1.
Polyacrylamideacrylate (PAN)‐based carbon fibers were submitted to nitric acid oxidation treatments to improve the interfacial adhesion of the carbon fiber (CF)‐reinforced polyimide (CF/PI) composite. The carbon fiber surfaces were characterized by X‐ray photoelectron spectroscopy (XPS). Nitric acid oxidation not only affects the oxygen concentration but also produces an appreciable change in the nature of the chemical functions, namely the conversion of hydroxy‐type oxygen into carboxyl functions. Nitric acid oxidation treatment modifies the element constituting the fiber, the nitrogen concentration being about 1.2 times higher at the fiber external surface compared to the untreated one. The mechanical and tribological properties of the polymide (PI) composites reinforced by the carbon fibers treated with nitric acid oxidation were investigated. Results showed that the tensile strength of the CF/PI composites improved remarkably due to nitric acid treatment along with enhancement in friction and wear performance. Copyright © 2009 John Wiley & Sons, Ltd.  相似文献   

2.
In this paper, the wear performance of an ultra‐high molecular weight polyethylene composites filled with wood fiber were studied using a pin‐on‐disc method. The effects of surface treatment of wood fiber and sliding load and on the friction and wear of the wood fiber/UHMWPE composite are reported. The test results showed that the sliding load is an important controlling factor; its effect is diminished when the wood fiber is modified.  相似文献   

3.
Blending polytetrafluoroethylene (PTFE) to polyamide‐6 (PA6) with and without maleic anhydride‐grafted polytetrafluoroethylene (PTFE‐g‐MA) was produced in a corotating twin screw extruder, where PTFE acts as the polymer matrix and PA6 as the dispersed phase. The effect of PTFE‐g‐MA on the tensile properties and tribological propertiesof PTFE/PA6 polymer blends is studied. Results show that the structural stability and morphology of the blends were greatly improved by PTFE‐g‐PA6 grafted copolymers, which were formed by the in situ reaction of anhydride groups with the amino end groups of PA6 during reactive extrusion forming an imidic linkage. The presence of PTFE‐g‐PA6 in the PTFE continuous phase improves the interfacial adhesion, as a result of the creation of an interphase that was formed by the interaction between the formed PTFE‐g‐PA6 copolymer in situ and both phases. Compared with thePTFE/PA6 without PTFE‐g‐MA, the PTFE/PA6 with PTFE‐g‐MAhad the lowest friction coefficient and wear under given applied load and reciprocating sliding frequency. The interfacial compatibility of the composite prevented the rubbing‐off of PA6, accordingly improved the friction and wear properties of the composite. Copyright © 2009 John Wiley & Sons, Ltd.  相似文献   

4.
The aramid fibers‐reinforced polyimide composites filled with talc were fabricated by means of a hot press molding technique, and mechanical and tribological behaviors were comparatively investigated. Experimental results showed that the elastic modulus of the composites increased with an increase of the talc, but the impact intensity and loss factor decreased. Besides, the coefficient of friction decreased with the increase of the talc content. To contrast the effects of the ultrahigh vacuum (VC), ultraviolet (UV) or atomic oxygen (AO) on the composites, experiments without irradiation or after UV or AO irradiation were conducted. Scanning electron microscopy and X‐ray photoelectron spectroscopy (XPS) analysis showed that UV or AO irradiation can change the surface structure and chemical composition of the polymer because of the photooxidation and chemical erosion. Copyright © 2012 John Wiley & Sons, Ltd.  相似文献   

5.
Wood‐fiber–reinforced polyimide (PI) has been widely used in many engineering fields because of its high specific strength and stiffness. However, PI does not adhere well with wood fibers because it has a low free surface energy. In addition, high viscosity in the melted phase causes poor impregnation. In this study, surface treatment methods, ie, coupling agents with plasma treatment on wood fibers, were applied to increase the interfacial strength between the wood fibers and the PI matrix. The modified wood fiber surfaces were analyzed by X‐ray photoelectron spectroscopy and scanning electron microscopy. To analyze the effectiveness of the surface treatment method, the interlaminar shear strength (ILSS) was measured using the 3‐point bending test. From the test results, the ILSS of the specimens treated with the silane coupling agent after the plasma treatment increased by 48.7% compared with those of the untreated specimens.  相似文献   

6.
Wood fiber–reinforced ultrahigh molecular weight polyethylene (wood fiber/UHMWPE) composites have been filled with acid‐treated clay to enhance the adhesion. According to the modification, the interlaminar shear strength of composites has been greatly improved. X‐ray photoelectron spectroscopy and scanning electron microscopy are used to examine the microscopic properties of resultant composites. The enhanced interlaminar shear strength is attributed to the clay interlock, which improves the wetting between wood fibers and resins.  相似文献   

7.
In this study, the effect of acid‐treated wood fiber modifications on the mechanical behaviors of HDPE/ABS blend is investigated. Wood fiber/HDPE/ABS composites were fabricated by incorporating acid‐treated wood fiber into HDPE/ABS blends. The results showed that both the tensile strength and flexural strength of wood fiber/HDPE/ABS composites were greater than those of HDPE/ABS blend, regardless of wood fiber modification. The results also showed that the impact strength of HDPE/ABS composites is improved by the addition of wood fiber. Scanning electron microscopic (SEM) examination of fractured surfaces showed that the improvement in the mechanical properties of the wood fiber/HDPE/ABS composites was attributed to the improved dispersion of wood fiber in the HDPE/ABS and the better interfacial characteristics caused by the acid treatment of the wood fiber.  相似文献   

8.
Pitch‐based short carbon fibers (CFs) were treated by air oxidation and cryogenic nitrogen, respectively. Thereafter the treated and untreated CFs were incorporated into polyimide (PI) matrix to form composites. The CFs before and after treatment were examined by XPS and SEM.The flexural strength of the specimen was determined in a three‐point test machine and the tribological properties of PI composites sliding against GCr15 steel rings were evaluated on an M‐2000 model ring‐on‐block test rig. The results show that the surface of the treated CFs became rougher. Lots of active groups formed on the CF surface after air oxidation.The treatment can effectively improve the mechanical and tribological properties in their PI composites due to the enhanced fiber‐matrix interfacial bonding. Copyright © 2008 John Wiley & Sons, Ltd.  相似文献   

9.
The effect of air oxidation and ozone surface treatment of carbon fibers (CF) on tribological properties of CF reinforced polytetrafluoroethylene (PTFE) composites under oil‐lubricated condition was investigated. Experimental results revealed that ozone treated CF reinforced PTFE (CF–PTFE) composite had the lowest friction coefficient and wear under various applied loads and sliding speeds compared with untreated and air‐oxidated composites. X‐ray photoelectron spectroscopy (XPS) study of carbon fiber surface showed that, after ozone treatment, oxygen concentration was obviously increased, and the amount of oxygen‐containing groups on CF surfaces was largely increased. The increase in the amount of oxygen‐containing groups enhanced interfacial adhesion between CF and PTFE matrix. With strong interfacial adhesion of the composite, stress could be effectively transmitted to carbon fibers; carbon fibers were strongly bonded with PTFE matrix and large scale rubbing‐off of PTFE was prevented, therefore, the tribological properties of the composite were improved. Copyright © 2009 John Wiley & Sons, Ltd.  相似文献   

10.
Ultra‐high‐molecular‐weight polyethylene (UHMWPE) fibers have been modified by plasma treatment to increase adhesion in high‐density polyethylene (HDPE) matrices. Results showed that surface roughness predominates for modified UHMWPE fibers, indicating that the plasma treatment favors the interaction with HDPE. Unmodified HDPE composite samples gave a lower interlaminar shear strength than did the samples that were incorporated with UHMWPE. The addition of unmodified UHMWPE fibers to the neat HDPE significantly increases interlaminar shear strengths of composites, up to 20 vol%. The oxygen concentration increased from 16.16 %to 21.99%, and the ratio of oxygen to carbon atoms increased significantly from 0.194 to 0.284 after oxygen plasma treatment for 5 minutes with a power of 300 W.  相似文献   

11.
The mechanical strength and modulus of chopped carbon fiber (CF)‐reinforced polybenzoxazine composites were investigated by changing the length of CFs. Tensile, compressive, and flexural properties were investigated. The void content was found to be higher for the short fiber composites. With increase in fiber length, tensile strength increased and optimized at around 17 mm fiber length whereas compressive strength exhibited a continuous diminution. The flexural strength too increased with fiber length and optimized at around 17 mm fiber length. The increase in strength of composites with fiber length is attributed to the enhancement in effective contact area of fibers with the matrix. The experimental results showed that there was about 350% increase in flexural strength and 470% increase in tensile strength of the composites with respect to the neat polybenzoxazine, while, compressive properties were adversely affected. The composites exhibited an optimum increase of about 800% in flexural modulus and 200% in tensile modulus. Enhancing the fiber length, leads to fiber entanglement in the composites, resulted in increased plastic deformation at higher strain. Multiple branch matrix shear, debonded fibers and voids were the failures visualized in the microscopic analyses. Defibrillation has been exhibited by all composites irrespective of fiber length. Fiber debonding and breaking were associated with short fibers whereas clustering and defibrillation were the major failure modes in long fiber composites. Increasing fiber loading improved the tensile and flexural properties until 50–60 wt% of fiber whereas the compressive property consistently decreased on fiber loading. Copyright © 2008 John Wiley & Sons, Ltd.  相似文献   

12.
Interfacial adhesion between the fiber and the matrix in a composite is a primary factor for stress transfer from the matrix to the fiber. In this study, oxygen plasma treatment method was applied to modify the fiber surface for improving interfacial adhesion of aramid fiber‐reinforced poly(phthalazinone ether sulfone ketone) (PPESK) composite. Composite interfacial adhesion properties were determined by interlaminar shear strength (ILSS) using a short‐beam bending test. The composite interfacial adhesion mechanism was discussed by SEM. The changes of chemical composition and wettability for plasma‐treated fiber surfaces stored in air as long as 10 days were investigated by XPS and dynamic contact angle analysis (DCAA), respectively. Results indicated that oxygen plasma treatment was an effective method for improving interfacial adhesion; plasma‐treated fiber surface suffered aging effects during storage in air. Copyright © 2008 John Wiley & Sons, Ltd.  相似文献   

13.
Changes in surface physicochemical structures of polyacrylonitrile‐based carbon fibers resulted from low current density electrochemical oxidation were monitored by scanning electron microscopy (SEM) and X‐ray photoelectron spectroscopy (XPS). The relationship between the interlaminar shear strength (ILSS) values of carbon fiber‐reinforced polymers (CFRPs) and carbon fiber surface chemistry including elemental ratios and the relative content of oxygen‐containing functional groups were researched. SEM results revealed that the electrochemical oxidation got rid of surface contaminants generated during the production process. XPS analysis showed that the relative contents of oxygen and nitrogen increased by 446% and 202%, respectively, after the electrochemical oxidation. Carbon fiber surface chemistry was of paramount importance to the interfacial properties of CFRPs. The higher the carbon fiber surface activity, the better the interfacial bonding was, and an increase in the acidic‐group contents was responsible for a higher ILSS value. However, when the current density increased to 1.0 A/m2, the interfacial bonding between carbon fiber and the epoxy resin became weak which led to the decline in ILSS values. Copyright © 2012 John Wiley & Sons, Ltd.  相似文献   

14.
The effect of different ratios of carbon fiber (CF) reinforcing polyimide (PI) and surface treatment of CF on the microstructure and wear resistance of surface layers was studied. The increase of CF content led to a gradual increase in the Interlaminar shear strength (ILSS) values, and the maximum ILSS value arises when the CF content is 15 vol%, with an improvement of 13.45% compared to virgin CF composites. The increased interfacial adhesion could be contributed mainly to the presence of branched PI at the interface region. SEM of the worn surface confirms that the plasma treatment efficiently improves the interfacial adhesion of CF/PI composite. Copyright © 2017 John Wiley & Sons, Ltd.  相似文献   

15.
PA6 composites with various contents of wood fibers were prepared. The effects of fiber content and ionic liquid surface treatment on the tribological behavior of PA6 composite were studied under different nominal pressures ranging from 50 to 300 N. The tribological mechanisms were discussed based on scanning electron microscopy inspections of the worn surfaces. The surface treatment of wood fibers improves the tribological performance of the neat polymer matrix. The modification can improve O/C and N/C on the surface of wood fiber, while the increase of nitrogen and oxygen content on wood fiber surface can improve the surface polarity of wood fiber and improve the infiltration and bonding between wood fiber and PA6 resin.  相似文献   

16.
In this study, a series of reinforced polyimide (PI)/carbon fiber (CF) composite foams were fabricated through thermal foaming of polyester ammonium salt (PEAS) precursor powders. The PEAS precursor powders containing different contents of chopped CF were synthesized from benzophenone‐3,3′,4,4′‐tetracarboxylic dianhydride (BTDA) and 4,4′‐diaminodiphenyl ether (ODA). The effects of different CF loadings on foaming behavior of PEAS/CF composite precursor powders, final cellular morphology, and physical properties of PI composite foams were investigated. The results revealed that the chopped CF acted as nucleation agent in the foaming process. The dispersion of CF can be evaluated using digital microscope. It is interesting to find that the chopped CF were highly oriented along the direction of cell arrises. As a result, the mechanical properties of PI foams were significantly enhanced owing to the incorporation of chopped CF. Furthermore, the thermal stability of PI composite foams were also slightly improved owing to fine dispersion of CF. In addition, the PI/CF composite foam shows uniform cell size distribution and the best comprehensive physical properties as chopped CF loading at around 6 wt%. Copyright © 2016 John Wiley & Sons, Ltd.  相似文献   

17.
In this work, ozone modification method and air‐oxidationwere used for the surface treatment of polyacrylonitrile(PAN)‐based carbon fiber. The surface characteristics of carbon fibers were characterized by XPS. The interfacial properties of carbon fiber‐reinforced (polyetheretherketone) PEEK (CF/PEEK) composites were investigated by means of the single fiber pull‐out tests. As a result, it was found that IFSS (interfacial shear strength) values of the composites with ozone‐treated carbon fiber are increased by 60% compared to that without treatment. XPS results show that ozone treatment increases the amount of carboxyl groups on carbon fiber surface, thus the interfacial adhesion between carbon fiber and PEEK matrix is effectively promoted. The effect of surface treatment of carbon fibers on the tribological properties of CF/PEEKcomposites was comparativelyinvestigated. Experimental results revealed that surface treatment can effectively improve the interfacial adhesion between carbon fiber and PEEK matrix. Thus the wear resistance was significantly improved. Copyright © 2009 John Wiley & Sons, Ltd.  相似文献   

18.
Surface treatment (ST) of carbon fibers (CF) leads to an enhancement in fiber‐matrix adhesion. However, it deteriorates the strength of a fiber which makes its reinforcing action less effective in a composite. These effects in opposite directions control the net strength of a composite, and hence, the treatment has to be judiciously applied, which would enhance the first factor and minimize the second one. Authors have recently reported on four effective techniques (using various doses) such as treatments with nanoparticles of Ytterbium fluoride (YbF3), cold remote nitrogen–oxygen plasma (CRNOP), γ‐ray irradiation and nitric acid oxidation. Amongst these methods, nitric acid oxidation is studied in depth in the literature, and γ‐ray irradiation is sparingly studied. However, nano‐YbF3 and CRNOP were first time reported in the literature by the authors. However, comparative aspects of all these methods were not addressed. In this paper, these aspects in details are discussed to lay down the right criteria for selection of a ST technique of CF to design the desired performance of a composite. The composites with polyetherimide and treated CF (including untreated) were developed and evaluated for various properties including tribological one. Treated CF based composites exhibited excellent mechanical and tribological properties (under harsh operative conditions with wear rates ≈ 1 × 10?15 m3/Nm and μ ≈ 0.09). It was concluded that for strength and tribo‐performance, different treatments and doses are to be employed. Overall nanosized‐YbF3 treatment of CF proved to be the most promising ST method. Copyright © 2013 John Wiley & Sons, Ltd.  相似文献   

19.
The aim of this investigation was to study the effect of surface thermal oxidation of bamboo/poly(methyl methacrylate) composite by irradiation. Thermal oxidative effects on the surface energy of bamboo fiber were measured by radiation as a function of exposure time and temperature. Oxidized bamboo/poly(methyl methacrylate), after exposure to air at temperatures of 100°C and 110°C, had a range of maximum surface energies from 38 to 41 mJ/m2. Comparisons between Fourier transform infrared carbonyl peak growth and the surface energy showed that both methods detect oxidation, though the increase in surface energy was detected before the carbonyl peak growth was noticeable. The work of adhesion predicted by the surface free energies obtained in this work between a coated calcium carbonate and bamboo fiber changes by 10% due to the oxidation of the polymer at 110°C. The structural results were discussed in the oxidation chemistry of the macromolecule.  相似文献   

20.
《先进技术聚合物》2018,29(2):906-913
Nylon 66 microcomposites with various weight percentage of titanium dioxide (TiO2) were prepared by a twin screw extruder and investigated for mechanical and tribological properties. Mechanical properties of the composite such as tensile strength/modulus, flexural strength/modulus, impact, and compressive strength first showed an increase up to 6 wt% TiO2 followed by a decrease at higher filler loading. The value of heat deflection temperature increased with the increase in wt% of TiO2. Sliding wear tests were performed on pin‐on‐disk equipment under different loads, sliding velocity, and sliding distance combinations. It was found that micro‐TiO2‐Nylon 66 composite exhibited reduced wear and coefficient of friction up to 6 wt% TiO2. Micro‐TiO2 at 2 wt% was most effective in improving the tribological properties of plain nylon 66. The worn surfaces were examined by scanning electron microscopy to understand the wear mechanism. The optimal combination from 2 wt% to 6 wt% micro‐TiO2‐Nylon 66 can be used depending upon the application requiring improvement in tribological or mechanical properties, respectively.  相似文献   