1.
2,5-Bis(4-aminophenyl)-3,4-diphenylthiophene, a polyimide-forming monomer, was prepared in three steps starting from benzyl chloride and sulfur. Novel polyimides were synthesized from the diamine and pyromellitic dianhydride or 3,3′, 4,4′-benzophenonetetracarboxylic dianhydride (BTDA). Polymerization was carried out either by the usual two-step procedure that included ring-opening polyaddition giving polyamic acids, followed by cyclodehydration to polyimides, or by the direct one-pot procedure involving cyclodehydration in situ. The polyimide derived from the diamine and BTDA, especially that prepared by the one-pot procedure in m-cresol containing isoquinoline, is soluble in various organic solvents and gave a yellow, transparent, tough, and flexible film. Solubility of this polyimide varied by the preparative method and by the copolymerization with bis(4-aminophenyl) ether. All the polyimides are highly thermally stable and exhibited no appreciable decomposition up to 450°C in air and nitrogen atmospheres.  相似文献   

2.
In this article a new synthesis of 3,3′-diaminobiphenyl (3,3′-DABP) is described, along with the preparation and characterization of polyamides and polyimides based on it. Reactivity of this monomer was calculated by a molecular simulation study, using ab initio quantum-mechanical methods. Terephthaloyl and isophthaloyl chloride were used for the synthesis of polyamides, while 3,3′,4,4′-biphenylenetetracarboxylic acid dianhydride and 4,4′-(hexafluoroisopropylidene) diphthalic anhydride were used for the synthesis of polyimides. Medium to high molecular weight polymers were attained, with inherent viscosities near or higher than 1.0 dL/g, the solubility of the 3,3′-DABP polymers was much better than that of the homologous polymers from benzidine (4,4′-DABP), the glass-transition temperatures were lower, by about 40°C, and the thermal resistance, as measured by thermogravimetry, was virtually the same. Amorphous films, made from cast polymer solutions, showed excellent mechanical properties, comparable to conventional aromatic polyamides and polyimides. Theoretical calculations demonstrated that the radius of giration, end-to-end distance and density of poly(3,3′-DABP-isophthalamide) were lower than those of poly(4,4′-DABP-isophthalamide), as a consequence of the chain folding induced in the backbone by the m-substitution in 3,3′-DABP. © 1999 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 37: 4646–4655, 1999  相似文献   

3.
New photosensitive polymides containing photosensitive disilane unit were synthesised from 1,2-bis(4-aminophenyl)tetramethyldisilane and various aromatic tetracarboxylic dianhydrides by the usual two-step procedure that includes ring-opening polyaddition to yield the precursor polyamic acids, followed by cyclodehydration giving the respective polyimides. The polymaic acids had inherent viscosities between 0.63 and 0.85 dL/g depending on the tetracarboxylic dianhydride used. Excepting the polyimide obtained from pyromellitic dianhydride, all other polyimides were soluble in N-methyl-2-pyrrolidone, m-cresol, and pyridine. While the polyimide containing diphenyl sulfone unit was amorphous, the other polyimides were semi-crystalline polymers based on their x-ray diffractograms. The polyimides had glass transition temperatures between 235 and 304°C. They were thermally stable up to 380°C in both air and nitrogen atmospheres. All the polyamic acids showed a drastic decrease in the inherent viscosity upon UV light irradiation, implying the inherent photosensitivity of the polymers containing the disilane moiety.  相似文献   

4.
Various phosphorus-containing polyimides were prepared by the reaction of 1-[(dialkoxyphosphinyl)methyl]-2,4- and -2,6-diaminobenzenes (1) with a tetracarboxylic dianhydride like pyromellitic dianhydride (PMDA) and benzophenone tetracarboxylic dianhydride (BTDA). In addition, copolyimides that contained approximately 3% phosphorus were prepared by the reaction of 1 and m-phenylenediamine (MPD) with the aforementioned tetracarboxylic dianhydrides. Elemental analysis, inherent viscosity, infrared (IR) spectroscopy, differential scanning calorimetry (DSC), and thermogravimetric analysis (TGA) studies were performed to characterize the polymers. Their thermal properties were compared with those of the corresponding common polyimides. It was shown that the molecular weight and thermal stability of the polymers were reduced as the concentration of the phosphorus moieties increased. The fire-resistance of the copolyimides was evaluated by determining their limiting oxygen index (LOI) value. Copolyimides that contained about 3% phosphorus showed an LOI value approximately 30% higher, than the value of the corresponding common polyimides. In addition, a model diamic acid and diimide was synthesized by the reaction of 1-[di(2-chloroethoxyphosphinyl)methyl]-2,4- and - 2,6-diaminobenzene (DCEPD) with phthalic anhydride and characterized by elemental analysis, IR, proton nuclear magnetic (1H-NMR) spectroscopy, DSC, and TGA. The pyrolysis behavior of the model compounds was investigated by gas chromatography-mass spectrometry (GC-MS). A direct cleavage of the P? C bond and a possible rearrangement to diisocyanates occurred during their pyrolysis.  相似文献   

5.
Alkylene-linked aromatic polyimides were prepared from a family of new dianhydride monomers and aromatic diamines. The dianhydrides were synthesized by Friedel-Crafts catalysis of the condensation of ditertiary alcohols with o-xylene, subsequent oxidation of the aryl methyl groups to carboxy, and finally, dehydration of the ortho-carboxy substituents to anhydride groups. Alkylene-linked aromatic polyimides, with up to 8 methylene groups in the polymer chain, are stable to 400°C in air and can be extruded or compression-molded at 300°C. In addition, these polymers are soluble in solvents within the solubility parameter range of 10.4 ± 1.2.  相似文献   

6.
New aromatic polyimides and polyamide-imides with phenylquinoxaline rings and dimethylsilane units have been synthesized by solution polycondensation reaction of aromatic diamines containing phenylquinoxaline units with bis(3,4-dicarboxyphenyl)-dimethylsilane dianhydride, or with a diacid chloride resulting from the reaction of this dianhydride with p-aminobenzoic acid. These polymers were easily soluble in organic solvents, such as N-methylpyrrolidinone and dimethylacetamide, and showed high thermal stability with decomposition temperature being above 440°C and glass transition temperature in the range of 245-285°C. Very thin coatings were deposited from polymer solutions onto silicon wafers and exhibited smooth, pinhole-free surface in atomic force microscopy investigations. Some of these polymers showed blue fluorescence in solution and films, with a maximum in the range of 415-425 nm.  相似文献   

7.
In this study, new monomers having siloxane groups were synthesized as an intermediate for preparation of siloxane modified polyimide polymers. Then with these monomers, the synthesis of uncrosslinked and crosslinked polyimide–siloxane hybrid polymer membranes were achieved. The purposes of the preparation of modified polyimides were to modify the thermal and chemical stability, and mechanical strength of polyimides, and to improve the gas separation properties of polymers. The new diamine monomer having siloxane groups was prepared from 3,5‐diaminobenzoic acid (3,5‐DABA) and 3‐aminopropyltrimethoxysilane (3‐APTMS) in N‐methyl‐2‐pyrollidone (NMP) at 180°C. The modified polyimide membranes having different amount of siloxane groups were synthesized from pyromellitic dianhydride (PMDA), 4,4‐oxydianiline (ODA), and 3,5‐diaminobenzamido‐N‐propyltrimethoxy silane (DABA/PTMS) in NMP using a two‐step thermal imidization process. The synthesis of modified polyimide membranes were characterized by Fourier transform infrared spectroscopy (FTIR). The thermal analysis of the polyimides were carried out by differential scanning calorimetry (DSC) and thermogravimetric analysis (TGA). Water absorption and swelling experiments were also carried out for the investigation of structural properties of polymers. FTIR observations confirmed that the polyimide membranes with new diamine intermediate were successfully obtained. Thermal analysis showed that the uncrosslinked copolyimides exhibited two glass transition temperatures, indicating that they were separated microphases and it was found that all the modified copolyimides had showed higher glass transition temperature (Tg) than unmodified polyimides. The separation properties of the prepared polyimide membranes were also characterized by permeability for O2 and N2 gases and ideal selectivity values were calculated. Copyright © 2009 John Wiley & Sons, Ltd.  相似文献   

8.
Novel polyimides and polyimides having phenoxathiin units have been prepared. Polyamides with inherent viscosities in the range of 0.5–2.9 were readily prepared by the polycondensations of phenoxathiin diamines with aromatic diacyl chlorides and of aromatic diamines with new phenoxathiin diacyl chlorides. The polyimides were synthesized from phenoxathiin diamines and pyromellitic dianhydride by using a two-step procedure. The polyamic acids which formed in the first step had inherent viscosities ranging from 1.0 to 1.6, and they were converted to the polyimides by thermal cyclodehydration. Some of the phenoxanthiin-containing polyamides were highly soluble in polar amide solvents and dimethyl sulfoxide. A series of novel polymers containing phenoxathiin units were much more thermostable than the corresponding polymers having open-chain diphenyl ether linkages.  相似文献   

9.
A facile synthesis of an optically active di‐isocyanate containing alkylene groups and a preformed imide structure is described. Polycondensation reactions of the prepared di‐isocyanate with pyromellitic dianhydride, benzophenone tetracarboxylic dianhydride, and hexafluoroisopropylidene diphthalic anhydride resulted in the preparation of optically active, thermally stable polyimides. The prepared monomer and polymers were characterized by conventional methods. Optical and physical properties of the polymers including thermal stability, thermal behavior, solution viscosity, and solubility behavior were studied. © 2001 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 39: 514–518, 2001  相似文献   

10.
1,1‐Bis[4‐(4‐aminophenoxy)phenyl]‐1‐phenylethane (BAPPE) was prepared through nucleophilic substitution reaction of 1,1‐bis(4‐hydroxyphenyl)‐1‐phenylethane and p‐chloronitrobenzene in the presence of K2CO3 in N,N‐dimethylformamide, followed by catalytic reduction with hydrazine and Pd/C. Novel organosoluble polyimides and copolyimides were synthesized from BAPPE and six kinds of commercial dianhydrides, including pyromellitic dianhydride (PMDA, Ia ), 3,3′,4,4′‐benzophenonetetracarboxylic dianhydride (BTDA, Ib ), 3,3′,4,4′‐ biphenyltetracarboxylic dianhydride (BPDA, Ic ), 4,4′‐oxydiphthalic anhydride (ODPA, Id ), 3,3′,4,4′‐diphenylsulfonetetracarboxylic dianhydride (DSDA, Ie ) and 4,4′‐hexafluoroisopropylidenediphthalic anhydride (6FDA, If ). Differing with the conventional polyimide process by thermal cyclodehydration of poly(amic acid), when polyimides were prepared by chemical cyclodehydration with N‐methyl‐2‐pyrrolidone as used solvent, resulted polymers showed good solubility. Additional, Ia,b were mixed respectively with the rest of dianhydrides (Ic–f) and BAPPE at certain molar ratios to prepare copolyimides with arbitrary solubilities. These polyimides and copolyimides were characterized by good mechanical properties together with good thermal stability. © 2000 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 38: 2082–2090, 2000  相似文献   

11.
As majority of polyheteroarylenes based on bis(naphthalic anhydrides), are difficult to process due to their infusiblity and insolubility in common organic solvents and solubility only in strong acids, this study is concerned with the synthesis and properties of new, easily processable polyimides and copolyimides containing naphthalene and oxadiazole rings. These polymers have been synthesized and their properties have been compared with regard to the influence of oxadiazole and naphthalene units on their physical properties. The polyimides were prepared by polycondensation reaction in solution of the aromatic diamines containing preformed oxadiazole ring with two dianhydrides having naphthalene units, at high temperature. Also, copolyimides were prepared by using a mixture of each naphthalene‐containing dianhydride, with hexafluoroisopropylidene‐dianhydride in the polycondensation reaction with the same diamino‐oxadiazoles. Most of the resulting polyimides and copolyimides were soluble in polar amidic solvents and in less polar solvents, and their solutions gave flexible films when spread onto glass plates. The thermal stability and glass transition temperature of these polyimides and copolyimides were measured and compared. The quality and the roughness of the spin‐coated films of these polymers were investigated by atomic force microscopy. The photoluminescence properties of the polymers in solution were studied to determine the color of emission. The UV absorption was also studied to determine the Stokes shift, and hence the possible reabsorption effects. The properties of the present polyimides make them attractive for applications in advanced optoelectronics and other related fields. Copyright © 2009 John Wiley & Sons, Ltd.  相似文献   

12.
2,2,′3,3′‐Biphenyltetracarboxylic dianhydride (2,2,′3,3′‐BPDA) was prepared by a coupling reaction of dimethyl 3‐iodophthalate. The X‐ray single‐crystal structure determination showed that this dianhydride had a bent and noncopolanar structure, presenting a striking contrast to its isomer, 3,3,′4,4′‐BPDA. This dianhydride was reacted with aromatic diamines in a polar aprotic solvent such as N,N‐dimethylacetamide (DMAc) to form polyamic acid intermediates, which imidized chemically to polyimides with inherent viscosities of 0.34–0.55 dL/g, depending on the diamine used. The polyimides from 2,2,′3,3′‐BPDA exhibited a good solubility and were dissolved in polar aprotic solvents and polychlorocarbons. These polyimides have high glass transition temperatures above 283°C. Thermogravimetric analyses indicated that these polyimides were fairly stable up to 500°C, and the 5% weight loss temperatures were recorded in the range of 534–583°C in nitrogen atmosphere and 537–561°C in air atmosphere. All polyimides were amorphous according to X‐ray determination. © 1999 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 37: 1425–1433, 1999  相似文献   

13.
A novel diamine, bis(3‐aminophenyl)‐4‐(1‐adamantyl)phenoxyphenyl phosphine oxide (mDAATPPO), was synthesized via the Williamson ether reaction of 4‐(1‐adamantyl)phenol and bis(3‐nitrophenyl)‐4‐fluorophenyl phosphine oxide, followed by reduction. The phenol group was prepared by the Friedel–Crafts reaction of 1‐bromoadamantane and phenol, whereas the phosphine oxide group was synthesized by the Grignard reaction of 1‐bromo‐4‐fluorobezene and diphenyl phosphinic chloride, followed by nitration. The monomer and its intermediate compounds were characterized with Fourier transform infrared, NMR, and melting‐point apparatus. The monomer was then used to prepare polyimides with 2,2‐bis(3,4‐dicarboxyphenyl)hexafluoropropane dianhydride, 3,3′,4,4′‐benzophenonetetracarboxylic dianhydride, 4,4′‐oxydiphthalic dianhydride, and pyromellitic dianhydride by the conventional two‐step synthesis: the preparation of poly(amic acid) followed by solution imidization. The molecular weights of the polyimides were controlled to 20,000 g/mol by off‐stoichiometry, and the synthesized polyimides were characterized with Fourier transform infrared, NMR, gel permeation chromatography, thermogravimetric analysis, and differential scanning calorimetry. In addition, the solubility, intrinsic viscosity, dielectric constant, and birefringence of the polyimides were evaluated. Novel polyimides with mDAATPPO exhibited good solubility, high glass‐transition temperatures (290–330 °C), excellent thermal stability (>500 °C), low dielectric constants (2.77–3.01), low refractive indices, and low birefringence values (0.0019–0.0030). © 2006 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 44: 2567–2578, 2006  相似文献   

14.
Two novel series of aromatic polyimides were prepared from 2,2′‐bis(4‐amino‐3‐trifluoromethylthylphenoxy) biphenyl, 2,2′‐bis(4‐amino‐3‐methoxyphenoxy)biphenyl with 3,3′,4,4′‐benzophenonetetracarboxylic dianhydride (BTDA), 3,3′,4,4′‐diphenylsulfonetetracarboxylic dianhydride (DSDA) via a one‐step procedure. The resulting polymers were fully characterized, and they exhibited excellent organosolubility. These polyimides are thermally stable with 5% weight loss over 430°C, and glass transition temperatures of the polyimides were found to be 225–262°C. Resistive switching devices with the configuration of Al/polymer/indium‐tin oxide were constructed from these polyimides by using conventional solution coating process. Devices with all polyimides exhibited nonvolatile and rewritable flash type memory characteristics with turn‐on voltage at ?1.1 to ?2.8 V. The ON/OFF current ratio of these devices was larger than 104, and the retention times can be as long as 104 s. The theoretical simulation based on the density functional theory suggested that greater distinct charge separation between the ground and charge transfer states led to a highly stable memory behavior. Copyright © 2016 John Wiley & Sons, Ltd.  相似文献   

15.
We have synthesized a novel dianhydride, 2,2′-dichloro-4,4′,5,5′-benzophenone tetracarboxylic dianhydride (DCBTDA). Polyimides were synthesized with DCBTDA or 3,3′,4,4′-benzophenone tetracarboxylic dianhydride (BTDA) and several relatively rigid meta- and para- substituted mononuclear diamines. The BTDA based systems were insoluble in dipolar, aprotic solvents whereas the DCBTDA based polymers displayed enhanced solubility in these solvents. The thermal stability of these polyimides was excellent as measured by 5% weight loss decomposition. The Tg's of the polymers were all above 290°C.  相似文献   

16.
New series of diamines having pyridine rings and o-, m-, or p-phenylenedioxy linkages were prepared by condensation of chloronitropyridine with isomeric dihydroxybenzenes followed by chemical reduction. The polymerization of the diamines with benzo-phenonetetracarboxylic acid dianhydride gave polyamic acids with the inherent viscosities in the range 0.21 to 1.30 dl/g. The conversion of these polyamic acids to polyimides was carried out thermally and the resulting polyimides exhibited very good solubility in organic solvents.  相似文献   

17.
Novel sul-containing fluorinated polyimides have been synthesized by the reaction of 2,2′-bis-(trifluoromethyl)-4,4′-diaminodiphenyl sulfide (TFDAS) with 1,4-bis-(3,4-dicarboxyphenoxy)benzene dianhydride (HQDPA), 2,2′-bis-(3,4-dicarboxyphenyl)hexafluoropropane dianhydride (6FDA), 4,4′-oxydiphthalicanhydride (ODPA) or 3,4,3′,4′-biphenyl-tetracarboxylic acid dianhydride (s-BPDA). The fluorinated polyimides, prepared by a one-step polycondensation procedure, have good solubility in many solvents, such as N-methyl-2-pyrrolidinone (NMP), dimethylacetamide (DMAc), dimethyl sulfoxide (DMSO), cyclohexanone, tetrahydrofuran (THF) and m-cresol. The molecular weights (Mn's) and polydispersities (Mn/Mw's) of polyimides were in the range of 1.24 × 105 to 3.21 × 105 and 1.59–2.20, respectively. The polymers exhibit excellent thermal stabilities, with glass-transition temperatures (Tg) at 221–275 °C and the 5% weight-loss temperature are above 531 °C. After crosslinking, these polymers show higher thermal stability. The films of polymers have high optical transparency. The novel sul-containing fluorinated polyimides also have low absorption at both 1310 and 1550 nm wavelength windows. Rib-type optical waveguide device was fabricated using the fluorinated polyimides and the near-field mode pattern of the waveguide was demonstrated.  相似文献   

18.
A series of thermally-stable, tough, linear polyimides containing amide linkages were prepared. These materials have potential as high temperature films and coatings as well as matrix resins in graphite reinforced structures. The new polyamide-imides were prepared by reacting a group of isomers of diaminobenzanilide (DABA) with 3,3′,4,4′-benzophenonetetracarboxylic dianhydride (BTDA) to form the polyamide-acid with subsequent thermal conversion to the polyamide-imide (PAI). Four polymers were synthesized from unsubstituted amide diamines and two others from N-substituted amide diamines. The properties of these polyamide-imides were compared to those of the polyimide of benzophenonetetracarboxylic dianhydride/3,3′-diaminobenzophenone (LARC–TPI) because their structures are similar, except for the presence of the more flexible amide linkages. These polymers exhibited high inherent viscosities and glass transition temperatures. They were made into tough, flexible films which showed good thermal stability and good resistance to organic solvents. Mechanical properties of the PAI films were better than those of LARC–TPI. Films of the 4,4′-isomer polyamide-imide exhibited an exceptionally high modulus and toughness during impact evaluation.  相似文献   

19.
A new six-membered tetracarboxylic dianhydride, 2,5-di(carboxymethyl)terephthalic dianhydride, was synthesized in six steps, starting with pyromellitic dianhydride. The polyimides were prepared from dianhydride and diamines in a two-step procedure. The polyamic acids, which were formed in the first step by the ring-opening polyaddition in DMAc, had inherent viscosities of 0.1–0.7 and were converted to the polyimides by thermal cyclodehydration. These polyimides were insoluble in organic solvents. Thermogravimetric analysis (TGA) in air and nitrogen atmospheres revealed that rapid decomposition began above 400°C for aromatic polyimides.  相似文献   

20.
Polyisophthalamides and polyterephthalamides were prepared by the solution polycondensation of the corresponding diacyl chlorides with 4,4′-diaminobibenzyl, trans-4,4′-diaminostilbene, and 4,4′-diaminotolan in N,N-dimethylacetamide (DMAc). Polypyromellitimides were synthesized in two steps by the ring-opening polyaddition of pyromellitic dianhydride with the aromatic diamines in DMAc, followed by thermal cyclodehydration. The amorphous polyisophthalamides were soluble in some amide solvents containing lithium chloride, while the polyterephthalamides having fair degree of crystallinity were insoluble in these solvents. The thermal stability of these aromatic polymers decreased in the order of the tolan-containing polymers > the stilbene-containing polymers > the bibenzyl-containing polymers, both in air and under nitrogen.  相似文献   