首页 | 本学科首页   官方微博 | 高级检索  
相似文献
 共查询到20条相似文献,搜索用时 31 毫秒
1.
Thirty-nine new submillimetre laser lines in CH2F2 and twelve in CD2Cl2 have been obtained in a Fabry-Perot FIR resonator by optically pumping with a CW12C18O2 laser. The wavelength range obtained for CH2F2 is 126m to 1091m and for CD2Cl2 212m to 774m. The wavelength measurements are accurate to within 5.10–3. The relative polarisations of the pump laser and the FIR laser output were also determined. Tentative assignments of the IR and FIR transitions were made using existing microwave data.  相似文献   

2.
Eleven new CW far infrared (FIR) laser lines have been observed in the 600 m–1200 m range from the CF2Cl2 (Fluorocarbon 12) molecule optically pumped by a CO2 laser. A 510–4–10–3 accuracy is achieved in the measurement of the FIR wavelengths.The frequency offset between the CO2 pump center and the absorption line centers are measured using the transferred Lamb dip technique. Owing to a recent spectroscopic study of the CF2 35Cl2 molecule three lines may be assigned with great confidence as rotational transitions in thev 6 vibrational band 923 cm–1 of this main isotope.  相似文献   

3.
We report here the discovery of 13 new far-infrared laser lines from12CH2F2 and seven new lines from13CH2F2. Most of the new lines were pumped by high-J lines of the 9R branch of a cw-CO2 laser. Wavelengths range from 97.6 to 616.18 μm. Frequency, pump offset, relative polarization, and relative intensity were measured for most of the new lines.  相似文献   

4.
Fifty-five new submillimeter laser lines from optically pumped CD2Cl2, have been obtained in a FIR metallic waveguide resonator. Twenty-seven lines, ranging from 184 m to 1387 m, and twenty-eight lines, from 219 m to 888 m, have been observed when using CW CO2 laser and CW N2O laser optical pumping, respectively. The accuracy of wavelength measurements are of the order of 3.10–3.  相似文献   

5.
The frequencies of 42 far-infrared laser lines have been measured by mixing with high-order harmonics of microwave frequencies in a Josephson junction. A total of 5 emissions between 334 and 1887 m have been measured from12C16O2-pumped methyl chloride (CH3Cl) and 37 emissions between 116 and 1092 m in12C18O2-pumped difluoromethane (CH2F2). Additional data is given on the laser emission characteristics.Division of Electrical Science, National Physical Laboratory  相似文献   

6.
We have obtained laser action on 34 far infrared lines for the first time in fully deuterated methyl alcohol with the13C isotope (13CD3OD), and we have measured the frequency of 13 lines. The molecule was pumped by a cw CO2 laser. We have measured the wavelength, the relative polarization, the relative intensity of most lines, the frequency, and the CO2 pump frequency offset of the strongest lines. The new lines are distributed in the wavelength region from 75.27 m to 464.7 m.Supported in part by a joint grant with the U.S. National Science Foundation grant # INT 80-19014 and the Brazilian Conselho Nacional de Pesquisas (CNPq).  相似文献   

7.
Heterodyne frequency measurements are reported for twenty optically pumped laser lines from various molecules including COF2, CD3F,13CD3F, and C2H5I.  相似文献   

8.
Li2O-ZrO2-SiO2: Ho3+ glasses mixed with three interesting d-block elemental oxides, viz., Nb2O5, Ta2O5 and La2O3, were prepared. Optical absorption and photoluminescence spectra of these glasses have been recorded at room temperature. The luminescence spectra of Nb2O5 and Ta2O5 mixed Li2O-ZrO2-SiO2 glasses (free of Ho3+ ions) have also exhibited broad emission band in the blue region. This band is attributed to radiative recombination of self-trapped excitons (STEs) localized on substitutionally positioned octahedral Ta5+ and Nb5+ ions in the glass network. The Judd-Ofelt theory was successfully applied to characterize Ho3+ spectra of all the three glasses. From this theory various radiative properties, like transition probability A, branching ratio βr and the radiative lifetime τr, for 5S2 emission levels in the spectra of these glasses have been evaluated. The radiative lifetime for 5S2 level of Ho3+ ions has also been measured and quantum efficiencies were estimated. Among the three glasses studied the La2O3 mixed glass exhibited the highest quantum efficiency. The reasons for such higher value have been discussed based on the relationship between the structural modifications taking place around the Ho3+ ions.  相似文献   

9.
We report for the first time wavelength, relative polarization, and frequency measurements for 47 new cw FIR laser lines in the wavelength region from 120 to 1714 m, all obtained by optically pumping CD2F2 with a CO2 laser. Relative output powers were also measured. For comparison, the 189.8 m line pumped by RI(34) is nearly five times as efficient as the 118.8 m methyl alcohol line.Contribution of the U.S. Government, not subject to copyright.  相似文献   

10.
Alkaline hexafluorostantanate red phosphors Na2SnF6:Mn4+ and Cs2SnF6:Mn4+ are synthesized by chemical reaction in HF/NaMnO4 (CsMnO4)/H2O2/H2O mixed solutions immersed with tin metal. X-ray diffraction patterns suggest that the synthesized phosphors have a tetragonal symmetry with the space group D4h14 (Na2SnF6:Mn4+) and a trigonal symmetry with the space group D3d3 (Cs2SnF6:Mn4+). Photoluminescence (PL) analysis, PL excitation (PLE) spectroscopy, and the Raman scattering techniques are used to investigate the optical properties of the phosphors. The Franck-Condon analysis of the PLE data yields the Mn4+-related optical transitions to occur at ∼2.39 and ∼2.38 eV (4A2g4T2g) and at ∼2.83 and ∼2.76 eV (4A2g4T1g) for Na2SnF6:Mn4+ and Cs2SnF6:Mn4+, respectively. The crystal field parameters (Dq) of the Mn4+ ions in the Na2SnF6 and Cs2SnF6 hosts are determined to be ∼1930 and ∼1920 cm−1, respectively. Temperature-dependent PL measurements are performed from 20 to 440 K in steps of 10 K, and the obtained results are interpreted by taking into account the Bose-Einstein occupation factor. Comprehensive discussion is given on the phosphorescent properties of a family of Mn4+-activated alkaline hexafluoride salts.  相似文献   

11.
We describe the structural properties and electrical characteristics of thin thulium oxide (Tm2O3) and thulium titanium oxide (Tm2Ti2O7) as gate dielectrics deposited on silicon substrates through reactive sputtering. The structural and morphological features of these films were explored by X-ray diffraction, X-ray photoelectron spectroscopy, secondary ion mass spectrometry, and atomic force microscopy, measurements. It is found that the Tm2Ti2O7 film annealed at 800 °C exhibited a thinner capacitance equivalent thickness of 19.8 Å, a lower interface trap density of 8.37 × 1011 eV−1 cm−2, and a smaller hysteresis voltage of ∼4 mV than the other conditions. We attribute this behavior to the Ti incorporated into the Tm2O3 film improving the interfacial layer and the surface roughness. This film also shows negligible degrees of charge trapping at high electric field stress.  相似文献   

12.
The potential energy surface and dipole moment surfaces of the ã4A2 electronic state of CH2+ are calculated ab initio using an augmented correlation-consistent polarized valence quadruple-ζ (aug-cc-pVQZ) basis set, with the incorporation of dynamical correlation using the coupled cluster method with single and double excitations and perturbatively connected triple excitations [CCSD(T)]. We use these surfaces in the MORBID program system to calculate rotation and rotation-vibration term values for ã-state CH2+, CD+2, and CHD+ and to simulate the rotation and rotation-vibration absorption spectrum of CH2+ in the ã4A2 electronic state. Our work is motivated by studies of CH2+ that use the Coulomb explosion imaging technique and by the goal of predicting spectra that may be obtained from discharge sources. Although the ã state is the lowest-lying excited state above the X?/Ã ground state pair, it turns out to be relatively high-lying, and we determine that Te(ã)=30447.5 cm−1. The equilibrium bond angle for ã-state CH2+ is only 77.1°; as a result the asymmetric top κ value is close to 0, and the molecule is equally far from the oblate and prolate symmetric top limits in this electronic state.  相似文献   

13.
In this work, the complete matrix of optical spectral levels in trigonal symmetry of 3d2 (3d8) ions are established on basis of strong field coupling mechanism by using two spin–orbit coupling parameters model. The contribution of the spin–orbit coupling of ligand to the optical spectra has been included in these formulas. As an application, the optical spectra of Cr4+ in Y2Ti2O7 and Y2Sn2O7 have been studied by the complete diagonalization (energy matrix) method. The covalent effect has been studied and the difficulty about Dq parameter in explanation of optical spectra of Cr-doped Y2Ti2O7 and Y2Sn2O7 is removed. The theoretical results are in good agreement with observed data.  相似文献   

14.
The Ca2Al2SiO7 samples doped with Ce3+ and Eu2+ are synthesized via a high temperature solid-state reaction. Ca2Al2SiO7: Ce3+ emits a strong UV-violet emission while Ca2Al2SiO7: Eu2+ emits a blue-green emission. The Stokes shift of the latter is greater due to a stronger crystal repulsion from ligands to Eu2+ ions. Ca2Al2SiO7: Ce3+ exhibits a stronger initial intensity and longer duration of afterglow due to the higher liberated probability of the trapped carriers. The thermoluminescence curves reveal that at least three traps exist in the phosphors. Ca2+ vacancies may enhance the electron trapping and then lead to a stronger afterglow. A possible explanation will be provided.  相似文献   

15.
Nanocrystalline Y2Si2O7:Eu phosphor with an average size about 60 nm is easily prepared using silica aerogel as raw material under ultrasonic irradiation and annealing temperature at 300-600 °C and this nanocrystalline decomposes into Y2O3:Eu and silica by heat treatment at 700-900 °C. The excitation broad band centered at 283 and 254 nm results from Eu3+ substituting for Y3+ in Y2Si2O7 and Y2O3/SiO2, respectively. Compared with Y2O3:Eu/SiO2 crystalline, the PL excitation and emission peaks of Y2Si2O7:Eu nanocrystalline red-shift and lead to the enhance of its luminescence intensity due to the different chemical surroundings of Eu3+ in above nanocrystallines. The decrease of PL intensity may be ascribed to quenching effect resulting from more defects in Y2O3:Eu/SiO2 crystalline.  相似文献   

16.
We have measured the output powers and relative polarizations of 66 cw FIR laser lines from CH2DOH (including 50 not previously reported), which were optically pumped by a CO2 laser. The frequencies of 43 of these lines were measured relative to stabilized CO2 lasers.  相似文献   

17.
通过固相反应法制备了Er3+/Yb3+共掺杂ZrO2-Al2O3粉末的样品,并对样品在980nm激光激发下的上转换发光特性进行了研究.从发射光谱可以发现,在可见光范围内有3个强的发光带,一个位于654nm附近的红光带和两个分别位于545nm、525nm附近的绿光带,分别对应于Er3+离子的以下辐射跃迁:4F9/24I15/24S3/24I15/22H11/24I15/2.其中又以Er3+离子的4F9/24I15/2跃迁产生的红色荧光辐射最强.对其上转换发光机制进行了分析,发现这三个发光过程都是双光子过程.对样品粉末进行了XRD检测,发现ZrO2主要以立方相为主,并且计算得到了这种立方结构的晶格常数.Al2O3固溶于ZrO2中,Al3+嵌入ZrO2后产生氧空位,导致ZrO2晶体的对称性降低,这种结构变化更有利于提高上转换效率,即上转换发光强度增强. 关键词: 3+/Yb3+')" href="#">Er3+/Yb3+ 上转换 2-Al2O3')" href="#">ZrO2-Al2O3 荧光 稀土  相似文献   

18.
谭鑫鑫  吕树臣 《光子学报》2014,39(7):1169-1175
采用共沉淀法制备了纳米晶ZrO2-Al2O3∶Er3+发光粉体.所制备的粉体室温下具有Er3+离子特征荧光发射,主发射在绿光,其中位于547 nm、560 nm的绿光最强,并得出稀土离子与基质之间有能量传递.对不同煅烧温度下的样品研究表明:因不同温度下所制得的样品晶相不同.研究了纳米晶ZrO2-Al2O3∶Er3+及ZrO2-Al2O3∶Er3+/Yb3+的上转换发光,并分析了上转换的跃迁机制.发现ZrO2-Al2O3∶Er3+的绿光为双光子过程,而ZrO2-Al2O3∶Er3+、Yb3+的上转换光谱中,红光和绿光也为双光子过程,而极弱的蓝光为三光子过程.讨论了Er3+的浓度猝灭现象.最适宜掺杂浓度的原子分数为2%(Er3+/Zr4+).  相似文献   

19.
崔彩娥  王森  黄平 《物理学报》2009,58(5):3565-3571
采用溶胶凝胶法制备了Sr3Al26:Eu2+,Dy3+红色长余辉发光材料,利用X射线衍射仪对材料的物相进行了分析,结果表明,1200℃下制备的样品的物相为Sr3Al26,少量的Eu和Dy掺杂没有影响样品的相组成.采用荧光分光光度计、照度计测定了样品的发光特性.结果表明Sr3Al2关键词: 红色长余辉 3Al26')" href="#">Sr3Al26 溶胶凝胶法  相似文献   

20.
Twenty-five new laser lines have been obtained in the wavelength region from 155 to 830 μm by optically pumping the CD2Cl2 (deuterated dichloromethane) molecule with a CW CO2 laser having a tunability range of 300 MHz. The wavelength, polarization relative to that of CO2 pumping radiation, and offset relative to the CO2 center frequency were determined for all of the new lines and some other already known laser emissions. For all of them we give also the relative intensity and the optimum pressure of operation. Permanent address: Depto de Física e Química da FEIS — UNESP 15.378-000 Ilha Solteira-SP, Brazil  相似文献   

设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号