针对当前0.40~2.50 μm宽光谱响应成像系统可见光波段颜色信息丢失,全波段只能灰度成像的问题,设计并制备了用于全天时、可见光色彩恢复、短波红外(Short-Wave Infrared,SWIR)多波段成像的滤光片。使用Essential Macleod膜系设计软件,通过三种设计方案进行参数和性能对比,最终采用短波通基础膜系的两级截止带构造蓝光(B)+SWIR、绿光(G)+SWIR、红光(R)+SWIR负滤光片膜系设计,采用长波通基础膜系实现0.42~2.50 μm通带膜系设计。以上四个滤光片的组合选用Ta2O5和SiO2为高低折射率材料在石英玻璃JGS-1基底上制备,经过测量通带的平均透过率均大于93.6%,通带平均透过率之差小于1.6%。最后用制备的滤光片进行拍照和计算,对色彩恢复功能进行验证。测试结果对宽光谱彩色成像技术的进一步研究具有参考价值。 相似文献
4.
本文论述用于激光荧光肺癌诊断图象处理系统滤光片的膜系设计,制备这套滤光片所采取的工艺措施,最后给出研制的结果。 相似文献
5.
基于光刻工艺的阶跃滤光片式微型分光器件研制 总被引:2,自引:0,他引:2
为了消除机械掩模的尺寸限制和阴影效应,采用基于光刻掩膜的组合刻蚀法来制备阶跃滤光片,并成功地实现了16×1通道阶跃滤光片式微型分光器件的制备,该分光器件中滤光片单元的宽度只有90 μm,总体尺寸不到2 mm.各滤光片通道分布在632.4 nm到739.6 nm之间,带宽均小于2.9 nm,透过率均高于70%.这样的阶跃滤光片最小单元尺寸可达微米量级,阴影效应可减小到微米甚至亚微米量级,与电荷耦合器件(CCD)完全匹配,可以作为微型分光器件来构建应用于空间等领域的微型光谱系统,从而促进相应光谱仪器的微型化. 相似文献
6.
7.
8.
9.
为了满足红外军用仪器的特殊要求,根据薄膜理论进行了红外双波段滤光膜的膜系设计;采用电子束真空镀膜的方法,通过对工艺参数的调整,在多光谱ZnS基底上镀制了1 064 nm高反、3~5μm高透的红外双波段滤光膜。利用低能离子轰击,使膜层与基底间的应力明显减小;使用BGS 6341薄膜应力测试仪,采用渐变梯度法,测得其压应力由122 MPa降到51 MPa。另外,通过低能离子轰击和真空退火处理,提高了膜层的抗损伤阈值。结果显示所镀膜层满足红外军用仪器的使用要求。 相似文献
10.
《光学技术》2021,47(5):561-564
为了研制具有高效电磁屏蔽功能的反红外、透1064nm激光的滤光片,基于金属薄膜诱导理论和多层薄膜的干涉原理,设计了诱导滤光膜的膜系结构,并讨论了金属Ag薄膜厚度误差对滤光片光谱性能的影响。采用离子束辅助沉积的方式制备膜系中的介质薄膜,采用离子束溅射方式制备了金属Ag薄膜;利用放大膜厚控制误差的方法,精确地监控薄层金属Ag膜的沉积厚度,同时避免了Ag膜被氧化。通过工艺实验,制备的滤光片在1064nm激光波长的透射率达到88%以上、中长波红外波段反射率达90%以上,对18~36GHz电磁波屏蔽效能达到23dB以上,具有良好的中长波红外及电磁波屏蔽功能。 相似文献
11.
12.
跑道形玻璃波导谐振腔滤波器的研制 总被引:1,自引:5,他引:1
采用Ag+-Na+离子工艺,在K9玻璃上制备了跑道形波导谐振腔滤波器.测试得到该滤波器自由光谱范围为FSR=0.177 nm,对比对为Cr=7.5 dB.同时分析得到耦合器的耦合系数为κ=0.916,耦合器和环形腔的损耗因子分别为δ=0.55,γ=0.48.耦合器的两波导几乎相连、条波导边缘不规则和一次离子交换波导表面缺陷是造成该波导滤波器具有较大损耗的主要原因.通过改进工艺技术降低波导损耗,该滤波器可以用于光通信、传感等领域,也可与其它波导结构相结合实现新的功能. 相似文献
13.
紫黄晶是珍贵的水晶变种,其紫-黄色区域分别具有特征的中红外吸收光谱,在不同温度具有不同变化规律,这些规律无法在单次、单点实验中加以总结。实验通过热处理和显微红外光谱技术,对不同温度淬火紫黄晶的紫-黄色区进行线扫描,分析一系列温度、空间变化下的中红外光谱,实验表明水对于紫黄晶的颜色影响不大,在加热过程中谱线会发生规律性变化。紫色区3 585和3 614 cm-1尖锐峰、3 400 cm-1附近宽泛峰同时变化表明宝石在受热过程以结构水变化为主,而受热后紫色区的特征峰减弱及黄区特征峰增强的现象可能与结构水中H+或其他阳离子的移动有关。同时发现对于热处理产生的黄晶,中红外光谱仍保持紫晶特征吸收光谱。 相似文献
15.
A novel method is employed to provide a quick and convenient means for converting a computer generated binary-phase-only filter (BPOF) into a representative optical element that can be tested in the laboratory. Intensity mapped BPOFs are generated using commercial transparency films and later the investigation extends to silver halide emulsions and photopolymers. Our results indicate that this can be a useful process with future applications for optical correlators and optical processors. The generated BPOFs can be made available not only for model verification, but also for direct fabrication of filter elements in an optical system — thus eliminating the need for more expensive alternatives. 相似文献
16.
A channel drop filter system that consists of two waveguides and three cavities is studied. One cavity couples with both waveguides, while the other two work as resonant mirrors to reflect the selected channel back into the system. The operation of this configuration is analyzed, using coupled mode theory. The conditions to achieve 100% in-plane channel transfer are derived. A method to suppress the side lobes of reflection and backward drop is also proposed. The direct coupling between the cavities is not required. The analysis is verified by two-dimensional finite difference time domain simulations in 2D hexagonal photonic crystals. 相似文献
17.
为了解决基于光纤布喇格光栅和压电陶瓷结构的任意光脉冲整形器在动态调谐时存在不足的问题,提出并设计了一种波长、相位、幅度参量独立可调的Bragg波导光栅滤波器,以实现谐振波长及谐振波相位快速独立的线性调控.理论分析表明:波长和相位的理论调谐效率分别为15.6pm/V和0.2π/V,滤波器的输出光强度可以通过偏振旋转器控制.基于转移矩阵理论的仿真分析发现:该滤波器在蚀刻占空比为1/2时反射率最大,光栅长度为10.869mm,蚀刻深度大于100nm时,可以获得98.4%以上的反射率和大于0.14nm的带宽;增大波长调谐电压会进一步降低滤波带宽. 相似文献
18.
在空间光通信系统中,为满足光学系统对滤光膜的特殊要求,研制出了一种近红外宽截止窄带滤光膜,实现了降低深背景范围内杂散光干扰的要求.通过对薄膜材料特性的研究、膜系设计曲线的不断优化,得到了相对易于制备的窄带滤光膜结构;采用电子束加热蒸发及离子辅助沉积技术制备薄膜,采用光控加晶控同时监控的方法监控膜层厚度,通过不断优化工艺参量,提高中心波长处的透过率,最终成功得到了光谱性能较好的滤光膜.经光谱测试表明:所镀膜层在800~1 530nm、1 600~1 800nm波段平均透过率低于0.3%,1 565nm单点透过率高于92%,通带半带宽为18nm,满足光学系统的使用要求. 相似文献
19.
20.
激光敌我识别系统中滤光膜的研制 总被引:7,自引:0,他引:7
根据激光敌我识别系统的使用要求,选择H4和SiO2作为高低折射率材料,借助Macleod和TFCalc软件进行膜系优化设计和分析。采用电子束真空镀膜的方法并加以离子辅助沉积技术,通过正交矩阵实验对材料的工艺参数进行调整和优化,利用基片的正反面分别对带通滤光片的长波反射带和短波反射带进行展宽,解决了单面膜层过厚难以控制的问题,制备了符合要求的激光滤光膜。镀膜后的基片在532,632,905,1064和1550nm波长处的透射率小于0.2%,808nm波长附近的平均透射率大于95%。并在532nm和1064nm波长处具有较高的激光损伤阈值,能承受恶劣的环境测试,满足激光敌我识别系统中光学仪器的使用要求。 相似文献