1.
Novel X‐type polyurethane 5 containing 4‐(2′,2′‐dicyanovinyl)‐6‐nitroresorcinoxy groups as nonlinear optical (NLO) chromophores, which constitute parts of the polymer backbone, was prepared and characterized. Polyurethane 5 is soluble in common organic solvents such as acetone and N,N‐dimethylformamide. It shows thermal stability up to 280 °C from thermogravimetric analysis with a glass transition temperature (Tg) obtained from differential scanning calorimetry thermogram of around 120 °C. The second harmonic generation (SHG) coefficient (d33) of poled polymer film at 1064‐nm fundamental wavelength is around 6.12 × 10?9 esu. The dipole alignment exhibits a thermal stability even at 5 °C higher than Tg, and there was no SHG decay below 125 °C due to the partial main chain character of the polymer structure, which is acceptable for NLO device applications. © 2012 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem, 2013  相似文献   

2.
A novel Y‐type poly[iminocarbonyloxyethyl‐5‐methyl‐4‐{2‐thiazolylazo‐4‐(1,2,2‐tricyanovinyl)}resorcinoxyethyloxycarbonylimino‐(3,3′‐dimethoxy‐4,4′‐biphenylene)] 4 containing 5‐methyl‐4‐{5‐(1,2,2‐tricyanovinyl)‐2‐thiazolylazo}resorcinoxy groups as nonlinear optical (NLO) chromophores, which constitute part of the polymer backbone, was prepared and characterized. Polyurethane 4 is soluble in common organic solvents such as acetone and N,N‐dimethylformamide. It showed a thermal stability up to 250 °C in thermogravimetric analysis thermogram and the glass‐transition temperature (Tg) obtained from differential scanning calorimetry thermogram was around 118 °C. The second harmonic generation coefficient (d33) of poled polymer films at 1560 nm fundamental wavelength was around 8.43 × 10?9 esu. The dipole alignment exhibited a thermal stability even at 12 °C higher than Tg, and there was no SHG decay below 130 °C due to the partial main‐chain character of the polymer structure, which is acceptable for NLO device applications. © 2010 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 48: 1166–1172, 2010  相似文献   

3.
Novel Y‐type polyester 4 containing 5‐methyl‐4‐{5‐(1,2,2‐tricyanovinyl)‐2‐thiazolylazo}resorcinoxy groups as nonlinear optical (NLO) chromophores, which are parts of the polymer backbone, was prepared, and its NLO properties were investigated. Polyester 4 is soluble in common organic solvents such as N,N‐dimethylformamide and dimethylsulfoxide. Polymer 4 shows a thermal stability up to 250 °C from thermogravimetric analysis with glass‐transition temperature obtained from differential scanning calorimetry of approximately 94 °C. The second harmonic generation (SHG) coefficient (d33) of poled polymer film at 1560‐nm fundamental wavelength is 8.12 × 10?9 esu. The dipole alignment exhibits a thermal stability even at 6 °C higher than glass‐transition temperature (Tg), and no significant SHG decay is observed below 100 °C due to the partial main‐chain character of polymer structure, which is acceptable for NLO device applications. © 2011 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem, 2011  相似文献   

4.
Two new semiconducting polymers poly{4,8‐bis(4‐decylphenylethynyl)benzo[1,2‐b:4,5‐b′]difuran} ( P1 ) and poly {4,8‐bis(4‐decylphenylethynyl)benzo[1,2‐b:4,5‐b′]difuran‐alt‐4,8‐bis(4‐decylphenylethynyl)benzo[1,2‐b:4,5‐b′]dithiophene} ( P2 ) have been synthesized. These polymers were tested in bulk heterojunction solar cells yielding power conversion efficiencies of 1.19% for P1 and 0.79% for P2 . The surface morphology of the solar cell devices indicated that both the polymers display a granular morphology with smoother films displaying higher power conversion efficiencies. © 2012 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem, 2012  相似文献   

5.
Novel X‐type polyurethane 4 containing 4‐(4‐nitrophenylazo)‐6‐nitroresorcinoxy groups as nonlinear optical (NLO) chromophores, which are parts of the polymer main chains, was prepared and characterized. Polyurethane 4 is soluble in common organic solvents such as acetone and N,N‐dimethylformamide. It shows thermal stabilities up to 270 °C from thermogravimetric analysis with glass transition temperature obtained from differential scanning calorimetry of about 134 °C. The second harmonic generation (SHG) coefficient (d33) of poled polymer film at 1064 nm fundamental wavelength is 5.37 × 10?9 esu. Polymer 4 exhibits a thermal stability up to Tg, and no significant SHG decay is observed below 135 °C, which is acceptable for NLO device applications. © 2013 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2014 , 52, 760–766  相似文献   

6.
A series of polyurethane hybrid networks have been synthesized using octakis(m‐isoprenyl‐α,α′‐dimethylbenzylisocyanato dimethylsiloxy) octasilsesquioxane (Q8M8TMI) as a crosslinking agent. The formation of the urethane linkages within the polyurethane hybrids was confirmed by photoacoustic FTIR spectroscopy. The TGA and DSC studies demonstrated that the incorporation of the POSS crosslinking agents altered the thermal properties of the polyurethanes, and that this was dependent on the length of the polyethylene glycol chain. © 2013 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2013 , 51, 5038–5045  相似文献   

7.
1‐{3,4‐Di‐(2‐hydroxyethoxy)phenyl}‐2‐(2‐thiophenyl)ethene (5) was prepared and condensed with terephthaloyl chloride to yield polyester (6). Polymer 6 was reacted with tetracyanoethylene to give a new Y‐type polyester (7) containing 1‐(3,4‐dioxyethoxy)phenyl‐2‐{5‐(2,2,3‐tricyanovinyl)‐2‐thiophenyl)}ethenyl groups as NLO‐chromophores, which are components of the polymer backbones. Polyester 7 is soluble in common organic solvents such as N,N‐dimethylformamide and acetone. Polymer 7 showed a thermal stability up to 300 °C in thermogravimetric analysis with glass transition temperature (Tg) obtained from differential scanning calorimetry near 126 °C. The second harmonic generation (SHG) coefficient (d33) of poled polymer film at the 1560 nm fundamental wavelength was around 6.57 × 10?9 esu. The dipole alignment exhibited high thermal stability up to the Tg, and there was no SHG decay below 125 °C due to the partial main‐chain character of polymer structure, which is acceptable for NLO device applications. © 2009 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 47: 1911–1919, 2009  相似文献   

8.
2,4‐Bis‐(3,4‐dicarboxyphenylcarboxyethoxy)‐1‐(2,2‐dicyanovinyl)benzene dianhydride (4) was prepared and reacted with 4,4′‐oxydianiline, 4,4′‐diaminobenzanilide and 4,4′‐(hexafluoroisopropylidene)dianiline to yield novel Y‐type polyimides 5‐7 containing 2,4‐dioxybenzylidenemalononitrile groups as nonlinear optical (NLO) chromophores, which constitute parts of the polymer backbone. The resulting polyimides 5‐7 are soluble in polar solvents such as dimethylsulfoxide and N,N‐dimethylformamide. Polymers 5‐7 showed a thermal stability up to 330 °C in thermogravimetric analysis thermograms with Tg values obtained from differential scanning calorimetry thermograms in the range 179–194 °C. The second harmonic generation (SHG) coefficients (d33) of poled polymer films at the 1064 nm fundamental wavelength were around 5.56 × 10?9 esu. The dipole alignment exhibited exceptionally high thermal stability even at 20 °C higher than the glass‐transition temperature there was no SHG decay below 215 °C because of the partial main‐chain character of polymer structure, which is acceptable for NLO device applications. © 2008 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 46: 3078–3087, 2008  相似文献   

9.
A series of dicyanomethylene‐substituted polymers having Y‐type molecular architecture were synthesized by Knoevenagel condensation reaction. The polymers were found to be soluble in organic solvents like tetrahydrofuran and chloroform. From gel permeation chromatography, the molecular weights of the polymers were found to be in the range of 15,300–33,800 g/mol. Thermal analysis showed that the polymers were stable up to 350 °C with glass transition temperature (Tg) in the range of 129–212 °C. These polymers were found to form good optical quality films. The order parameter was calculated to be in the range of 0.01–0.48. Atomic force microscopy indicated prominent morphology changes due to alignment of dipoles after poling. By using Nd:YAG laser of 1064 nm, angular dependence and temperature dependence of second‐harmonic generation intensity were investigated. The geometry optimization, shape of polymers, and restricted torsion angle between acceptor and donor substituents (push–pull system) were calculated. © 2012 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem, 2013  相似文献   

10.
Liquid‐crystalline, segmented polyurethanes with methoxy–biphenyl mesogens pendant on the chain extender were synthesized by the conventional prepolymer technique and esterification reaction. Two, side‐chain, liquid‐crystalline (SCLC) polyurethanes with mesogens having spacers of six and eight methylene units were prepared. The structures of the mesogenic units and SCLC polyurethanes were confirmed by Fourier transform infrared spectroscopy and 1H NMR. Polymer properties were also examined by solubility tests, water uptakes, and inherent viscosity measurements. Differential scanning calorimetry studies indicated that the transition temperature of the isotropic to the liquid‐crystalline phase decreased with increasing spacer length. Wide‐angle X‐ray diffraction (WAXD) studies revealed the existence of liquid‐crystalline phases for both SCLC polyurethanes. Polarized optical microscopic investigations further confirmed the thermotropic liquid‐crystalline behaviors and nematic mesophases of both samples. Thermogravimetric analysis displayed better thermal stabilities for both SCLC polymers and indicated that the presence of mesogenic side chains may increase the thermal stability of segmented polyurethanes. © 2003 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 42: 290–302, 2004  相似文献   

11.
2,5‐Bis‐(3,4‐dicarboxyphenylcarboxyethoxy)‐4′‐nitrostilbene dianhydride was prepared and reacted with 1,4‐phenylenediamine, 4,4′‐oxydianiline, 4,4′‐diaminobenzanilide, and 4,4′‐(hexafluoroisopropylidene)dianiline to yield unprecedented novel T‐type polyimides ( 4 – 7 ) containing 2,5‐dioxynitrostilbenyl groups as nonlinear optical chromophores, which constituted parts of the polymer backbones. 4 – 7 were soluble in polar solvents such as acetone and N,N‐dimethylformamide. They showed thermal stability up to 300 °C in thermogravimetric analysis thermograms; the glass‐transition temperatures obtained from differential scanning calorimetry thermograms were around 153 °C. The second harmonic generation (SHG) coefficients (d33) of poled polymer films at the 1064‐cm?1 fundamental wavelength were around 4.35 × 10?9 esu. The dipole alignment exhibited exceptionally high thermal stability even at 45 °C higher than the glass‐transition temperature, and there was no SHG decay below 200 °C because of the partial main‐chain character of the polymer structure, which was acceptable for nonlinear optical device applications. © 2004 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 42: 3189–3199, 2004  相似文献   

12.
Four linear polymers containing pendant azo moiety were synthesized through click chemistry for second‐order nonlinear optical study. The polymers were found soluble in most of the polar organic solvents such as tetrahydrofuran (THF), chloroform, and dimethyl formamide (DMF). The polymers showed thermal stability up to 300 °C and glass transition temperatures (Tg) in the range of 120–140 °C. The molecular weights (Mw) of these polymers (measured by gel permeation chromatography) were in the range 37,900–55,000 g/mol. The polymers were found to form optically transparent films by solution casting from THF solution. Order parameters were calculated from UV–vis absorption spectra. The morphology changes in the films after poling were characterized by atomic force microscopy. The angular dependence, temperature dependence, and time dependence of second harmonic generation (SHG) intensity were obtained by using 1064 nm Nd:YAG laser. The SHG intensity remained unchanged up to 95 °C. At room temperature, it remained stable up to 8 days after initial drop of about 14%. © 2012 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem, 2012  相似文献   

13.
A series of novel conjugated poly(aryleneethynylene)s (PAEs) co‐containing BODIPY have been synthesized and characterized, and their third‐order nonlinear optical properties were studied using the Z‐scan technique. Interestingly, by introducing the BODIPY skeleton into the PAE backbone, the polymers showed that their nonlinear optical properties were dependent on the BODIPY component. From poly‐4 to poly‐1, the third‐order nonlinear optical properties of the polymers enhanced regularly with the increase of the BODIPY component of the copolymers, indicating that the BODIPY component played decisive roles in enhancing the nonlinear optical properties. © 2008 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 46: 7401–7410, 2008  相似文献   

14.
2,3-Bis-(3,4-dicarboxyphenylcarboxyethoxy)-4′-nitrostilbene dianhydride (4) was prepared and reacted with 1,4-phenylenediamine, 4,4′-oxydianiline, 4,4′-diaminobenzanilide and 4,4′-(hexafluoroisopropylidene)dianiline to yield novel polyimides 5-8 containing 2,3-dioxynitrostilbenyl groups as NLO-chromophores, which constituted parts of the polymer backbones. The resulting polyimides 5-8 were soluble in polar solvents such as acetone and DMF. Polymers 5-8 showed a thermal stability up to 300 °C in TGA thermograms with Tg values obtained from DSC thermograms in the range of 135-160 °C. The SHG coefficients (d33) of poled polymer films at the 1064 cm−1 fundamental wavelength were around 5.26 × 10−9 esu. The dipole alignment exhibited exceptionally high thermal stability even at 30 °C higher than Tg and there was no SHG decay below 170-190 °C due to the partial main chain character of polymer structure, which was acceptable for NLO device applications.  相似文献   

15.
Poly{bis(4,4′‐tert‐butyl‐2,2′‐bipyridine)–(2,2′‐bipyridine‐5,5′‐diyl‐[1,4‐phenylene])–ruthenium(II)bishexafluorophosphate} ( 3a ), poly{bis(4,4′‐tert‐butyl‐2,2′‐bipyridine)–(2,2′‐bipyridine‐4,4′‐diyl‐[1,4‐phenylene])–ruthenium(II)bishexafluorophosphate} ( 3b ), and poly{bis(2,2′‐bipyridine)–(2,2′‐bipyridine‐5,5′‐diyl‐[1,4‐phenylene])–ruthenium(II)bishexafluorophosphate} ( 3c ) were synthesized by the Suzuki coupling reaction. The alternating structure of the copolymers was confirmed by 1H and 13C NMR and elemental analysis. The polymers showed, by ultraviolet–visible, the π–π* absorption of the polymer backbone (320–380 nm) and at a lower energy attributed to the d–π* metal‐to‐ligand charge‐transfer absorption (450 nm for linear 3a and 480 nm for angular 3b ). The polymers were characterized by a monomodal molecular weight distribution. The degree of polymerization was approximately 8 for polymer 3b and 28 for polymer 3d . © 2004 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 42: 2911–2919, 2004  相似文献   

16.
The annealing at 373 K of ultrastrong, gel‐spun polyethylene (PE) has been studied. At this temperature, the fibers show no significant shrinkage. Still, a significant decrease in the mechanical properties is observed. The fibers have been analyzed with differential scanning calorimetry (DSC), temperature‐modulated differential scanning calorimetry (TMDSC), atomic force microscopy (AFM), and small‐angle X‐ray scattering (SAXS). During the annealing, the glass transition of the intermediate phase is exceeded, as shown by DSC. When split for structure analysis by AFM, the annealed fibers undergo plastic deformation around the base fibrils instead of brittle fracture. The quasi‐isothermal TMDSC experiments are compared to the minor structural changes seen with SAXS and AFM. The loss of performance of the PE fibers at 373 K is suggested to be caused by the oriented intermediate phase, and not by major changes in the structure or morphology. The overall metastable, semicrystalline structure is shown by TMDSC to posses local regions that can melt reversibly. © 2003 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 41: 403–417, 2003  相似文献   

17.
The oxidative copolymerization of indene with styrene, α‐methylstyrene, and α‐phenylstyrene is investigated. Copolyperoxides of different compositions have been synthesized by the free‐radical‐initiated oxidative copolymerization of indene with vinyl monomers. The compositions of the copolyperoxides obtained from the 1H and 13C NMR spectra have been used to determine the reactivity ratios of the monomers. The reactivity ratios indicate that indene forms an ideal copolyperoxide with styrene and α‐methylstyrene and alternating copolyperoxides with α‐phenylstyrene. Thermal degradation studies via differential scanning calorimetry and electron‐impact mass spectroscopy support the alternating peroxide units in the copolyperoxide chain. The activation energy for thermal degradation suggests that the degradation is dependent on the dissociation of the peroxide (? O? O? ) bonds in the backbone of the copolyperoxide chain. Their flexibility has been examined in terms of the glass‐transition temperature. © 2002 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 40: 2004–2017, 2002  相似文献   

18.
In a continuation of our research on new chromophores for photoinitiators (PIs), we investigated a triple‐bond‐containing benzophenone derivative. 1,5‐Diphenyl‐1,4‐pentadiyn‐3‐one ( 2 ) was prepared from phenylacetylene and ethyl formate by a one‐pot reaction. Differential scanning photocalorimetry experiments in lauryl acrylate of 2 showed surprisingly high activity for the double‐bond conversion and rate of polymerization at the lowest PI concentrations and even without any coinitiator. By the application of monomers with abstractable hydrogens, significant improvement in the photoreactivity was observed. Ultraviolet–visible spectroscopy revealed strong absorption up to 350 nm. Steady‐state photolysis experiments proved that the photochemistry of this compound was faster than that of benzophenone. © 2004 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 43: 101–111, 2005  相似文献   

19.
Morphologies of poly(ε‐caprolactone)‐b‐poly(ethylene glycol)‐b‐poly(ε‐caprolactone) (PCL‐PEG‐PCL) triblock copolymer self‐assemblies in the diluted solution and in gel were studied by atomic force microscopy (AFM). The copolymer self‐assembled into wormlike aggregates, of uniform diameter, in water. The wormlike aggregates arranged in order to form separate clusters in the diluted copolymer solution; at a higher copolymer concentration, the clusters became bigger and bigger, and packed together to form gel. Copyright © 2008 John Wiley & Sons, Ltd.  相似文献   

20.
Nontoxic and biodegradable poly(?‐caprolactone)‐b‐poly(ethylene glycol)‐b‐poly(?‐caprolactone) triblock copolymers were synthesized by the solution polymerization of ?‐caprolactone in the presence of poly(ethylene glycol). The chemical structure of the resulting triblock copolymer was characterized with 1H NMR and gel permeation chromatography. In aqueous solutions of the triblock copolymers, the micellization and sol–gel‐transition behaviors were investigated. The experimental results showed that the unimer‐to‐micelle transition did occur. In a sol–gel‐transition phase diagram obtained by the vial‐tilting method, the boundary curve shifted to the left, and the gel regions expanded with the increasing molecular weight of the poly(?‐caprolactone) block. In addition, the hydrodynamic diameters of the micelles were almost independent of the investigated temperature (25–55 °C). The atomic force microscopy results showed that spherical micelles formed at the copolymer concentration of 2.5 × 10?4 g/mL, whereas necklace‐like and worm‐like shapes were adopted when the concentration was 0.25 g/mL, which was high enough to form a gel. © 2006 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 45: 605–613, 2007  相似文献   