This contribution describes the homopolymerization of styrene and the copolymerization of ethylene and styrenic comonomers mediated by the single-site bimetallic "constrained geometry catalysts" (CGCs), (mu-CH2CH2-3,3'){(eta(5)-indenyl)[1-Me2Si(tBuN)](TiMe2)}2 [EBICGC(TiMe2)2; Ti2], (mu-CH2CH2-3,3'){(eta(5)-indenyl)[1-Me2Si(tBuN)](ZrMe2)}2 [EBICGC(ZrMe2)2; Zr2], (mu-CH2-3,3'){(eta(5)-indenyl)[1-Me2Si(tBuN)](TiMe2)}2 [MBICGC(TiMe2)2; C1-Ti2], and (mu-CH2-3,3'){(eta(5)-indenyl)[1-Me2Si(tBuN)](ZrMe2)}2 [MBICGC(ZrMe2)2; C1-Zr2], in combination with the borate activator/cocatalyst Ph3C+ B(C6F5)4- (B1). Under identical styrene homopolymerization conditions, C1-Ti2 + B1 and Ti2 + B1 exhibit approximately 65 and approximately 35 times greater polymerization activities, respectively, than does monometallic [1-Me2Si(3-ethylindenyl)(tBuN)]TiMe2 (Ti1) + B1. C1-Zr2 + B1 and Zr2 + B1 exhibit approximately 8 and approximately 4 times greater polymerization activities, respectively, than does the monometallic control [1-Me2Si(3-ethylindenyl)(tBuN)]ZrMe2 (Zr1) + B1. NMR analyses show that the bimetallic catalysts suppress the regiochemical insertion selectivity exhibited by the monometallic analogues. In ethylene copolymerization, Ti2 + B1 enchains 15.4% more styrene (B), 28.9% more 4-methylstyrene (C), 45.4% more 4-fluorostyrene (D), 41.2% more 4-chlorostyrene (E), and 31.0% more 4-bromostyrene (F) than does Ti1 + B1. This observed bimetallic chemoselectivity effect follows the same general trend as the pi-electron density on the styrenic ipso carbon (D > E > F > C > B). Kinetic studies reveal that both Ti2 + B1 and Ti1 + B1-mediated ethylene-styrene copolymerizations follow second-order Markovian statistics and tend to be alternating. Moreover, calculated reactivity ratios indicate that Ti2 + B1 favors styrene insertion more than does Ti1 + B1. All the organozirconium complexes (C1-Zr2, Zr2, and Zr1) are found to be incompetent for ethylene-styrene copolymerization, yielding only mixtures of polyethylene and polystyrene. Model compound (mu-CH2CH2-3,3'){(eta(5)-indenyl)[1-Me2Si(tBuN)][Ti(CH2Ph)2]}2 {EBICGC[Ti(CH2Ph)2]2; Ti2(CH2Ph)4} was designed, synthesized, and structurally characterized. In situ activation studies with cocatalyst B(C6F5)3 suggest an eta(1)-coordination mode for the benzyl groups, thus supporting the proposed polymerization mechanism. For ethylene-styrene copolymerization, polar solvents are found to increase copolymerization activities and coproduce atactic polystyrene impurities in addition to ethylene-co-styrene, without diminishing the comonomer incorporation selectivity. Both homopolymerization and copolymerization results argue that substantial cooperative effects between catalytic sites are operative.  相似文献   

2.
This communication reports the styrene homopolymerization behavior and ethylene-styrene copolymerization behavior of the covalently linked bimetallic constrained geometry catalyst (mu-CH2CH2-3,3'){(eta5-indenyl)[1-Me2Si(tBuN)](TiMe2)}2 (Ti2), which is the first single-site catalyst that effects not only styrene homopolymerization with high activity, but also efficient ethylene-styrene copolymerization over a broad styrene composition range (0-76% at 20 degrees C, 1.0 atm ethylene pressure). In styrene homopolymerization, a 50x increase in polymerization activity is achieved with Ti2 vs the mononuclear analogue, Ti1, using an identical trityl borate cocatalyst and polymerization conditions. In ethylene + styrene copolymerization, Ti2 enchains approximately 20% more styrene than Ti1 under identical reaction conditions. 13C NMR spectroscopy indicates that greater than two consecutive styrene units are enchained in the copolymer backbone produced by Ti2 + Ph3C+B(C6F5)4-. End group analysis of the styrene homopolymer produced by Ti2 + Ph3C+B(C6F5)4- suggests that 1,2-regiochemistry is installed in approximately 50% of the initiation steps. This unusual microstructure is believed to be related to the bimetallic catalyst structure.  相似文献   

3.
This Communication describes the implementation of a new binuclear homometallic organotitanium "constrained geometry catalyst" (CGC), (mu-CH2CH2-3,3'){ (eta5-indenyl )[1-Me2Si (tBuN)](TiMe2)}2[EBICGC(TiMe2)2; Ti2], together with the bifunctional activators (Ph3C+)2[1,4-(C6F5)3BC6F4B(C6F5)3]2- (B2) and new bisborane 1,4-(C6F5)2BC6F4B(C6F5)2 (BN2) in ethylene + alpha-olefin copolymerization processes. Specifically examined are the comonomers 1-octene and poorly responsive isobutene. Large increases in comonomer enchainment efficiency into the polyethylene microstructure are observed versus the corresponding mononuclear catalyst [1-Me2Si(3-ethylindenyl)(tBuN)]TiMe2 (Ti1) + Ph3C+B(C6F5)4- (B1) or B(C6F5)3 (BN) under identical polymerization conditions. In ethylene + 1-octene copolymerization, 11 times more 1-octene incorporation is observed for Ti2 + B2 vs Ti1 + B1. In ethylene + isobutene copolymerization, 5 times more isobutene incorporation is observed for Ti2 + BN2 vs Ti1 + BN.  相似文献   

4.
A new multicenter ethylene polymerization process is described whereby two different single-site catalysts, one competent for producing vinyl-terminated oligomers or macromonomers and one competent for producing high-molecular weight ethylene-alpha-olefin copolymers, are held in close spatial proximity via ion-pairing with a dianionic binuclear bis-borate cocatalyst. Ethylene polymerizations mediated by stoichiometrically appropriate quantities of Me2Si(tBuN)(eta5-3-ethylindenyl)ZrMe2 and Me2Si(tBuN)(eta5-C5Me4)TiMe2 activated by the bis-borate cocatalyst [Ph3C+]2[1,4-(C6F5)3BC6F4B(C6F5)3-2] yield a more homogeneous polyethylene product when compared to control polymerizations using the mononuclear activator [Ph3C+][B(C6F5)4-]. The bulk and spectroscopic properties of the polymer produced using the binuclear activator are consistent with highly branched polyethylene.  相似文献   

5.
This contribution describes the implementation of the binuclear organotitanium "constrained geometry catalysts" (CGCs), (mu-CH(2)CH(2)-3,3'){(eta(5)-indenyl)[1-Me(2)Si((t)()BuN)](TiMe(2))}(2)[EBICGC(TiMe(2))(2); Ti(2)] and (mu-CH(2)-3,3'){(eta(5)-indenyl)[1-Me(2)Si((t)BuN)](TiMe(2))}(2)[MBICGC(TiMe(2))(2); C1-Ti(2)], in combination with the bifunctional bisborane activator 1,4-(C(6)F(5))(2)BC(6)F(4)B(C(6)F(5))(2) (BN(2)) in ethylene + olefin copolymerization processes. Specifically examined are the classically poorly responsive 1,1-disubstituted comonomers, methylenecyclopentane (C), methylenecyclohexane (D), 1,1,2-trisubstituted 2-methyl-2-butene (E), and isobutene (F). For the first three comonomers, this represents the first report of their incorporation into a polyethylene backbone via a coordination polymerization process. C and D are incorporated via a ring-unopened pathway, and E is incorporated via a novel pathway involving 2-methyl-1-butene enchainment in the copolymer backbone. In ethylene copolymerization, Ti(2) + BN(2) enchains approximately 2.5 times more C, approximately 2.5 times more D, and approximately 2.3 times more E than the mononuclear catalyst analogue [1-Me(2)Si(3-ethylindenyl)((t)BuN)]TiMe(2) (Ti(1)) + B(C(6)F(5))(3) (BN) under identical polymerization conditions. Polar solvents are found to weaken the catalyst-cocatalyst ion pairing, thus influencing the comonomer enchainment selectivity.  相似文献   

6.
IntroductionThe discovery of metallocene catalyst systems hasprovided a unique opportunity for producing novel tai-lor-made polyethylenes[1—3]. The introduction of func-tional groups into polyethylene chainsviacatalyzed co-polymerization can produce nove…  相似文献   

7.
Various half-sandwich titanium complexes containing iminoimidazolidide ligands, CpTiCl(2)[1,3-R(2)(CH(2)N)(2)C=N] (1a-d) [R = Ph (a), 2,6-Me(2)C(6)H(3) (b), cyclohexyl (c), (t)Bu (d)], have been employed as the catalyst precursors for ethylene polymerisation, syndiospecific styrene polymerisation, and copolymerisation of ethylene with 1-hexene in the presence of MAO cocatalyst; 1d showed the highest catalytic activity for ethylene polymerisation whereas 1b showed the highest activity for syndiospecific styrene polymerisation.  相似文献   

8.
The synthesis and reactivity of [Tp*Zr(CH2Ph)2][B(C6F5)4] (2, Tp* = HB(3,5-Me2pz)3, pz = pyrazolyl) have been explored to probe the possible role of Tp'MR2+ species in group 4 metal Tp'MCl3/MAO olefin polymerization catalysts (Tp' = generic tris(pyrazolyl)borate). The reaction of Tp*Zr(CH2Ph)3 (1) with [Ph3C][B(C6F5)4] in CD2Cl2 at -60 degrees C yields 2. 2 rearranges rapidly to [{(PhCH2)(H)B(mu-Me2pz)2}Zr(eta2-Me2pz)(CH2Ph)][B(C6F5)4] (3) at 0 degrees C. Both 2 and 3 are highly active for ethylene polymerization and alkyne insertion. Reaction of 2 with excess 2-butyne yields the double insertion product [Tp*Zr(CH2Ph)(CMe=CMeCMe=CMeCH2Ph)][B(C6F5)4] (4). Reaction of 3 with excess 2-butyne yields [{(PhCH2)(H)B(mu-Me2pz)2}Zr(Cp*)(eta2-Me2pz)][B(C6F5)4] (6, Cp* = C5Me5) via three successive 2-butyne insertions, intramolecular insertion, chain walking, and beta-Cp* elimination.  相似文献   

9.
The reaction of (bpzmp)Zr(CH2Ph)3 with B(C6F5)3 produces the active ethylene polymerisation catalyst [(bpzmp)Zr(CH2Ph)2]+[PhCH2B(C6F5)3]- which showed a temperature dependent polymerisation mechanism identified by variable temperature 1H NMR analysis of the catalyst solution.  相似文献   

10.
This work analyzes stereochemical aspects of olefin polymerization processes mediated by the C1-symmetric constrained geometry catalyst H2Si(ind)(tBuN)TiCH3+ (ind = indenyl), including the role of the cocatalyst/counteranion. The energetics of catalyst activation are first analyzed and shown to compare favorably with experiment. The energetics of heterolytic ion pair separation are next scrutinized, and the effects of solvation environment are assessed. Computed thermodynamic profiles for ethylene insertion at H2Si(ind)(tBuN)TiCH3+ indicate that the kinetics of insertion processes at the H2Si(ind)(tBuN)TiR+ cation can be analyzed in terms of SCF potential energies. We next compare the energetic profile for ethylene insertion at the naked H2Si(ind)(tBuN)TiCH3+ cation with that at the related H2Si(ind)(tBuN)TiCH3+H3CB(C6F5)3- ion pair to understand counterion effects. It is seen that the counterion, although affecting overall catalytic activity, does not significantly influence enchainment stereochemistry or polymer microtacticity. Next, the second ethylene insertion at H2Si(ind)(tBuN)Ti(nC3H7)+H3CB(C6F5)3- is analyzed to evaluate counteranion influence on the propagation barrier. It is found that the ethylene uptake transition state is energetically comparable to the first insertion transition state and that solvation has negligible effects on the energetic profile. These findings justify analysis of the propylene insertion process within the less computationally demanding "naked cation" model. Thus, monomer enchainment at H2Si(ind)(tBuN)TiR+ is analyzed for H2Si(ind)(tBuN)TiCH3+ + propylene (first insertion) and for H2Si(ind)(tBuN)Ti(iC4H6)+ + propylene (second insertion). Data describing the first insertion highlight the sterically dominated regioselection properties of the system with activation energies indicating that olefin insertion regiochemistry is predominantly 1,2 (primary), while the second insertion similarly reflects the catalyst stereoinduction properties, with steric effects introduced by the growing chain (mimicked by an isobutyl group) preferentially favoring insertion pathways that afford isotactic enrichment, in agreement with experiment.  相似文献   

11.
The family of ligands containing an N2O2S2 core, namely, 1,2-di(3-Me-5-t-Bu-salicylaldimino-o-phenylthio)ethane (H2L1), 1,3-di(3-Me-5-t-Bu-salicylaldimino-o-phenylthio)propane (H2L2), 1,4-di(3-Me-5-t-Bu-salicylaldimino-o-phenylthio)butane (H2L3), and 1,2-di(3-Me-5-t-Bu-salicylaldamino-o-phenylthio)ethane (H2L4), have been prepared and complexed with a variety of vanadium chlorides and alkoxides to afford complexes of the form [V(X)L1] (X = O (1), Np-tol (2), Cl (3)), [V(O)(L2,3)] (L2 (4), L3 (5)), and [V(L4)] (6). Crystal structure determinations of H2L1 and H2L4 show the molecule to be centrosymmetric about the bridging ethane moiety, with structural determination of 1 and 3 revealing isostructural monomeric complexes in which the ligand chelates in such a way as to afford pseudo-octahedral coordination at the vanadium center. Prolonged reaction of H2L1 with [V(Np-tol)(OEt)3] led, via oxidative cleavage of the C-S bond, to the bimetallic complex [V2L1(3-Me,5-t-Bu-salicylaldimino-o-phenylthiolate)2] [VL'] (7), as characterized by single-crystal X-ray crystallography. 7 was also isolated from the reaction of H2L4 and [VO(On-Pr)3]. The ability of 1-7 to catalyze the homopolymerization of ethylene and the copolymerization of ethylene/1-hexene in the presence of dimethylaluminum chloride (DMAC) has been assessed: screening reveals that for ethylene homopolymerization 1-7 are all highly active (>1000 g/mmol.h.bar), with the highest activity (ca. 11 000 g/mmol.h.bar) observed using catalyst 3; the use of trimethyl aluminum (TMA) or methylaluminoxane (MAO) as the cocatalyst led only to poorly active systems producing negligible polymer. Analysis of the polyethylene produced showed high molecular weight linear polymers with narrow polydispersities. For ethylene/1-hexene copolymerization, activities as high as 1,190 g/mmol.h.bar were achieved (4); analysis of the copolymer indicated an incorporation of 1-hexene in the range of 5-13%.  相似文献   

12.
Cp*ZrMe3 reacts with silica pretreated at 800 degrees C, SiO(2-(800)) through two pathways: (a) protolysis of a Zr-Me group by surface silanols and (b) transfer of a methyl group to the surface by opening of strained siloxane bridges, in a relative proportion of ca. 9/1, respectively, affording a well-defined surface species [([triple bond]SiO)ZrCp*(Me)2], 3, but with two different local environments 3a, [([triple bond]SiO)ZrCp*(Me)2][[triple bond]Si-O-Si[triple bond]], and the other with 3b, [structure: see text]. The reaction of the species 3 with B(C6F5)3 is controlled by this local environment and gives three surface species [([triple bond]SiO)ZrCp*(Me)](+)[MeB(C6F5)3]- [[triple bond]Si-O-Si[triple bond]], 4a (20%), [([triple bond]SiO)ZrCp*(Me)](+)[(Me)B(C6F5)3]- [[triple bond]Si-Me], 4b (10%), and [([triple bond]SiO)2ZrCp*](+)[(Me)B(C6F5)(3)](-)[[triple bond]Si-O-Si[triple bond]], 5 (70%). On the contrary, the reaction of Cp*Zr(Me)3, Cp2Zr(Me)2 with [[triple bond]SiO-B(C6F5)3](-)[HNEt2Ph]+, 6, leads to a unique species [([triple bond]SiO)B(C6F5)3](-)[Cp*Zr(Me)2.NEt2Ph]+, 7, and [([triple bond]SiO)ZrCp2](+)[(Me)B(C6F5)3]-, 9 respectively. The complexes 4 and 7 are active catalysts in ethylene polymerization at room temperature, 93 and 67 kg PE mol Zr1- atm(-1) bar(-1), respectively, indicating that covalently bounded Zr catalyst 4 is slightly more active than the "floating" cationic catalyst 7.  相似文献   

13.
The solution structures of the metallocenium homogeneous polymerization catalyst ion-pairs [Cp(2)ZrMe](+)[MeB(C(6)F(5))(3)](-) (1), [(1,2-Me(2)Cp)(2)ZrMe](+)[MeB(C(6)F(5))(3)](-) (2), [(Me(2)SiCp(2))ZrMe](+)[MeB(C(6)F(5))(3)](-) (3), [Me(2)C(Fluorenyl)(Cp)ZrMe](+)[FPBA](-) (FPBA = tris(2,2',2' '-nonafluorobiphenyl)fluoroaluminate) (4), [rac-Et(Indenyl)(2)ZrMe](+)[FPBA](-) (5), [(Me(5)Cp)(2)ThMe](+)[B(C(6)F(5))(4)](-) (6), [(Me(2)SiCp(2))Zr(Me)(THF)](+)[MeB(C(6)F(5))(3)](-) (7), [(Me(2)SiCp(2))Zr(Me)(PPh(3))](+)[MeB(C(6)F(5))(3)](-) (8), [(Me(2)SiCp(2))Zr(Me)(THF)](+)[B(C(6)F(5))(4)](-) (9), [(Me(2)Si(Me(4)Cp)(t-BuN)Zr(Me)(solvent)](+)[B(C(6)F(5))(4)](-) (solvent = benzene, toluene) (10), [(Cp(2)ZrMe)(2)(mu-Me)](+)[MePBB](-) (PBB = tris(2,2',2"-nonafluorobiphenyl)borane) (11), and [(Cp(2)Zr)(2)(mu-CH(2))(mu-Me)](+)[MePBB](-) (12), having the counteranion in the inner (1, 3, 4, 5, and 6) or outer (7, 8, 9, 10, 11, and 12) coordination sphere, have been investigated for the first time in solvents with low relative permittivity such as benzene or toluene by (1)H NOESY and (1)H,(19)F HOESY NMR spectroscopy. It is found that the average interionic solution structures of the inner sphere contact ion-pairs are similar to those in the solid state with the anion B-Me (1, 3) or Al-F (5) vectors oriented toward the free zirconium coordination site. The HOESY spectrum of complex 6 is in agreement with the reported solid-state structure. In contrast, in outer sphere contact ion-pairs 7, 8, 9, and 10, the anion is located far from the Zr-Me(+) moiety and much nearer to the Me(2)Si bridge than in 3. The interionic structure of 8 is concentration-dependent, and for concentrations greater than 2 mM, a loss of structural localization is observed. PGSE NMR measurements as a function of concentration (0.1-5.0 mM) indicate that the tendency to form aggregates of nuclearity higher than simple ion-pairs is dependent on whether the anion is in the inner or outer coordination sphere of the metallocenium cation. Complexes 2, 3, 4, 5, and 6 show no evidence of aggregation up to 5 mM (well above concentrations typically used in catalysis) or at the limit of saturated solutions (complexes 3 and 6), while concentration-dependent behavior is observed for complexes 7, 8, 10, and 11. These outer sphere ion-pairs begin to exhibit significant evidence for ion-quadruples in solutions having concentrations greater than 0.5 mM with the tendency to aggregate being a function of metal ligation and anion structure. Above 2 mM, compound 8 exists as higher aggregates that are probably responsible for the loss of interionic structural specificity.  相似文献   

14.
Thermally pretreated catalysts were prepared by heating MgCl2/THF/TiCl4 (TT-0) at 80°C for 5 min (TT-1) and 60 min (TT-2), and at 108°C for 5 min (TT-3) and 60 min (TT-4). Ethylene–1-hexene copolymers were prepared with these catalysts. The TT-1 catalyst produced more blocky and higher 1-hexene content polymer than TT-0, 2, 3, and 4. Temperature rising elution fractionation (TREF) analysis was used to investigate the chemical composition distribution of the ethylene–1-hexene copolymer, exhibiting bimodal distribution for TT-0 and trimodal for TT-1, 2, 3, and 4. A portion of higher hexene content of the copolymer markedly increased when the copolymerization was performed with TT-1, indicating that copolymerization active sites were newly generated. Portion of homopolyethylene increased drastically when the copolymerization was performed with TT-4, indicating that ethylene homopolymerization active sites were increased. Gel permeation chromatography (GPC) also revealed that three kinds of active sites existed on the catalyst. 13C-NMR spectrum of each fraction after TREF analysis suggested that the isospecific active site could polymerize 1-hexene well, resulting in random and alternating copolymers. A scheme for generation of the active site and change of its nature during thermal treatment of bimetallic complex catalyst is proposed. © 1998 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 36: 291–300, 1998  相似文献   

15.
��־ǿ 《高分子科学》2013,31(1):110-121
A supported TiCl4/MgCl2 catalyst without internal electron donor (O-cat) was prepared firstly. Then it was modified by 2,6-diisopropylphenol to make a novel modified catalyst (M-cat). These two catalysts were used to catalyze ethylene/1-hexene copolymerization and 1-hexene homopolymerization. The influence of cocatalyst and hydrogen on the catalytic behavior of these two catalysts was investigated. In ethylene/1-hexene copolymerization, the introduction of 2,6-iPr2C6H3O-groups did not deactivate the supported TiCl4/MgCl2 catalyst. Although the 1-hexene incorporation in ethylene/1-hexene copolymer prepared by M-cat was lower than that prepared by O-cat, the composition distribution of the former was narrower than that of the latter. Methylaluminoxane (MAO) was a more effective activator for M-cat than triisobutyl-aluminium (TIBA). MAO led to higher yield and more uniform chain structure. In 1-hexene homopolymerization, the presence of 2,6-iPr2C6H3O-groups lowered the propagation rate constants. Two types of active centers with a chemically bonded 2,6-iPr2C6H3O-group were proposed to explain the observed phenomena in M-cat.  相似文献   

16.
Pulsed field gradient spin-echo (PGSE) NMR and cryoscopic measurements have been performed on a series of homogeneous metallocene polymerization catalyst ion-pairs to determine if aggregation is a significant phenomenon under typical polymerization conditions. Cryoscopic measurements on [(Me5Cp)2ZrMe]+[MeB(C6F5)3]- (1), [rac-Et(Indenyl)2ZrMe]+[MeB(C6F5)3]- (2), [(1,2-Me2Cp)2ZrCHTMS2]+[MeB(C6F5)3]- (3), [Me2Si(Me4Cp)(t-BuN)TiMe]+[MeB(C6F5)3]- (4), [Me2Si(Me4Cp)(t-BuN)ZrMe]+[MeB(C6F5)3]- (5), and [Me2C(Fluorenyl)(Cp)ZrMe]+[MeB(C6F5)3]- (6) were carried out in benzene in the 10-18 millimolal concentration range. PGSE measurements, using (p-tolyl)4Si as an internal standard, were also performed on catalyst ion-pairs 1, 4, 6, [(Me5Cp)2ThMe]+[B(C6F5)4]- (7), [(Me2SiCp2)ZrMe]+[MeB(C6F5)3]- (8), and [Cp2ZrMe]+[MeB(C6F5)3]- (9) in the 0.8-10.0 millimolar range. All results are consistent with a 1:1 ion-pair structural model and show little evidence for ion-quadruples or higher-order aggregates.  相似文献   

17.
The new binuclear phenoxyiminato zirconium complex {1,7-(O)2C10H4-2,7-[CH=N(2,6-iPr2C6H3)]2}Zr2Cl6(THF)2 (FI2-Zr2) polymerizes ethylene with greater activity (approximately 8x) than the mononuclear analogue. Also, this catalyst produces high molecular weight ethylene + 1-hexene copolymers, while the mononuclear analogue yields only traces of copolymer under identical conditions. This ability to produce copolymers suggests cooperativity between the two Zr centers which promotes 1-hexene co-enchainment.  相似文献   

18.
Bimetallic dichlorotitanium complexes, {2,6-[eta(5)-2,5-Me2C5H2](2)-4-R-C6H2N-microN}{Ti(IV)Cl2}2 (, R=Me; , R=F) and 4,4'-A[{2-(eta(5)-2,3,5-Me3C5H)C6H3NC6H11-kappaN}Ti(IV)Cl2]2 (, A=CH2; , A=O; , A=ortho-C6H4) are prepared via a key step of the Suzuki-coupling reaction of 2-dihydroxyboryl-3-methyl-2-cyclopenten-1-one () with dibromo-compounds. The solid state structure of was determined by X-ray crystallography. Complexes and are not active for ethylene/1-hexene copolymerization. Meanwhile, the complexes are highly active and their activities are higher than that of the mononuclear analogue, {2-(eta(5)-2,3,5-Me3C5H)C6H3NC6H11-kappaN}Ti(IV)Cl2 (). The molecular weights of the polymers obtained with the bimetallic complexes are higher than that of the polymer obtained using . Slightly higher contents of long-chain-branching are observed for the copolymers obtained using the bimetallic system.  相似文献   

19.
A number of half-zirconocene anilide complexes of the type Cp*ZrCl(2)[N(2,6-R(1)(2)C(6)H(3))R(2)] [R(1) = (i)Pr (1, 3), Me (2); R(2) = Me (1, 2), Bn (3)] and Cp*ZrCl[N(2,6-Me(2)C(6)H(3))Me](2) (4) (Cp* = pentamethylcyclopentadienyl) were synthesized from the reactions of Cp*ZrCl(3) with the lithium salts of the corresponding anilide in diethyl ether at room temperature. All new zirconium complexes were characterized by (1)H and (13)C NMR and elemental analysis. Molecular structures of complexes 1, 2 and 4 were determined by single crystal X-ray diffraction analysis. Upon activation with Al(i)Bu(3) and Ph(3)CB(C(6)F(5))(4), complexes 1-4 exhibit good catalytic activity for ethylene polymerization, and produce polyethylene with a moderate molecular weight. Among these zirconium complexes, complex 1 shows the highest catalytic activity while complex 4 shows the lowest catalytic activity for ethylene polymerization. Complexes 1-3 also exhibit moderate catalytic activity for copolymerization of ethylene with 1-hexene, and produce copolymers with relatively high molecular weight and reasonable 1-hexene incorporation. In addition, the activation procedure of these catalyst systems were studied by (1)H NMR spectroscopy.  相似文献   

20.
The reactions of three types of group 4 metal olefin polymerization catalysts, (C(5)R(5))(2)ZrX(2)/activator, (C(5)Me(5))TiX(3)/MAO (MAO = methylalumoxane), and (C(5)Me(4)SiMe(2)N(t)Bu)MX(2)/activator (M = Ti, Zr), with vinyl chloride (VC) and VC/propylene mixtures have been investigated. Two general pathways are observed: (i) radical polymerization of VC initiated by radicals derived from the catalyst and (ii) net 1,2 VC insertion into L(n)MR(+) species followed by beta-Cl elimination. rac-(EBI)ZrMe(mu-Me)B(C(6)F(5))(3) (EBI = 1,2-ethylenebis(indenyl)) reacts with 2 equiv of VC to yield oligopropylene, rac-(EBI)ZrCl(2), and B(C(6)F(5))(3). This reaction proceeds by net 1,2 VC insertion into rac-(EBI)ZrMe(+) followed by fast beta-Cl elimination to yield [rac-(EBI)ZrCl][MeB(C(6)F(5))(3)] and propylene. Methylation of rac-(EBI)ZrCl(+) by MeB(C(6)F(5))(3)(-) enables a second VC insertion/beta-Cl elimination to occur. The evolved propylene is oligomerized by rac-(EBI)ZrR(+) as it is formed. At high Al/Zr ratios, rac-(EBI)ZrMe(2)/MAO catalytically converts VC to oligopropylene by 1,2 VC insertion into rac-(EBI)ZrMe(+), beta-Cl elimination, and realkylation of rac-(EBI)ZrCl(+) by MAO; this process is stoichiometric in Al-Me groups. The evolved propylene is oligomerized by rac-(EBI)ZrR(+). Oligopropylene end group analysis shows that the predominant chain transfer mechanism is VC insertion/beta-Cl elimination/realkylation. In the presence of trace levels of O(2), rac-(EBI)ZrMe(2)/MAO polymerizes VC to poly(vinyl chloride) (PVC) by a radical mechanism initiated by radicals generated by autoxidation of Zr-R and/or Al-R species. CpTiX(3)/MAO (Cp = C(5)Me(5); X = OMe, Cl) initiates radical polymerization of VC in CH(2)Cl(2) solvent at low Al/Ti ratios under anaerobic conditions; in this case, the source of initiating radicals is unknown. Radical VC polymerization can be identified by the presence of terminal and internal allylic chloride units and other "radical defects" in the PVC which arise from the characteristic chemistry of PCH(2)CHCl(*) macroradicals. However, this test must be used with caution, since the defect units can be consumed by postpolymerization reactions with MAO. (C(5)Me(4)SiMe(2)N(t)Bu)MMe(2)/[Ph(3)C]][B(C(6)F(5))(4)] catalysts (M = Ti, Zr) react with VC by net 1,2 insertion/beta-Cl elimination, yielding [(C(5)Me(4)SiMe(2)N(t)Bu)MCl][B(C(6)F(5))(4)] species which can be trapped as (C(5)Me(4)SiMe(2)N(t)Bu)MCl(2) by addition of a chloride source. The reaction of rac-(EBI)ZrMe(2)/MAO or [(C(5)Me(4)SiMe(2)N(t)Bu)ZrMe][B(C(6)F(5))(4)] with propylene/VC mixtures yields polypropylene containing both allylic and vinylidene unsaturated chain ends rather than strictly vinylidene chain ends, as observed in propylene homopolymerization. These results show that the VC insertion of L(n)M(CH(2)CHMe)(n)R(+) species is also followed by beta-Cl elimination, which terminates chain growth and precludes propylene/VC copolymerization. Termination of chain growth by beta-Cl elimination is the most significant obstacle to metal-catalyzed insertion polymerization/copolymerization of VC.  相似文献   