1.
We have studied the interface and thin film formation of the organic molecular semiconductor 3,4,9,10 perylene tetracarboxylic dianhydride (PTCDA) on clean and on hydrogen passivated Si(0 0 1) surfaces. The studies were made by means of high resolution X-ray photoelectron spectroscopy (HRXPS), near edge X-ray absorption fine structure (NEXAFS), low energy electron diffraction (LEED), and atomic force microscopy (AFM). On the passivated surface the LEED pattern is somewhat diffuse but reveals that the molecules grow in several ordered domains with equivalent orientations to the substrate. NEXAFS shows that the molecules are lying flat on the substrate. The Si 2p XPS line shape is not affected when the film is deposited so it can be concluded that the interaction at the interface between PTCDA and the substrate is weak. The evolution of the film formation appears to be homogeneous for the first monolayer with a nearly complete coverage of flat lying molecules based on the XPS attenuation. For layer thickness of 0.5-2 monolayers (ML) the molecules start to form islands, attracting the molecules in between, leaving the substrate partly uncovered. For thicker films there is a Stranski-Krastanov growth mode with thick islands and a monolayer thick film in between. For the clean surface the ordering of the film is much lower and angle resolved photoelectron spectroscopy (ARPES) of the molecular orbitals have only a small dependence of the emission angle. NEXAFS shows that the molecules do not lie flat on the surface and also reveal a chemical interaction at the interface.  相似文献   

2.
The interaction between C60 molecules and the Si(100) surface and the preparation of silicon-carbide thin films by thermal reaction of C60 molecules with the Si(100) surface have been investigated using X-ray photoelectron spectroscopy, ultraviolet photoelectron spectroscopy, reflection high-energy electron diffraction and atomic force microscopy measurements. The effects of annealing temperature and C60 coverage on the SiC formation will be discussed. It is found that the C60 molecules bond covalently with silicon, and the number of bonds increase upon increasing the annealing temperature. Annealing at T≥830°C entails the formation of stoichiometric silicon carbide clusters that coalesce to form a continuous SiC layer when the C60 coverage is greater than one monolayer. Deep pits acting as silicon diffusion channels are present with dimensions that increase with the amounts of C60.

The interaction of C60 with the SiC surface was also investigated. It is found that a similar covalent interaction is present in the two systems C60/Si and C60/SiC.  相似文献   


3.
The reaction of formic acid on Si(1 1 1)-7 × 7 was investigated using X-ray photoelectron spectroscopy (XPS), ultraviolet photoelectron spectroscopy (UPS) and high-resolution electron energy loss spectroscopy (HREELS). The hydroxyl and carbonyl O 1s core levels of chemisorbed formic acid display chemical shifts of 2.4 and 0.2 eV respectively, compared with those of physisorbed molecules. The HREELS spectra of chemisorbed formic acid show the absence of stretching and bending modes of the O-H bond, the appearance of Si-H (2089 cm−1) and the Si-O (680 cm−1) stretching modes and the retained stretching mode of CO at 1703 cm−1. Our results clearly suggest that formic acid dissociates to form monodentate formate species and H-atom on the adatom-rest atom pair of Si(1 1 1)-7 × 7.  相似文献   

4.
We present the results of scanning tunneling microscopy (STM) and photoemission spectroscopy (PES) of the Ta/Si(1 1 1)-7 × 7 system after deposition of Ta at substrate temperatures from 300 to 1250 K. The coverage of Ta varied from 0.05 up to 2.5 of a monolayer (ML). STM shows that at 300 K and coverage less than 1 ML, a disordered chemisorbed phase is formed. Deposition on a hot surface (above 500 K) produces round 3D clusters randomly distributed on the surface. Cluster height and their diameter are found to change drastically with annealing temperature and the Ta coverage. Analysis of photoemission data of the Si 2p core levels shows that at room temperature and at coverage ?1 ML core level binding energy shifts and intensity variations of Si surface related components are observed, which clearly indicate that the reaction starts already at 300 K. Shifts in the binding energy, changes of the peak shapes and intensity of the Ta 4f doublet at higher temperatures can be explained by the formation of stable silicide on the surface.  相似文献   

5.
MnSi is a ferromagnetic compound with a Curie temperature of 29 K. Recent theoretical studies predict that 2 ML of MnSi epitaxially grown on Si show a ferromagnetic metallic ground state with spin polarization of about 50%. This would allow the development of spintronic devices based on the injection of spin-polarized current from a ferromagnetic metal into a semiconductor.In this context the possibility of growing in situ MnSi on the Si(1 1 1) surface has been explored. Thermal reaction, crystalline structure and electronic properties of the grown films have been studied in situ by photoemission spectroscopy (PES), X-ray absorption spectroscopy (XAS), and low energy electron diffraction (LEED). Depositing a thin film of Mn on Si(1 1 1) the formation of ordered islands (with dimensions dependent on the amount of deposited Mn) is driven by annealing at selected temperatures, as already observed. Our preliminary studies show that by simultaneously depositing Mn and Si in 1:1 stoichiometry on Si(1 1 1) a large improvement in the homogeneity of the MnSi films is achieved.  相似文献   

6.
The initial stages of iron silicide growth on the Si(1 0 0)2 × 1 surface during solid-phase synthesis were investigated by photoelectron spectroscopy using synchrotron radiation. The experiments were made on iron films of 1-50 monolayer (ML) thickness in the temperature range from room temperature to 750 °С. Our results support the existence of three stages in the Fe deposition on Si(1 0 0) at room temperature, which include formation of the Fe-Si solid solution, Fe3Si silicide and an iron film. The critical Fe dose necessary for the solid solution to be transformed to the silicide is found to be 5 ML. The solid-phase reaction was found to depend on the deposited metal dose. At 5 ML, the reaction begins at 60 °С, and the solid-phase synthesis leads to the formation of only metastable silicides (FeSi with the CsCl-type structure, γ-FeSi2 and α-FeSi2). A specific feature of this process is Si segregation on the silicide films. At a thickness of 15 ML and more, we observed only stable phases, namely, Fe3Si, ε-FeSi and β-FeSi2.  相似文献   

7.
Sub-monolayer and monolayer of lead phthalocyanine deposited on InSb(1 0 0) (4 × 2)/c(8 × 2) surface have been investigated by scanning tunneling microscopy and low energy electron diffraction. Molecules first adsorb on the indium rows of the (4 × 2)/c(8 × 2) structure in the [1 1 0] direction and diffuse at the surface in order to form two-dimensional islands. The molecule-substrate interaction stabilizes the PbPc molecules on the In rows. It weakens the interaction between molecules located in adjacent rows resulting in numerous gliding planes between the molecular chains, in the direction parallel to the rows. At monolayer completion, a long-range one-dimensional order is adopted by the molecules in the [1 1 0] direction.  相似文献   

8.
Results of an STM study of dissociative GeH4 adsorption on Si(1 1 1)-(7 × 7) at 300 K show that GeH4 adsorbs under scission of two Ge-H bonds according to GeH4(g) + 4db → GeH2(ad) + 2H(ad). GeH2 binds to two adatom dangling bonds in a bridged configuration, while the two released hydrogen atoms saturate two additional dangling bonds. The GeH4 sticking coefficient under these conditions is 1.2 × 10−6, one order of magnitude smaller than for SiH4.  相似文献   

9.
The growth and thermal stability of ultrathin ZrO2 films on the Si-rich SiC(0 0 0 1)-(3 × 3) surface have been explored using photoelectron spectroscopy (PES) and X-ray absorption spectroscopy (XAS). The films were grown in situ by chemical vapor deposition using the zirconium tetra tert-butoxide (ZTB) precursor. The O 1s XAS results show that growth at 400 °C yields tetragonal ZrO2. An interface is formed between the ZrO2 film and the SiC substrate. The interface contains Si in several chemically different states. This gives evidence for an interface that is much more complex than that formed upon oxidation with O2. Si in a 4+ oxidation state is detected in the near surface region. This shows that intermixing of SiO2 and ZrO2 occurs, possibly under the formation of silicate. The alignment of the ZrO2 and SiC band edges is discussed based on core level and valence PES spectra. Subsequent annealing of a deposited film was performed in order to study the thermal stability of the system. Annealing to 800 °C does not lead to decomposition of the tetragonal ZrO2 (t-ZrO2) but changes are observed within the interface region. After annealing to 1000 °C a laterally heterogeneous layer has formed. The decomposition of the film leads to regions with t-ZrO2 remnants, metallic Zr silicide and Si aggregates.  相似文献   

10.
Adsorption structures of the pentacene (C22H14) molecule on the clean Si(0 0 1)-2 × 1 surface were investigated by scanning tunneling microscopy (STM) in conjunction with density functional theory calculations and STM image simulations. The pentacene molecules were found to adsorb on four major sites and four minor sites. The adsorption structures of the pentacene molecules at the four major sites were determined by comparison between the experimental and the simulated STM images. Three out of the four theoretically identified adsorption structures are different from the previously proposed adsorption structures. They involve six to eight Si-C covalent chemical bonds. The adsorption energies of the major four structures are calculated to be in the range 67-128 kcal/mol. It was also found that the pentacene molecule hardly hopped on the surface when applying pulse bias voltages on the molecule, but was mostly decomposed.  相似文献   

11.
Thermal (300 K) and electron-induced reactions of benzene (Bz), chlorobenzene (ClPh), 1,2-dichlorobenzene (1,2-diClPh) and 1,4-dichlorobenzene (1,4-diClPh) with Si(1 0 0)2 × 1 have been examined by scanning tunneling microscopy (STM). Thermal reactions of Bz yielded predominantly the quadruply-σ-bound tight bridge, TB, configuration on top of the Si dimer-rows, For ClPh and 1,2-diClPh, which resembled one another, thermal reaction led with 45-50% yield to the doubly-σ-bound butterfly, BF, configuration, also on top of the dimer-row, and with 20% yield to a novel ‘displaced’, D, configuration to one side of a dimer-row. The adsorbate 1,4-diClPh was alone in favouring a configuration in which neighbouring dimer-rows were ‘linked’ (L) by a bright-feature centrally located between the dimer-rows. By ab initio calculation, we interpret D as due to the rupture of one C-Cl bond per adsorbate molecule, and L to the rupture of two C-Cl’s. The breaking of this weak bond is followed in the former case by attachment of the aromatic ring to one dimer-row, and in the latter to attachment to two adjacent dimer-rows. Application of a −5 V voltage pulse to the STM tip substantially increased the percentage of row-linking structures, L, for 1,4-diClPh, but neither −5 V nor +4-6 V volt pulses resulted in L-type binding of Bz. The postulated L product of 1,4-diClPh, with an aromatic ring linking the two inner Si atoms of adjacent dimer-rows and the two Cl’s on the outer Si atoms of the dimer-rows, is shown to be in accord with ab initio simulation of the observed STM image.  相似文献   

12.
The development of contact potential difference (CPD) inhomogeneities on oxide-covered silicon samples was investigated by monitoring the CPD of a clean Si(0 0 1) 2 × 1 surface during exposure to molecular oxygen with Kelvin Probe Force Microscopy. A steady fluctuation level is reached within the completion of a monolayer of oxide. Non-continuous oxygen exposure at room temperature and at lower temperatures unequivocally demonstrates the coexistence of two oxidation processes. One of these processes involves a metastable precursor to oxygen dissociation.  相似文献   

13.
Laterally resolved topography and Contact Potential Difference (CPD) images, acquired during the exposure of clean Si(1 1 1) 7 × 7 to molecular oxygen at room temperature, show a heterogeneous oxidation process, without preference for step edges. The increase of and lateral changes in work function variations show that the CPD variations of the final oxide film are related to the silicon/oxide interface. The molecular Höfer precursor has a pronounced influence on the development of the interface bonding.  相似文献   

14.
We have investigated the adsorption mechanism of SiO molecule incident on a clean Si(1 0 0) p(2 × 2) reconstructed surface using density functional theory based methods. Stable adsorption geometries of SiO on Si surface, as well as their corresponding activation and adsorption energies are identified. We found that the SiO molecule is adsorbed on the Si(1 0 0) surface with almost no activation energy. An adsorption configuration where the SiO binds on the channel separating the dimer rows, forming a Si-O-Si bridge on the surface, is the energetically most favourable geometry found. A substantial red-shift in the calculated vibrational frequencies of the adsorbed SiO molecule in the bridging configurations is observed. Comparison of adsorption energies shows that SiO adsorption on a Si(1 0 0) surface is energetically less favourable than the comparable O2 adsorption. However, the role of SiO in the growth of silicon sub-oxides during reactive magnetron plasma deposition is expected to be significant due to the relatively large amount of SiO molecules incident on the deposition surface and its considerable sticking probability. The stable adsorption geometries found here exhibit structural properties similar to the Si/SiO2 interface and may be used for studying SiOx growth.  相似文献   

15.
Molecular electroactive monolayers have been produced from vinylferrocene (VFC) via light-assisted surface anchoring to H-terminated n- and p-Si(1 0 0) wafers prepared via wet chemistry, in a controlled atmosphere. The resulting Si-C bound hybrids have been characterized by means of XPS and AFM. Their performance as semiconductor functionalized electrodes and their surface composition have been followed by combining electrochemical and XPS measurements on the same samples, before and after use in an electrochemical cell. White-light photoactivated anchoring at short (1 h) exposure times has resulted in a mild route, with a very limited impact on the initial quality of the silicon substrate. In fact, the functionalized Si surface results negligibly oxidized, and the C/Fe atomic ratio is close to the value expected for the pure molecular species. The VFC/Si hybrids can be described as (η5-C5H5)Fe2+(η5-C5H4)-CH2-CH2-Si species, on the basis of XPS results. Electrochemical methods have been applied in order to investigate the role played by a robust, covalent Si-C anchoring mode towards substrate-molecule electronic communication, a crucial issue for a perspective development of molecular electronics devices. The response found from cyclic voltammograms for p-Si(1 0 0) functionalized electrodes, run in the dark and under illumination, has shown that the electron transfer is not limited by the number of charge carriers, confirming the occurrence of electron transfer via the Si valence band. The hybrids have shown a noticeable electrochemical stability and reversibility under cyclic voltammetry (cv), and the trend in peak current intensity vs. the scan rate was linear. The molecule-Si bond is preserved even after thousands of voltammetric cycles, although the surface coverage, evaluated from cv and XPS, decreases in the same sequence. An increasingly larger surface concentration of Fe3+ at the expenses of Fe2+ redox centers has been found at increasing number of cv’s, experimentally associated with the growth of silicon oxide. Surface SiO groups from deprotonated silanol termination, induced by the electrochemical treatments, are proposed as the associated counterions for the Fe3+ species. They could be responsible for the observed decrease in the electron transfer rate constant with electrode ageing.  相似文献   

16.
Photoelectron spectroscopy, low-energy electron diffraction, and scanning probe microscopy were used to investigate the electronic and structural properties of graphite layers grown by solid state graphitization of SiC(0 0 0 1) surfaces. The process leads to well-ordered graphite layers which are rotated against the substrate lattice by 30°. On on-axis 6H-SiC(0 0 0 1) substrates we observe graphitic layers with up to several 100 nm wide terraces. ARUPS spectra of the graphite layers grown on on-axis 6H-SiC(0 0 0 1) surfaces are indicative of a well-developed band structure. For the graphite/n-type 6H-SiC(0 0 0 1) layer system we observe a Schottky barrier height of ?B,n = 0.3 ± 0.1 eV. ARUPS spectra of graphite layers grown on 8° off-axis oriented 4H-SiC(0 0 0 1) show unique replicas which are explained by a carpet-like growth mode combined with a step bunching of the substrate.  相似文献   

17.
Morphology of high-vacuum deposited rubrene thin films on the annealed (0 0 0 1) vicinal sapphire surfaces was studied by atomic force microscopy in non-contact mode. Atomic force microscopy images of rubrene thin films indicate that a regular array of steps on the sapphire surface acts as a template for the growth of the arrays of rubrene nanosize wires. To further demonstrate that morphological features of a substrate are crucial in determining the morphology of rubrene layers we have grown rubrene on the sapphire surfaces that were characterized by the terrace-and-step morphology with islands. We have found preferential nucleation of rubrene molecules at the intersection between a terrace and a step, as well as around the islands located on terraces.  相似文献   

18.
The room temperature deposition of PTCDA on hydrogen passivated Si(1 1 1), as a function of evaporation temperature and dosing time, has been studied by STM. At low evaporation temperature, 200 °C, clusters with an average size of 3.5 nm are formed on the surface. The mobility of the small clusters is so high, even at room temperature, that most of the clusters are trapped at surface defects. By increasing the evaporation temperature to 230 °C, larger clusters are formed which have lower mobility. The growth process is identified as a Volmer-Weber mechanism. On increasing the evaporation temperature further to 250 °C, crystals with dendritic shape are formed with an average size of 150 nm. The terraces of the crystal are formed with the (1 0 2) basal plane of the α-phase. Molecular resolution on the terrace also allows us to identify the molecular mechanism involved in the growth of the dendritic crystals.  相似文献   

19.
In this work we show the adsorption of acetonitrile (CH3CN) and acrylonitrile (CH2CHCN) on Si(0 0 1)-2 × 1 at room temperature by increasing the molecular doses. Especially, by means of XPS and LEED data, we stress the action of these molecules on the silicon surface locating the dangling-bonds quasi-saturation within 10 L. The shortage of nitrogen XPS signal and some anomalies in carbon spectra point to an invading action from a traditional X-ray source (Al-Kα line) against chemisorbed molecules. In particular, we think that a long exposure to this radiation could break carbon-silicon bonds changing some adsorption geometries and making desorb molecular fragments.  相似文献   

20.
Using scanning tunneling microscopy (STM), it has been found that the reconstruction of Si(1 1 4) is transformed irreversibly from a 2 × 1 structure composed of dimer (D), rebonded atom (R), and tetramer (T) rows (phase A) to a different kind of 2 × 1 structure composed of D, T, and T rows (phase B) by C incorporation. It has been confirmed by high-resolution synchrotron core-level photoemission spectroscopy (PES) that such an irreversible structural transformation is due to stable subsurface C atoms. They induce anisotropic compressive stress on the surface, which results in insertion of Si dimers to an R row to form a T row.  相似文献   