1.
The variation of the axial and radial components of the residual stresses in fiber-reinforced polyethylene with distance from the fiber has been investigated. It is shown that, irrespective of the agent employed, coupling leads to an increase in stresses. The values obtained for the residual stresses are compared with the adhesion strength determined by the shearing method. The effect of a structure-forming agent on the residual stresses is investigated.Mendeleev Moscow Chemical Engineering Institute. Translated from Mekhanika Polimerov, No. 4, pp. 722–724, July–August, 1971.  相似文献   

2.
In real composite materials an additional phase may exist between the fiber and the matrix. This phase, commonly known as the interphase, is a local region that results from the matrix bonds with the fiber surface or the fiber sizing. The differing thermal expansions or contractions of the fiber and matrix cause thermally induced stresses in composite materials. In the present study, a four-cylinder model is proposed for the determination of residual thermal stresses in unidirectional composite materials. The elastic modulus of the interphase is a function of the interphase radius and thickness. The governing equations in terms of displacements are solved in the form of expansion into a series [1]. The effective elastic characteristics are obtained using the finite element approach. The effect of the interphase thickness and different distributions of the interphase Young's modulus on the thermal residual stress field in unidirectional composite materials is investigated.For Pt. 1, see [1].Published in Mekhanika Kompozitnykh Materialov, Vol. 33, No. 2, pp. 200–214, March–April, 1997.  相似文献   

3.
Conclusions The residual thermal stresses in the constituents of a fiber-reinforced epoxy have been predicted using a concentric three-cylindrical (fiber-interphase-matrix) assemblage analysis. The interphase has been treated as a region with a variable Young's modulus — a direct consequence of the changes in the microstructure of the matrix near the fiber surface. The Navier equations of elasticity have been solved in series form solutions for each type of property variation.A parametric study is used to demonstrate the fact that changes in the interphase properties can drastically affect the residual stresses in the interphase.Published in Mekhanika Kompozitnykh Materialov, Vol. 30, No. 5, pp. 579–589, September–October, 1994.  相似文献   

4.
The effect of the chemical and thermal shrinkage of the epoxy matrix on the structural residual stresses in plastics reinforced with anisotropic fibers has been investigated. The process of residual stress formation in all stages of a given curing regime is examined with reference to a regular triangular fiber distribution. The model of a hardening hypoviscoelastic medium [8] is used to describe the variation of the rheological properties of the matrix. The effect of the cooling rate on the residual stresses is investigated with reference to a single inclusion.Moscow Power Engineering Institute. Translated from Mekhanika Polimerov, No. 3, pp. 409–415, May–June, 1976.  相似文献   

5.
The effect of the parameters of heat treatment and programmed winding under tension on the residual stresses in thin-walled coiled parts made from glass plastic by the "dry" winding of a heated glass strip on an unheated mandrel is studied experimentally. The effect of the thickness of the parts on the maximum radial residual stresses is considered. A method is proposed for regulating the residual stresses in parts with very thick walls.Translated from Mekhanika Polimerov, No. 1, pp. 75–80, January–February, 1972.  相似文献   

6.
The determination of the residual stresses in glass-reinforced plastics elements is considered. It is shown that these stresses reach appreciable values and should be taken into account in strength calculations. Quantitative data are supplied for a series of materials. At normal operating temperatures the residual stresses are stable.Moscow Aviation Technological Institute. Translated from Mekhanika Polimerov, No. 6, pp. 1117–1119, November–December, 1969.  相似文献   

7.
The results of an experimental investigation of the residual stresses in wound glass-reinforced plastic rings are presented. The residual stresses were determined by the Davidenkov method. The dependence of the maximum tensile and compressive circumferential stresses on ring thickness and polymerization temperature is investigated. The experimental data are compared with the results of calculations based on the theory proposed in [1, 2].Moscow Power Engineering Institute. Translated from Mekhanika Polimerov, No. 6, pp. 1116–1119, November–December, 1970.  相似文献   

8.
The results of a photoelastic investigation of the distributions of shrinkage and temperature residual stresses in glued joints and coatings are compared. The degree of nonuniformity of the residual stress distribution over the length and thickness is determined as a function of the scale factor. It is shown that the bulk of the residual stresses in metal joints glued with K-115 epoxy adhesive are temperature stresses, which may reach 130 kgf/cm2. The shrinkage and temperature residual stress distributions are similar in character.Kucherenko Central Scientific-Research Institute of Building Structures. Translated from Mekhanika Polimerov, No. 4, pp. 738–742, July–August, 1971.  相似文献   

9.
The effect of crystalline structure on the internal stresses in polyethylene coatings has been studied. An equation for the internal stresses in crystallizing polymer coatings has been derived. The important role of orientation processes is demonstrated.Leningrad Lensovet Technological Institute. Translated from Mekhanika Polimerov, Vol. 4, No. 6, pp. 992–996, November–December, 1968.  相似文献   

10.
The temperature stresses in polyethylene composites with fibrous fillers have been estimated. It is shown that they do not represent a threat to the adhesion bond or the cohesion strength of the components of the systems investigated. Model experiments have revealed the presence of an adhesion interaction between the filler and the matrix in the composite itself and have made it possible to estimate the actual threat posed by the temperature stresses. The mechanism of action of the filler particles on the thermal expansion of the composite is explained.Institute of Polymer Mechanics, Academy of Sciences of the Latvian SSR, Riga. Translated from Mekhanika Polimerov, No. 6, pp. 1049–1056, November–December, 1970.  相似文献   

11.
A previously proposed method is used to obtain expressions for calculating the residual stresses as a function of the physicomechanical properties of the polymer matrix and the reinforcement ratio. The calculation results are presented and the corresponding state of stress and strain analyzed. There are considerable deviations (in the magnitude and distribution of the stresses) from models that neglect or only take partly into account the interaction of the fibers.Moscow Ordzhonikidze Aviation Institute. Translated from Mekhanika Polimerov, Vol. 4, No. 6, pp. 1051–1058, November–December, 1968.  相似文献   

12.
Research on the effect of technological factors on the strength of reinforced-plastics structures is reviewed. Attention is concentrated on structures in the form of bodies of revolution fabricated by the winding technique. The influence of the winding parameters and the curing regime on the residual stresses is discussed. Data on the variation of the mechanical properties of the resin in the course of the curing process are examined. The contributions of chemical and thermal shrinkage to residual stress formation are compared. Methods of reducing the residual stresses are considered.Presented at the 2nd All-Union Conference on Polymer Mechanics, Riga, November 10–12, 1971.Moscow Power Engineering Institute. Translated from Mekhanika Polimerov, No. 3, pp. 529–540, May–June, 1972.  相似文献   

13.
The kinetics of the temperature residual stresses and strains in thick-walled reinforced-plastic cylinders and rings have been experimentally investigated employing a special procedure for continuously monitoring the internal strains and stresses in the various zones of the semifinished product during the heat treatment stage. The effect of the resin polymerization (polycondensation) temperature and the mandrel material on the magnitude and distribution of the temperature stresses is considered. The total residual stresses have been determined by a nondestructive strain-gauge method with differentiation of the components.Translated from Mekhanika Polimerov, No. 6, pp. 1040–1046, November–December, 1971.  相似文献   

14.
The effect of structural residual stresses on the strength of a glass-reinforced plastic loaded along and across the fibers is investigated. It is established that the residual stresses lead to an increase in the strength of the glass-reinforced plastic across the fibers and to cracking of the polymer matrix in tension along the fibers, but have practically no effect on the combined deformation of the matrix and the fibers in compression.Moscow Ordzhonikidze Aviation Institute. Translated from Mekhanika Polimerov, No. 3, pp. 475–480, May–June, 1969.  相似文献   

15.
A method is proposed for determining the residual stresses and strains in wound glass-reinforced plastic products. The fabrication process is divided into five stages: winding, heating polymerization, cooling, and removal from the mandrel. The initial stresses that develop during winding and the subsequent stress increment associated with heating are taken into account. Polymerization is treated as a process during which the mechanical and thermophysical properties of the material change. Chemical shrinkage of the resin and its filtration through the fiberglass are disregarded. Equations are derived for the residual radial and peripheral stresses in the finished product, for the residual change in inside diameter, and for the temperature at which the product is released from the mandrel during the cooling process. The experimental data relating to two types of wound products are discussed. The results of a computation of the residual stresses and the residual changes in inside diameter are compared with the experimental data.Moscow Power Engineering Institute. Translated from Mekhanika Polimerov, Vol. 5, No. 1, pp. 134–139, January–February, 1969.  相似文献   

16.
The thermoelastic residual stresses in anisotropic rings and cylinders with characteristics that vary over the thickness are determined. The calculation of the stresses in wound glass-reinforced plastic parts is illustrated by examples.Institute of Polymer Mechanics, Academy of Sciences of the Latvian SSR, Riga, Moscow Power Engineering Institute. Translated from Mekhanika Polimerov, No. 4, pp. 686–691, July–August, 1971.  相似文献   

17.
The stresses on the interatomic bonds in the interior and at the surface of polyethylene terephthalate film in uniaxial tension have been determined by means of infrared transmission and reflection spectroscopy. The stresses are found using the shift in the frequency of the atomic vibrations produced by the application of a mechanical load. It is shown that the stresses on some bonds in the specimen reach 700 kgf/mm2, i.e., approach their theoretical strength. The concentration of these bonds in a surface layer 1 µ thick is approximately an order greater than the concentration in the interior of the specimen.A. F. Ioffe Physicotechnical Institute, Academy of Sciences of the USSR, Leningrad. Translated from Mekhanika Polimerov, No. 3, pp. 512–514, May–June, 1976.  相似文献   

18.
A technique for calculating the residual stresses in wound components made out of mixed carbon-fiber-and glass-fiber-reinforced plastics and the results of the calculations are presented. The effect of the conditions under which the components are wound on the magnitude and nature of the residual stresses distribution in components made out of combined composites is investigated. The results of the calculations are compared with the experimental values.Translated from Mekhanika Polimerov, No. 6, pp. 996–1004, November–December, 1975.  相似文献   

19.
The residual stresses in thin-wall plastic rings reinforced with glass and prepared by the method of consolidating the layers in combination with various winding regimes have been studied experimentally. It is shown that variation of the winding regime from one layer to another can change the distribution of the stresses through the thickness of the ring.Moscow Energy Institute. Translated from Mekhanika Polimerov, No. 1, pp. 174–176, January–February, 1972.  相似文献   

20.
The results from experimental and theoretical investigation of the creep of polyethylene terephthalate film during stepwise varying stresses under conditions of uniaxial extension are given.Izhevsk Mechanical Institute. Translated from Mekhanika Polimerov, No. 5, pp. 929–933, September–October, 1972.  相似文献   