首页 | 本学科首页   官方微博 | 高级检索  
相似文献
 共查询到20条相似文献,搜索用时 15 毫秒
1.
The influence of miscibility on the transport properties of polymer electrolyte blends composed of a proton conductor and an insulator was investigated. The proton‐conductive component in the blends was sulfonated poly(ether ketone ketone) (SPEKK), while the nonconductive component was either poly(ether imide) (PEI) or poly(ether sulfone) (PES). The phase behavior of PEI‐SPEKK blends was strongly influenced by the sulfonation level of the SPEKK. At low sulfonation levels (ion‐exchange capacity (IEC) = 0.8 meq/g), the blends were miscible, while at a slightly higher level (IEC = 1.1 meq/g), they were only partially miscible and for IEC ≥ 1.4 meq/g they were effectively immiscible over the entire composition range. The PES‐SPEKK blends were miscible over the entire range of SPEKK IEC considered in this study (0.8–2.2 meq/g). At high IEC (2.2 meq/g) and at low mass fractions of SPEKK (<0.5), the miscible blends (PES‐SPEKK) had higher proton conductivities and methanol permeabilities than the immiscible ones (PEI‐SPEKK). The opposite relationship was observed for high mass fractions of SPEKK (>0.5). This behavior was explained by the differences in morphology between these two blend systems. At low IEC of SPEKK (0.8 meq/g), where both PEI‐SPEKK and PES‐SPEKK blend systems exhibited miscibility, the transport properties were not significantly different. © 2006 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 44: 2253–2266, 2006  相似文献   

2.
Hybrid organic/inorganic composite polymer electrolyte membranes based on a poly(vinylidene fluoride‐co‐chlorotrifluoroethylene) grafted membrane and varying concentrations of zeolite were investigated for application in proton exchange membrane fuel cells (PEMFC). A proton conducting comb copolymer consisting of poly(vinylidene fluoride‐co‐chlorotrifluoroethylene) backbone and poly(styrene sulfonic acid) (PSSA) side chains, i.e. P(VDF‐co‐CTFE)‐g‐PSSA (graft copolymer) with 47 wt% of PSSA was synthesized using atom transfer radical polymerization (ATRP) and solution blended with zeolite. Upon incorporation of zeolite, the symmetric stretching band of both SO group (1169 cm?1) and the ? OH group (3426 cm?1) shifted to lower wavenumbers. The shift in these FT‐IR spectra suggests that the zeolite particles strongly interact with the sulfonic acid groups of PSSA chains. When the weight percent of zeolite 5A is above 7%, the proton conductivity at room temperature was reduced to 0.011 S/cm. The water uptake of the composite membranes decreased from 234 to 125% with an increase of the zeolite 5A weight percent to 10 wt%. The decrease in water uptake is likely a result of the decrease in the number of available water absorption sites because of the hydrogen bonding interactions between the zeolite particles and the graft copolymer matrix. This behavior is successfully investigated by scanning electron microscopy (SEM). The results of thermal gravimetric analysis (TGA) also showed that all the membranes were stable up to 300°C. Copyright © 2009 John Wiley & Sons, Ltd.  相似文献   

3.
Two new kinds of fluorine‐containing polybenzimidazoles (PBI), poly(2,2′‐(tetrafluoro‐p‐phenylene)‐5,5′‐bibenzimidazole) and poly(2,2′‐tetradecafluoroheptylene‐5,5′‐bibenzimidazole), were synthesized by condensation polymerization of 3,3′‐diaminobenzidine and perfluoroterephthalic acid (or perfluoroazelaic acid), with polyphosphoric acid as solvent. Thermogravimetric analysis results show that the fluorine‐containing polymers synthesized exhibit promising thermal stability. The film‐forming properties of the fluorine‐containing polymers are improved over nonfluorinated PBI. The introduction of fluorine into the backbone of the polymers has significant positive affection on their chemical oxidation stability demonstrated by Fenton test. Compared with poly(2,2′‐(m‐phenylene)‐5,5′‐bibenzimidazole)/phosphoric acid (PA) composite membrane, the resulting fluorinated membranes with a same PA doping level exhibit better flexibility and higher proton conductivity. The maximum proton conductivity gained is 3.05 × 10?2 S/cm at 150 °C with a PA doping level of 7. © 2010 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 48: 2115–2122, 2010  相似文献   

4.
A series of poly(arylene ether sulfone)‐block‐sulfonated polybutadiene (PAES‐b‐sPB) with different ion exchange capacities (IECs) were synthesized and evaluated as proton exchange membranes (PEMs) for possible applications in fuel cells. These sulfonated block copolymers were synthesized via condensation reaction between modified PAES and PB prepolymers, followed by selective post‐sulfonation of PB blocks using acetyl sulfate as the sulfonating reagent. The sulfonic groups were only attached onto PB blocks due to the high reactivity of double bonds to acetyl sulfate. The success of synthesis and selective post‐sulfonation were all confirmed by the Fourier transform infrared (FT‐IR) and nuclear magnetic resonance (NMR) spectra. PAES‐b‐sPB had good film‐forming ability and thermal stability. Mechanical properties of membranes varied with the sulfonation. The presence of sulfonic groups increased the tensile strength and Young's modulus but decreased the elongation at break. Transmission electron microscopy (TEM) images showed large ionic aggregates in membranes. Phase separation as well as the interconnected sulfonate groups which only localized on flexible PB blocks led to these ionic domains. The proton conductivity increased with the increasing IEC and temperature. With relatively low IEC, most membranes still exhibited sufficient proton conductivity. The above results indicated this strategy could be a prospective choice to prepare novel PEMs. Copyright © 2010 John Wiley & Sons, Ltd.  相似文献   

5.
Phosphoric acid doped polybenzimidazole (PBI) membranes have been covalently cross‐linked with dichloromethyl phosphinic acid (DCMP). FT‐IR measurements showed new bands originating from bonds between the hydrogen bearing nitrogen in the imidazole group of PBI and the CH2 group in DCMP. The produced cross‐linked membranes show increased mechanical strength, making it possible to achieve higher phosphoric acid doping levels and therefore higher proton conductivity. Oxidative stability is significantly improved and thermal stability is sufficient in a temperature range of up to 250°C, i.e. within the temperature range of operation of PBI‐based fuel cells. Copyright © 2008 John Wiley & Sons, Ltd.  相似文献   

6.
A concept of preparing high‐temperature proton exchange membranes with layer‐by‐layer (LBL) self‐assembly technique was proposed and the sulfonated polyetheretherketone (SPEEK) and polyurethane (PU) with 200 LBL deposition cycles denoting (SPEEK/PU)200 membrane was prepared in this research. Owing to the strong electrostatic interaction between ? group in SPEEK and ? C? N+ group in PU, (SPEEK/PU)200 membrane with LBL self‐assembly structure showed a favorable structural stability. The phosphoric acid (PA)‐doped (SPEEK/PU)200 membrane showed a higher proton conductivity relative to PA doped SPEEK/PU membrane by solution casting method (SPEEK/PU)200/40%PA membrane possessed a proton conductivity value of 2.90 × 10?2 S/cm at 150 °C under anhydrous conditions. The LBL self‐assembly structure provided a possibility to reduce the negative effect from polymer skeleton blocking charge carrier species even immobilizing protons. Moreover, the (SPEEK/PU)200 membrane presented the particularly noteworthy mechanical property even with PA doping. The tensile stress values at break were 72.8 and 24.1 MPa, respectively, for (SPEEK/PU)200 and (SPEEK/PU)200/40%PA membrane at room temperature, which were obviously higher than the reported values of 15.9 and 2.81 MPa for SPEEK/PU and SPEEK/PU/60%PA membrane. © 2017 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2017 , 55 , 3446–3454  相似文献   

7.
Hydrophilic/hydrophobic block copolymers as proton exchange membranes (PEMs) has become an emerging area of research in recent years. These copolymers were obtained through moderate temperature (~ 100 °C) coupling reactions, which minimize the ether‐ether interchanges between hydrophobic and hydrophilic telechelic oligomers via a nucleophilic aromatic substitution mechanism. The hydrophilic blocks were based on the nucleophilic step polymerization of 3,3′‐disulfonated, 4,4′‐dichlorodiphenyl sulfone with an excess 4,4′‐biphenol to afford phenoxide endgroups. The hydrophobic (fluorinated) blocks were largely based on decafluoro biphenyl (excess) and various bisphenols. The copolymers were obtained in high molecular weights and were solvent cast into tough membranes, which had nanophase separated hydrophilic and hydrophobic regions. The performance and structure‐property relationships of these materials were studied and compared to random copolymer systems. NMR results supported that the multiblock sequence had been achieved. They displayed superior proton conductivity, due to the ionic proton conducting channels formed through the self‐assembly of the sulfonated blocks. The nano‐phase separated morphologies of the copolymer membranes were studied and confirmed by atomic force microscopy. Through control of a variety of parameters, including ion exchange capacity and sequence lengths, performances as high, or even higher than those of the state‐of‐the‐art PEM, Nafion, were achieved. © 2009 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 47: 1038–1051, 2009  相似文献   

8.
The synthesis of a novel aromatic sulfonic acid bearing an amino function H2N? C2H4? S? C2H4? C6H4? SO3Na ( 1 ) from the radical addition of mercaptoethylamine hydrochloride onto styrene sodium sulfonate, and its subsequent grafting onto poly(vinylidene fluoride‐co‐hexafluoropropylene), poly(VDF‐co‐HFP), copolymer are presented. First, the radical telomerization, carried out under radical conditions and in water, led to various products [monoadduct ( 1 ), multiadducts, and polymers], the amounts of which depend on the experimental conditions and [mercaptan]0/[monomer]0 initial molar ratio (R0). An R0 ≥ 1 led to the monoadduct ( 1 ) only and achieved in ~85% yield. The zwitterionic isomer was obtained mainly and its chemical modification was possible to get an original aromatic sodium sulfonate containing an amino end group. A kinetic study of the telomerization was presented for R0 < 1. Thermogravimetric analysis of the telomer showed that this compound was stable up to 200 °C. Second, the grafting of ( 1 ) onto poly(VDF‐co‐HFP) copolymer was also investigated. Such a grafting proceeded as expected by a classic mechanism of grafting of amines. Molar percentages of grafted telomer were assessed by 1H NMR spectroscopy and by elemental analysis. Ion exchange capacity (IEC) values of the membranes were deduced from the mol % grafted telomer. Scanning electron microscopy pictures showed a good homogeneity in the cross‐section of membranes, and energy dispersive X‐ray evidenced that all SO3Na groups of the grafted amine were changed into SO3H after treatment with concentrated HCl. Method involving an impedance analyzer, working at increasing high frequencies was used to assess the protonic conductivities, σ. These values were lower than that of Nafion117®, but σ increased with the IEC to 0.4 mS/cm at room temperature and 95% relative humidity. Water and methanol uptakes were also assessed, and it was shown that σ increased when water uptakes increased. Membranes started to decompose from 170 °C under air. © 2008 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 47: 121–136, 2009  相似文献   

9.
10.
Proton‐exchange membranes (PEM), suitable for micro and small sized fuel cells, were obtained by blending sulfonated poly(ether ketone ketone) (SPEKK) polymers with different ionic exchange capacity (IEC). This approach was used to limit the amount of swelling caused by water sorption without significantly decreasing the proton conductivity of the membrane. In particular a membrane with a cocontinuous biphasic morphology was obtained by blending two SPEKKs, with respectively, an IEC equal to 1.2 and 2.08 in the weight ratio 60/40, casted from 5% (w/v) solutions in dimethylacetamide. The effect of a cocontinuous morphology on water sorption and proton conductivity in comparison to neat SPEKK was investigated. In the range of temperatures between 40 and 70 °C, which is typical for small and micro fuel cells conditions, it was found that the ratio of proton conductivity to water sorption could be maximized. This has been attributed to the presence of percolative pathways for proton transport provided by the cocontinuous morphology along with the constraint effect of the less sulfonated component on the overall capacity of swelling of the membrane. © 2007 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 45: 395–404, 2007  相似文献   

11.
Hydrophobic‐hydrophilic sequence multiblock copolymers, based on alternating segments of phenoxide terminated fully disulfonated poly(arylene ether sulfone) (BPS100) and fluorine‐terminated poly(arylene ether sulfone) (6FBPS0) were synthesized and evaluated for application as proton exchange membranes. By utilizing mild reaction conditions the ether–ether interchange reactions were minimized, preventing the randomization of the multiblock copolymers. Tough, ductile, transparent membranes were solution cast from the block copolymers and were characterized with regard to intrinsic viscosity, morphology, water uptake, and proton conductivity. The conductivity values of the 6FBPS0‐BPSH100 membranes were compared to Nafion 212 and a partially fluorinated sulfonated poly(arylene ether sulfone) random copolymer (6F40BP60). The nanophase separated morphology was confirmed by transmission electron microscopy and small angle X‐ray scattering, and enhanced proton conductivity at reduced relative humidity was observed with longer block lengths. © 2013 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem, 2013  相似文献   

12.
Throughout this work, the synthesis, thermal as well as proton conducting properties of acid doped heterocyclic polymer were studied under anhydrous conditions. In this context, poly(1‐vinyl‐1,2,4‐triazole), PVTri was produced by free radical polymerization of 1‐vinyl‐1,2,4‐triazole with a high yield. The structure of the homopolymer was proved by FTIR and solid state 13C CP‐MAS NMR spectroscopy. The polymer was doped with p‐toluenesulfonic acid at various molar ratios, x = 0.5, 1, 1.5, 2, with respect to polymer repeating unit. The proton transfer from p‐toluenesulfonic acid to the triazole rings was proved with FTIR spectroscopy. Thermogravimetry analysis showed that the samples are thermally stable up to ~250 °C. Differential scanning calorimetry results illustrated that the materials are homogeneous and the dopant strongly affects the glass transition temperature of the host polymer. Cyclic voltammetry results showed that the electrochemical stability domain extends over 3 V. The proton conductivity of these materials increased with dopant concentration and the temperature. Charge transport relaxation times were derived via complex electrical modulus formalism (M*). The temperature dependence of conductivity relaxation times showed that the proton conductivity occurs via structure diffusion. In the anhydrous state, the proton conductivity of PVTri1PTSA and PVTri2PTSA was measured as 8 × 10?4 S/cm at 150 °C and 0.012 S/cm at 110 °C, respectively. © 2010 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 48: 1016–1021, 2010  相似文献   

13.
A high molecular weight, thermally and chemical stable hexafluoroisopropylidene containing polybenzimidazole (6F‐PBI) was synthesized from 3,3′‐diaminobenzidine (TAB) and 2,2‐bis(4‐carboxyphenyl) hexafluoropropane (6F‐diacid) using polyphosphoric acid (PPA) as both the polycondensation agent and the polymerization solvent. Investigation of polymerization conditions to achieve high molecular weight polymers was explored via stepwise temperature control, monomer concentration in PPA, and final polymerization temperature. The polymer characterization included inherent viscosity (I.V.) measurement and GPC as a determination of polymer molecular weight, thermal and chemical stability assessment via thermo gravimetric analysis and Fenton test, respectively. The resulting high molecular weight polymer showed excellent thermal and chemical stability. Phosphoric acid doped 6F‐PBI membranes were prepared using the PPA process. The physiochemical properties of phosphoric acid doped membranes were characterized by measuring the phosphoric acid doping level, mechanical properties, and proton conductivity. These membranes showed higher phosphoric acid doping levels and higher proton conductivities than the membranes prepared by the conventional membrane fabrication processes. These membranes had sufficient mechanical properties to be easily fabricated into membrane electrode assemblies (MEA) and the prepared MEAs were tested in single cell fuel cells under various conditions, with a focus on the high temperature performance and fuel impurity tolerance. © 2009 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 47: 4064–4073, 2009  相似文献   

14.
Partially disulfonated hydroquinone (HQ)‐based poly(arylene ether sulfone) random copolymers were synthesized and characterized for application as proton exchange membranes. The copolymer composition was varied in the degree of disulfonation. The copolymers were characterized by 1H NMR, Differential Scanning Calorimetry (DSC), and other analytical techniques. The copolymer with a 25% degree of disulfonation showed the best balance between water uptake and proton conductivity. The copolymers showed substantially reduced methanol permeability compared with Nafion® and satisfactory direct methanol fuel cell performance. The methanol selectivity improved significantly in comparison to Nafion® 117. At a given ionic composition, the HQ‐based system showed higher water uptake and proton conductivity than the biphenol‐based (BPSH‐xx) poly(arylene ether sulfone)s copolymers. © 2008 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 47: 384–391, 2009  相似文献   

15.
Novel epoxy‐based semi‐interpenetrating polymer networks (semi‐IPNs) of aromatic polyimide, derived from 2,2‐benzidinedisulfonic acid (BDSA), were prepared through a thermal imidization reaction. Dynamic scanning calorimetry (DSC) and Fourier transform infrared spectroscopy (FTIR) were utilized to verify the synchronization of the imidization of sulfonated poly(amic acid) (SPAA) and the crosslinking reactions of epoxy. The semi‐IPNs of epoxy/sulfonated polyimides (SPI‐EPX) exhibit excellent film‐forming characteristics and mechanical integrity at room temperature. Conductivities at 100 °C of 0.0243 S cm?1 (SPI‐EP30) and 0.0141 S cm?1 (SPI‐EP50) were obtained, which are similar to that of the Nafion 117 (0.0287 S cm?1). The increase in the conductivity of SPI‐EP(30,40) with temperature is more rapid than that of Nafion 117. The SPI‐EPX exhibited lower methanol permeability than did Nafion117. The hydrolytic stability of the SPI‐EPX was followed by FTIR spectroscopy at regular intervals. SPI‐EPX prepared using epoxy‐based semi‐IPNs of sulfonated polyimide, SPI‐EP(40,50), exhibited higher hydrolytic stability than the phthalic polyimides (five‐membered ring polyimides).The microstructure was analyzed using atomic force microscopy (AFM) in the tapping mode, which demonstrated that SPI‐EP50 exhibited a nanophase that was separated into an essentially reticulated and venous hydrophobic and hydrophilic domains. Transmission electron microscopy (TEM) confirmed widespread and well‐connected hydrophilic domains, proving the higher hydrolytic stability and strong proton‐transporting properties of the SPI‐EPX membrane. © 2008 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 46: 2262–2276, 2008  相似文献   

16.
17.
This paper describes our work on the synthesis of a series of sulfonated homo‐/co‐polyimides (SPI) which were obtained by post‐sulfonation method over three steps. In the first step, 4,4′‐oxydianiline (ODA) and 4,4′‐diaminodiphenylsulfone (DDS) dissolved in N‐methyl pyrrolidone (NMP) were reacted with benzophenonetetracarboxylic dianhydride (BTDA) in order to yield poly(amic acid) (PAA). Secondly, precipitated PAA was sulfonated via concentrated sulfuric acid (95–98%) at room temperature to give post‐sulfonated PAA (PSPAA). Finally, PSPAA was converted into post‐sulfonated PI (PSPI) by the thermal imidization method. PSPIs with ion exchange capacity (IEC) ranging from 0.20 to 0.67 meq/g were prepared. The thermal properties of the PSPIs were evaluated and high desulfonation temperature was found in the range of 190–350°C, suggesting the high stability of sulfonic acid groups. In water, PSPI‐5 membrane displayed similar proton conductivity to Nafion®117, whereas this membrane showed poor conductivity in dry state. All PSPIs displayed good solubility in common polar aprotic solvents such as NMP and dimethylacetamide (DMAc). Furthermore, the effects of post‐sulfonation reaction on chemical structure, thermal oxidative behavior, and physical properties of the PSPI membranes such as membrane quality/stability and water uptake were discussed. Copyright © 2008 John Wiley & Sons, Ltd.  相似文献   

18.
In this paper, three organic intercalating agents containing cations [hexadecyl trimethyl ammonium bromide (CTAB), poly(acrylamide‐co‐diallyldimethylammonium chloride), and quaternized polyethyleneimine] are used to prepare intercalated montmorillonites (MMT) by ion‐exchange method. Then the modified MMTs are doped with vinylbenzyl chloride and styrene copolymer [poly(vinylbenzyl chloride‐co‐styrene)] for fabricating composite anion‐exchange membranes (AEM). Fourier transform infrared, X‐raydiffraction, thermogravimetric analysis, scanning electron microscopy, and Mastersizer laser particle size analyzer are employed to characterize the structure and morphology of MMTs and AEMs. The successful intercalation of MMTs is approved, and the MMT intercalated by CTAB shows an interlayer distance of 2.31 nm. The properties of the composite membranes including water uptake, mechanical property, and ionic conductivity are investigated. Among all the AEMs, the composite membrane containing MMT sheets with CTAB demonstrates better compositive performances. It presents an ionic conductivity of 2.09 × 10?2 S cm?1 at 80°C and good alkaline solution stability. Copyright © 2016 John Wiley & Sons, Ltd.  相似文献   

19.
Acrylic acid was grafted onto FEP by simultaneous radiation technique and the resulting membranes were sulfonated. Results of dynamic mechanical properties of the membranes showed that storage modulus and temperature at tan δ(max) increases on grafting. X‐ray diffraction (XRD) analysis of the grafted and sulfonated membranes showed decreasing trend in crystallinity with increase in degree of grafting. From scanning electron microscopy (SEM) studies it was confirmed that grafting takes place by the front mechanism. Copyright © 2004 John Wiley & Sons, Ltd.  相似文献   

20.
In this research a series of pore‐filling electrolyte membranes were prepared, based on a sulfonated and hydrogenated styrene/butadiene block copolymer (SHSBS) and plasma‐treated microporous polyethylene (PE) membranes. The pore‐filling electrolyte membranes were characterized by means of scanning electronic microscopy (SEM), infrared spectroscopy (FTIR‐ATR), and dynamic mechanical analysis (DMA). In addition, the water uptake and methanol/water uptake capacities of these membranes were determined using several methanol in water solutions, as well as the permeability coefficients, for both water and methanol, using a 2 M methanol in water solution and pure methanol. Finally, electrical behavior was recorded by means of electrochemical impedance spectroscopy (EIS) and the four probe technique (FPT). The SEM images recorded show good coating of the pore‐filling electrolyte membranes on the plasma‐treated PE matrices, and DMA shows the proper relaxations of the two components: PE and SHSBS. Furthermore, the methanol/water absorption capacity was observed to diminish with plasma treatment of the matrix. Methanol permeability of the pore‐filling electrolyte membranes is notably lower than that of the Nafion® membrane, ion conductivity moving in the order of 10−2 S cm−1. Both of these characteristics qualify the experimental membranes as candidates to be applied as proton exchangers in fuel cells (FCs). © 2008 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 46: 1684–1695, 2008  相似文献   