Hyperbranched star polymer HBPS-(PPEGMA) x was synthesized by atom transfer radical polymerization (ATRP) using hyperbranched polystyrene (HBPS) as macroinitiator and poly(ethylene glycol) methyl ether methacrylate (PEGMA) as monomer. The structure of the prepared hyperbranched star polymer was characterized by 1H NMR, ATR-FTIR, and GPC. Polymer electrolytes based on HBPS-(PPEGMA) x , lithium salt, and/or nano-TiO2 were prepared. The influences of lithium salt concentration and type, nano-TiO2 content, and size on ionic conductivity of the obtained polymer electrolytes were investigated. The results showed that the low crystallinity of the prepared polymer electrolyte was caused by the interaction between lithium salt and polymer. The addition of TiO2 into HBPS-(PPEGMA) x /LiTFSI improved the ionic conductivity at low temperature. The prepared composite polymer electrolyte showed the highest ionic conductivity of 9?×?10?5 S cm?1 at 30 °C when the content of TiO2 was 15 wt% and the size of TiO2 was 20 nm.  相似文献   

2.
Solid polymer electrolytes based on high molecular weight poly(ethylene oxide) (PEO) complexed with lithium difluoro(oxalato)borate (LiDFOB) salt in various EO:Li molar ratios from 30:1 to 8:1 were prepared by using solution casting technique. Ion–polymer interaction, structural, thermal, and ionic conductivity studies have been reported by Fourier transform infrared spectroscopy (FTIR), X-ray diffraction (XRD), polarized optical microscopy (POM), differential scanning calorimeter (DSC), and impedance analysis. FTIR spectral studies suggested that the interaction of Li+ cations with the ether oxygen of PEO, where a triple peak broad band centered at 1105 cm?1, corresponds to C–O–C stretching and extreme deformation occurs. XRD, POM, and DSC indicated that the inclusion of LiDFOB salt could reduce the crystallinity of PEO. The melting temperature of PEO shifted to lower temperature side by the addition of LiDFOB. The glass transition temperature obtained for the system 10:1 was ?38.2 °C. An increase in the ionic conductivity from 3.95?×?10?9 to 3.18?×?10?5 S/cm at room temperature (23 °C) was obtained through the addition of LiDFOB to a high molecular weight PEO. In addition, the ionic conductivity of the polymer electrolyte films followed an Arrhenius relation, and the activation energy decreased with increasing LiDFOB concentration.  相似文献   

3.
Poly(vinylidene fluoride)-based polymer electrolytes using ionic liquid 1-butyl-3-methylimidazolium bis(trifluoromethylsufonyl)imide as the plasticizer were prepared by solution casting method. The effects of the solvent evaporation temperature (SET) and ionic liquid content (ILC) on the properties and structures of the polymer electrolytes were investigated by characterization of scanning electron microscope (SEM), X-ray diffraction (XRD), thermogravimetric analysis (TGA), differential scanning calorimetry, as well as mechanical and ionic conductivity test. It was confirmed that both SET and ILC had significant influence on the morphology, degree of crystallinity, mechanical properties, and ionic conductivity of the prepared polymer electrolytes. With ILC of 40 %, an excellent polymer electrolyte can be obtained at SET of 60 °C, which exhibited ionic conductivity up to ca. 10?4 S/cm at room temperature, accompanied by excellent tensile strength of 22.8 MPa and elongation at break of 540 %.  相似文献   

4.
In the present work, a series of single-ion conducting composite polymer electrolytes based on lithium polyvinyl alcohol oxalate borate (Li(PVAOB)) and poly(polyethylene glycol methacrylate) (PPEGMA) were produced. PEGMA was polymerized into PPEGMA, and the Li(PVAOB) was prepared from poly (vinyl alcohol) (PVA), oxalic acid, and boric acid. Li(PVAOB) was blended with PPEGMA at different stoichiometric ratios to obtain a single-ion conducting system. All the electrolytes were characterized by Fourier transformation infrared spectroscopy (FT-IR), thermogravimetry analysis (TGA), differential scanning calorimeter (DSC), and scanning electron microscopy (SEM) techniques. These results verified the interaction between host and guest polymers, sufficient thermal stability within the measured conductivity domain, and the homogeneity of the composite electrolytes. The effect of PPEGMA onto the ionic conductivity was investigated using impedance spectroscopy. The Li(PVAOB)-60PPEGMA is the optimum content, and this sample has a maximum ionic conductivity of 3 × 10?4 S/cm at 100 °C which is approximately five orders of magnitude higher than neat Li(PVAOB). Activation energy (E a ) of ionic transport decreased from 11.9 to 0.27 kJ/mol, suggesting a much faster ionic mobility for higher PPEGMA-containing samples.  相似文献   

5.
Solid polymer electrolytes (SPEs) based on poly (vinyl chloride)/poly (ethyl methacrylate) [PVC/PEMA] blend complexed with zinc triflate [Zn(CF3SO3)2] salt have been prepared using solution casting technique. Thin film samples containing various blend ratios of PVC/PEMA with fixed composition of salt have been examined by means of complex impedance analysis, and as a consequence, the typical composition corresponding to PVC (30 wt%)/PEMA (70 wt%) has been identified as the optimized blend exhibiting the highest room temperature ionic conductivity of 10?8 Scm?1. The ionic conductivity of the optimized blend was further enhanced from 10?8 to 10?6 Scm?1 by adding the chosen salt in different weight percentages at 301 K. The occurrence of complexation of the polymer blend and an evidence of interaction of cations, namely Zn2+ ions with the polymer blend, have been confirmed by Attenuated total reflectance-Fourier transformed infrared (ATR-FTIR) spectroscopy measurement studies. The efficacy of ion-polymer interactions was estimated by means of an evaluation of transport number data pertaining to Zn2+ ions which was found to be 0.56. The apparent changes resulting in the structural properties of these polymer electrolytes possessing a honeycomb-like microporous structure were identified using X-ray diffraction (XRD) and scanning electron microscopic (SEM) studies. Such promising features of the present polymer blend electrolyte system appear to suggest possible fabrication of new rechargeable zinc batteries involving improved device characteristics.  相似文献   

6.
Plasticized polymer electrolytes comprising of ethylene carbonate as the plasticizing agent in poly (vinyl chloride) [PVC]–poly (butyl methacrylate) [PBMA] blended polymer electrolytes were prepared by solution casting technique. Complex formation, structural elucidation, conductivity, dielectric parameters (?′, ?″, M′, and M″), thermal stability, and surface morphology are brought out from FTIR, XRD, ac impedance analysis, dielectric studies, thermogravimetry/differential thermal analysis, and scanning electron microscopic studies, respectively. Polymer electrolytes are found to exhibit higher ionic conductivity at higher concentration of plasticizer at the cost of their mechanical stability. Conductivity of 1.879 × 10?4 S cm?1 is exhibited by the polymer electrolyte consisting of 69% of plasticizer with appreciable thermal stability up to 523 K. Temperature and frequency dependence of conductivity is found to follow Vogel Tammann Fulcher relation and Jonscher power law, respectively. Real and imaginary parts of dielectric constants are found to decrease with increase in frequency which could be due to the electrode polarization effect.  相似文献   

7.
Poly(ethylene glycol)/poly(2-acrylamido-2-methyl-1-propane sulfonic acid) (PEG/PAMPS) with a transparent appearance were prepared in the presence of ammonium persulfate (APS) as an initiator at 70 °C for 24 h. PEG/PAMPS-based polymer gel electrolytes in a motionless and uniform state were obtained by adding the required amount of liquid electrolytes to a dry PEG/PAMPS polymer. Liquid electrolytes include organic solvents with high boiling points (-1-methyl-2-pyrrolidone (NMP) and γ-butyrolactone (GBL)) and a redox couple (alkali metal iodide salt/iodine). The optimized conditions for PEG/PAMPS-based gel electrolytes based on the salt type, the concentration of alkali metal iodide salt/iodine, and solvent volume ratio were determined to be NaI, 0.4 M NaI/0.04 M I2, and NMP:GBL (7:3, v/v), respectively. The highest ionic conductivity and the liquid electrolyte absorbency were 2.58 mS cm?1 and 3.6 g g?1 at 25 °C, respectively. The ion transport mechanism in both the polymer gel electrolytes and liquid electrolytes is investigated extensively, and their best fits with respect to the temperature dependence of the ionic conductivity are determined with the Arrhenius equation.  相似文献   

8.
Two water-soluble and biodegradable polymers: xanthan gum (XG) and poly(vinyl alcohol) (PVA) were used to synthesize ecologically friendly solid polymer electrolyte (SPE) matrices. While XG is a natural polymer, PVA is a synthetic one, but both are colorless and form transparent membranes. To obtain ionic conductivity properties, the samples were doped with acetic acid and characterized by electrochemical impedance spectroscopy (EIS), X-ray diffraction, UV-Vis spectroscopy, and tensile test. The best results of ionic conductivity of 1.97 × 10?4 and 7.41 × 10?4 S/cm at room temperature and 80 °C, respectively, were obtained for the sample containing 55 wt% of acetic acid. Moreover, this electrolyte was found to be predominantly amorphous with transmittance in the visible region of 80% and absorbance values below 0.5 between 240 and 375 nm. Tensile test of this sample, applied up to 18 N of maximum force, resulted in strain of 2322% and Young’s modulus of 0.02 MPa. The obtained results showed that these new eco-friendly materials are promising for use as electrolytes in electrochemical devices.  相似文献   

9.
The influence of tetrabutylammonium iodide on the polyvinylidene fluoride-poly(methyl methacrylate)-ethylene carbonate (PVDF-PMMA-EC)-I2 polymer blend electrolytes was investigated and optimized for use in a dye-sensitized solar cell. The different weight ratios (50, 60, 70, and 80 %) of tetrabutylammonium iodide (TBAI)-added PVDF-PMMA-EC-I2 polymer electrolytes were prepared. The prepared solid polymer blend electrolytes were characterized by using various techniques such as Fourier transform infrared (FT-IR) spectroscopy, differential scanning calorimetry (DSC), and electrochemical impedance spectroscopy (EIS). The FT-IR spectra revealed the interaction among all composition of polymer electrolytes. The influence of TBAI salt on the ionic conductivity of polymer electrolytes was studied using electrochemical impedance spectroscopy. The polymer electrolyte containing 60 % of TBAI in PVDF-PMMA-EC-I2 showed the highest room temperature conductivity of 5.10?×?10?3 S cm?1. The fabricated DSSC using PVDF-PMMA-EC-I2 polymer electrolytes with 60 % of TBAI showed the best performance with a short-circuit current density of 8.0 mA cm?2, open-circuit voltage of 0.66 V, fill factor of 0.65, and the overall power conversion efficiency of 3.45 % under an illumination of 100 mW cm?2. Hence, the weight content of organic iodide salt in polymer electrolytes influences the overall performance of dye-sensitized solar cells.  相似文献   

10.
The proton conducting solid-state polymer electrolyte comprising blend of poly(vinyl alcohol) (PVA) and poly(N-vinylimidazole) (PVIM), ammonium tetrafluoroborate (NH4BF4) as salt, and polyethylene glycol (PEG) (molecular weight 300 and 600) as plasticizer is prepared at various compositions by solution cast technique. The prepared films are characterized by Fourier transform infrared spectroscopy, differential scanning calorimetry, X-ray diffraction, and scanning electron microscopy analysis. The conductivity–temperature plots are found to follow an Arrhenius nature. The conductivity of solid polymer electrolytes is found to depend on salt and plasticizer content and also on the dielectric constant value and molecular weight of the plasticizer. Maximum ionic conductivity values of 2.20?×?10?4 and 1.28?×?10?4?S?cm?1 at 30 °C are obtained for the system (PVA–PVIM)?+?20 wt.% NH4BF4?+?150 wt.% PEG300 and (PVA–PVIM)?+?20 wt.% NH4BF4?+?150 wt.% PEG300, respectively. The blended polymer, complexed with salt and plasticizer, is shown to be a predominantly ionic conductor. The proton transport in the system may be expected to follow Grotthuss-type mechanism.  相似文献   

11.
Thin films of blend polymer electrolytes comprising poly(vinyl alcohol) (PVA) and poly(vinyl pyrrolidone) (PVP) complexed with ammonium thiocyanate (NH4SCN) salt in different compositions have been prepared by solution casting technique using distilled water as solvent. The prepared films have been investigated by different experimental techniques. The complexation of these films has been studied by FTIR spectroscopy. The increase in amorphousness of the films with increase in NH4SCN content has been confirmed by XRD analysis. The addition of ammonium thiocyanate salt to PVA-PVP polymer blend shows a shift in Tg of the blend. The effect of salt concentration and temperature on the ionic conductivity of the polymer blend films has been analyzed using AC impedance spectroscopy. The maximum conductivity of 6.85 × 10?4 S cm?1 at room temperature has been observed for the blend with 50 mol% PVA-50 mol% PVP complexed with 40 mol% NH4SCN. The activation energy has been found to be minimum (0.24 eV) for this sample. Wagner’s polarization technique shows that the charge transport in these blend films is predominantly due to ions. Using the highest conductivity blend polymer electrolyte, a proton battery has been fabricated and its discharge characteristics have been studied.  相似文献   

12.
Polymer electrolyte system based on poly(vinyl alcohol) (PVA)-chitosan blend doped with ammonium bromide (NH4Br) has been prepared by solution cast method. Fourier transform infrared (FTIR) spectroscopy analysis confirms the complexation between salt and polymer host. The highest ionic conductivity obtained at room temperature is (7.68?±?1.24)?×?10?4 S cm?1 for the sample comprising of 30 wt% NH4Br. X-ray diffraction (XRD) patterns reveal that PVA-chitosan with 30 wt% NH4Br exhibits the most amorphous structure. Thermogravimetric analysis (TGA) reveals that the electrolytes are stable until ~260 °C. The conductivity variation can also be explained by field emission scanning electron microscopy (FESEM) study. Dielectric properties of the electrolytes follow non-Debye behavior. The conduction mechanism of the highest conducting electrolyte can be represented by the correlated barrier hopping (CBH) model. From linear sweep voltammetry (LSV) result, the highest conducting electrolyte is electrochemically stable at 1.57 V.  相似文献   

13.
W. N. S. Sajiri  H.J. Woo 《Ionics》2017,23(10):2657-2662
Poor conductivity and toxic technological garbage of polymer electrolyte has delayed energy storage application in electric vehicles. Biodegradable gel polymer electrolytes (GPEs) based on poly (ε-caprolactone) (PCL) are prepared. PCL is used to immobilize liquid electrolyte containing lithium bis(trifluoromethanesulfonyl) imide, ethylene carbonate, and propylene carbonate. Impedance spectroscopy, X-ray diffraction, and differential scanning calorimetry are used to characterize the ionic conductivity and structural and thermal properties of GPEs, respectively. For jelly-like GPEs, it exhibits liquid-like ionic conductivity of 1.69 × 10?3 S cm?1 at room temperature with a composition ratio (PCL:LiTFSI:EC:PC) of (22.5:7.5:35:35) (w/w). Results show that the polymer matrix forms cross-linked network within the liquid electrolyte, acting like an adhesive to hold the high fluidity liquid molecules. In temperature dependence studies, the GPEs are observed to obey Arrhenius equation indicating that ion transport occurs via hopping mechanism. The findings in XRD and DSC are in good agreement with conductivity results.  相似文献   

14.
The present study investigates the ion transport properties and structural analysis of plasticized solid polymer electrolytes (SPEs) based on carboxymethyl cellulose (CMC)-NH4Br-PEG. The SPE system was successfully prepared via solution casting and has been characterized by using electrical impedance spectroscopy (EIS), Fourier transform infrared (FTIR) spectroscopy, and x-ray diffraction (XRD) technique. The highest conductivity of the SPE system at ambient temperature (303 K) was found to be 1.12?×?10?4 S/cm for un-plasticized sample and 2.48?×?10?3 S cm?1 when the sample is plasticized with 8 wt% PEG. Based on FTIR analysis, it shows that interaction had occurred at O–H, C=O, and C–O moiety from CMC when PEG content was added. The ionic conductivity tabulation of SPE system was found to be influenced by transport properties and amorphous characteristics as revealed by IR deconvolution method and XRD analysis.  相似文献   

15.
This paper reports the polyethylene oxide/polyvinylpyrrolidone (PEO/PVP) blend with cobalt chloride (CoCl2) films prepared using spin coating method on blue star glass substrate. The XRD analysis shows the decrease in the crystallinity nature of the CoCl2 with addition of the dopant. The FT-IR analysis reveals that interaction between cobalt ions with polymer blend confirms the complexation. The maximum ionic conductivity 0.65?×?10?4 S cm?1 was observed for PEO (45 %)/PVP (45 %)/CoCl2 (10 %) at 30 °C. The optical energy band gaps decreases and Urbach energy were observed increases with increasing the dopant concentration. The DSC/TGA results showed that thermal stability of films enhanced with dopant concentration. Cyclic voltammogram (CV) study shows that the electrochemical strength improves with dopant concentration. These obtained results imply that polymer blend electrolytes are suitable candidature for various applications such as electronic and optical devices like electro-chromic display, fuel cells, gas sensors and solid state batteries.  相似文献   

16.
A series of solid polymer electrolytes (SPEs) based on poly (ethylene oxide)/polylactic acid (PEO/PLA) with liquid crystal ionomer (LCI) intercalated montmorillonite (MMT) nanocomposites (LCI-MMT) has been prepared by solution blending method. The effects of LCI-MMT on the structural, crystallization, thermal, and ionic conductivity properties of solid polymer electrolytes have been analyzed. It is demonstrated that the incorporation of LCI-MMT into the blend suppressed the crystallinity of PEO and increased the crystallinity of PLA. The maximum ionic conductivity is found to be in the range of 1.05?×?10?5 S/cm for 0.5 wt% LCI-MMT, which is higher than that of the LCI-MMT-free polymer electrolyte (5.36?×?10?6 S/cm) at room temperature.  相似文献   

17.
We report blend-based plastic polymer electrolyte (i.e., polyethylene oxide (PEO)–polydimethyl siloxane (PDMS)–lithium hexafluorophosphate (LiPF6)) with substantial improvement in DC conductivity at ambient and subambient temperatures when compared with literature reports. Conductivity variation with salt concentration, investigated within ±30 °C range, indicates an optimum conductivity of 5.6?×?10?5 S cm?1 at 30 °C for Ö/Li ~10 with a further lowering by one order at 0 °C and it remains unaltered at ?10 °C. Enhanced conductivity in this blend electrolyte, though lower than two copolymer counterparts, is attributed to very low glass transition temperatures of the host polymers. X-ray diffraction (XRD) and scanning electron microscopy (SEM) suggest an effective blending between the two polymers with an effective interaction between the Li salt and the blend polymer matrix. Raman spectroscopy results indicated that cation (Li+) coordination occurs at the C=Ö site in PEO out of the two electron-rich sites (i.e., CÖ and Si–Ö–Si) in the PEO–PDMS blend. The blend electrolytes are predominantly ionic (t ion ~97 %).  相似文献   

18.
Nano-composite polymer electrolytes containing poly(vinylidene fluoride-co-hexafluoropropylene) (PVdF-HFP), ammonium tetrafluoroborate (NH4BF4), and nano-size fumed silica (SiO2) have been prepared and characterized by complex impedance spectroscopy. Ionic conductivity of polymer has been found to increase with the addition of NH4BF4, and a maximum conductivity of 3.62 × 10?6 S/cm has been obtained at 30 wt% NH4BF4. The formation of ion aggregates at high concentration of salt has been explained by Bjerrum’s law and mass action considerations. The conductivity of polymer electrolytes has been increased by three orders of magnitude (10?6 to 10?3 S/cm) with the addition of plasticizer, and a maximum conductivity of 1.10 × 10?3 S/cm has been observed at 80 wt% DMA. An increase in conductivity with the addition of nano-size fumed silica is attributed due to the formation of space-charge layers. A maximum conductivity of 7.20 × 10?3 S/cm has been observed for plasticized nano-composite polymer electrolytes at 3 wt% SiO2. X-ray diffraction analysis of polymer electrolyte system was also carried out. A small change in conductivity of nano-composite polymer electrolytes observed over the 30–130 °C temperature range and for a period of 30 days is also desirable for their use in various applications.  相似文献   

19.
High molecular weight polymer poly(vinylidenefluoride-co-hexafluoropropylene) (PVdF-HFP), ionic liquid 1-ethyl-3-methylimidazolium bis(fluorosulfonyl)imide (EMIMFSI), and salt lithium bis(trifluoromethanesulfonyl)imide (LiTFSI)-based free-standing and conducting ionic liquid-based gel polymer electrolytes (ILGPE) have been prepared by solution cast method. Thermal, electrical, and electrochemical properties of 80 wt% IL containing gel polymer electrolyte (GPE) are investigated by thermogravimetric (TGA), impedance spectroscopy, linear sweep voltammetry (LSV), and cyclic voltammetry (CV). The 80 wt% IL containing GPE shows good thermal stability (~?200 °C), ionic conductivity (6.42?×?10?4 S cm?1), lithium ion conductivity (1.40?×?10?4 S cm?1 at 30 °C), and wide electrochemical stability window (~?4.10 V versus Li/Li+ at 30 °C). Furthermore, the surface of LiFePO4 cathode material was modified by graphene oxide, with smooth and uniform coating layer, as confirmed by scanning electron microscopy (SEM), and with element content, as confirmed by energy dispersive X-ray (EDX) spectrum. The graphene oxide-coated LiFePO4 cathode shows improved electrochemical performance with a good charge-discharge capacity and cyclic stability up to 50 cycles at 1C rate, as compared with the without coated LiFePO4. At 30 °C, the discharge capacity reaches a maximum value of 104.50 and 95.0 mAh g?1 for graphene oxide-coated LiFePO4 and without coated LiFePO4 at 1C rate respectively. These results indicated improved electrochemical performance of pristine LiFePO4 cathode after coating with graphene oxide.  相似文献   

20.
An attempt has been made to prepare a new proton-conducting polymer electrolyte based on poly(vinyl alcohol) doped with ammonium fluoride (NH4F) by solution casting technique. The complex formation between polymer and dissociated salt has been confirmed by X-ray diffraction and Fourier transform infrared spectroscopy studies. The highest ionic conductivity has been found to be 6.9?×?10?6?Scm?1 at ambient temperature (303 K) for 85PVA:15NH4F polymer electrolyte. The conductance spectra contain a low frequency plateau region and high frequency dispersion region. The dielectric spectra exhibit the low frequency dispersion, which is due to space charge accumulation at the electrode–electrolyte interface. The modulus spectra indicate non-Debye nature of the material. The highest ionic conductivity polymer electrolyte 85PVA:15NH4F has low activation energy 0.2 eV among the prepared polymer electrolytes.  相似文献   