L. S. Fomenko S. V. Lubenets V. S. Bobrov A. N. Izotov 《Physics of the Solid State》1998,40(3):453-457
The microhardness of La2CuO4 and La1.85Sr0.15CuO4 crystals is measured in the temperature range 81–292 K, and the influence of various factors on it is investigated. The thermal
activation parameters of the plastic deformation process in the vicinity of the indenter impression are estimated. The change
of the phase state of the compound La1.85Sr0.15CuO4 at the temperature T
0=180 K and the appearance of domain (twin) boundaries formed in the ferroelastic tetraortho transition are not seen in the
temperature dependence of the microhardness. The results of the study are compared with previously published results for YBa2CuO7−x
crystals.
Fiz. Tverd. Tela (St. Petersburg) 40, 493–497 (March 1998) 相似文献
4.
5.
Y. Takahashi 《Zeitschrift für Physik B Condensed Matter》1987,68(4):411-416
The frequency dependence of the reflectivity spectra of doped La2–x
Sr
x
CuO4 in a high frequency region is analyzed based on a picture of correlated hole hopping within a lower Hubbard subband. It is shown that experimental trends are fairly well accounted for by this model, suggesting that the normal state of this compound is quite different from the metallic state. 相似文献
6.
N. Pyka L. Pintschovius A. Yu. Rumiantsev 《Zeitschrift für Physik B Condensed Matter》1991,82(2):177-181
The magnetic excitations in La2CuO4 and La1.9Sr0.1CuO4 were studied by inelastic neutron scattering up to energies of 76 meV. For the pure sample, the results forE15 meV can be well described by conventional spin wave theory with a spin wave velocity c=0.89±0.07 eVÅ. For lower energies, the observed intensities were somewhat higher than expected from spin wave theory and did not follow the Bose-Einstein factor. For the doped sample, the linewidth in constant-E scans at smallE shows a very short correlation length of =7.5 Å only, which is considerably below the value expected from the concentration dependence reported by other authors. An increase of the linewidth for largeE indicates a reduced spin-wave stiffness when compared to the undoped material. However, the use of a spin-wave picture may not be appropriate as the standard expression for damped spin waves in a paramagnetic material is in serious conflict with experiment. 相似文献
7.
We have grown La1.48Nd0.4Sr0.12CuO4/La0.67Sr0.33MnO3 (LNSCO/LSMO) bilayer structure on SrTiO3 (0 0 1) substrate. Both temperature dependences of resistivity and magnetization curves show anomalies between 60 < T < 80 K, where a low-temperature orthorhombic (LTO) to low-temperature tetragonal (LTT) structural transition is observed in LNSCO bulk crystal. It is suggested that the formation of domains in LSMO layer can relax the strains caused by the LTO–LTT transition in LNSCO layer. 相似文献
8.
9.
10.
R. K. Kremer E. Sigmund V. Hizhnyakov F. Hentsch A. Simon K. A. Müller M. Mehring 《Zeitschrift für Physik B Condensed Matter》1992,86(3):319-324
We report on the formation of conducting phases in slightly doped La2CuO4 samples by the existence of a percolative phase separation. Phase separation can be quenched by rapid cooling and can be restored by the application of a 3 T magnetic field. Magnetically polarizable quasiparticles are shown to be formed by hole doping which fuse to form percolative conducting and below 37 K superconducting phases. 相似文献
11.
12.
13.
14.
15.
C. Politis J. Geerk M. Dietrich B. Obst 《Zeitschrift für Physik B Condensed Matter》1987,66(2):141-146
High-T
c superconductivity withT
c onsets up to 42 K (midpoint: 37 K, zero resistance: 34 K) is observed in X-rays homogeneous single phase La1.8Sr0.2CuO4. The quarternary compounds La2–x
Ba
x
CuO4 and La2–x
Sr
x
CuO4 (0x0.3 for Ba and 0x<1 for Sr, depending on the heating conditions) are mixed-valence oxygen defect oxides, characterized by the presence of Cu2+ and Cu3+ simultaneously. These oxides have a tetragonal symmetry (space group:I 4/mmm) similar to that of K2NiF4. We report the synthesis, characterization, and superconducting properties of various high-temperature superconducting La–Ba–Cu–O and La–Sr–Cu–O compounds. Through the substitution of Sr for Ba in these oxygen defect compounds an increasing superconducting transition temperature onset from 28 K to 35 K for La1.8Sr0.1Ba0.1CuO4 was observed. A positive initial pressure coefficient ofdTc/dp=290 (mK/kbar) has been found for La1.8Sr0.2CuO4 with a magnetic susceptibility change consistent with the 100% diamagnetic expectation value. 相似文献
16.
17.
18.
19.
测量了La2CuO4掺Zn样品在不同降温速率下(330K保温05h,然后分别以6Kh,02Ks的速度降到8K)的直流磁化率和热电势.实验结果表明,反铁磁温度TN不随降温速率变化而变化,其直流磁化率也未受很大影响.高温热电势弱的温度依赖关系表明为极化子气体的贡献.热电势在转折温度Tdrop之下的快速降低是由于二维反铁磁涨落的贡献.热电势在更低温度的拐点TS与载流子的局域化有关.降温速率变化时,Tdrop和TS都有明显的变化.Zn掺杂对Tdrop和TS没有明显影响,但导致了更强的载流子局域化.讨论了上述现象产生的物理图像
关键词:
La2CuO4
直流磁化率
热电势 相似文献