首页 | 本学科首页   官方微博 | 高级检索  
相似文献
 共查询到20条相似文献,搜索用时 15 毫秒
1.
In this article distribution of nanoclay between the two phases of a new class of dynamically vulcanized TPV based on POE/EVA(Polyethylene octene elastomer/ethylene vinyl acetate copolymer) elastomers prepared with various amounts of organoclay (0.5, 1 and 3 wt%) using dicumyl peroxide (DCP) as vulcanizing agent by reactive melt blending process has been studied. Different specimens of POE and POE/EVA blend with and without clay were prepared. The effects of organoclay on mechanical properties, swelling kinetics, crystallinity, vulcanization characteristics, dynamic mechanical behaviour, electrical properties and morphology were studied. DMA and morphological analysis revealed the formation of a Thermoplastic vulcanizate. XRD analysis showed decrease in crystallinity on addition of EVA in POE matrix. However, morphological observation of the fractured surface suggested that the smaller EVA domain was quite uniformly distributed into the POE phase and the clay phase was predominantly dispersed in the EVA phase of the TPVs and 0.5% clay mainly improved the mechanical properties and elongation of the blends. Swelling characteristics, electrical properties and storage modulus were also improved with the clay in case of the blend containing higher EVA content which further supports the fact that nanoclay was preferably distributed in the more polar EVA phase.  相似文献   

2.
Polylactide-based systems composed of an organoclay (Cloisite® 30B) and/or a compatibilizer (Exxelor VA1803) prepared by melt blending were investigated. Two types of not compatibilized nanocomposites containing 3 wt% or 10 wt% of the organoclay were studied to reveal the effect of the filler concentration on the nanostructure and physical properties of such systems. The 3 wt%-nanocomposite was also additionally compatibilized in order to improve the nanoclay dispersion. Neat polylactide and polylactide with the compatibilizer processed in similar conditions were used as reference samples. The X-ray investigations showed the presence of exfoliated nanostructure in 3 wt%-nanocomposite. Compatibilization of such system noticeably enhanced the degree of exfoliation of the organoclay. Viscoelastic spectra (DMTA) showed an increase of the storage and loss moduli with the increase of the organoclay content and dispersion. Dielectric properties of the nanocomposites show a weak influence of the nanoclay on segmental (αS) and local (β)-relaxations in PLA, except for the highest nanoclay content. Above Tg a strong increase of dc conductivity related to ionic species in the clay is observed. It gives rise also to the Maxwell-Wagner-Sillars interfacial polarization and both real and imaginary parts of ε strongly increase. In the temperature dependence of low frequency dielectric constant and mechanical moduli (at 1 Hz) an additional maximum around 80-90 °C is observed due to cold crystallization of PLA.  相似文献   

3.
Crosslink network evolution of brominated butyl rubber (BIIR)/ethylene–propylene–diene-monomer rubber (EPDM) blends during peroxide vulcanization is studied at a meso-scale level. In this work, EPDM is added as a co-agent to increase the crosslink density of BIIR vulcanization. With increasing EPDM content from 0 to 20 phr, the maximum torque of BIIR/EPDM compounds during vulcanization increases by 73%, reaching to 3.40 dNm. Vulcanization kinetic study shows that addition of EPDM favors to the crosslinking of BIIR compound. Meanwhile, the addition of 20 phr EPDM contributes to an increase in the crosslink density of BIIR/EPDM(80/20) vulcanizate, avoiding downward trend at post-cure period in comparison with BIIR only. Crosslink network evolution of BIIR/EPDM blends is divided into three periods during peroxide vulcanization at 150 °C. The role of EPDM in the crosslink network evolution is studied by proton nuclear magnetic resonance, and a “network patching” mechanism is proposed in which EPDM is implied to work as patch on damaged crosslink network resulted from the degradation nature of BIIR.  相似文献   

4.
In this study, relatively large amounts of polypropylene (PP), ethylene‐propylene‐diene (EPDM), and multi‐walled carbon nanotube (MWCNT) were melt‐mixed with and without DCP. Dynamically vulcanized PP/EPDM (TPV)/MWCNT nanocomposites were prepared by two methods: the MWCNTs were added either before or after the dynamic vulcanization of the blends. The effects of composition, rotor speed, and dynamic vulcanization on their surface resistivity were investigated. The surface resistivity of uncross‐linked PP/EPDM/MWCNT nanocomposites increases with increasing the content of EPDM. At PP/EPDM (70/30 wt%) nanocomposite with 1.5 phr MWCNT, slightly lower surface resistivity is obtained by increasing the rotor speed during mixing. However, for PP/EPDM (50/50 wt%) and PP/EPDM (30/70 wt%) nanocomposites, surface resistivity decreases with increasing the rotor speed from 30 to 60 rpm. But further increase in rotor speed (90 rpm) leads to an increase of surface resistivity. When the MWCNTs were added after the dynamic vulcanization of the blends, the surface resistivity of TPV70/MWCNTnanocomposite is lower than that of uncross‐linked PP/EPDM/MWCNT nanocomposite. However, when the MWCNTs were added before the dynamic vulcanization of the blends, the surface resistivity of TPV70/MWCNT nanocomposite is >1012 Ω/square. Copyright © 2010 John Wiley & Sons, Ltd.  相似文献   

5.
A thermoplastic elastomer (TPE) of ethylene propylene diene terpolymer (EPDM) and nylon with excellent mechanical properties was prepared by dynamic vulcanization. The effects of the curing systems, compatibilizer, nylon content and reprocessing on the mechanical properties of EPDM/nylon TPEs were investigated in detail. Experimental results indicate that maleic anhydride (MAH) grafted EPR has a better performance in compatibilizing the EPDM/nylon blends compared with other compatibilizers containing acid group. Tensile strength and elongation at break go through a maximum value at a compatibilizer resin content (on total rubber dosage) of 20%. EPDM/nylon TPE using sulfur as curative has higher tensile strength and elongation than that of TPE using phenolic resin or peroxide as curatives. Tensile strength and elongation at break increase with increasing nylon content. Scanning electron microscopy results show that rubber particles distributed at an average size of 1 μm in dynamic vulcanized EPDM/MAH-g-EPR/nylon TPE.  相似文献   

6.
In situ polymerized PS/EPDM blends were prepared by dissolving poly(ethylene-co-propylene-co-2-ethylidene-5-norbornene) (EPDM) in styrene monomer, followed by bulk polymerization at 60 °C and 80 °C . EPDM has excellent resistance to such factors as weather, ozone and oxidation, attributed to its non-conjugated diene component, and it could be a good alternative for substituting polybutadiene-based rubbers in PS toughening. The in situ polymerized blends were characterized by dynamic mechanical analysis, thermogravimetric analysis, gel permeation chromatography, and tensile and Izod impact resistance tests. The PS/EPDM blends are immiscible and present two phases, a dispersed elastomeric phase (EPDM) in a rigid PS matrix whose phase behavior is strongly affected by the polymerization temperature. Mechanical properties of the blends are influenced by the increase in the average size of EPDM domains with the increase in the polymerization temperature and EPDM content. The blends polymerized at 60 °C containing 5 wt% of EPDM presents an increase in the impact resistance of 80% and containing 17 wt% of EPDM presents an increase in the strain at break of 170% in comparison with the value of PS. The blend polymerized at 80 °C containing 17 wt% of EPDM presents an increase in the strain at break of 480% and in impact resistance of 140% in comparison with the value of PS.  相似文献   

7.
Summary: This study intends to replace polyethylene multi-layer films used in food packaging industry with single-layer polyethylene nanocomposites films. Nanocomposites of LDPE/LLDPE/ montmorillonite organoclay were prepared by melt compounding in a twin extruder and then film blown to prepare thin films. LLDPE-g-MA was used as compatibilizer to achieve better interaction between the blend and organoclay. Various compositions of organoclay and compatibilizer were prepared. The structure of nanocomposites was characterized by XRD and TEM. Permeability properties were measured using a permeability measuring set-up and aspect ratio of the particles was evaluated using permeability data. The results showed that addition of organoclay even at low level (below 5 phr) had significant effect on barrier properties of the nanocomposites. Oxygen permeability decreased by 50% by adding only 3 phr of nanoclay into the blend. Crystalline structure of the nanocomposites was studied by DSC. Addition of clay also led to increase in melting point and somewhat decrease in the crystalline level. Given the fact that crystals are effectively non-permeable, the concomitant reduction in crystallinity of the blend with decrease in permeability suggests that barrier properties arise from tortuousity of nanoparticles in the blend.  相似文献   

8.
The aim of this study is to investigate the performance of nanoclay reinforced unsaturated polyester (UP) resin under impact loads. Nanocomposite specimens containing nanoclay in 0, 1.5, and 3 (wt%) were prepared by melt mixing method. X‐ray diffraction, transmission electron microscopy analysis, scanning electron microscope photographs, and viscosity changes in liquid state resin confirmed exfoliation and intercalation of the nanoclay in the UP resin system used. Tensile modulus showed an increase with increase in nanoclay content. However, the tensile strength and elongation at break exhibited reducing performance with increase in nanoclay content. Izod impact test results indicated better performance for the specimens containing nanoclay reinforcements, with 1.5 (wt%) of nanoclay specimens showing the highest value. High velocity impact tests were carried out using gas gun in velocity range of 20–100 m/sec and harden steel hemispherical tip projectile with diameter of 8.7 mm and weight of 11.54 g. Results for high velocity impact test indicated better performance by the specimens containing nanoclay, with 1.5 (wt%) nanoclay showing the highest attained value. Damage assessments of impact area for all specimens showed spalling type brittle failure with punch out and sever fragmentation pattern. Copyright © 2011 John Wiley & Sons, Ltd.  相似文献   

9.
The purpose of this work was to study the effect of dendrimer modified clay minerals on the structure and properties of ethylene-propylene-diene monomer (EPDM) nanocomposites.Flame-retardant and dendrimer modified organic montmorillonite (FR-DOMt) was successfully prepared by Na+-montmorillonite, tetrahydroxymethyl phosphonium chloride (THPC), N, N-dihydroxyl-3-aminomethyl propionate, and boric acid. This dendritic type of organoclay (OC) was used in preparation of EPDM/FR-DOMt nanocomposites. The properties of these nanocomposites were studied. The dispersion status of the layered silicates in EPDM was revealed by X-ray diffractometer (XRD), scanning electron microscopy (SEM), and transmission electron microscopy (TEM). XRD and TEM results showed that FR-DOMt was exfoliated in the EPDM matrix when 10 phr of FR-DOMt was incorporated. The mechanical behavior, thermal stability, and flame retardance of the samples were examined. The experimental data demonstrated that the EPDM hybrids owned an improved tensile strength and elongation at break. In addition, the nanocomposites exhibited higher thermal stability and flame retardance than that of unfilled EPDM matrix.  相似文献   

10.
The effect of nanoclay addition in Glass Fiber Reinforced Epoxy (GFRE) composites on impact response was studied. The epoxy nanocomposite matrix with 1.5 and 3.0 wt% loading of I.30E nanoclay was produced by high shear mixing. Hybrid GFRE nanoclay composite plates were manufactured by hand layup and hot pressing techniques using electrical grade-corrosion resistant (E-CR) glass fiber mats. The laminates were then subjected to low-velocity impact with energies between 10 and 50 J. Addition of nanoclay was found to improve peak load and stiffness of GFRE. Nanoclay loading of 1.5 wt% resulted in optimum properties, with 23% improvement in peak load and 11% increase in stiffness. A significant reduction in physical damage was also observed for hybrid nanocomposite samples as compared to GFRE. This was mainly attributed to transition in damage mechanism due to nanoclay addition. Clay agglomeration in samples with 3.0 wt% loading contributed towards limiting the improvement in impact resistance.  相似文献   

11.
In this work, polypropylene (PP)/ethylene-propylene-diene monomer (EPDM)/butadiene acrylonitrile rubber (NBR) TPVs with different EPDM/NBR ratios were prepared by the core-shell dynamic vulcanization. The relationship between the core-shell structure and mechanical properties of the TPVs were thoroughly investigated. The formation of core-shell structure by adding NBR is conducive to the mechanical properties of the TPVs. The ratio of EPDM to NBR has an important effect on the structure and performances of the final products, and there is a critical ratio for this effect change. Transmission electron microscope (TEM), tensile test, reprocessing test, ageing test, rheological behavior test and stress relaxation were used to characterize the morphology and properties of the TPVs in detail. It was found that when the ratio of EPDM/NBR was 2:4, the tensile strength increased by ~14% compared with PP/EPDM TPV without NBR. Meanwhile, the reprocessing properties, rheological characteristics and instantaneous tensile deformation, etc. all exhibited sudden changes at this critical ratio.  相似文献   

12.
In the present investigation, authors made an attempt to study the sliding wear behavior of polypropylene/ultrahigh molecular weight polyethylene (PP/UHMWPE, 90/10) blends loaded with 30% carbon short fibers (CSF) as reinforcement and nanoclay as filler material. The nanocomposites have been prepared with varying amounts viz., 0, 1, 2 and 3 wt% of nanoclay. The composites were prepared by melt mixing at 60 rpm extruder speed and compression moulding at 180°C. From all the composites, 6 mm diameter and 25 mm length sliding wear specimens were prepared. Sliding wear loss, specific wear rate and coefficient of friction were investigated by using computerized pin-on–disc machine at normal applied loads of 20, 30 and 40 N; at a sliding velocity of 1.5 m/s and at two abrading distances viz., 200 and 300 m. The wear behavior data reveals that 3 wt% nanoclay filled composite exhibits higher wear resistance and lowest specific wear rate as compared to other nanocomposites. Also morphological study was carried out for wear out surfaces of all the composites using scanning electron microscopy (SEM).  相似文献   

13.
High oxygen barrier films were prepared based on low‐density polyethylene (LDPE)/ethylene vinyl alcohol (EVOH)/ nanoclay and polyethylene‐grafted‐maleic anhydride (LDPE‐g‐MA) as a compatibilizer. Box–Behnken statistical experiment design methodology was employed to study the effects of nanoclay, LDPE‐g‐MA, and EVOH presence and their contents on various properties of the final films. The R2 parameter varied between 0.89 and 0.99 for all the obtained responses. The morphology of the samples was evaluated. Results of oxygen transfer rate (OTR) test indicated that the addition of EVOH up to 30 wt% to neat LDPE can decrease oxygen permeability significantly. The addition of nanoclay also decreased the permeability of resulting films but, LDPE‐g‐MA reduced the permeability of the films only at an optimal content. Elastic modulus was increased with the addition of nanoclay, EVOH, and LDPE‐g‐MA to the matrix. An increase in EVOH content in the samples improved the tensile strength. Effect of nanoclay on tensile strength was highly dependent on the presence of a compatibilizer. The addition of compatibilizer to the samples and increasing its content enhanced the tensile strength of the specimens. Incorporation of nanoclay, EVOH, and LDPE‐g‐MA to the LDPE matrix and increasing the amount of these components in the samples led to higher storage modulus, zero shear rate viscosity, and shear thinning exponent, but, lowered the terminal slope and the frequency of intersection point of storage modulus (G′) and loss modulus (G″). The only exception was that EVOH increment resulted in a lower shear thinning exponent. Copyright © 2016 John Wiley & Sons, Ltd.  相似文献   

14.
Water blown rigid polyurethane foams (PUF) with organoclay/organically modified nanoclay (ONC) were prepared and their properties such as density, mechanical, morphological, insulation, thermal and flame retardant properties were studied. In this investigation, the ONC content was varied from 1 to 10 parts per hundred of polyol (php) by weight. It was observed that the compressive strength of ONC filled PUF increased up to 3 php of ONC loading and then it decreased. Wide angle X-ray diffraction and transmission electron microscopy studies indicated the exfoliated dispersion of ONC in PUF. The thermal conductivity of ONC filled PUF decreases up to 5 php and then increases. The glass transition temperature (Tg) of PUF decreases on loading of ONC. The TGA analysis shows that there is slight increase in degradation temperature with increase in ONC loading. The flame retardant properties (LOI and flame spread rate) are improved slightly on addition (3 php) of ONC filled PUF.  相似文献   

15.
In this work, the effect of quaternary ammonium salt containing nanoclay content (1–5 wt%) on phase morphology, rheology, cure kinetics, and mechanical properties of the vinyl ester resin (VER)‐based nanocomposites was studied. The morphological characterization including d‐spacing measurement, microscopy observation and phase‐height image processing were performed on the prepared nanocomposites using small angel X‐ray scattering (SAXS), transmission electron microscopy (TEM) and atomic force microscopy (AFM). According to the results obtained from these techniques, it was concluded that an intercalated morphology existed for all the nanocomposites. The kinetic analyses of the isothermal curing followed by storage modulus obtained from the rheometry experiments are shown to be an affective rheological characteristic to investigate the cure behavior of VER/clay nanocomposites. In addition, the most important finding regarding the effect of nanoclay on the cross‐linking behavior of VER systems lays on the chemisorption and physisorption of the reacting monomers and initiator molecules on the nanoclay platelets surface which is found to be responsible for the retardation of the cure reaction caused by organoclay. Eventually, the mechanical characterizations were performed through the tensile, flexural and impact analysis tests. In this case, a considerable improvement of the bulk mechanical responses such as tensile and flexural strengths and also the corresponding moduli were observed for the nanocomposites. Copyright © 2011 John Wiley & Sons, Ltd.  相似文献   

16.
As the most successful commercialized thermoplastic vulcanizates (TPVs), polypropylene (PP)/ethylene propylene rubber (EPDM) TPVs exhibit poor oil resistance. In this work, we prepared PP/EPDM/butadiene acrylonitrile rubber (NBR) ternary TPVs with good oil resistance using core‐shell dynamic vulcanization. According to the theoretical analysis of the spreading coefficient and the transmission electron microscopy results, the rubber phases exhibited a special core‐shell structure, in which the cross‐linkedNBR‐core was encapsulated by the EPDM‐shell. The core‐shell structure effectively improved the interfacial compatibility between PP and NBR phase as the EPDM‐shell could avoid the direct contact of them, thus improving the mechanical properties of the TPVs. For example, the PP/EPDM/NBR (40/30/30) ternary TPV showed enhanced tensile strength of 12.57 MPa, compared with 10.71 MPa of PP/EPDM (40/60) TPV and 11.11 MPa of PP/NBR (40/60) TPV, respectively. Moreover, the oil resistance of the TPVs was also improved. Compared with PP/EPDM TPV, the change rates in mass, volume, tensile strength and elongation at break of PP/EPDM/NBR TPV after oil immersion decreased by 42.18%, 48.69%, 52.68% and 28.77%, respectively.  相似文献   

17.
In this study, high oxygen barrier nanocomposite films were prepared by melt blending of low-density polyethylene/ethylene vinyl alcohol/nanoclay/polyethylene-grafted-maleic anhydride (LDPE/EVOH/nanoclay/LDPE-g-MA). Effect of each component presence was determined by using Box-Behnken experiment design methodology. For all the responses obtained, R 2 was between 0.956 and 0.981 indicating a very good fitting of the experimental data with the response surface method (RSM) in the models. Oxygen transfer rate (OTR) results shown that the addition of EVOH, compatibilizer, and nanoclay in formulations significantly decreases oxygen permeability. The experimental results showed that addition of 30 wt % EVOH, 4 wt % nanoclay, and 5 wt % LDPE-g-MA to the LDPE matrix gave the best oxygen barrier properties. The crystallization behaviors of the samples and thermal analysis have been characterized by using differential scanning calorimetry (DSC). The addition of nanoclay to the blends has resulted in increased crystallinity of LDPE phase. The state of nanoclay dispersion in the samples was examined by the X-ray diffraction (XRD) tests. The reduction of EVOH and nanoclay content, as well as the increase of LDPE-g-MA, has resulted in the better dispersion of nanoclay in the polymer matrix. The morphology of specimens was observed by using energy-dispersive X-ray spectroscopy (EDX) and scanning electron microscopy (SEM).  相似文献   

18.
The bisphenol‐A type epoxy resin was combined with layered clays. Three types of epoxy/clay nanocomposites were prepared by different clay pretreatment methods, that is, the slurry (clay swelling with polar solvent), organo, and solubilization (organoclay swelling with polar solvent) methods. The organo and solubilization systems showed good dispersibility. The basal spacing of the layered clays in the obtained nanocomposites was evaluated by XRD and TEM observations. The basal spacing of the nanoclay in the solubilization system drastically increased. The mechanical properties were improved with the increase in the clay dispersion. A high modulus and fracture toughness were obtained by improvement of the clay dispersion into the matrix. © 2009 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 47: 1753–1761, 2009  相似文献   

19.
A novel amorphous polyamide/montmorillonite nanocomposite based on poly(hexamethylene isophthalamide) was successfully prepared by melt intercalation. Wide angle X-ray diffraction and transmission electron microscopy showed that organoclay containing quaternary amine surfactants with phenyl and hydroxyl groups was delaminated in the polymer matrix resulting in well-exfoliated morphologies even at high montmorillonite content. Differential scanning calorimetry results indicated that clay platelets did not induce the formation of a crystalline phase in this amorphous polymer. Tensile tests demonstrated that the addition of nanoclay caused a dramatic increase in Young's modulus (almost twofold) and yield strength of the nanocomposites compared with the homopolymer. The nanocomposites exhibited ductile behavior up to 5 wt % of nanoclay. The improvement in Young's modulus is comparable with semicrystalline aliphatic nylon 6 nanocomposites. Both the main chain amide groups and the amorphous nature of the polyamide are responsible for enhancing the dispersion of the nanofillers, thereby, leading to improved properties of the nanocomposites. The structure-property relationship for these nanocomposites was also explored. © 2008 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 46: 2605–2617, 2008  相似文献   

20.
In this study, the radiation degradation/modification of the vulcanized EPDM and the effects of dose rate, peroxide type/content in vulcanization system and ENB content of EPDM were studied to investigate the change in the extend of the modification/degradation of the mechanical properties of vulcanized EPDM via gamma irradiation. In addition, thermal, dynamic mechanical, ATR-FTIR, TGA, TGA-FTIR tests were carried out to understand the change of properties of vulcanized EPDM via irradiation.Samples were irradiated with two different dose rates of 1280 and 64.6 Gy/h. Total dose of irradiation was up to 184 kGy. The FTIR spectral analysis showed structural changes of EPDM via irradiation. It was observed that the dose rate changed the mechanical properties with different extends. The change of ENB content of EPDM and peroxide type and content in vulcanization system affect extend of the modification/degradation of the EPDM's properties.  相似文献   

设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号