共查询到20条相似文献,搜索用时 0 毫秒
1.
Arun Kashinath Salunke Mukesh Kumar Madhra Mamta Sharma Susanta Banerjee 《Journal of polymer science. Part A, Polymer chemistry》2002,40(1):55-69
A series of poly(arylene ether)s were successfully prepared by aromatic, nucleophilic substitution reactions with various perfluoroalkyl‐activated bisfluoromonomers with 4,4′‐bishydroxybiphenyl and 4,4′‐bishydroxyterphenyl. 4,4′‐Bishydroxyterphenyl was synthesized through the Grignard coupling reaction of magnesium salt of 4‐bromoanisole with dibromobenzene followed by demethylation with pyridine–hydrochloride. The products obtained by the displacement of fluorine atoms exhibited good inherent viscosity, up to 0.77 dL/g, and number‐average molecular weights up to 69,300. These poly(arylene ether)s showed very good thermal stability, up to 548 °C for 5% weight loss according to thermogravimetric analysis under synthetic air, and high glass‐transition temperatures, up to 259 °C according to differential scanning calorimetry, depending on the exact repeat unit structure. These polymers were soluble in a wide range of organic solvents, such as N‐methylpyrrolidone, dimethylformamide, tetrahydrofuran, toluene, and CHCl3, and were insoluble in dimethyl sulfoxide and acetone. Thin films of these poly(arylene ether)s showed good transparency and exhibited tensile strengths up to 132 MPa, moduli up to 3.34 GPa, and elongations at break up to 84%, depending on their exact repeating unit structures. These values are comparable to those of high‐performance thermoplastic materials such as poly(ether ether ketone) (PEEK) and Ultem poly(ether imide) (PEI). These poly(arylene ether)s exhibited low dielectric constants. © 2001 John Wiley & Sons, Inc. J Polym Sci Part A: Polym Chem 40: 55–69, 2002 相似文献
2.
Yong Ding Antisar R. Hlil Allan S. Hay 《Journal of polymer science. Part A, Polymer chemistry》1998,36(8):1201-1208
Novel poly(arylene ether)s, poly(arylene thioether)s, and poly(arylene sulfone)s were synthesized from the dihydroxy(imidoarylene) monomer 1 . The syntheses of poly(arylene ether)s were carried out in DMAc in the presence of anhydrous K2CO3 by a nucleophilic substitution reaction between the bisphenol and activated difluoro compounds. Poly(arylene thioether)s were synthesized according to the recently discovered one-pot polymerization reaction between a bis(N,N′-dimethyl-S-carbamate) and activated difluoro compounds in the presence of a mixture of Cs2CO3 and CaCO3. The bis(N,N′-dimethyl-S-carbamate) 3 was synthesized by the thermal rearrangement reaction of bis(N,N′-dimethylthiocarbamate) 2 , which was synthesized from 1 by a phase-transfer catalyzed reaction. The poly(arylene thioether)s were further oxidized to form poly(arylene sulfone)s, which would be very difficult, if not impossible, to synthesize by other methods. All of the polymers described have extremely high Tgs and thermal stability as determined from DSC and TGA analysis. Poly(arylene sulfone)s have the highest Tgs and they are in the range of 298–361°C. © 1998 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 36: 1201–1208, 1998 相似文献
3.
Fumio Keitoku Masa-Aki Kakimoto Yoshio Imai 《Journal of polymer science. Part A, Polymer chemistry》1994,32(2):317-322
Novel methyl-substituted aromatic poly (ether sulfone)s and poly (ether ketone)s were synthesized from combinations of 3,3′,5,5′-tetramethylbipheny-4,4′-diol and 2,2′,3,3′,5,5′-hexamethylbiphenyl-4,4′-diol, and 4,4′-dichlorodiphenyl sulfone and 4,4′-difluorobenzo-phenone by nucleophilic aromatic substitution polycondensation. The polycondensations proceeded quantitatively in a N-methyl-2-pyrrolidone-toluene solvent system in the presence of anhydrous potassium carbonate to afford the polymers with inherent viscosities between 0.86 and 1.55 dL/g. The methyl-substituted poly (ether sulfone)s and poly (ether ketone)s showed good solubility in common organic solvents such as chloroform, tetrahydrofuran, pyridine, m-cresol, and N,N-dimethylacetamide. The tetramethyl- and hexamethyl-substituted aromatic polyethers had higher glass transition temperatures than the corresponding unsubstituted polymers, and did not decompose below 350°C in both air and nitrogen atmospheres. The films of the methyl-substituted poly (ether ketone)s became insoluble in chloroform by the irradiation of ultraviolet light, indicating the occurrence of photochemical crosslinking reactions. © 1994 John Wiley & Sons, Inc. 相似文献
4.
Abbas‐Alli G. Shaikh Allan S. Hay 《Journal of polymer science. Part A, Polymer chemistry》2002,40(4):496-510
The bisphenol 4,4″‐dihydroxy‐5′‐phenyl‐m‐terphenyl ( 4 ), containing a 1,3,5‐triphenylbenzene moiety, was synthesized from a pyrylium salt obtained by the reaction of benzaldehyde with p‐methoxyacetophenone with boron trifluoride etherate as a condensing agent. Polymers were obtained from 4 by a nucleophilic displacement reaction with various activated difluoro monomers and with K2CO3 as a base. A series of new poly(arylene ether)s ( 8a – 8f ) were obtained that contained phenyl‐substituted m‐terphenyl segments in the polymer chain. Polymers with inherent viscosities of 0.41–0.99 dL/g were obtained in yields greater than 96%. The polymers were soluble in a variety of organic solvents, including nonpolar solvents such as toluene. Clear, transparent, and flexible films cast from CHCl3 showed high glass‐transition temperatures (Tg = 198–270 °C) and had excellent thermal stability, as shown by temperatures of 5% weight loss greater than 500 °C. 4 was converted via N,N‐dimethyl‐O‐thiocarbamate into the masked dithiol 4,4″‐bis(N,N′‐dimethyl‐S‐thiocarbamate)‐5′‐phenyl‐m‐terphenyl and was polymerized with activated difluoro compounds in the presence of a mixture of Cs2CO3 and CaCO3 as a base in diphenyl sulfone as a solvent. A series of new poly(arylene thioether)s ( 9a – 9e ) were obtained with Tg values similar to those of 8a – 8e . 9a – 9e were further oxidized into poly(arylene sulfone)s with Tg values 40–80 °C higher than those for 8a – 8e and 9a – 9e . These polymers also had good solubility in organic solvents. A sulfonic acid group was selectively introduced onto the pendent phenyl group of polymers 8a and 8f by reaction with chlorosulfonic acid. The polymers were soluble in dipolar aprotic solvents and formed films via casting from dimethylformamide. Polymers 8a – 8f , 11a , and 11f showed blue and red fluorescence under ultraviolet–visible light with emission maxima at 380–440 nm. © 2002 John Wiley & Sons, Inc. J Polym Sci Part A: Polym Chem 40: 496–510, 2002; DOI 10.1002/pola.10136 相似文献
5.
《Journal of polymer science. Part A, Polymer chemistry》2018,56(13):1358-1365
A multiblock copolymer consisting of hard (poly(arylene ether sulfone)) and soft (poly(alkyl disulfide)) segments was successfully synthesized by oxidative coupling of the corresponding thiol‐terminated oligomers. Its structure was confirmed by 1H and 13C NMR spectroscopy. The GPC data (Mw = 82,000, Mw/Mn = 2.7) and inherent viscosity (0.67 dL g−1) indicated the formation of a high‐molecular‐weight multiblock copolymer, while AFM and DSC indicated a microphase‐separated morphology. Tensile testing of the multiblock copolymer films showed a large elongation at break, which is characteristic of microphase‐separated hard/soft multiblock copolymers. Over 90% of the elongation at break of damaged samples (notched or cut) was recovered by UV irradiation. The elongation recovery was proportional to the UV irradiation energy, and the high recovery was achieved by relatively weak irradiation (<170 J cm−2). The high content of disulfide bonds in the multiblock copolymer resulted in a lower self‐healing energy. © 2018 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2018 , 56, 1358–1365 相似文献
6.
Shigeru Matsuo 《Journal of polymer science. Part A, Polymer chemistry》1994,32(11):2093-2098
A series of new poly(arylene ether phenyl-s-triazine)s was prepared by the nucleophilic aromatic substitution polymerization of the potassium salt of bisphenols with 2,4-bis (halophenyl)-6-phenyl-s-triazine in N-methyl-2-pyrrolidone at elevated temperature. The polymers with inherent viscosities exceeding 0.5 were obtained after polymerization for 1 h using 2,4-bis(fluorophenyl)-6-phenyl-s-triazine as a monomer. The glass transition temperatures of the resulting polymers ranged from 200 to 260°C depending on the bisphenol used in the polymer synthesis. The poly(arylene ether phenyl-s-triazine)s demonstrated excellent thermal stabilities in excess of 490°C (5% weight loss in air). The isothermal TGA measurements (400°C under air or nitrogen atmosphere) revealed that the 4,4'-biphenol- and hydroquinone-based poly(arylene ether phenyl-s-triazine)s belong to the most superior class of heat resistant polymers, such as polyimide Kapton?. The mechanical properties of these polymers are also described. © 1994 John Wiley & Sons, Inc. 相似文献
7.
Yu Chen Jarrett R. Rowlett Chang Hyun Lee Ozma R. Lane Desmond J. VanHouten Mingqiang Zhang Robert B. Moore James E. McGrath 《Journal of polymer science. Part A, Polymer chemistry》2013,51(10):2301-2310
Hydrophobic‐hydrophilic sequence multiblock copolymers, based on alternating segments of phenoxide terminated fully disulfonated poly(arylene ether sulfone) (BPS100) and fluorine‐terminated poly(arylene ether sulfone) (6FBPS0) were synthesized and evaluated for application as proton exchange membranes. By utilizing mild reaction conditions the ether–ether interchange reactions were minimized, preventing the randomization of the multiblock copolymers. Tough, ductile, transparent membranes were solution cast from the block copolymers and were characterized with regard to intrinsic viscosity, morphology, water uptake, and proton conductivity. The conductivity values of the 6FBPS0‐BPSH100 membranes were compared to Nafion 212 and a partially fluorinated sulfonated poly(arylene ether sulfone) random copolymer (6F40BP60). The nanophase separated morphology was confirmed by transmission electron microscopy and small angle X‐ray scattering, and enhanced proton conductivity at reduced relative humidity was observed with longer block lengths. © 2013 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem, 2013 相似文献
8.
Shigeru Matsuo Ken-Ichi Mitsuhashi 《Journal of polymer science. Part A, Polymer chemistry》1994,32(10):1969-1975
Poly(arylene ether ketone)s containing imide units were prepared by the aromatic nucleophilic displacement reaction of the potassium salts of bisphenols with bis(4-fluorobenzoyl)phthalimides in N-methyl-2-pyrrolidone at elevated temperature. The polymers having inherent viscosities of 0.34–0.77 dL/g were obtained in 2 h. The polymers exhibited glass transition temperatures ranging from 216 to 268°C and decomposition temperatures (5% weight loss under air atmosphere) ranging from 450–570°C mainly depending on the bisphenols used in the polymer synthesis. The isothermal TGA measurements (400°C under air or nitrogen atmosphere) revealed that the 4,4'-biphenol- and hydroquinone-based poly(arylene ether ketone imide)s belong to a superior class of heat resistant polymers. The mechanical properties of these polymers are also described. © 1994 John Wiley & Sons, Inc. 相似文献
9.
David J. T. Hill David A. Lewis James H. O'Donnell Peter J. Pomery James L. Hedrick James E. McGrath 《先进技术聚合物》1991,2(1):15-20
The radiation resistance of a series of aromatic polysulfones comprising alternating units of diphenyl sulfone and various aromatic diols has been investigated by measuring volatile products, soluble fractions and electron spin resonance (ESR) spectra. The yields of radicals at 77 K observed by ESR and of SO2 at 423 K have indicated that biphenol gives enhanced resistance to Y radiation, and tetramethyl bisphenol-A decreased resistance, relative to bisphenol-A, bisphenol-S and hydroquinone. The protective effect of bisphenol was confirmed by lower scission and crosslinking yields determined from the soluble fractions after high doses. 相似文献
10.
Poly(arylene ether sulfone) copolymers derived from 9,9-bis(4-hydroxyphenyl)fluorene, bisphenol S and 4,4′-difluorodiphenylsulfone and poly(arylene ether ketone) copolymers derived from 4-phenoxybiphenyl, diphenyl ether and isophthaloyl chloride were prepared as precursor polymers for sulfonation reaction in which sulfonic groups are introduced quantitatively into specified positions. Sulfonation reaction for these two series of copolymers by concentrated sulfuric acid was successfully carried out to give sulfonated polymers with controlled positions and degree of sulfonation. Thermal stability, moisture absorption and proton conductivity for these two series of copolymers were measured and the results were compared to those of perfluorosulfonic acid polymers. 相似文献
11.
D. S. Sharapov V. V. Shaposhnikova S. N. Salazkin I. A. Mamedova L. V. Dubrovina I. V. Blagodatskikh T. A. Babushkina 《Russian Chemical Bulletin》2004,53(9):2041-2044
Poly(arylene ether ketones) with preset molecular weights (reduced viscosity from 0. 2 to 0.82 dL g–1) containing terminal phenolic groups were synthesized by the reactions of 4,4-difluorobenzophenone with bisphenol A or phenolphthalein in the presence of K2CO3 in N,N-dimethylacetamide. The influence of an excess of bisphenols on the molecular weights of the polymers obtained was studied. The structures of the polymers were confirmed by 1H NMR spectroscopy. The molecular weight distributions of the polymers were determined.Published in Russian in Izvestiya Akademii Nauk. Seriya Khimicheskaya, No. 9, pp. 1958–1961, September, 2004. 相似文献
12.
13.
We have synthesized new poly(arylene ether sulfone) (PAES) and polydimethylsiloxane (PDMS) segmented block copolymers where the PAES segments contain 20–30% of 4,4′-dihydroxyterphenol (DHTP) and 70–80% of bisphenol A (BA) units. The tensile and thermal properties of these new polymeric materials were measured and were compared to those of existing bisphenol A PAES–PDMS segmented block copolymers (BA PAES-b-PDMS). Also, a high molecular weight BA–DHTP PAES random copolymer containing 80% BA and 20% DHTP was prepared and its properties were compared to Udel®, a commercial PAES based on BA. The BA–DHTP PAES random copolymer had a significantly higher modulus, 1800 MPa and a higher Tg, 196 °C when compared to Udel®. In the segmented block copolymer materials, increased modulus and tensile strain at break (elongation) were also found when DHTP was incorporated into the PAES segments. 相似文献
14.
Bin Zhang S. Richard Turner 《Journal of polymer science. Part A, Polymer chemistry》2011,49(20):4316-4324
trans‐1,4‐Cyclohexylene ring containing acid chloride monomers were incorporated into poly(arylene ether sulfone) (PAES) backbones to study their effect on mechanical and thermal properties. The trans‐1,4‐cyclohexylene ring containing acid chloride monomers were synthesized and characterized by NMR and high‐resolution mass spectrum. trans‐1,4‐Cyclohexylene containing PAESs were synthesized from the acid chloride monomers and hydroxyl terminated polysulfone oligomers with a pseudo‐interfacial method and a solution method. These PAESs, with trans‐1,4‐cyclohexylene ring containing ester linkages, were fully characterized by NMR, thermogravimetric analysis, differential scanning calorimetry (DSC), size exclusion chromatography, and dynamic mechanical analysis (DMA). The tensile properties were also evaluated. The polymers made with the pseudo‐interfacial method had relatively low molecular weights when compared to the solution method where much higher molecular weight polymers were obtained. Crystallinity was promoted in the low molecular weight biphenol‐based PAES samples with the pseudo‐interfacial method. The crystallinity was confirmed by both the DSC and the wide angle X‐ray diffraction results. The tensile test results of the high molecular weight polymers suggested that incorporation of the trans‐1,4‐cyclohexylene ring containing linkage slightly improved the ultimate elongations while maintaining the Young's moduli. The trans‐1,4‐cyclohexylene ring containing PAESs also showed higher sub‐Tg relaxations in DMA when compared with their terephthaloyl containing analog. © 2011 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem, 2011 相似文献
15.
Jae‐Pil Kim Jae‐Wook Kang Jang‐Joo Kim Jae‐Suk Lee 《Journal of polymer science. Part A, Polymer chemistry》2003,41(10):1497-1503
Fluorinated dihydroxy phosphine oxide monomers were synthesized via chlorination, Grignard, and demethylation techniques. The prepared monomer was successfully polymerized with each of the three perfluorinated monomers (decafluorobiphenyl, decafluorobenzophenone, and pentafluorophenylsulfide) by nucleophilic aromatic substitution. The average molecular weight ranged between 7800 and 14,900 g/mol. The glass‐transition temperatures of the polymers were registered in the range of 185–235 °C, and all the polymers exhibited high thermal stability up to 326–408 °C. The results of the refractive‐index measurements indicated control of the refractive index between 1.5181 and 1.5536 and an optical loss of 0.53 dB/cm at 1550 nm. © 2003 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 41: 1497–1503, 2003 相似文献
16.
J. G. Smith J. W. Connell P. M. Hergenrother 《Journal of polymer science. Part A, Polymer chemistry》1993,31(12):3099-3108
Poly(arylene ether)s containing N-arylenebenzimidazole groups were prepared by the aromatic nucleophilic displacement reaction of two new bis(hydroxyphenyl-N-arylenebenzimidazole)s with activated aromatic difluorides in sulfolane at 200°C in the presence of anhydrous potassium carbonate. The bis(hydroxyphenyl-N-arylenebenzimidazole)s were prepared from bis(o-aminoanilino) arylenes and phenyl-4-hydroxybenzoate. The polymers were soluble in N-methyl-2-pyrrolidinone and m-cresol and exhibited inherent viscosities from 0.37–0.86 dL/g and glass transition temperatures from 219–289°C. Thermogravimetric analyses showed 5% weight losses from 463–506°C in air and 467–522°C in nitrogen. Unoriented thin films exhibited tensile strengths, moduli, and break elongations at 23°C of 10.2–12.5 ksi, 318–365 ksi, and 4–7%, respectively, and at 177°C of 5.1–6.9 ksi, 256–296 ksi, and 1–5%, respectively. A 50 : 50 random copolymer prepared from 1,3-bis(4-fluorobenzoyl) benzene, 1,1'-(4,4'-biphenylene)-bis[2-(4-hydroxyphenyl)benzimidazole], and 5,5'-bis[2-(4-hydroxyphenyl)benzimidazole] exhibited higher moisture absorption and lower tensile properties than those predicted by a rule of mixtures relationship. The chemical, physical, and mechanical properties of these polymers are discussed. © 1993 John Wiley & Sons, Inc.? 相似文献
17.
Sheng-Huei Hsiao Perng-Chih Huang 《Journal of polymer science. Part A, Polymer chemistry》1998,36(10):1649-1656
Two sulfonyl group-containing bis(ether anhydride)s, 4,4′-[sulfonylbis(1,4-phenylene)dioxy]diphthalic anhydride ( IV ) and 4,4′-[sulfonylbis(2,6-dimethyl-1,4-phenylene)dioxy]diphthalic anhydride (Me- IV ), were prepared in three steps starting from the nucleophilic nitrodisplacement reaction of the bisphenolate ions of 4,4′-sulfonyldiphenol and 4,4′-sulfonylbis(2,6-dimethylphenol) with 4-nitrophthalonitrile in N,N-dimethylformamide (DMF). High-molar-mass aromatic poly(ether sulfone imide)s were synthesized via a conventional two-stage procedure from the bis(ether anhydride)s and various aromatic diamines. The inherent viscosities of the intermediate poly(ether sulfone amic acid)s were in the ranges of 0.30–0.47 dL/g for those from IV and 0.64–1.34 dL/g for those from Me- IV. After thermal imidization, the resulting two series of poly(ether sulfone imide)s had inherent viscosities of 0.25–0.49 and 0.39–1.19 dL/g, respectively. Most of the polyimides showed distinct glass transitions on their differential scanning calorimetry (DSC) curves, and their glass transition temperatures (Tg) were recorded between 223–253 and 252–288°C, respectively. The results of thermogravimetry (TG) revealed that all the poly(ether sulfone imide)s showed no significant weight loss before 400°C. The methyl-substituted polymers showed higher Tg's but lower initial decomposition temperatures and less solubility compared to the corresponding unsubstituted polymers. © 1998 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 36: 1649–1656, 1998 相似文献
18.
Byungchan Bae Shinya Kawamura Kenji Miyatake Masahiro Watanabe 《Journal of polymer science. Part A, Polymer chemistry》2011,49(17):3863-3873
Random and multiblock sulfonated poly(arylene ether sulfone)s (SPEs) containing various azole groups such as oxadiazole and triazole were synthesized and characterized for fuel cell application. Successful preparation of SPE membranes depended on the structure of azole groups, which affected solubility of precursors and the resulting SPEs. Although oxadiazole groups were incorporated into hydrophobic component, they were found to be hydrophilic to give higher proton conductivity. Introduction of oxadiazole groups into random SPE gave comparable proton conductivity to that of Nafion NRE at >60% relative humidity at 80 °C. Block copolymer structure further increased the proton diffusion coefficient without increasing ion exchange capacity. Hydrolytic and oxidative stability of the SPE membranes was affected by both hydrophilic and hydrophobic components. Oxadiazole groups gave negative impact on hydrolytic and mechanical stability to the SPE membranes. © 2011 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem, 2011 相似文献
19.
首先分别合成了主链上含有查尔酮结构的疏水段和侧链上含有叔胺的亲水段,然后通过疏水段与亲水段的末端缩合反应合成了一系列光敏性聚芳醚砜两亲嵌段聚合物,其结构和热性能分别通过1 H NMR,FT-IR,UV-Vis光谱,TGA和万能力学试验机等进行表征测试.该两亲性嵌段聚合物具有良好的溶解性、热稳性、力学性能和光敏性,在紫外光谱322nm处有最大吸收峰,在常温下经紫外光照射,分子链之间发生[2+2]环加成反应,聚合物分子之间形成交联结构,最大交联度可达到64%. 相似文献
20.
J. W. Connell P. M. Hergenrother 《Journal of polymer science. Part A, Polymer chemistry》1991,29(11):1667-1674
Poly(arylene ether imidazole)s were prepared by the aromatic nucleophilic displacement reaction of a bisphenol imidazole with activated aromatic dihalides. The polymers had glass transition temperatures ranging from 230 to 318°C and number-average molecular weights as high as 82,000 g/mol. Thermogravimetric analysis showed a 5% weight loss occurring ~ 400°C in air and ~ 500°C in nitrogen. Typical neat resin mechanical properties obtained at room temperature included tensile strength and tensile modulus of 14.2 and 407 ksi and fracture energy (Glc) of 23 in. lb/in.2 Titanium-to-titanium tensile shear strengths measured at 23 and 200°C were 4800 and 3000 psi, respectively. In addition, preliminary data were obtained on carbon fiber laminates. The chemistry, physical, and mechanical properties of these polymers are discussed. 相似文献