Thermal stability of poly(vinyl chloride)/poly(ethylene oxide) (PVC/PEO) blends has been investigated by thermogravimetric analysis (TGA) in dynamic and isothermal heating regime. PVC/PEO blends were prepared by hot-melt extrusion (HME). According to TG analysis, PEO decomposes in one stage, while PVC and PVC/PEO blends in two degradation stages. In order to evaluate the effect of PEO content on the thermal stability of PVC/PEO blends, different criteria were used. It was found that thermal stability of PVC/PEO blends depends on the blend composition. The interactions of blends components with their degradation products were confirmed. By using multiple heating rate kinetics the activation energies of the PVC/PEO blends thermal degradation were calculated by isoconversional integral Flynn–Wall–Ozawa and differential Friedman method. According to dependence of activation energy on degree of conversion the complexity of degradation processes was determined.  相似文献   

2.
The thermooxidative degradation of poly(vinyl chloride)/chlorinated polyethylene blends of different compositions was investigated by means of isothermal thermogravimetry in flowing atmosphere of synthetic air at temperatures 240–270 °C. The main degradation processes are dehydrochlorination of PVC and CPE. For calculation of the apparent activation energy and apparent pre-exponential factor two kinetic methods were used: isoconversional method and Prout–Tompkins method. True compensation dependency between Arrhenius parameters, obtained using Prout–Tompkins model, was found. Calculated kinetic parameters of isothermal thermooxidative degradation are close to those from non-isothermal degradation and confirm the assumption of the main degradation process in PVC/CPE blends.  相似文献   

3.
The miscibility, morphology, and thermal properties of poly(vinyl chloride) (PVC) blends with different concentrations of poly(methyl methacylate) (PMMA) have been studied. The interaction between the phases was studied by FTIR and by measuring the glass transition temperature (Tg) of the blends using differential scanning calorimetry. Distribution of the phases at different compositions was studied through scanning electron microscopy. The FTIR and SEM results show little interaction and gross phase separation. The thermogravimetric studies on these blends were carried out under inert atmosphere from ambient to 800 °C at different heating rates varying from 2.5 to 20 °C/min. The thermal decomposition temperatures of the first and second stage of degradation in PVC in the presence of PMMA were higher than the pure. The stabilization effect on PVC was found most significant with 10 wt% PMMA content in the PVC matrix. These results agree with the isothermal degradation studies using dehydrochlorination and UV-vis spectroscopic results carried out on these blends. Using multiple heating rate kinetics the activation energies of the degradation process in PVC and its blends have been reported.  相似文献   

4.
The thermal degradation of poly(vinyl chloride)/chlorinated poly(ethylene) (PVC/CPE) blends of different compositions was investigated by means of dynamic and isothermal thermogravimetric analysis in flowing atmosphere of nitrogen. Kinetic parameters (the apparent activation energy E, and pre-exponential factor Z) were calculated after Flynn-Wall-Ozawa method for the first stage of dynamic degradation of PVC/CPE blends, and after Flynn method for the isothermal degradation. In both cases, there is the compensation dependence between the values E and logZ. The values of compensation ratios as well as the characteristics of TG and DTG curves, confirm the stabilizing effect of CPE on PVC dehydrochlorination. This revised version was published online in July 2006 with corrections to the Cover Date.  相似文献   

5.
The morphology, thermal and mechanical properties of polystyrene (PS) blends with 2.5-20 wt% of poly(vinyl chloride) (PVC) have been studied. The measurement of the glass transition temperature (Tg) from the maxima of tan δ data using dynamic mechanical thermal analysis showed that the blends were incompatible and homogenously distributed only within a limited range of PVC contents in PS. The value of the storage modulus was found to increase initially but then decreased with further addition of PVC in the matrix. Distribution of the phases in the virgin and degraded blends was also studied through scanning electron microscopy. The thermogravimetric studies on these blends were carried out under inert atmosphere from ambient to 800 °C at different heating rates varying from 2.5 to 20 °C/min. The thermal decomposition temperatures of blends were found higher than that of pure PS which indicated the stabilizing effects of PVC on PS. The effect varies with the heating rates and the composition of the blends and the phenomenon has been explained due to changing morphology of the blends with composition and the degradation time which affect the interfacial interaction between the degrading products from the polymer components. The kinetic parameters of the degradation process calculated from a method described by Ozawa have been reported for these blends.  相似文献   

6.
The PVC/ABS blends were degradated by means of isothermal thermogravimetry at temperatures at 210...240°C in nitrogen. Applying the stationary point method to the data obtained from thermogravimetric curves, apparent activation energy, preexponential factor and compensation parameter for each blend were calculated. The constancy of compensation parameters points to an unchanged mechanism of poly (vinyl-chloride) (PVC) thermal degradation in the presence of acrylonitrile butadiene-styrene (ABS). Upon increasing the fraction of ABS in the blend up to 50% only the kinetics of the process is changed.  相似文献   

7.
Nonisothermal and isothermal crystallization behaviors of the hyperbranched poly(ε‐caprolactone) (HPCL)/poly(vinyl chloride) (PVC) and linear poly(ε‐caprolactone) (LPCL)/(PVC) blends were characterized with various blend composition such as 100/0, 95/5, 90/10, and 80/20, respectively. HPCL was synthesized through polycondensation of AB2 macromonomer while LPCL and PVC were commercially purchased. The architectural characterization performed on 1H NMR spectra revealed that HPCL consisted of about 3 AB2 units and the linear segments consisted of 25 ε‐CL units. Through the nonisothermal crystallization analyses by modified Avrami approach with DSC crystallization exotherms, it was found that the crystallization rate was retarded by the increase in the noncrystallizable component (PVC) in the blends. This is in good agreement with the results of the isothermal crystallization analyses where time resolved small angle light scattering (SALS) and polarized optical microscopy (POM) were used. The effect of molecular architectural difference between HPCL and LPCL on the crystallization of their binary blends with PVC was elucidated by comparing the crystallization kinetic parameters. Both the nonisothermal and isothermal crystallization analyses showed that the crystallization rates of HPCL/PVC blends was faster than LPCL/PVC blends at given blend compositions. The faster crystallization of the HPCL/PVC blends is ascribed to the two specific architectural characteristics of HPCL; the branched structure and the incorporated long linear segments. © 2007 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 45: 577–589, 2007  相似文献   

8.
Three series of MBS core-shell impact modifiers were prepared by grafting styrene and methyl methacrylate onto PB or SBR seed latex in emulsion polymerization. All the MBS modifiers were designed to have the same total chemical composition, and MMA/Bd/St equals 30/42/28, which is a prerequisite for producing transparent blends with PVC. Under this composition, there were three different ways of arrangement for styrene in MBS, which led to the different structure of MBS modifier. The concentration of MBS in PVC/MBS blends was kept at a constant value of 20 wt.%. The effects of arrangement of St in MBS on the mechanical and optical properties of PVC/MBS blends were studied. The notched Izod impact test results showed that the MBS with a PB homopolymer core grafted with St had a lowest brittle-ductile transition (BDT) temperature and BDT temperature increased with the amount of St copolymerized with Bd in the core of MBS. The transparency of blends also increased with the amount of St copolymerized with Bd in the core. TEM results showed that the arrangement of St in MBS influenced the deformation behavior. Two deformation modes were observed in the blends: cavitation and shear yielding. When all St was grafted onto the PB rubber, both cavitation and debonding were observed, which relieve the triaxial tension and promote the shear yielding of the PVC matrix. When all St was copolymerized with Bd in MBS, no cavitation could be observed and only the shear yielding of the PVC matrix took place.  相似文献   

9.
In situ degradation of poly(vinyl chloride)/poly (N-vinyl-2- pyrrolidone) (PVC/PVP) blends has been studied by Fourier-transform Raman spectroscopy. PVP acts as a destabilizer in the thermal degradation of PVC as manifested by the reduction of temperature for the onset of degradation and the time the polymer is held at a particular temperature for this onset. Increasing the amount of PVP in the blends decreases the dehydrochlorination temperature and time. In blends containing high PVP concentrations, polyene bands dominate over nondegraded PVC bands. Maximum polyene lengths of around 35 were achieved. High PVP ratios and prolonged degradation at higher temperatures resulted in a decrease in mean polyene length due to crosslinking and oxidative scission.  相似文献   

10.
Extensively studied thermal degradation of polyvinyl chloride (PVC) occurs with formation of free hydrogen chloride and conjugated double bonds absorbing light in visible region. Thermogravimetric monitoring of PVC blends degradation kinetics by the loss of HCl is often complicated by evaporation and degradation of plasticizers and additives. Spectroscopic PVC degradation kinetics monitoring by absorbance of forming conjugated polyenes is specific and should not be affected by plasticizers loss. The kinetics of isothermal degradation monitored by thermal gravimetric analysis in real time was compared with batch data obtained by UV/Visible absorption spectroscopy. Effects of plasticizer on kinetics of polyene formation were examined. Thermal degradation of PVC films plasticized with di-(2-ethylhexyl) phthalate (DEHP) and 1,2,4-benzenedicarboxylic acid, tri-(3-ethylhexyl) ester (TOTM) was monitored by conjugated double bonds light absorption at 350 nm at 160, 180, and 200 °C. Plasticizer-free PVC powder degradation kinetics and that of plasticized films were also obtained thermogravimetrically at temperatures ranging from 160 to 220 °C. Plasticizer-free PVC powder degradation and spectroscopically monitored degradation of plasticized PVC films occurred with the same apparent activation energy of ≈150 kJ mol−1. No difference in degradation kinetics of films plasticized with DEHP and TOTM was detected.  相似文献   

11.
Thermal stability of solution-cast blends of poly(vinylchloride) and NR-b-PU block copolymers of three different chain extender diols was studied by thermogravimetry. Thermal degradation of individual components and their blends were investigated with special reference to blend ratio. As the block copolymer content in the blends increased their thermal stability was also found to increase. Enhanced thermal stability of PVC is believed due to the favorable interaction with PVC and the PU hard segments of the block copolymer. DTG curves were used for the determination of different stages involved in the degradation. Activation energy for degradation was determined from Coats–Redfern plot.  相似文献   

12.
This paper describes a method to obtain polymer blends by the absorption of a liquid solution of monomer, initiator, and a crosslinking agent in suspension type porous poly(vinyl chloride) (PVC) particles, forming a dry blend. These PVC/monomer dry blends are reactively polymerized in a twin‐screw extruder to obtain the in situ polymerization in a melt state of various blends: PVC/poly(methyl methacrylate) (PVC/PMMA), PVC/poly(vinyl acetate) (PVC/PVAc), PVC/poly(butyl acrylate) (PVC/PBA) and PVC/poly(ethylhexyl acrylate) (PVC/PEHA). Physical PVC/PMMA blends were produced, and the properties of those blends are compared to reactive blends of similar compositions. Owing to the high polymerization temperature (180°C), the polymers formed in this reactive polymerization process have low molecular weight. These short polymer chains plasticize the PVC phase reducing the melt viscosity, glass transition and the static modulus. Reactive blends of PVC/PMMA and PVC/PVAc are more compatible than the reactive PVC/PBA and PVC/PEHA blends. Reactive PVC/PMMA and PVC/PVAc blends are transparent, form single phase morphology, have single glass transition temperature (Tg), and show mechanical properties that are not inferior than that of neat PVC. Reactive PVC/PBA and PVC/PEHA blends are incompatible and two discrete phases are observed in each blend. However, those blends exhibit single glass transition owing to low content of the dispersed phase particles, which is probably too low to be detected by dynamic mechanical thermal analysis (DMTA) as a separate Tg value. The reactive PVC/PEHA show exceptional high elongation at break (~90%) owing to energy absorption optimized at this dispersed particle size (0.2–0.8 µm). Copyright © 2005 John Wiley & Sons, Ltd.  相似文献   

13.
This paper presents an initial attempt at describing poly(vinyl chloride) (PVC) thermal degradation through a semi-detailed and lumped kinetic model. A mechanism of 40 species and pseudocomponents (molecules and radicals) involved in about 250 reactions permits quite a good reproduction of the main characteristics of PVC degradation and volatilization. The presence of the two step mechanism—the first step of which corresponds to dehydrochlorination and the second to the tar release and residue char formation—are correctly predicted both in quantitative terms and in the temperature ranges. The model was validated by comparison with several thermo gravimetric analyses, both dynamic at different heating rates, and isothermal. When compared with the typical one step global apparent degradation models, the approach proposed here spans quite large operative ranges, especially when it comes to predicting product distributions. The initial results of these product predictions, even though quite preliminary, are encouraging and confirm the validity of the model.  相似文献   

14.
A series of blends of poly(vinyl chloride) (PVC) and polyaniline (PANI) was prepared by solution casting and investigated by methods of thermal analysis, namely thermogravimetric analysis (TG), coupled with Fourier transform infrared spectroscopy (TG-FT/IR) and differential scanning calorimetry (DSC). It was found that the thermal stability of this polymer system depends on the composition of blend; the main product of prevailing PVC decomposition process — hydrogen chloride — seems to play specific role during degradation since it can react with PANI structures, characterized by different protonation degree. This revised version was published online in August 2006 with corrections to the Cover Date.  相似文献   

15.
A set of materials has been prepared by sol–gel process containing different quantities of hydroxyapatite (0, 2.5 and 5% HAp w/w) using as silica precursors glycidyloxypropyltrimethoxysilane (GPTMS) and triethoxyvinylsilane (VTES). In order to optimize the curing process to obtain sintherized systems (inorganic network) or hybrid systems (organic–inorganic) a TG and FTIR studies have been developed and degradation kinetic triplet parameters were obtained (the activation energy, pre-exponential factor, and function of degree of conversion). The kinetic study was analyzed by means of an integral isoconversional non-isothermal procedure (model free), and the kinetic model was determined by the Coats–Redfern method and through the compensation effect (IKR). All the systems followed the n = 6 kinetic model. The addition of HAp increases the thermal stability of the systems. The isothermal degradation was simulated from non-isothermal data, and the curing process could be defined to obtain the two types of materials. Temperature under 250 °C allows the formation of hybrids networks.  相似文献   

16.
通过UV-Vis、FTIR、DSC、以及色差、力学性能的测试表征,实时追踪分析了在紫外光老化过程中,含Pb、Sn以及Ca-Zn热稳定剂的PVC体系微观结构和宏观性能的演变过程.结果表明,在相同光老化条件下,PVC/Pb、PVC/Sn和PVC/Ca-Zn体系的微观结构变化规律基本一致,过程中主要的化学反应是,大分子吸收光能后,发生脱HCl生成共轭双键的反应、生成羰基的氧化反应、交联反应和降解反应;不同热稳定剂的作用,主要表现在对于微观结构变化的幅度和动力学过程的影响不同.相应地,3种体系的外观色差和力学性能的变化规律也相似,但色差的变化程度和速度以及老化后力学性能的保持率因所含热稳定剂的不同而不同,其中含Sn体系的颜色稳定性最好,含Pb体系的力学性能保持率最高。  相似文献   

17.
利用二次电子衬度曲线法测定了聚氯乙烯甲基丙烯酸甲酯丁二烯苯乙烯共聚物(PVCMBS)共混物冲击断面的形貌特征及对应的分形维数值.结果表明,材料的断口或微观结构并不是严格的分形结构,这种自相似性仅存在于一定尺码范围内,不同断面形貌特征所对应的分形维数测量值不同,随着MBS用量增加,PVCMBS共混物缺口冲击强度随满足自相似原理的形貌特征所对应的分形维数值增大而增大.本文从理论上讨论了材料断裂韧性与分形维数的关系.  相似文献   

18.
The aim of this work was to study the thermo-oxidative dehydrochlorination of rigid and plasticised poly(vinyl chloride)/poly(methyl methacrylate) blends. For that purpose, blends of variable compositions from 0 to 100 wt% were prepared in the presence (15, 30 and 50 wt%) and in the absence of diethyl-2-hexyl phthalate as plasticiser. Their miscibility was investigated by using differential scanning calorimetry (DSC) and Fourier transform infrared spectroscopy (FTIR). Their thermo-oxidative degradation at 180 ± 1 °C was studied and the amount of HCl released from PVC was measured by a continuous potentiometric method. Degraded samples were characterised, after purification, by FTIR spectroscopy and UV-visible spectroscopy. The results showed that the two polymers are miscible up to 60 wt% of poly(methyl methacrylate) (PMMA). This miscibility is due to a specific interaction of hydrogen bonding type between carbonyl groups (CO) of PMMA and hydrogen (CHCl) groups of PVC as shown by FTIR analysis. On the other hand, PMMA exerted a stabilizing effect on the thermal degradation of PVC by reducing the zip dehydrochlorination, leading to the formation of shorter polyenes.  相似文献   

19.
The degradation of the binary polymer blends, poly(vinyl acetate)/poly(vinyl chloride), poly(vinyl acetate)/poly(vinylidene chloride) and poly(vinyl acetate)/polychloroprene has been studied by using thermal volatilization analysis, thermogravimetry, evolved gas analysis for hydrogen chloride and acetic acid, and spectroscopic methods. For the first two systems named, strong interaction occurs in the degrading blend, but the polychloroprene blends showed no indication of interaction. In the PVA/PVC and PVA/PVDC blends, hydrogen chloride from the chlorinated polymer causes substantial acceleration in the deacetylation of PVA. Acetic acid from PVA destabilizes PVC but has little effect in the case of PVDC because of the widely differing degradation temperatures of PVA and PVDC. The presence of hydrogen chloride during the degradation of PVA results in the formation of longer conjugated sequences, and the regression in sequence length at high extents of deacetylation found for PVA degraded alone is not observed.  相似文献   

20.
The thermal decomposition under non-oxidative conditions of a copolymer of vinylidene cyanide (VCN) and 2,2,2-trifluoroethyl methacrylate (MATRIF) was investigated by thermogravimetry (TG) and Pyrolysis-GC-MS. The type and composition of the pyrolytic products and the shape of the TG curve indicate that both the main thermal degradation process, with onset at 368 °C, and a minor weight loss at around 222 °C are mainly associated with random main-chain scission. The kinetic parameters were determined by means of dynamic and, in the case of the main degradation stage, also isothermal methods. The results obtained from the dynamic methods (Friedman, Flynn-Wall-Ozawa, and Kissinger, respectively) are in good agreement with those obtained from isothermal TG data. The activation energy was in the 177-213 kJ/mol range for the first stage, and 224-295 kJ/mol for the second stage, the highest respective values being determined from the kinetic analysis according to the Kissinger method.  相似文献   

设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号