共查询到20条相似文献,搜索用时 0 毫秒
1.
An‐Ru Guo Xiao‐Jian Yang Peng‐Fei Yan Yi‐Xian Wu 《Journal of polymer science. Part A, Polymer chemistry》2013,51(19):4200-4212
Cationic polymerizations of isobutylene (IB) with H2O/FeCl3/isopropanol (iPrOH) initiating system were conducted in nonpolar hydrocarbon media, such as n‐hexane or mixed C4 fractions at ?40 to 20 °C. This cationic polymerization is a chain‐transfer dominated process via highly selective β‐proton elimination from ? CH3 in the growing chain ends, leading to formation of highly reactive polyisobutylenes (HRPIBs) with large contents (> 90 mol %) of exo‐olefin end groups (structure A ). The content of structure A remained nearly constant at about 97 mol % during polymerization and isomerization via carbenium ion rearrangement could be suppressed in nonpolar media. First‐order kinetics with respect to monomer concentration was measured for selective cationic polymerization of IB in the mixed C4 fraction feed at ?30 °C and the apparent rate constant for propagation was 0.028 min?1. High polymerization temperature (Tp) or [FeCl3] accelerate β‐proton elimination or isomerizations and simultaneously decrease selectivity of β‐proton abstraction from ? CH3. Molecular weight decreased and molecular weight distribution (MWD) became narrow with increasing Tp or [FeCl3]. To the best of our knowledge, this is the first example to achieve high quality HRPIBs with near 100% of exo‐olefin terminals and relatively narrow MWD (Mw/Mn = 1.8) by a single‐step process in nonpolar hydrocarbon media. © 2013 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2013 , 51, 4200–4212 相似文献
2.
Yan Li Yixian Wu Xu Xu Lihu Liang Guanying Wu 《Journal of polymer science. Part A, Polymer chemistry》2007,45(14):3053-3061
The cationic polymerizations of isobutylene (IB) initiated by an H2O/AlCl3 system were carried out in a mixture of n‐hexane/methylene dichloride of 60/40 v/v at ?50 °C in the presence of various external electron pair donors (EDs), including methyl benzoate (MB), ethyl benzoate (EB), and methyl acrylate (MA). The effects of the concentrations of EDs ([ED]) and polymerization time on monomer conversion and kinetics of IB polymerization were also investigated. The complexes between AlCl3 and the esters were soluble in the polymerization system at ?50 °C. The polymers with high molecular weights and relatively narrow molecular weight distributions were obtained in the presence of the EDs. The rate of polymerization decreased with increasing [ED]. The kinetic orders of the EDs were remarkably dependent on their chemical structure, steric hindrance from moieties, and concentration in the polymerization system. The reaction order of MB was determined to be around ?1.3 when [MB] ≤ 0.40 mmol/L, whereas it was ?12.9 when [MB] ≥ 0.40 mmol/L. The reaction order of EB was determined to be ?1.36 when [EB] ≤ 0.41 mmol/L, whereas it was ?3.36 when [EB] ≥ 0.41 mmol/L. The reaction order of MA was determined to be ?1.85 when [MA] ≤ 0.48 mmol/L, whereas it was ?16.7 when [MA] ≥ 0.48 mmol/L. © 2007 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 45: 3053–3061, 2007 相似文献
3.
The cationic polymerization of isobutylene coinitiated by Al(i-Bu)Cl2(Al) was carried out in mixed butane–butene fractions at −50 °C. The expected polymerization processes induced by the trace of moisture with Al system in the presence of a small amount of external electron-donor modifiers, such as methyl acrylate (MA) and dimethyl sulfoxide (DMSO), were obtained. The experimental results showed that these polymerizations produced polymers with relatively high number-average molecular weights and narrow molecular weight distributions (1.5–2.2). That the gel permeation chromatography traces of the polymers depended on the types and concentrations of external donors suggested that there existed competitive complexation reactions of various electron donors (H2O, MA, and DMSO) with the Al Lewis acid. The roles of external electron donors were to take part in the initiation step by competitive complexation and to modify the reactivity of the growing chain ends in the propagation step by mediation and/or solvation, which impaired the high reactivity of the original growing chain ends. © 2002 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 40: 2209–2214, 2002 相似文献
4.
Irina V. Vasilenko Dmitriy I. Shiman Sergei V. Kostjuk 《Journal of polymer science. Part A, Polymer chemistry》2012,50(4):750-758
The cationic polymerization of isobutylene using 2‐phenyl‐2‐propanol (CumOH)/AlCl3OBu2 and H2O/AlCl3OBu2 initiating systems in nonpolar solvents (toluene, n‐hexane) at elevated temperatures (?20 to 30 °C) is reported. With CumOH/AlCl3OBu2 initiating system, the reaction proceeded by controlled initiation via CumOH, followed by β‐H abstraction and then irreversible termination, thus, affording polymers (Mn = 1000–2000 g mol?1) with high content of vinylidene end groups (85–91%), although the monomer conversion was low (≤35%) and polymers exhibited relatively broad molecular weight distribution (MWD; Mw/Mn = 2.3–3.5). H2O/AlCl3OBu2 initiating system induced chain‐transfer dominated cationic polymerization of isobutylene via a selective β‐H abstraction by free base (Bu2O). Under these conditions, polymers with very high content of desired exo‐olefin terminal groups (89–94%) in high yield (>85%) were obtained in 10 min. It was shown that the molecular weight of polyisobutylenes obtained with H2O/AlCl3OBu2 initiating system could be easily controlled in a range 1000–10,000 g mol?1 by changing the reaction temperature from ?40 to 30 °C. The MWD was rather broad (Mw/Mn = 2.5–3.5) at low reaction temperatures (from ?40 to 10 °C), but became narrower (Mw/Mn ≤ 2.1) at temperatures higher than 10 °C. © 2011 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem, 2012 相似文献
5.
Shokyoku Kanaoka Toshinobu Higashimura 《Journal of polymer science. Part A, Polymer chemistry》1999,37(19):3694-3701
In contrast to the common view, living cationic polymerization of p-methoxy- and p-t-butoxystyrenes proceeded in polar solvents such as EtNO2/CH2Cl2 mixtures, and involvement of free ionic growing species therein was examined. For example, the two alkoxystyrenes were polymerized with the isobutyl vinyl ether-HCl adduct/ZnCl2 initiating system at −15°C in such polar solvents as CH2Cl2 or EtNO2/CH2Cl2 [1/1 (v/v)], as well as toluene. The number average molecular weight (M̄n) of the polymers increased in direct proportion to the monomer conversion, even after sequential monomer addition, and the molecular weight distribution (MWD) stayed very narrow throughout the reaction. In addition, the M̄n agreed with the calculated values, assuming that one adduct molecule generates one living polymer chain. In these polar media the addition of a common ion salt retarded the polymerization, indicating that dissociated ionic species are involved in the propagating reaction. © 1999 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 37: 3694–3701, 1999 相似文献
6.
Motomasa Yonezumi Nanako Takano Shokyoku Kanaoka Sadahito Aoshima 《Journal of polymer science. Part A, Polymer chemistry》2008,46(20):6746-6753
A quite small dose of a poisonous species was found to induce living cationic polymerization of isobutyl vinyl ether (IBVE) in toluene at 0 °C. In the presence of a small amount of N,N‐dimethylacetamide, living cationic polymerization of IBVE was achieved using SnCl4, producing a low polydispersity polymer (weight–average molecular weight/number–average molecular weight (Mw/Mn) ≤ 1.1), whereas the polymerization was terminated at its higher concentration. In addition, amine derivatives (common terminators) as stronger bases allow living polymerization when a catalytic quantity was used. On the other hand, EtAlCl2 produced polymers with comparatively broad MWDs (Mw/Mn ~ 2), although the polymerization was slightly retarded. The systems with a strong base required much less quantity of bases than weak base systems such as ethers or esters for living polymerization. The strong base system exhibited Lewis acid preference: living polymerization proceeded only with SnCl4, TiCl4, or ZnCl2, whereas a range of Lewis acids are effective for achieving living polymerization in the conventional weak base system such as an ester and an ether. © 2008 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 46: 6746–6753, 2008 相似文献
7.
<正>The cationic polymerizations of isobutylene(IB) coinitiated by AlCl_3 were carried out in solvent mixture of n-hexane /methylene dichloride(n-hex/CH_2Cl_2) of 60/40 V/V in the presence of ethyl benzoate(EB) at various temperatures range from-80℃to-30℃.The effects of EB concentration([EB]) and polymerization temperature on monomer conversion,weight-average molecular weight(M_w) and molecular weight distribution(MWD,M_w/M_n) of polyisobutylene (PIB) products were investigated.The rate of polymerization decreased while M_w of PIB products increased with increasing [EB].The polymers with high molecular weight could be prepared in the presence of a suitable amount of EB.Significantly, the polymers with high M_w of 80.2×10~4 and 65.4×10~4 could be produced at-80℃and-70℃at[EB]=0.24×10~(-3) mol/L respectively,which were much higher than that(M_w=57.9×10~4) of PIB prepared at-100℃in the absence of EB.A simple but effective method for preparing the high molecular weight polyisobutylenes was developed in this work.It has been also found that the activation energy for propagation(E_p) depended on the polymerization temperature range in the presence of EB.An obvious inflection of the linear plots of lnX_n versus 1/T_p occurred at the temperature range from-60℃to-50℃at four different concentrations of EB from 0.19×10~(-3) mol/L to 0.33×10~(-3) mol/L,and thus the inflection temperature(T_(inf)) was in the range of-60℃to-50℃.When[EB]was in the range of 0.24×10~(-3) mol/L to 0.33×10~(-3) mol/L,E_p was determined to be around-12 kJ/mol when the polymerization was carried out at temperatures from-80℃to T_(inf) and to be around-28 kJ/mol at temperatures from T_(inf) to-15℃respectively. 相似文献
8.
Yoshiaki Terada Shokyoku Kanaoka Toshinobu Higashimura 《Journal of polymer science. Part A, Polymer chemistry》2000,38(1):229-236
Cationic polymerization of n‐butyl propenyl ether (BuPE; CH3CH CHOBu, cis/trans = 64/36) was examined with the HCl–IBVE (isobutyl vinyl ether) adduct/ZnCl2 initiating system at −15 ∼ −78 °C in nonpolar (hexane, toluene) and polar (dichloromethane) solvents, specifically focusing on the feasibility of its living polymerization. In contrast to alkyl vinyl ethers, the living nature of the growing species in the BuPE polymerization was sensitive to polymerization temperature and solvent. For example, living cationic polymerization of IBVE can be achieved even at 0 °C with HCl–IBVE/ZnCl2, whereas for BuPE whose β‐methyl group may cause steric hindrance ideal living polymerization occurred only at −78 °C. Another interesting feature of this polymerization is that the polymerization rate in hexane is as large as in dichloromethane, much larger than in toluene. A new method in determining the ratio of the living growing ends to the deactivated ones was developed with a devised monomer‐addition experiments, in which IBVE that can be polymerized in a living fashion below 0 °C was added to the almost completely polymerized solution of BuPE. The amount of the deactivated chain ends became small in hexane even at −40 °C in contrast to other solvents. Thus hexane turned out an excellent solvent for living cationic polymerization of BuPE. © 2000 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 38: 229–236, 2000 相似文献
9.
A. V. Orlinkov T. V. Chulochnikova A. I. Nesmelov V. B. Murachev E. A. Ezhova A. M. Evtushenko 《Russian Chemical Bulletin》1996,45(5):1124-1127
The effects of the nature of halogens in the initiatingtert-butyl halide-aluminum-containing Lewis acid system on the number average molecular weightM
n
and the structure of end groups of polyisobutylene macromolecules obtained in the cationic polymerization of isobutylene in hexane at -78 °C were studied. An increase inM
n
is observed in the transition from chlorine to bromine and iodine, accompanied by a decrease in the fraction of end C=C groups and an increase in the relative content of C-Hal groups (Hal = Cl, Br, and I). When atoms of different halogens are present in the counterion, more bulky atoms preferentially participate in the formation of the end groups. The results are interpreted within the framework of the principle of hard and soft acids and bases.Translated fromIzvestiya Akademii Nauk. Seriya Khimicheskaya, No. 5, pp. 1184–1187, May, 1996. 相似文献
10.
A trivalent iron chloride (FeCl3) catalyst induced both living cationic and radical polymerizations of various monomers in the presence of an appropriate additive or ligand to yield polymers with controlled molecular weights and narrow molecular-weight distributions. The in-situ mechanistic transformation from a living cationic to a radical growing species during the styrene polymerization was achieved in a FeCl3-based system with the simple addition of phosphine followed by an elevation of the reaction temperature. The growing cationic species was effectively converted into the radical species to produce a series of block copolymers that consist of styrene and various acrylic monomers. 相似文献
11.
Murachev V. B. Ezhova E. A. Nesmelov A. I. Byrikhin V. S. 《Russian Chemical Bulletin》2003,52(2):403-409
The influence of small concentrations (1—8 mmol L–1) of arenes (viz., hexafluorobenzene, chlorobenzene, benzene, toluene, and mesitylene) on the molecular weight, molecular weight distribution, and degree of functionalization by terminal olefin groups was studied for polymers prepared by low-temperature (–78 °C) isobutylene polymerization in n-hexane initiated by the MeOH—AlBr3 and ButCl—AlBr3 systems. The criteria extent of livingness k
el/k
p were calculated, where k
el and k
p are the rate constants of proton elimination and chain propagation, respectively. It was established that arenes can be involved in proton elimination from the growing carbocation, and their activity in this process increases with an increase in the basicity. Arenonium ions formed by the interaction of arenes with the components of the initiating system or with the growing ionic active centers can form complexes with counteranions, thus retarding proton elimination with the transfer to the counterion. 相似文献
12.
Ludk Toman Miroslav Janata Jií Spv
ek Petr Vl
ek Petra Ltalov Antonín Sikora Bohumil Masa 《Journal of polymer science. Part A, Polymer chemistry》2005,43(17):3823-3830
ABCBA‐type pentablock copolymers of methyl methacrylate, styrene, and isobutylene (IB) were prepared by the cationic polymerization of IB in the presence of the α,ω‐dichloro‐PS‐b‐PMMA‐b‐PS triblock copolymer [where PS is polystyrene and PMMA is poly(methyl methacrylate)] as a macroinitiator in conjunction with diethylaluminum chloride (Et2AlCl) as a coinitiator. The macroinitiator was prepared by a two‐step copper‐based atom transfer radical polymerization (ATRP). The reaction temperature, ?78 or ?25 °C, significantly affected the IB content in the resulting copolymers; a higher content was obtained at ?78 °C. The formation of the PIB‐b‐PS‐b‐PMMA‐b‐PS‐b‐PIB copolymers (where PIB is polyisobutylene), prepared at ?25 (20.3 mol % IB) or ?78 °C (61.3 mol % IB; rubbery material), with relatively narrow molecular weight distributions provided direct evidence of the presence of labile chlorine atoms at both ends of the macroinitiator capable of initiation of cationic polymerization of IB. One glass‐transition temperature (Tg), 104.5 °C, was observed for the aforementioned triblock copolymer, and the pentablock copolymer containing 61.3 mol % IB showed two well‐defined Tg's: ?73.0 °C for PIB and 95.6 °C for the PS–PMMA blocks. © 2005 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 43: 3823–3830, 2005 相似文献
13.
Yu Shinke Arihiro Kanazawa Shokyoku Kanaoka Sadahito Aoshima 《Journal of polymer science. Part A, Polymer chemistry》2013,51(22):4828-4834
The living cationic polymerization of 6‐tert‐butoxy‐2‐vinylnaphthalene (tBOVN), a vinylnaphthalene derivative with an electron‐donating group, was achieved with a TiCl4/SnCl4 combined initiating system in the presence of ethyl acetate as an added base at –30 °C. The absence of side reactions at low temperature was confirmed by 1H NMR analysis of the resulting polymer. In contrast to this controlled reaction at –30 °C, reactions performed at higher temperature, such as 0 °C, frequently involved unwanted intramolecular or intermolecular Friedel–Crafts reactions of naphthalene rings due to the high electron density of these rings. The cationic polymerization of 6‐acetoxy‐2‐vinylnaphthalene, a derivative with an acetoxy group, was also controlled under similar conditions, but chain transfer reactions were not completely suppressed during the polymerization of 2‐vinylnaphthalene. The glass transition temperature (Tg) of the obtained poly(tBOVN) was 157 °C, a value higher by 94 °C than that of the corresponding styrene derivative. © 2013 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2013 , 51, 4828–4834 相似文献
14.
Motomasa Yonezumi Reiko Takaku Shokyoku Kanaoka Sadahito Aoshima 《Journal of polymer science. Part A, Polymer chemistry》2008,46(6):2202-2211
Cationic polymerization of α‐methyl vinyl ethers was examined using an IBEA‐Et1.5AlCl1.5/SnCl4 initiating system in toluene in the presence of ethyl acetate at 0 ~ ?78 °C. 2‐Ethylhexyl 2‐propenyl ether (EHPE) had a higher reactivity, compared to corresponding vinyl ethers. But the resulting polymers had low molecular weights at 0 or ?50 °C. In contrast, the polymerization of EHPE at ?78 °C almost quantitatively proceeded, and the number‐average molecular weight (Mn) of the obtained polymers increased in direct proportion to the EHPE conversion with quite narrow molecular weight distributions (weight‐average molecular weight/number‐average molecular weight ≤ 1.05). In monomer‐addition experiments, the Mn of the polymers shifted higher with low polydispersity as the polymerization proceeded, indicative of living polymerization. In the polymerization of methyl 2‐propenyl ether (MPE), the living‐like propagation also occurred under the reaction conditions similar to those for EHPE, but the elimination of the pendant methoxy groups was observed. The introduction of a more stable terminal group, quenched with sodium diethyl malonate, suppressed this decomposition, and the living polymerization proceeded. The glass transition temperature of the obtained poly(MPE) was 34 °C, which is much higher than that of the corresponding poly(vinyl ether). This poly(MPE) had solubility characteristics that differed from those of poly(vinyl ethers). © 2008 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 46: 2202–2211, 2008 相似文献
15.
Turgut Nugay Balazs L. Keszler Tejal Deodhar Nihan Nugay Joseph P. Kennedy 《Journal of polymer science. Part A, Polymer chemistry》2017,55(22):3716-3724
We describe the discovery of novel low cost bifunctional initiators 2,4,7,9‐tetramethyl‐tricyclo[6.2.0.036]deca‐1(8),2,6‐triene‐4,9‐diol (bBCB‐diOH) and 4,9‐dichloro,2,4,7,9‐tetramethyl‐tricyclo[6.2.0.036]deca‐1(8),2,6‐triene (bBCB‐diCl), for living cationic bidirectional polymerization of olefins, for example, isobutylene. bBCB‐diOH was quantitatively synthesized in one step by UV radiation of commercially available diacetyl durene (DAD) and bBCB‐diCl by hydrochlorination of bBCB‐diOH. These molecules, in conjunction with TiCl4 coinitiator, initiate the living polymerization of isobutylene. Livingness was demonstrated by linear conversion versus molecular weight (MW) plots and narrow MW distributions. Polymerizations are slower than those initiated by the universally used “hindered” bifunctional initiator 5‐tert‐butyl‐1,3‐bis(1‐chloro‐1‐methyl)benzene and are suitable for rate studies. Herein, we report the synthesis, by the use of bBCB‐diCl, of relatively low MW (M n < 3000 g mol?1) allyl‐telechelic polyisobutylene (PIB) used for the synthesis of PIB‐based polyurethanes and that of relatively high MW (M n > 30,000) living PIB telechelics for the synthesis of thermoplastic elastomers. © 2017 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2017 , 55 , 3716–3724 相似文献
16.
Motomasa Yonezumi Shokyoku Kanaoka Sadahito Aoshima 《Journal of polymer science. Part A, Polymer chemistry》2008,46(13):4495-4504
Cationic polymerization of 2,3‐dihydrofuran (DHF) and its derivatives was examined using base‐stabilized initiating systems with various Lewis acids. Living cationic polymerization of DHF was achieved using Et1.5AlCl1.5 in toluene in the presence of THF at 0 °C, whereas it has been reported that only less controlled reactions occurred at 0 °C. Monomer‐addition experiments of DHF and the block copolymerization with isobutyl vinyl ether demonstrated the livingness of the DHF polymerization: the number–average molecular weight of the polymers shifted higher with low polydispersity as the polymerization proceeded after the monomer addition. Furthermore, this base‐stabilized cationic polymerization system allowed living polymerization of ethyl 1‐propenyl ether and 4,5‐dihydro‐2‐methylfuran at ?30 and ?78 °C, respectively. In the polymerization of 2,3‐benzofuran, the long‐lived growing species were produced at ?78 °C. The obtained polymers have higher glass transition temperatures compared to poly(acyclic alkyl vinyl ether)s. © 2008 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 46: 4495–4504, 2008 相似文献
17.
Alexei V. Radchenko Sergei V. Kostjuk Irina V. Vasilenko François Ganachaud Fyodor N. Kaputsky Yohann Guillaneuf 《Journal of polymer science. Part A, Polymer chemistry》2008,46(20):6928-6939
A kinetic study of the living cationic polymerization of p‐methoxystyrene using 1‐(4‐methoxyphenyl)ethanol ( 1 )/B(C6F5)3 initiating system in a mixture of CH3CN with CH2Cl2 1:1 (v/v) at room temperature was carried out utilizing a wide variety of conditions. The polymerization proceeded in a living fashion even in the presence of a large amount of water ([H2O]/[B(C6F5)3] ratio up to 20) to afford polymers whose Mn increased in direct proportion to monomer conversion with fairly narrow MWDs (Mw/Mn ≤ 1.3). The investigation revealed that the rate of polymerization was first‐order in B(C6F5)3 concentration, while a negative order in H2O concentration close to ?2 was obtained. It was also found that the rate of polymerization decreased with lowering temperature, which could be attributed to a decreased concentration in free Lewis acid, the true coinitiator of polymerization. A mechanistic scheme to explain the kinetic behavior of living p‐methoxystyrene polymerization is proposed, which has been validated by PREDICI simulation on multiple‐data curves obtained by 1H NMR in situ polymerization experiment. © 2008 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 46: 6928–6939, 2008 相似文献
18.
Masami Kamigaito Mitsuo Sawamoto Toshinobu Higashimura 《Journal of polymer science. Part A, Polymer chemistry》1991,29(13):1909-1915
Trimethylsilyl halides (Me3SiY), in conjunction with zinc halides (ZnX2) (Y and X:I, Br, Cl), were employed to investigate the living cationic polymerization of isobutyl vinyl ether (IBVE) in toluene at ?15°C in the presence of p-methoxybenzaldehyde; with the aldehyde and IBVE monomer, Me3SiY yields an initiating species [Me3Si? O? CHC6H4(OMe) ? CH2CH(OiBu) ? Y] that triggers the IBVE polymerization via the activation of its carbon-halogen bond (C? Y) by ZnX2 into Cδ+…?Yδ?…?ZnX2. Living polymerizations occurred with the silyl iodide and bromide irrespective of the type of ZnX2, either when Y = X (Me3Sil/Znl2 and Me3SiBr/ZnBr2) or when Y ≠ X (Me3Sil/ZnBr2, Me3SiI/ZnCl2, and Me3SiBr/Znl2). With these five initiating systems, the number-average molecular weights (M?n) of the polymers increased in proportion to monomer conversion, and the molecular weight distributions (MWDs) of the polymers were narrow (M?w/M?n = 1.1?1.2). The Me3SiCl-based systems (Me3SiCl/ZnCl2 and Me3SiCl/Znl2), in (Me3SiCl/Znl2), in contrast, failed to give perfectly living polymerization; the M?n indeed increased with conversion, but the MWDs of the polymers were broader (M?w/M?n = 1.3?1.5). Thus, the living nature of the polymerizations with Me3SiY/Znx2 is primarily determined by the halogen Y in Me3SiY, which generates the terminal carbon-halogen bond (C? Y) that is activated by ZnX2 for the propagation via a species Cδ+…?Yδ?…?ZnX2. For Y?, not only the iodide but the bromide anion also is suited for living cationic polymerization. The virtual absence of the effects of X in ZnX2 implies that the halogen exchange between ZnX2 and Y from Me3 SiY at the growing end (Cλ+…?Yδ?…?ZnX2 ?Cδ+…?Xδ?…?ZnXY) is absent or negligible. 相似文献
19.
20.
Sergei V. Kostjuk Hui Yee Yeong Brigitte Voit 《Journal of polymer science. Part A, Polymer chemistry》2013,51(3):471-486
This review highlights recent approaches toward polyisobutylene (PIB) by an energy efficient room temperature cationic polymerization. Special focus is laid on our own work using modified Lewis acids and nitrile‐ligated metal complexes associated with weakly coordinating anions. In both cases, suitable conditions have been found for efficient production of PIB characterized by medium to low molar masses and a high content of exo double bonds as end groups—the typical features of highly reactive PIB, an important commercial intermediate toward oil and gasoline additives. These and other approaches demonstrate that the cationic polymerization of isobutylene is still not fully explored, and new innovative catalyst systems can lead to surprising results of high commercial interest. © 2012 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem, 2013 相似文献