以辛酸亚锡为催化剂, 胆固醇(CHOL)为共引发剂引发D,L-丙交酯开环聚合, 制备了胆固醇-g-聚(D,L-乳酸)(CHOL-g-PDLLA)低聚物, 采用偏光显微镜(POM)和差示扫描量热(DSC)方法考察了其液晶特性. 通过静电纺丝技术制备了CHOL/PDLLA和CHOL-g-PDLLA /PDLLA复合纳米纤维膜, 对其形貌、界面相容性、孔隙率、拉伸性能和细胞相容性进行了研究. 结果表明, CHOL-g-PDLLA为一种热致胆甾型液晶, 液晶温度区间为21.8~74.5 ℃; CHOL-g-PDLLA/PDLLA复合纳米纤维膜的纤维形态良好, 表面均匀光滑, 孔隙率在70%~75%之间, 且其界面相容性优于相应的CHOL/PDLLA. 随着CHOL和CHOL-g-PDLLA含量的增加, 复合纳米纤维膜的拉伸强度逐渐下降, 但CHOL-g-PDLLA/PDLLA复合纳米纤维膜的拉伸强度显著大于CHOL/PDLLA. 体外骨髓间充质干细胞培养结果显示, CHOL-g-PDLLA/PDLLA复合纳米纤维膜具有良好的细胞相容性, 且优于相应的PDLLA和CHOL/PDLLA纳米纤维膜.  相似文献   

2.
静电纺丝法制备NiO纳米纤维及其表征   总被引:8,自引:0,他引:8  
纳米级NiO因具有优良的催化和热敏等性能而被广泛用于催化剂[1]、电池电极[2,3]、光电转化材料[4~6]、电化学电容器[7~8]等诸多方面.迄今,已成功地制备出N iO的纳米颗粒[9]、纳米线[10]及纳米薄膜[11],但是对于具有准一维结构的NiO纳米纤维的制备及性能研究尚未见报道.  相似文献   

3.
在静电纺丝纳米纤维中加入纳米填料——石墨烯(G),有助于提高纳米纤维的性能,扩展其应用领域。本文综述了近年来国内外静电纺丝制备石墨烯基复合纳米纤维的研究现状,重点介绍了石墨烯与聚酰胺(PA)、聚甲基丙烯酸甲酯(PMMA)、聚丙烯腈(PAN)、二氧化钛(TiO2)等复合纳米纤维制备的研究进展及其在光催化剂、超级电容器、染料敏化太阳能电池(DSSCs)、传感器、生物医学等方面的应用潜力,展望了石墨烯基复合纳米纤维的发展前景。  相似文献   

4.
静电纺丝技术就是通过带电聚合物溶液或熔体的喷射来制备纳米纤维,是一种制备纳米纤维材料简单有效的技术。醋酸纤维素(CA)易溶于有机溶剂,常作为纤维素的替代材料应用于静电纺丝领域。本文总结了近年来国内外采用静电纺丝技术制备CA复合纳米纤维的研究新进展,重点介绍了CA/CNTs复合纳米纤维、CA/金属粒子复合纳米纤维、CA/金属氧化物复合纳米纤维、CA基载药复合纳米纤维、CA/PAN复合纳米纤维、CA/PVA复合纳米纤维、CA/CS复合纳米纤维等CA复合纳米纤维的研究进展以及潜在的应用领域。  相似文献   

5.
碳纳米管(CNTs)作为增强材料与聚合物复合制成纳米纤维,有助于提高纳米纤维性能,扩展其应用领域。本文综述了近年来国内外静电纺丝制备CNTs基复合纳米纤维的研究现状,重点介绍了CNTs/PAN复合纳米纤维、CNTs/PANI/PEO复合纳米纤维、CNTs/PVA复合纳米纤维、CNTs/PA复合纳米纤维、CNTs/TiO2复合纳米纤维的研究进展及其在纳米传感器、电磁干扰、超级电容器、染料敏化太阳能电池(DSSCs)、组织工程支架、药物控制释放等方面的应用潜力,展望了CNTs基复合纳米纤维的发展前景。  相似文献   

6.
采用静电纺丝技术将导电聚苯胺(PANI)和铕/铽稀土配合物掺杂到高分子基质聚乙烯吡咯烷酮(PVP)中,制备出荧光导电复合纳米纤维。用扫描电镜(SEM)、荧光光谱仪(FL)、宽频介电松驰谱仪对荧光导电复合纳米纤维的性能进行分析,结果显示,在270nm紫外光激发下,铕系列与铽系列复合纳米纤维分别发出红光和绿光。同时,复合纳米纤维的电导率可以达到1.18×10~(-6) S/cm,两种复合纳米纤维同时具有优异的荧光性能及良好的导电功能。  相似文献   

7.
静电纺丝法制备超细聚苯乙烯纳米纤维   总被引:1,自引:0,他引:1  
采用静电纺丝方法制备了超细聚苯乙烯纤维, 通过向溶液中添加有机胺盐并降低溶液浓度将纤维的平均直径降至100 nm, 并研究了盐的添加量对纤维直径的影响.  相似文献   

8.
静电纺丝法制备Y2O3纳米纤维与表征   总被引:1,自引:0,他引:1  
采用静电纺丝法制备了PVA/Y(NO3)3复合纳米纤维,在适当的温度下进行热处理,得到Y2O3纳米纤维. 利用XRD,SEM,TG-DTA,FTIR等现代分析手段对样品进行了表征. XRD分析表明,PVA/Y(NO3)3复合纤维为无定型,焙烧温度在600 ℃以上得到晶态单相的Y2O3纳米纤维,属于立方晶系,空间群为Ia3. SEM分析表明,PVA/Y(NO3)3复合纤维表面光滑,平均直径为110 nm. 焙烧温度对Y2O3纳米纤维的形成有重要影响. 600 ℃焙烧得到的Y2O3纳米纤维的平均直径约50 nm,900 ℃焙烧得到的Y2O3纳米纤维由纳米颗粒堆积而成,部分已断裂. TG-DTA和FTIR分析表明,PVA,Y(NO3)3以及水分在600 ℃以上时完全分解挥发,最终样品为晶态单相的Y2O3纳米纤维.  相似文献   

9.
聚氧化乙烯(PEO)是一种多功能的水溶性聚合物,因其良好的水溶性、低毒性、容易制备等优点而广泛应用于各种领域。本文综述了近年来国内外静电纺丝制备聚氧化乙烯复合纳米纤维的研究现状,重点介绍了CS/PEO复合纳米纤维、PANi/PEO复合纳米纤维、SA/PEO复合纳米纤维、Cellulose/PEO复合纳米纤维、MEH-PPV/PEO复合纳米纤维的研究进展及其在传感器、组织工程支架、过滤材料、医学领域的外伤敷料、电磁屏蔽材料领域的应用,分析了其潜在的应用领域,展望了聚氧化乙烯复合纳米纤维的发展前景。  相似文献   

10.
静电纺丝法制备聚丙烯腈/聚苯胺复合纳米纤维及其表征   总被引:1,自引:0,他引:1  
利用静电纺丝技术,以聚丙烯腈(PAN)和苯胺(ANI)为前驱物,用过硫酸胺(APS)溶液在低温下缓慢氧化聚合,制备了PAN/PANI复合纳米纤维,直径约500 nm.通过扫描电子显微镜(SEM)、红外光谱(FTIR)、X射线衍射(XRD)和激光拉曼(RAMAN)光谱仪等测试手段对材料的形貌和结构进行了表征.探讨了材料制备过程中影响纤维形貌、尺寸、均匀度的因素和PANI含量对复合纤维导电性能的影响,结果表明,PAN浓度、ANI的加入量和电压是影响纤维特性的主要因素;PANI在PAN基体中呈纳米尺寸分布,复合纳米纤维具有良好的导电性能,导电率可达10-2S/cm.  相似文献   

11.
首先,采用乳酸为引发剂,辛酸亚锡为催化剂,引发丙交酯开环聚合制得具有缩聚活性的L-聚乳酸和D-聚乳酸;然后,将两者熔融共混后进行固相缩聚,合成了一系列立体嵌段聚乳酸。采用核磁共振(NMR)、凝胶渗透色谱(GPC)及差示扫描量热仪(DSC)分析了产物的链结构、重均分子量、热性能,并探讨了均相晶体和立体复合晶体共存情况下的固相缩聚机理。结果表明,固相缩聚产物分子量增长的适宜反应条件为:反应时间30h,较低的催化剂含量,L-聚乳酸质量分数为80%。L-聚乳酸和D-聚乳酸共混物较低的初始立体复合晶体结晶度有利于后续固相缩聚过程中产物分子量的增长;固相缩聚不仅发生在异链之间,而且也发生在同链之间。  相似文献   

12.
13.
聚乳酸/蒙脱土纳米复合材料的结构和热性能   总被引:6,自引:0,他引:6  
聚乳酸/蒙脱土纳米复合材料的结构和热性能;聚乳酸;蒙脱土;纳米复合材料;插层  相似文献   

14.
In this study an integrated methodology was proposed for the selection of solvent systems to produce electrospinnable solutions that form defect‐free poly(lactic acid) (PLA) fibers with narrow diameter distributions. The solvent systems were chosen using a thermodynamic approach, combined with electrical and rheological property criteria. More specifically, the three step methodology includes (1) initial choice of solvent by solubility evaluation to meet thermodynamic criteria, (2) electrical properties, that is, conductivity and dielectric constant adjustment by using solvent mixtures to meet electrical property criteria, and (3) critical entanglement concentration (Ce) determination by viscosity measurements, supported by elastic and plastic moduli measurements, followed by concentration adjustment to meet rheological criteria. All three criteria need to be met to ensure defect‐free nanofiber morphology. The methodology was demonstrated using PLA solutions that were characterized in terms of thermodynamic properties, conductivity, surface tension, and viscosity measurements. These data were analyzed and related to the nanofiber morphology and diameter as determined from scanning electron microscopy (SEM). Measurements of the elastic (G′) and the plastic (G″) moduli of PLA solutions showed a sharp increase of G′ at the chain entanglement concentration. © 2016 Wiley Periodicals, Inc. J. Polym. Sci., Part B: Polym. Phys. 2016 , 54, 1483–1498  相似文献   

15.
由于聚乳酸具有良好生物相容性与降解性,故可用作控释给药系统的载体材料.有关聚乳酸及其共聚物微球药物载体、释放行为及微球表面引入基团使之功能化的方法研究已有报道.以其它生物大分子材料作为囊壁材料的缓释微胶囊也有报道,但以聚乳酸制备中空微囊型的药物释放载体却鲜有研究.通过控制分子量、微囊大小、囊壁厚度等参数,  相似文献   

16.
通过溶液浇铸法制备不同组分的左旋聚乳酸(PLLA)和聚(L-2-羟基-3-甲基丁酸)(PL-2H3MB)共混物.运用差示扫描量热仪(DSC)、偏光显微镜(POM)、广角X射线衍射(WAXD)和热重分析仪(TGA)分析共混物的结晶、熔融行为和热稳定性.通过观察到DSC加热曲线中新的熔融峰判断PLLA和PL-2H3MB共晶...  相似文献   

17.
通过熔融纺丝法成功制备了聚乳酸荧光防伪纤维。分别采用DSC、XRD、纤维强度仪、荧光光谱仪、荧光显微镜等探讨了荧光粉含量对聚乳酸荧光防伪纤维的结晶结构、力学性能与荧光性能的影响,并利用激光共聚焦显微镜对防伪纤维进行了3D荧光分布模拟分析。研究结果表明:聚乳酸荧光防伪纤维在紫外光激发下,在530nm处出现最强发射峰,纤维呈黄绿色荧光;随着荧光粉含量的增加,纤维的荧光强度增加,但荧光粉在基体中的团聚现象逐渐加剧,纤维的断裂强度逐渐降低;激光共聚焦显微镜可较好地模拟荧光防伪纤维中荧光粉的分布情况。  相似文献   

18.
19.
Coelectrospun polylactide(PLA)/gelatin (GE) composite fibrous matrixes have been identified to exhibit much improved performances compared to the respective components; however, the reasons for their water contact angles decreasing to zero at proper PLA/GE ratios remain unclear. To get a deep understanding of the phenomenon, PLA and GE were coelectrospun with different PLA/GE ratios in this study. Although the resulting composite fibers were homogeneous in appearance, they were detected different microscopic structures by transmission electron mircroscope (TEM) and via morphological observations after selective removal of either PLA or GE component. Together with the results of degradation study in phosphate buffered solution, a kind of cocontinuous phase separation microstructure could be identified for the PLA(50 wt%)/GE(50 wt%) composite fibers, which also showed the water contact angle of 0°. This value was far lower than those of electrospun PLA (~123°) and GE (~42°) fibrous matrixes. The X‐ray photoelectron spectrometry (XPS) data revealed that the polar side groups of protein macromolecules have moved toward composite fiber surface with solvent evaporation during electrospinning, due to the hydrophobic interaction between PLA and GE. Then the excellent hydrophilicity of PLA(50 wt%)/GE(50 wt%) composite fibers could be suggested as the consequence of: (1) the cocontinuous phase separation structure could provide more interface and void for water molecules penetrating; and (2) the accumulation of polar groups on composite fiber surface significantly increased the surface wettability. Copyright © 2010 John Wiley & Sons, Ltd.  相似文献   

20.
聚乙烯醇明胶混合水溶液的静电纺丝   总被引:1,自引:0,他引:1  
将聚乙烯醇与明胶混合水溶液进行静电纺丝,制备了聚乙烯醇与明胶混合超细纤维及其电纺膜,研究了混合纺丝液的组成对纺丝液的粘度、表面张力和电导率的影响,观察了纤维的微观形貌,并对电纺膜进行了差示扫描量热测定.结果表明:当混合液中明胶含量小于20 9/6时,静电纺丝可以稳定进行.随着明胶含量由5%逐渐增加至25%,混合超细纤维的平均直径先是由260nm逐渐下降至207 nm而后又逐渐增加至320 nm.明胶的含量低于15%时,不影响其混合电纺膜中PVA的结晶.  相似文献   