Poly(vinyl alcohol) (PVA) cryogels (PVACGs) are obtained and studied. The PVACGs are formed by freezing–defrosting of polymer solutions in dimethyl sulfoxide (DMSO) or its mixtures with one of the first members of the series low-molecular-mass aliphatic alcohols (methanol, ethanol, n-propanol, and n-butanol). PVA content in these solutions is 100 g/L, while the concentration of an aliphatic alcohol is varied in a range of 0.44–2.55 mol/L depending on its nature. The polymer solutions are subjected to the cryogenic treatment at temperatures 30, 40, or 50°C lower than the crystallization temperature of DMSO (+18.4°C). The frozen samples are defrosted at a heating rate of 0.03°C/min. It is shown that, in a certain range of lowmolecular-mass alcohol content in an initial system, its cryogenic treatment yields coarse-pored heterophase cryogels that have higher rigidity and heat endurance than those of DMSO–PVA cryogels. It has been shown that polymer cryoconcentration and phase separation play important roles in the formation of a cellular microstructure and an increase in the rigidity and heat endurance of PVACGs obtained in the presence of low-molecular-mass alcohols.  相似文献   

2.
The microstructure of complex and composite poly(vinyl alcohol) (PVA) cryogels containing water-soluble chitosan hydrochloride (ChHC) of dispersed particles of water-insoluble chitosan base (Ch), respectively, has been studied by optical microscopy and attenuated total reflection FTIR spectroscopy. The macroporous morphology of cryogels has been studied using preparations in the form of thin (~10 μm) sections and discs 1 mm thick. The introduction of non-gelling additives (NaCl and ChHC) into an initial PVA solution causes significant changes in the size and shapes of macropores in the complex cryogels formed by freezing–defrosting, as compared with the pores in the samples obtained under the same conditions without additives. The reasons for the changes are the process of phase segregation and the influence of low- and high-molecular-weight electrolytes on crystallization of ice, which plays the role of a porogen upon cryotropic gelation of aqueous PVA solutions. As a result of an alkaline treatment of the complex cryogels, which transforms ChHC into Ch, microcoagulation of chitosan yields discrete, almost spherical, particles with sizes of about 1–5 μm. IR spectral studies have shown that concentration gradients of the gelling and nongelling polymers arise along the thickness of the gel discs, with PVA concentration prevailing near the lower surface and ChHC or Ch concentration dominating near the upper surface of the disc.  相似文献   

3.
Graft polymerization using potassium diperiodatocuprate as initiator was found to be an effective and convenient method for grafting functional polymer of N,N-dimethylaminoethyl methacrylate (DMAEMA) onto superporous polyacrylamide gels, so-called cryogels (pAAm cryogels). It was possible to achieve grafting degrees up to 110% (w/w). The two-step graft polymerization i.e. first activation of the matrix followed by displacement of initiator solution with the monomer solution, decreased pronouncedly the soluble homopolymer formation. The efficiency of graft polymerization using a two-step technique increased up to 50% (w/w) at a monomer conversion of 10%, compared to 10% graft efficiency with 60-70% monomer conversion for one-step direct graft polymerization. The pAAm cryogels grafted in one-step and two-step procedures, respectively, behaved similarly when binding low-molecular weight ligand but showed very different behavior for sorption of a high-molecular-weight ligand, bovine serum albumin (BSA). The differences in behavior were rationalized assuming different structure of the graft polymer layers and tentacle-type BSA binding to the grafted polymer.  相似文献   

4.
Complex macroporous poly(vinyl alcohol) (PVA) cryogels have been obtained by cryogenic treatment (freezing at–20°C for 12 h followed by defrosting at a rate of 0.03°C/min) of PVA–chitosan hydrochloride mixed solutions. The subsequent alkaline treatment of the cryogels has resulted in the transformation of the water-soluble salt form of chitosan into its insoluble basic form, which coagulates inside the bulk of the continuous phase of PVA cryogel into small particles with sizes of 2–5 µm. In the resulting composite cryogels, these particles play the role of an “active” filler, which increases the rigidity and heat endurance of the gel material. It has been shown that the sorption capacity of such chitosan particles entrapped into the bulk of composite cryogels with respect of bivalent copper ions is noticeably higher than the sorption capacity of ground chitosan particles incorporated as a discrete filler into the continuous phase PVA cryogels. The study of the properties of PVA–chitosan hydrochloride mixed solutions revealed that these polymers are, to a large extent, compatible with one another in a common solvent at a low ionic strength. Therefore, liquidliquid phase separation of these systems due to the thermodynamic incompatibility of macromolecules of different natures is observed only upon increasing the ionic strength by adding a low-molecular-mass salt (NaCl, 0.15 mol/L) to the solution.  相似文献   

5.
The mechanism of cryotropic gelation in moderately frozen solutions of chitosan crosslinked by glutaric aldehyde is studied. Chitosan cryogels with large pores are synthesized at a low content of crosslinking agent in the reaction mixture or under conditions that do not lead to gelation at temperatures above 0°C. The dependences of the yield of gel fractions, the degree of swelling of the polymer phase of cryogels, and the hydrodynamic characteristics of cryogels on the temperature of synthesis are shown to be extremal. This result may be explained by the competition between the cryoconcentration of reagents in the nonfrozen liquid microphase, which assists the development of a crosslinked polymer network, and such factors as an increase in the viscosity of the reaction mixture and a reduced reagent mobility, which prevent gelation. The morphology of chitosan cryogels is studied, and the character of the macroporous structure of the samples prepared at different temperatures is shown to exert a stronger effect on the hydrodynamic characteristics of a cryogel than the degree of swelling of crosslinked polymers in the walls of its macropores.  相似文献   

6.
Composite cryogels simulating the properties of waterproof screens of hydraulic structures, such as protruding dykes and dams, have been obtained by a cryogenic treatment (freezing at –10…–30°C followed by incubation in the frozen state for 12 h and defrosting at a rate of 0.03°C/min) of suspensions of calcium-carbonate-containing (marble or coquina) or cellulose-containing (microcrystalline cellulose or sawdust) particles in aqueous poly(vinyl alcohol) solutions. Viscometric examinations of initial suspensions have shown that adhesion contacts arise between filler particles, as well as discrete and continuous phases, already at the stage of suspension preparation, thereby affecting the properties of resulting cryogels. This is most pronounced when high-porosity sawdust is used as a filler. It has been shown that all the dispersed materials used in the work are “active” fillers for poly(vinyl alcohol) cryogels, these fillers increasing the rigidity of the formed composites. Therewith, porous particles, into which the polymer solution can penetrate, are more efficient. The dependence of the composite rigidity on the temperature of the cryogenic treatment has, as a rule, a bell-shaped pattern with a maximum in the region of –20°C. Being tested for water permeability, the obtained model composite cryogels have exhibited pronounced antifiltration properties (the filtration coefficient is ≤(1–2) × 10–9 cm/s), thus indicating that such materials are promising for solving problems relevant to the protection of fascine hydraulic structures from erosion with snow water.  相似文献   

7.
The photophysical behavior of a hydrophobically tailored water-soluble polymer, pyrene-end-capped poly(ethylene oxide) (PYPY), has been studied in aqueous buffered bovine serum albumin (BSA) and human serum albumin (HSA) media. In buffered aqueous solution the polymer shows dual emission corresponding to the monomer and the excimer of pyrene moiety. The relative intensity of the monomer to the excimer emission shows interesting variation with the addition of BSA and HSA and is indicative of significant interaction of these albumin proteins with the polymer. The binding interaction has been shown to have a prominent role on the steady state fluorescence anisotropy of the two emission bands. Attempt has been made to determine the micropolarities of the protein microenvironments from a comparison of the variation of the monomer to excimer relative fluorescence intensities of the probe in water–dioxane mixtures with varying composition.  相似文献   

8.
The multicomponent self-diffusion of the polyvinyl alcohol (PVA) cryogels prepared by a freezing-thawing treatment of aqueous and water-DMSO solutions of PVA has been studied with the NMR FT-PGSE method. The temperature dependencies of the self-diffusion coefficients, Ds, for the PVA chains have a maximum at 45 degrees C due to the syneresis of cryogels. They are quite different from the monotonous increase of Ds for the aqueous solutions of PVA. Evaluated apparent activation energies, Ea, of the self-diffusion for the PVA chains in the PVA solutions and cryogels in D2O are practically the same and equal 22-24 kJ/mol below the crucial point. The proton spin-lattice relaxation times, T1, of the PVA chain also coincide with one another for solutions and cryogels. This means that molecular packing in cryogels depends mainly on the dimensions of the ice and polymer microcrystallites formed by freezing the solution. Above the crucial point polymer compartments become firmer, and the chain mobility somewhat reduces. The strength of cryogels also increases along with growing the DMSO contents and decreases by the BSA addition. For estimation of the cryogel morphology, effects of the restricted diffusion of both the water and PVA in a q-space have been taken into account. By the introduction of DMSO to cryogels the solvent filled pores become smaller, and channels become much shorter. The diameter of the PVA filaments is similar to those for all the cryogels, but the length of filaments with D2O is twice that for cryogels with a mixed solvent. Entrapment of BSA in the cryogel matrix by preparation leads to the increase of an average diameter of the water filled pores and destroys molecular packing the cryogel. Copyright 1999 Academic Press.  相似文献   

9.
The present paper discusses synthesis, characterization, and blood compatibility studies of macroporous cryogels of PVA and starch. Biocompatible spongy porous hydrogels of polyvinyl alcohol–starch have been synthesized by repeated freezing–thawing methods and characterized by Infra red (FTIR) and environmental scanning electron microscopy (ESEM) techniques, respectively, to gain insights for structural and morphological features. The FTIR analysis of prepared cryogels indicated that starch was introduced into the network of cryogel possibly via formation of hydrogen bonds between the PVA and starch clusters. The “cryogels” were evaluated for their water uptake potentials and influence of various factors such as chemical architecture of the spongy hydrogels, pH and temperature of the swelling bath were investigated on the degree of water sorption by the cryogels. The hydrogels were also swollen in salt solutions and various simulated biological fluids. The biocompatibility of the prepared cryogels was judged by in vitro methods of blood–clot formation viz. percent haemolysis and protein (BSA) adsorption. The cryogels were also studied for their pores morphology and percent porosity and the effect of chemical composition on the extent of porosity was also investigated.  相似文献   

10.
A novel macroporous poly(glycidyl methacrylate-triallyl isocyanurate-divinylbenzene) matrix was prepared by a radical suspension copolymerization. The matrix contained epoxy groups, so diethylaminohydroxypropyl groups were coupled to the matrix, leading to an anion-exchange resin. We studied the components, surface and pore structures of the anion-exchange resin by Fourier transform infared spectroscopy and scanning electron microscopy (SEM). SEM observations showed that the resin abounded in macropores as large as 3 to 8 microns both in the surface and the interior. The back-pressure of the column packed with the resin was modest even at a high flow-rate (60.2 cm/min). Then, bovine serum albumin (BSA) was used as a model protein to examine the adsorption properties of the anion-exchange resin. The results showed that under optimum conditions the resin had a capacity as high as 22.8 mg BSA/g wet resin, or 68.7 mg/g dry resin. The adsorbed protein could be desorbed by increasing the liquid phase ionic strength. Most importantly, the matrix had little nonspecific adsorption for BSA before introducing the ion-exchange groups.  相似文献   

11.
The macroporous conducting polymer cryogels were prepared by the oxidation of aniline hydrochloride in the frozen aqueous solutions of poly(vinyl alcohol) at ? 24 °C. Corresponding polyaniline aerogels supported with poly(vinyl alcohol) have been obtained after thawing of cryogels followed by freeze-drying. Silver was deposited on the composites using the ability of polyaniline to reduce silver ions after the immersion in silver nitrate solutions. Swollen cryogels were coated only on the surface with macroscopic silver particles due to the closed-pore structure in cryogels and limited penetration of silver ions into macropores. The diffusion of silver ions to freeze-dried aerogels was better and further improved by vacuum treatment. Silver microcubes were produced in the pores, the weight fraction of silver in dry composites being typically several per cent, a maximum 13 wt%. The conductivity of the aerogels compressed to pellets depended on the processing and the highest value was 0.27 S cm?1. The aerogels containing silver were characterized in detail with Raman spectroscopy.  相似文献   

12.
Macroporous viscoelastic poly(vinyl alcohol) (PVA) cryogels were prepared from aqueous PVA solutions containing additives (0–1.2 mol/l) of alkali metal chlorides (LiCl, NaCl, KCl, CsCl) by cryogenic treatment (freezing at −20°C for 12 h and subsequent thawing at a rate of 0.03°C/min). Shear moduli and fusion temperatures of corresponding samples were determined and the structure of thin sections was studied by optical microscopy with subsequent processing and analysis of images obtained. It was shown that the rigidity, heat endurance, and mean pore sizes of formed cryogels monotonically decrease with increasing content of chaotropic lithium chloride. In the case of other three salts, the dependences of rheological characteristics of cryogels on the concentration of low-molecular-weight electrolyte were extreme due to the competition between factors that promote and prevent PVA cryotropic gelation. At the same time, fusion temperatures of gel samples increased steadily with increasing content of these salts. Microscopic studies revealed substantial (by factor of two to three) decrease in macropore sizes even at low content of salt compared to mean cross sections of pores in cryogel containing no additive; morphometric analysis of obtained images makes it possible to reveal the linear correlations between the rheological characteristics of cryogels formed in the presence of LiCl and the sizes of their macropores.  相似文献   

13.
A Fourier transform infrared (FTIR) spectroscopy assay to measure hydrogen–deuterium exchange (HDX) in surface‐adsorbed protein monolayers is developed to provide information on protein tertiary structure, because the typical secondary structural analysis of our surface and solution protein samples proved to be very similar. Adsorbed protein HDX is quantified by exposing the protein to a 50% deuterated NaPO4 buffer solution and then measuring the normalized intensity change of the amide II band in the FTIR reflection spectrum. When collected as a function of exchange time, this intensity follows the kinetics of the exposure of the protein amides to solvent. HDX kinetics have been obtained for bovine serum albumin (BSA) in solution and adsorbed to gold surfaces. Using experiments designed to allow comparisons between protein in solution and on surfaces, the extent of HDX was found to increase over that observed for BSA in solution, consistent with an increase in the exposure of albumin amide groups and protein unfolding upon adsorption. We also show that BSA adsorbs to the surface of gold in multilayers and that the increase in amide exposure is present only in the first adsorbed monolayer. Published in 2009 by John Wiley & Sons, Ltd.  相似文献   

14.
Poly(vinyl alcohol) cryogels are obtained and investigated. The cryogels are prepared by freezing an initial polymer solution (100 g/L) at chilling rates of 1.85, 0.3, 0.03, or 0.003°C/min followed by defrosting the frozen (?20°C/12 h) preparations at heating rates of 0.3, 0.03, or 0.003°C/min. It is shown that a noticeable influence of the chilling rate on the rigidity and heat endurance of the gel matrix is observed at very slow regimes of chilling (on the order of thousandths of degree centigrade per minute). One of the reasons for a reduction in the rigidity of resulting cryogels and the fusion enthalpy of the nodes in their supramolecular networks is the formation of a homo-phase hydrogel during the long-term exposure of the concentrated polymer solution to low temperatures prior to the onset of ice crystallization. The effect of the regime of chilling the polymer solution being frozen on the porous structure of cryogels resulting from the thawing of the preparations is ambiguous due to the multifactor character of this effect; therefore, in many cases, well-defined structure-property correlations are not observed.  相似文献   

15.
In this paper, graphene oxide nanosheets (GOS) are functionalized by bovine serum albumin (BSA) via diimide-activated amidation under ambient conditions. The obtained GOS–BSA conjugate is highly water-soluble. Results of atomic force microscopy (AFM), Raman spectra and Fourier transform infrared spectroscopy analysis confirm that GOS–BSA conjugate contains both GOS and BSA protein. AFM image shows that GOS are fully exfoliated. Results of cyclic volatammograms show that the protein in the GOS–BSA conjugate retains its bioactivity. The present method may also provide a way to synthesize graphene-based composites with other biomolecules.  相似文献   

16.
Rheological properties of the cryogels produced by freezing of concentrated aqueous solutions of poly(vinyl alcohol) have been studied. These properties were shown to depend on the polymer concentration in the initial solution, on PVA molecular weight, cryostructurization duration and temperature. Electron microscopy demonstrates the heterogeneous porous structure of these cryogels and the dependence of the observed pattern on the conditions of formation of the studied objects.  相似文献   

17.
Foams have been generated from aqueous poly(vinyl alcohol) solution by two different methods: dispersion (mechanical) method, i.e., by bubbling a gas through a porous medium into the aqueous poly(vinyl alcohol) solution, and the condensation (chemical) method, i.e., by performing a gas-generating reaction directly in the polymer solution. The effect of the formation method on foam stability and dispersity has been studied. The foam produced by the condensation method of foaming the aqueous poly(vinyl alcohol) solution with nitrogen is more stable and finely dispersed and has a higher expansion ratio than that obtained by bubbling the gas through the polymer solution. Foamed cryogels have been formed by freezing-thawing the foam resulting from the chemical reaction in the polymer solution. The values of the elasticity modulus, melting temperature, and thermal conductivity of the cryogels have been determined.  相似文献   

18.
An experimental study on the interplay of sorbent structure and fluid phase conditions (pH) has been carried out examining adsorption and transport of bovine serum albumin (BSA) and a monoclonal antibody (IgG 2a) on SP Sepharose Fast Flow and SP Sepharose XL. SP Sepharose Fast Flow is characterised by a relatively open pore network, while SP Sepharose XL is a composite structure with ligand-carrying dextran chains filling the pore space. Both adsorbents have similar ionic capacity. Protein transport and adsorption profiles were evaluated using confocal laser scanning microscopy. Under all investigated conditions, BSA uptake could be adequately explained by a pore diffusion mechanism. The adsorption profiles obtained for IgG 2a, however, indicated that changes in fluid phase conditions as well as a change in the solid phase structure could result in a more complex uptake mechanism as compared to pore diffusion alone. This mechanism results in a fast transport of proteins into the adsorbent, followed by an overshoot of protein in the center of the sorbent and a setback towards a homogeneous adsorption profile.  相似文献   

19.
周艳梅  徐文国  童爱军 《分析化学》2006,34(11):1551-1554
报道了以氨丙基硅胶为载体,将其表面醛基化后通过亚胺键共价键合牛血清白蛋白,再用两种硅烷化试剂氨丙基三乙氧基硅烷和正辛基三甲氧基硅烷进行聚合,合成表面印迹牛血清白蛋白分子印迹聚合物的方法。本方法以共价键印迹蛋白质,用草酸洗脱。表面印迹有利于大分子蛋白质向印迹位点的扩散和再结合,合成的印迹聚合物对牛血清白蛋白的吸附率达44.5%,而其它蛋白的吸附率小于17%,显示对模板蛋白具有特异吸附能力。  相似文献   

20.
A complex of physicochemical methods was used to study the aggregation characteristics of an imidazolium-containing amphiphile and its ability for complex formation with bovine serum albumin (BSA). Tensiometry showed that adding BSA to the surfactant decreases the aggregation threshold of the system by a factor of 50. Dynamic light scattering established, that the size of the surfactant–BSA complexes depends on the size of the polypeptide (6–10 nm) and is independent on the concentrations of the surfactant and BSA. The Stern?Volmer constants and surfactant?protein binding constants were calculated from fluorescence spectroscopy data.  相似文献   