. It is concluded that the proposed data reduction scheme is adequate for assessing the cohesive law in pure mode I of P. pinaster.  相似文献   

7.
The propensity of the transition of fracture type in either brittle or ductile cracked solid under mixed-mode I and III loading conditions is investigated. A fracture criterion based on the competition of the maximum normal stress and maximum shear stress is utilized. The prediction of the fracture type is determined by comparing τmax/σmax at a critical distance from the crack tip to the material strength ratio τC/σC, i.e., (τmax/σmax)<(τC/σC) for tensile fracture and (τmax/σmax)>(τC/σC) for shear fracture, where σC (τC) is the fracture strength of materials in tension (shear). Mixed mode I/III fracture tests were performed using circumferentially notched cylindrical bars made of PMMA and 7050 aluminum alloy. Fracture surface morphology of the specimens reveals that: (1) for the brittle material, PMMA, only tensile type of fracture occurs, and (2) for the ductile material, 7050 aluminum alloy, either tensile or shear type of fracture occurs depending on the mode mixity. The transition (in ductile material) or non-transition (in brittle material) of the fracture type and the fracture path observed in experiments were properly predicted by the theory. Additional test data from open literature are also included to validate the proposed theory.  相似文献   

8.
The maximum energy release rate criterion, i.e., G max criterion, is commonly used for crack propagation analysis. This fracture criterion is based on the elastic macroscopic strength of materials. In the present investigation, however, the G max criterion has been modified in order to accommodate the consideration of plastic strain energy. This modified criterion is extended to study the fatigue crack growth characteristics of mixed-mode cracks. To predict crack propagation due to fatigue loads, a new elasto–plastic energy model is presented. This new model includes the effects of material properties such as strain hardening exponent n, yield strength σ y , and fracture toughness and stress intensity factor ranges. The results obtained are compared with those obtained using the commonly employed crack growth law and the experimental data.  相似文献   

9.
The constraint of a thin silver interlayer is used to create high triaxial stresses to evaluate the applicability of theoretical models for ductile fracture. Rice and Tracey's model for cavity expansion under high triaxial states of stress and Huanget al.'s model for cavity instability were considered. The experimentally determined m / y values suggest that further investigation of the Huanget al. theory is warranted. Microstructural analysis revealed that multiple cavities were initially present in the silver interlayers, and the number and size of the cavities increased as failure was approached. Finite element analysis and experimental results showed excellent agreement in a computational determination of cavity instability. Thus, it appears that ductile fracture in constrained thin interlayers can be explained with unstable cavity growth.  相似文献   

10.
Interfacial fracture of adhesive bonds undergoing large-scale yielding is studied using a combined experimental/finite-element approach. The full range of in-plane mode mixity is produced over bond thickness ranging from 30 to 500 μm using the scarf and the ENF joint geometries. Novel techniques for introducing pre-cracks and surface decoration, together with in situ observations, facilitate accurate determination of the bond-average and the local shear strains at the crack tip during the onset as well as the rest of the crack propagation event. The crack generally grew along one of the two interfaces of the bond, although the failure was always fully cohesive. The local shear strain at the crack tip is independent of the bond thickness, and, under quasi-static conditions, it remains constant throughout the growth, which make it a viable fracture parameter. This quantity strongly depends on the mode mixity, the sign of the phase angle (i.e., shearing direction) and the crack speed, however.A finite-element analysis is used to obtain the crack tip deformation field for an interface crack in adhesively bonded scarf and ENF joints. Large-strain and quasi-static conditions are assumed. A distinct material model in the fracture process zone that allows for volume change in the post-yield regime is incorporated into the analysis. The local deformation is characterized by a pair of bond-normal and tangential displacements corresponding to the nodal points adjacent to the crack tip. The critical values of these quantities are obtained when the FEM bond-average shear strain at the crack tip becomes equal to its experimental counterpart. The so defined critical local displacements, after an appropriate normalization, seem to conform to a single-valued, linear type interrelationship over the entire range of mode mixity. The fact that this relationship is independent of the bond thickness, and furthermore it encompasses both cases of positive and negative phase angles, makes it a viable candidate for characterizing mixed-mode interfacial fracture under large-deformation conditions.  相似文献   

11.
A new data reduction scheme is proposed for measuring the critical fracture energy of adhesive joints under pure mode II loading using the End Notched Flexure test. The method is based on the crack equivalent concept and does not require crack length monitoring during propagation, which is very difficult to perform accurately in these tests. The proposed methodology also accounts for the energy dissipated at the Fracture Process Zone which is not negligible when ductile adhesives are used. Experimental tests and numerical analyses using a trapezoidal cohesive mixed-mode damage model demonstrated the good performance of the new method, namely when compared to classical data reduction schemes. An inverse method was used to determine the cohesive properties, fitting the numerical and experimental load–displacement curves. Excellent agreement between the numerical and experimental R-curves was achieved demonstrating the effectiveness of the proposed method.  相似文献   

12.
A FEM analysis for studying mixed-mode fracture problem of chopped strand mat glass fibre reinforced polyester laminate is presented. The analysis is formulated on the basis of 8-node quadrilateral isoparametric element. The collapsed triangular quarter-point singular elements were used for calculating stress intensity factors KΙ and K.The crack propagation process was computed by implementing constraint release technique. Three different approaches to the solution of stress intensity factors KΙ and K were compared. The effect of constraint condition imposed upon the displacement of the three collapsed nodes of the crack tip elements on the KΙ and K results was evaluated. The mixed-mode critical stress intensity factors KΙC and KⅡC were estimated for CSM-GRP through the consideration of KΙ and K calculated and the measured failure load and critical crack length in the experiment.  相似文献   

13.
Quantifying high temperature damage is an issue that can hardly be dealt with experimentally because of the complexity of the loading control, of temperature and of moisture. The experimental investigation was carried out. The measurement of the mechanical characteristics (fracture energy, tensile strength, elastic modulus and thermal damage parameter) of five cementitious materials, cement paste, mortar, ordinary concrete and two HPC concretes were performed by three-point bending tests after heating/cooling cycles at 120, 250 and 400 °C. The tests showed that the cementitious materials behave almost identical when the fracture energy Gf is considered as a function of maximum temperature. The thermal damage due to heating from 120 to 400 °C increases the fracture energy by 50% with the reference tests at room temperature. A more tortuous crack surface is one reasonable explanation for the significant increase in Gf. It is demonstrated that the temperature exposure makes all cementitious materials tested significantly more ductile and less resistant.  相似文献   

14.
15.
The paper presents an improved formulation of mixed-mode fracture criteria. Both the fracture toughness KIC and KIIC are taken into account. Consequently, the crack propagation direction and the fracture envelope in the and plane depends on the toughness ratio . In the plane only one envelope for each criterion is obtained.  相似文献   

16.
A novel experimental technique is presented that combines the optical method of caustics and the full-field lateral shearing interferometer of coherent gradient sensing (CGS) in one setup. Collimated light transmitted through a deformed specimen is separated into two legs. One is processed by the lateral shearing interferometer and is recombined with the other on a single image plane. By adjusting the optical path length of each leg, a combination lateral shearing interferogram/caustic image is generated. When this technique is applied to a fracture specimen, information about the stress intensity factor can be obtained from the caustic and the CGS interference fringes for exactly the same deformation field. This allows for a direct comparison between the two methods when investigating phenomena such asK-dominance, three-dimensional deformation and so on. In this paper, the technique is presented in detail, and its feasibility is tested by application to mode I and mixed-mode crack tip deformation fields.  相似文献   

17.
A methodology for determining the cohesive fracture parameters associated with pull-out of spot welds is presented. Since failure of a spot weld by pull-out occurs by mixed-mode fracture of the base metal, the cohesive parameters for ductile fracture of an aluminum alloy were determined and then used to predict the failure of two very different spot-welded geometries. The fracture parameters (characteristic strength and toughness) associated with the shear and normal modes of ductile fracture in thin aluminum alloy coupons were determined by comparing experimental observations to numerical simulations in which a cohesive-fracture zone was embedded within a continuum representation of the sheet metal. These parameters were then used to predict the load–displacement curves for ultrasonically spot-welded joints in T-peel and lap-shear configurations. The predictions were in excellent agreement with the experimental data. The results of the present work indicate that cohesive-zone models may be very useful for design purposes, since both the strength and the energy absorbed by plastic deformation during weld pull-out can be predicted quite accurately.  相似文献   

18.
Fatigue crack growth studies in rail steels and associated weld metal have shown that (a) deformed rail steel exhibited fatigue crack growth rates that are slightly faster than undeformed rail steel and (b) weld metal growth data are appreciably faster than rail steel growth results and exhibit growth rate plateaux that reside above the upper bound reported for rail steel fatigue crack growth.In rail steel microstructures at low ΔK levels fatigue crack extension occurred by a ductile striated growth mechanism. However at Kmax values approaching 40 MPa √m transgranular cleavage facets initially formed and their incidence increased with Kmax until final fast fracture. The average cleavage facet size agreed well with pearlite nodule dimensions of 60–100 μm.The weld metal microstructure was much coarser than the rail steel and contained highly directional columnar grain growth. At all ΔK levels the dominant fracture mode was transgranular cleavage containing small isolated regions of ductile striated fatigue crack growth. The cleavage facet size varied from 150 to 600 μm; such a large variation was explained by the fact that in general crack extension tended to occur in association with the proeutectoid ferrite phase.  相似文献   

19.
In this paper, we proposed a new cr tenon or mixea-moae brittle fracture, i.e., the strain energy criterion, which can be stated as (K/KⅠc)2 +(K/KⅠc)2+(K/KⅡc)2=1. This criterion is shown to be in good agreement with known experimental data.In this paper, an experimental criterion:(K/KⅠc)m+(K/KⅡc)n=1, 1≤nm≤2.is also proposed.  相似文献   

20.
The effect of constraint on brittle fracture of solids under predominantly elastic deformation and mode I loading conditions is studied. Using different cracked specimen geometry, the variation of constraint is achieved in this work. Fracture tests of polymethyl methacrylate were performed using single edge notch, compact tension and double cantilever beam specimens to cover a bread range of constraint. The test data demonstrate that the apparent fracture toughness of the material varies with the specimen geometry or the constraint level. Theory is developed using the critical stress (strain) as the fracture criterion to show that this variation can be interpreted using the critical stress intensity factorK Cand a second parameterT orA 3,whereT andA 3are the amplitudes of the second and the third term in the Williams series solution, respectively. The implication of this constraint effect to the ASTM fracture toughness value, crack tip opening displacement fracture criterion and energy release rateG Cis discussed. Using the same critical stress (strain) as the fracture criterion, the theory further predicts crack curving or instability under mode I loading conditions. Experimental data are presented and compared with the theory.  相似文献   