The highly selective, fast and effective sample pretreatment technique molecularly imprinted solid-phase extraction (MISPE) can overcome the low sensitivity of the highly efficient capillary electrophoresis-UV method (CE-UV). In this work, narrowly dispersible bisphenol A (BPA)-imprinted polymeric microspheres with a high capacity factor of k′ = 6.8 and an imprinted factor of I = 6.53 were investigated as selective solid-phase extraction (SPE) sorbents for use in extraction of BPA from different sample matrices (tap water, wastewater, Yangtze River water, soil from the Yangtze River, shrimp and human urine). Washing and eluting protocols of MISPE were optimized. Under optimal conditions, recoveries of MISPE were investigated. Recoveries were basically constant and the relative standard deviation (RSD) was lower than 5.8% when loading volumes changed from 1 to 50 mL. Recoveries ranged from 71.20% to 86.23% for different sample matrices. Compared with C18 SPE, MISPE had higher selectivity and recovery for BPA. BPA was determined with good accuracy and precision in different complex samples using CE-UV coupled with MISPE. Spiked recoveries ranged from 95.20% to 105.40%, and the RSD was less than 7.2%. Because a large loading volume was achieved, the enrichment efficiency of pretreatment and the sensitivity of this method were improved. The limits of detection of this MISPE-CE-UV method for BPA in tap water, wastewater, Yangtze River water, soil from the Yangtze River, shrimp and human urine were 3.0 μg L− 1, 5.4 μg L− 1, 6.9 μg L− 1, 2.1 μg L− 1, 1.8 μg L− 1 and 84 μg L− 1, respectively.  相似文献   

2.
A cross‐linked methacrylate molecularly imprinted polymer (poly‐4‐vinylpyridine‐co‐trimethylolpropane‐trimethacrylate) selective for bisphenol A (BPA) was synthesized, using a fluorinated BPA derivative (4,4′‐(hexafluoroisopropylidene)‐diphenol) as a mimic template, and applied to the analysis of real‐world samples of process and potable waters. The molecularly imprinted polymer also showed a high affinity and selectivity for 17‐β‐estradiol and ethynylestradiol. A method to analyze BPA, 17‐β‐estradiol, and ethynylestradiol at ultratrace levels was thus developed from a screening procedure to monitor endocrine‐disrupting chemicals in water samples. The method consists of the BPA‐selective cleanup by molecularly imprinted SPE using cartridges packed with the polymer developed, its recovery by stir bar sorptive extraction after ad hoc derivatization to obtain the corresponding BPA‐acetate, and its analysis by GC‐time window‐SIM‐MS after online thermal desorption. The method showed good linearity in the working range (R2=0.9969), high repeatability (RSD% <10.1), recoveries always above 90%, and very low LOD (10 pg/L) and LOQ (1 ng/L) and can easily be extended to the determination of 17‐β‐estradiol and ethynylestradiol ultratraces. The method's effectiveness was evaluated by analyzing the real‐world water samples; it enabled preconcentration and detection of BPA at ultratrace levels.  相似文献   

3.
A key issue in the synthesis of molecularly imprinted polymers (MIPs) is the identification and optimisation of the main factors that affect the material structure and its molecular recognition properties. This paper describes the application of an experimental design and multivariate analysis method for the synthesis of bisphenol A (BPA)-selective MIPs. Six factors with a large impact on the MIP synthesis and its analytical performance have been optimised: the amount of template, the type and the percentage of functional and cross-linking monomers, the polymerisation method (i.e. thermal or UV initiation) and the porogenic solvent. The polymers have been prepared in small-scale (mini-MIPs) and, after careful removal of the template, their BPA rebinding capacity has been evaluated and related to the MIP composition. Among the two functional monomers tested, namely 4-vinylpyridine (4-vpy) and methacrylic acid (MAA), the former rendered the best selectivity for BPA analysis. The partial least squares (PLS) models revealed that the photoinitiated polymers with a 1:1 ratio of 4-vinylpyridine to cross-linker (EDMA or TRIM) yield the highest specific binding. Such procedure is time and cost effective and can be used as a general tool in the preparation of MIPs for different analytes.  相似文献   

4.
A bisphenol A (BPA) molecularly imprinted polymer, the composition of which was optimised using a chemometric approach, has been applied to the selective preconcentration of the template from aqueous samples. The selectivity of the polymer toward BPA and related compounds was evaluated chromatographically. The BPA-imprinted polymer was packed in a column and used for continuous on-column solid-phase extraction (MISPE) of aqueous samples followed by subsequent analysis by HPLC with fluorescence detection of the eluted fractions. The composition of the washing solvent applied in the MISPE procedure was optimised to favour the specific interactions of the MIP with BPA and to remove the non-selectively bound matrix components. The MISPE method has proven to be effective for selective preconcentration of BPA in aqueous samples (recoveries >84% obtained in the eluate for 10–100 mL sample volumes) enabling detection and quantification limits of 1.0 and 3.3 ng mL–1, respectively (based on 25 mL sample size). Analytical recoveries were between 92 and 101% for river water samples spiked with known amounts of BPA (30, 60, and 80 ng mL–1); relative standard deviations (RSD) were lower than 5.0%.  相似文献   

5.
Leakage of the residual template molecules is one of the biggest challenges for application of molecularly imprinted polymer (MIP) in solid-phase extraction (SPE). In this study, bisphenol F (BPF) was adopted as a dummy template to prepare MIP of bisphenol A (BPA) with a superparamagnetic core–shell nanoparticle as the supporter, aiming to avoid residual template leakage and to increase the efficiency of SPE. Characterization and test of the obtained products (called mag-DMIP beads) revealed that these novel nanoparticles not only had excellent magnetic property but also displayed high selectivity to the target molecule BPA. As mag-DMIP beads were adopted as the adsorbents of solid-phase extraction for detecting BPA in real water samples, the recoveries of spiked samples ranged from 84.7% to 93.8% with the limit of detection of 2.50 pg mL−1, revealing that mag-DMIP beads were efficient SPE adsorbents.  相似文献   

6.
Molecular imprinted polymer (MIP) as solid-phase microextraction (SPME) fibers coating has gained great attention in recent years. In this study, a simple preparation approach for bisphenol A (BPA) MIP coating with controlled thickness on fused-silica capillaries was developed. A capillary was inserted into a larger bore capillary to form a sleeve as mold. The prepolymer solution containing the template BPA was introduced into the interspace between the two capillaries for polymerization under photoirradiation. The larger bore capillary was removed away after the polymerization, and MIP coating with certain thickness on the surface of the inserted capillary was obtained. SPME conditions based on the MIP-coated fibers were optimized, and the extraction performance of the fibers with different thickness coating was compared. Finally, the MIP fibers were used for selective extraction of BPA spiked in tap water, human urine, and milk samples. The average recoveries of spiked BPA in the three samples were 92.5%, 81.6%, and 87.5%, respectively. The present analytical performance is not up to par for applicability to real environmental matrices. Further improvement will be necessary for analysis of real complex samples.  相似文献   

7.
环丙沙星分子印迹聚合物的合成及识别性能研究   总被引:1,自引:0,他引:1  
采用分子印迹技术合成了以环丙沙星为印迹分子,以甲基丙烯酸和4-乙烯基吡啶同时为功能单体的分子印迹聚合物。运用平衡结合实验研究了印迹聚合物的吸附特性和选择识别能力。Scatchard分析表明,在所研究的浓度范围内,分子印迹聚合物中形成了两类不同的结合位点。底物选择实验表明,这种聚合物对环丙沙星呈现高的选择结合能力。  相似文献   

8.
Yang Y  Long Y  Cao Q  Li K  Liu F 《Analytica chimica acta》2008,606(1):92-97
Bilirubin (BR) imprinted polymer was successfully prepared using supramolecular host compound β-cyclodextrin (β-CD) as functional monomer. The adsorption equilibrium was attained in about 4 h, which indicated that the adsorption kinetics was comparatively fast. The results of adsorption and selectivity experiments indicated that BR-imprinted β-CD polymer was able to bind BR specifically and reversibly. The specific recognition of BR-imprinted β-CD polymer for BR may be due to the cooperative effects of inclusion interaction and hydrogen bonding. This BR-imprinted β-CD polymer was further applied to eliminate BR in human serum sample. It was verified that the binding specificity of the BR-imprinted polymer for BR was essentially sufficient in the presence of other compounds coexisting in serum sample. Therefore, as a reusable material possessing high affinity and selectivity, BR-imprinted β-CD polymer has a potential application perspective as a clinical hemoperfusion material.  相似文献   

9.
Zhan W  Wei F  Xu G  Cai Z  Du S  Zhou X  Li F  Hu Q 《Journal of separation science》2012,35(8):1036-1043
A water compatible molecularly imprinted polymers (MIPs) coated stir bar for bisphenol A(BPA) was prepared with 3,3',5,5'-tetrabromobisphenol A as the dummy template molecule in this study. The dummy molecularly imprinted polymers coated stir bar (DMIPs-SB) showed better selectivity than the bars coated with polydimethylsiloxane or non-imprinted polymers when used to extract BPA and its three analogues. The saturated adsorption amount of the DMIPs coating was 3.0 times over that of the non-imprinted polymers coating. To achieve the optimum extraction performance, several parameters, including extraction and desorption time, pH value, adsorption temperature and stirring speed were investigated. The high-performance liquid chromatography combined with the DMIPs-SB was employed in the analysis of BPA in aqueous solution. The linear range of BPA concentration in aqueous medium was 0.0228-2.28 ng/mL with correlation coefficient of 0.9994 and the detection limit was about 6.84 × 10(-3) ng/mL based on three times ratio of signal to noise. This method was directly applied to the determination of trace BPA in milk with satisfactory results.  相似文献   

10.
A novel nanocomposite of molecularly imprinted polymers and graphene sheets was fabricated and used to obtain a highly conductive acetylene black paste electrode with high conductivity for the detection of bisphenol A. The two‐dimensional structure and the chemical functionality of graphene provide an excellent surface for the enhancement of the sensitivity of the electrochemical sensor and the specificity of molecularly imprinted polymers to improve detection of bisphenol A. The synergistic effect between graphene and molecularly imprinted polymers confers the nanocomposite with superior conductivity, broadened effective surface area and outstanding electrochemical performance. Factors affecting the performance of the imprinted sensor such as molecularly imprinted polymers concentration, foster time and scan rate are discussed. The sensor successfully detects bisphenol A with a wide linear range of 3.21 × 10?10 to 2.8 × 10?1 g/L (R = 0.995) and a detection limit of 9.63 × 10?11g/L. The fabricated sensor also possessed high selectivity and stability and exhibits potential for environmental detection of contaminants and food safety inspection.  相似文献   

11.
Molecularly imprinted polymers (MIPs) were prepared using bisphenol A (BPA) as a template by precipitation polymerization. The polymer that had the highest binding selectivity and ability was used as solid-phase extraction (SPE) sorbents for direct extraction of BPA from different biological and environmental samples (human serum, pig urine, tap water and shrimp). The extraction protocol was optimized and the optimum conditions were as follows: conditioning with 5 mL methanol–acetic acid (3:1), 5 mL methanol, 5 mL acetonitrile and 5 mL water, respectively, loading with 5 mL aqueous samples, washing with 1 mL acetonitrile, and eluting with 3 mL methanol. MIPs can selectively recognize, effectively trap and preconcentrate BPA over a concentration range of 2–20 μM. Recoveries ranged from 94.03 to 105.3 %, with a relative standard deviation lower than 7.9 %. Under the optimal condition, molecularly imprinted SPE recoveries of spiked human serum, pig urine, tap water and shrimp were 65.80, 82.32, 76.00 and 75.97 %, respectively, when aqueous samples were applied directly. Compared with C18 SPE, a better baseline, better high-performance liquid chromatography separation efficiency and higher recoveries were achieved after molecularly imprinted SPE.   相似文献   

12.
Molecularly imprinted polymers (MIPs) were prepared for adenosine-5′-monophosphate (AMP), a substrate of AMP-activated protein kinase. The template molecule was formed by the vinylphenylboronate diester of adenosine on which 5′-free hydroxide was protected by tert-butyldimethylsilyl group in order to mimic the steric hindrance of the phosphate moiety of AMP. Molecular imprinting was performed by complexing acrylamide and the template in a highly cross-linked polymer. MIPs were tested in batch experiments with aqueous samples of nucleotides and a number of parameters were investigated. The use of tetrabutylammonium hydroxide (TBAH) was necessary to obtain a rebinding of nucleotides on MIP. The adsorption of AMP was optimal in 5 mM ammonium acetate buffer solution pH 9.5 for 30 min, with 30 mM of TBAH. The imprinted polymer was selective for AMP towards others nucleotides or deoxi analogues.  相似文献   

13.
An easy-to-use colorimetric test-system for the efficient detection of creatinine in aqueous samples was developed. The test-system is based on composite molecularly imprinted polymer (MIP) membranes with artificial receptor sites capable of creatinine recognition. A thin MIP layer was created on the surface of microfiltration polyvinylidene fluoride (PVDF) membranes using method of photo-initiated grafting polymerization. The MIP layer was obtained by co-polymerization of a functional monomer (e.g. 2-acrylamido-2-methyl-1-propanesulfonic acid, itaconic acid or methacrylic acid) with N, N′-methylenebisacrylamide as a cross-linker. The choice of the functional monomer was based on the results of computational modeling. The creatinine-selective composite MIP membranes were used for measuring creatinine in aqueous samples. Creatinine molecules were selectively adsorbed by the MIP membranes and quantified using color reaction with picrates. The intensity of MIP membranes staining was proportional to creatinine concentration in an analyzed sample. The colorimetric test-system based on the composite MIP membranes was characterized with 0.25 mM detection limit and 0.25–2.5 mM linear dynamic range. Storage stability of the MIP membranes was estimated as at least 1 year at room temperature. As compared to the traditional methods of creatinine detection the developed test-system is characterized by simplicity of operation, small size and low cost.  相似文献   

14.
One of the main challenges in the molecularly imprinted polymers (MIP) field is the proper MIP design for water-soluble compounds because of appearance of serious drawbacks in polar solvents and insolubility of those compounds in non-polar solvents which are commonly used for MIP synthesis. In this work a novel and simple method for synthesis of molecularly imprinted polymers for a water-soluble compound was introduced. Pyridoxine was chosen as a target molecule and the ion-pair complex formed between pyridoxine ion (Py+) and dodecyl sulfate ion (DS) was transferred into the chloroform via liquid-liquid extraction. Then polymerization was carried out in chloroform. The molecular mechanics and density functional theory were proposed to screen proper monomer. Binding energy, ΔE, of a template and a monomer as a measure of their interaction was considered. Ion-pair [Py+-DS] was supposed as a template molecule and acrylic acid, methacrylic acid, allyamine, vinylpridine and 2-hydroxy ethyl methacrylate were as tested monomers. The MIP synthesized using acrylic acid showed the highest selectivity to pyridoxine as predicted from the ΔE calculation. The obtained MIP showed very high affinity against vitamin B6 in comparison to non-imprinted polymers (NIP). It was proved that the obtained MIP with introduced method was much better than that prepared in methanol as porogen. It was showed that the MIP prepared by this new method could be used as an adsorber for extraction and determination of pyridoxine in real and synthetic samples.  相似文献   

15.
以双酚A为模板分子,3-氨基丙基乙氧基硅烷为功能单体,通过溶胶-凝胶反应合成双酚A分子印迹纳米硅胶微球。以印迹微球为固相萃取吸附剂,优化固相萃取条件,确定二氯甲烷为上样溶剂。固相萃取选择性实验表明,在双酚A及其结构类似物四溴双酚A、双酚C、壬基酚的混合物溶液中,印迹萃取柱对双酚A具有良好的选择性能,回收率达到90.7%。浓度为2.5和5μmol/L的加标罐装食品样品,经印迹萃取柱预处理,液相色谱检测得到回收率72%~84%,相对标准偏差2.9%~4.4%。  相似文献   

16.
A method employing molecularly imprinted polymer (MIP) as selective sorbent for solid-phase extraction (SPE) to pretreat samples was developed. The polymers were prepared by precipitation polymerization with andrographolide as template molecule. The structure of MIP was characterized and its static adsorption capacity was measured by the Scatchard equation. In comparison with C(18)-SPE and non-imprinted polymer (NIP) SPE column, MIP-SPE column displays high selectivity and good affinity for andrographolide and dehydroandrographolide for extract of herb Andrographis paniculata (Burm.f.) Nees (APN). MIP-SPE column capacity was 11.9±0.6 μmol/g and 12.1±0.5 μmol/g for andrographolide and dehydroandrographolide, respectively and was 2-3 times higher than that of other two columns. The precision and accuracy of the method developed were satisfactory with recoveries between 96.4% and 103.8% (RSD 3.1-4.3%, n=5) and 96.0% and 104.2% (RSD 2.9-3.7%, n=5) for andrographolide and dehydroandrographolide, respectively. Various real samples were employed to confirm the feasibility of method. This developed method demonstrates the potential of molecularly imprinted solid phase extraction for rapid, selective, and effective sample pretreatment.  相似文献   

17.
Cotinine, the main metabolite of nicotine in human body, is widely used as a biomarker for assessment of direct or passive exposure to tobacco smoke. A method for molecularly imprinted solid-phase extraction (MISPE) of cotinine from human urine has been investigated. The molecularly imprinted polymer (MIP) with good selectivity and affinity for cotinine was synthesized using cotinine as the template molecule, methacrylic acid as the functional monomer, and ethylene glycol dimethacrylate as the cross-linker. The imprinted polymer was evaluated for use as a SPE sorbent, in tests with aqueous standards, by comparing recovery data obtained using the imprinted form of the polymer and a non-imprinted form (NIP). Extraction from the aqueous solutions resulted in more than 80% recovery. A range of linearity for cotinine between 0.05 and 5 μg mL−1 was obtained by loading 1 mL blank urine samples spiked with cotinine at different concentrations in acetate buffer of pH 9.0, and by using double basic washing and acidic elution. The intra-day coefficient of variation (CV) was below 7% and inter-day CV was below 10%. This investigation has provided a reliable MISPE–HPLC method for determination of cotinine in human urine from both active smokers and passive smokers. Figure  相似文献   

18.
In this work, a novel approach of preparing molecularly imprinted film‐derivatized silica monolith materials was developed by a two‐step procedure. The silica monolithic support was first prepared by the sol–gel method with tetramethoxysilane as the precursor. Subsequently, vinyl groups were introduced onto the surface of silica monolith by immobilization of γ‐methacryloxypropyltrimethoxysilane. The prepolymerization mixtures, consisting of methacrylic acid as a functional monomer, ethylene dimethacrylate as a crosslinker, sulfamethazine as a template molecule and an ionic liquid as porogen, were injected into the silica monolith immobilized vinyl groups to form the molecularly imprinted films on the surface of the vinyl functionalized silica monolith. The monolithic materials were characterized by SEM, Fourier transform IR and solid‐state reflection UV spectra. The resulted imprinted materials were evaluated under CEC and HPLC mode. The results indicated that there were enough recognition sites on the surface of the imprinted film‐derivatized monolithic materials for selectively recognizing sulfamethazine from the sulfonamide mixture. Ionic liquids, which was utilized as the porogens, could improve the flow‐through property and the imprinting effect of the molecularly imprinted film‐functionalized silica monolithic materials.  相似文献   

19.
A monolithic molecularly imprinted polymer (monolithic MIP) for sulfamethoxazole (SMO) was prepared by in situ polymerization method as the HPLC stationary phase. By optimizing the polymerization conditions, the monolithic MIP showed highly specific recognition for the template SMO over its three structurally related analogs. As shown by SEM and the pore size distribution profile, the resultant MIP monolith showed a main pore diameter of 594 nm and a large specific surface area of 124 m2 g−1, this allowed the mobile phase to flow through the column with low backpressure. Furthermore, the recognition abilities of the monolithic MIP in aqueous and organic media were studied. The results exhibited that the monolithic MIP possessed excellent recognition ability in aqueous media. Hydrophobic interactions, in addition to shape recognition, were the dominant effect for recognition in the mobile phase with high water content. Moreover, the binding sites and the dissociation constant were also determined by frontal chromatography as 122 μmol g−1 and 1.88 × 10−5 mol L−1, respectively, which demonstrated that the obtained SMO-MIP monolith had a high binding capacity and strong affinity ability to the template molecule. Furthermore, the resultant SMO-MIP monolith was used as HPLC column directly to determine the SMO contents in three kinds of pharmaceutical tablets with the optimized aqueous mobile phase.  相似文献   

20.
合成了甲福明的分子印迹聚合物,以此聚合物为识别物质,在线分离富集甲福明,建立了一种测定甲福明的流动式化学发光但感器。N-溴代丁二酰亚胺(NBS)和荧光素与甲福明发生化学反应,产生强的化学发光。甲福明质量浓度在2×10-8~8×10-6g/mL范围内同发光强度成良好线性关系,方法的检出限为6×10-9g/mL,相对标准偏差小于5%(n=9)。选择性实验表明将分子印迹聚合物作为识别物质应用于化学发光分析中,能大大提高化学发光分析方法的选择性。该传感器可逆性强、稳定性好,可重复使用100次以上,已用于人体尿样中甲福明的测定。  相似文献   