首页 | 本学科首页   官方微博 | 高级检索  
相似文献
 共查询到19条相似文献,搜索用时 62 毫秒
1.
采用高温固态反应法制备了具有钙钛矿结构的锰氧化物La0.67Ca0.33MnO3,利用X射线衍射、超导量子干涉仪等实验技术研究其结构和磁性质。应用标度律对起依赖于磁场的始磁化强度在t→0时的行为用临界指数β随磁场变化进行描述。临界指数β随着磁场的增大而减小,说明在临界点附近,磁场的增大导致自旋有序度的增加。  相似文献   

2.
A colossal electroresistance effect is found in Nd0.67Sr0.33MnO3-δ polycrystalline ceramics with a very slight oxygen deficiency ~ ~ 0.05. The electroresistance behaviour of Nd0.67Sr0.33MnO3-δ(δ= 0.05) displays the striking similarity to its counterpart magnetoresisnce. It reveals that the boundary effect plays an important role in electroresistance and the same physical origin is likely responsible for both magnetoresistance and electroresistance effects in Nd0.67Sr0.33MnO3-δ polycrystals.  相似文献   

3.
 研究了制备压力对纳米块状样品La2/3Sr1/3MnO3的结构、磁学和电学性质的影响。结果表明:样品的晶粒尺寸随制备压力的增加而变小,且不同样品的磁电阻效应不同。低场磁电阻效应在整个实验温区都随制备压力的升高而变弱,这主要是由制备压力使样品晶粒界面连接更紧密所导致;T<200 K时,高场磁电阻效应随制备压力的升高而变强,T>200 K时,高场磁电阻效应随制备压力的升高反而变弱,这主要是由制备压力改变样品的晶粒尺寸所引起。  相似文献   

4.
江阔 《物理学报》2010,59(4):2801-2807
通过对La0.8Sr0.2Mn1-yCoyO3(y≤02)饱和磁矩和输运的测量,研究了Co对La0.8Sr0.2MnO3的磁电阻影响机制.结果表明,在La0.8Sr0.2Mn1-yCoyO3y≤02)中Co3+离子是低自旋态.由于Mn3+—O—Co3+—O—Mn3+类型的磁交换与Mn3+-Mn4+离子间双交换作用相比较弱,Curie温度TC附近的磁电阻随着Co掺杂量的增加而降低.与此相反,由于Co2+离子与eg巡游电子的反铁磁交换耦合作用,低温区间的磁电阻随着Co掺杂量的增加而升高. 关键词: 低自旋 磁电阻 磁交换作用  相似文献   

5.
江阔 《中国物理 B》2010,19(4):2801-2807
通过对La0.8Sr0.2Mn1-yCoyO3(y≤02)饱和磁矩和输运的测量,研究了Co对La0.8Sr0.2MnO3的磁电阻影响机制.结果表明,在La0.8Sr0.2Mn1-yCoyO3y≤02)中Co3+离子是低自旋态.由于Mn3+—O—Co3+—O—Mn3+类型的磁交换与Mn3+-Mn4+离子间双交换作用相比较弱,Curie温度TC附近的磁电阻随着Co掺杂量的增加而降低.与此相反,由于Co2+离子与eg巡游电子的反铁磁交换耦合作用,低温区间的磁电阻随着Co掺杂量的增加而升高.  相似文献   

6.
常雷  蒋毅坚 《物理学报》2009,58(3):1997-2001
利用脉冲激光沉积技术在LaAlO3(00l)单晶衬底上制备了La067Ba033MnO3薄膜,研究了CO2激光辐照对La067Ba033MnO3薄膜的微结构和磁电性能的影响.结果表明,经激光辐照后,La067Ba033MnO3薄膜的结晶性增强,薄膜应变减小;薄膜表面形貌由“岛状”结构变为“平原"结构,且粗糙度大大降低;同时,薄膜的饱和磁化强度、铁磁居里温度、金属—绝缘态转变温度和磁电阻增大,而矫顽场和电阻率减小.根据对传统退火效应的分析和理论计算,认为激光辐照导致的表面微结构的变化以及薄膜的氧含量和均匀性的提高对La067Ba033MnO3薄膜的磁电性能的改善与优化密切相关. 关键词: 庞磁电阻 激光辐照 脉冲激光溅射沉积  相似文献   

7.
严资杰  袁孝  徐业彬  高国棉  陈长乐 《物理学报》2007,56(10):6080-6083
在室温下利用波长532nm,脉冲宽度7ns的纳秒脉冲激光研究了不同电压和激光能量密度作用下Pr0.7Ca0.3MnO3薄膜的瞬态光响应特性.在激光能量密度为275.16mJ/cm2时,其最大电阻变化率达到92.3%,响应时间约36ns.室温下电压变化对薄膜的光响应特性影响不大,而诱导光能量密度的影响则很明显,能量密度越大,电阻变化越大,响应时间越短,并且电阻变化和响应时间均与激光能量密度呈非线性关系.这种光响应来源于薄膜中的光致非稳态绝缘体-金属相变,有望在新型光电器件上获得应用.  相似文献   

8.
用磁控溅射法制备了GdFeCo/TbFeCo交换耦合两层薄膜,利用不同温度的克尔磁滞回线和VSM磁滞回线研究了读出层(GdFeCo)变温磁化方向变化过程.结果表明,随温度升高读出层从平面磁化转变为垂直磁化,交换耦合两层薄膜具有中心孔探测磁超分辨的基本性能.转变过程主要受饱和磁化强度(Ms)的影响,在GdFeCo的补偿温度附近,读出层的磁化强度较小,退磁场能也较小,在交换耦合的作用下,使读出层(GdFeCo)的磁化方向发生转变.磁化方向的转变在75℃~125℃的温度范围内变化较快.  相似文献   

9.
钙钛矿(La1-yTby)0.67Sr0.33MnO3的超巨磁电阻效应   总被引:4,自引:4,他引:4       下载免费PDF全文
采用固相反应烧结法制成了钙钛矿(La1-yTby)0.67Sr0.33MnO3(y=0—1)多晶样品.研究了样品的微观结构,常温、低温下的磁性,样品的磁电阻随温度、成分的变化关系,电阻随温度变化特性等.并在y=0.40样品中,170K附近、最大磁化场为7T时,观察到了900%的巨磁电阻. 关键词:  相似文献   

10.
La0.67Pb0.33MnO3的磁性及输运特性   总被引:7,自引:0,他引:7       下载免费PDF全文
利用固相反应烧结法制备了La067Pb033MnO3单相多晶样品.研究了其结构、磁性及输运特性.结果表明,样品呈菱面相晶体结构,空间群为R3C,居里温度TC(=353K)非常接近TMI(=360K).在居里温度附近,发生铁磁-顺磁转变,导电特性由金属特征向半导体特征过渡.磁电阻在居里点达到极大值.当H=16T时,磁电阻的极大值为145%;当H=08T时,磁电阻的极大值为9%.输运性质表明,TTMI时 关键词: 磁电阻 输运特性 磁极化子 钙钛石  相似文献   

11.
We measured the temperature dependence of the linear high field Hall resistivity of ( K) and ( K) thin films in the temperature range from 4 K up to 360 K in magnetic fields up to 20 T. At low temperatures we find a charge-carrier density of 1.3 and 1.4 holes per unit cell for the Ca- and Sr-doped compound, respectively. In this temperature range electron-magnon scattering contributes to the longitudinal resistivity. At the ferromagnetic transition temperature a dramatic drop in the number of charge-carriers n down to 0.6 holes per unit cell, accompanied by an increase in unit cell volume, is observed. Corrections of the Hall data due to a non saturated magnetic state will lead a more pronounced charge-carrier density collapse. Received 22 July 1999 and Received in final form 7 October 1999  相似文献   

12.
Electrical resistance (R) measurements of a bulk La0.33Nd0.33Ca0.33MnO3 perovskite in magnetic fields up to 40 kOe have revealed anomalous temperature hysteretic effects both in 0 Oe and 20 kOe magnetic fields. The sharp peak observed in the R vs. T plot indicates the occurrence of metal-to-insulator (M-I) transition at a temperature of T MI=110 K and 140 K, for cooling and warming paths, respectively. An applied magnetic field of 20 kOe reduces the resistance and shifts T MI to 160 K and 185 K for cooling and warming, respectively. We have observed a much higher resistance in the cooling path than in the warming path leading to the hysteretic resistance ratio (R cool/R warm) of 200 at 110 K and 1.8 at 160 K for 0 Oe and 20 kOe, respectively. Record values of colossal magnetoresistance (CMR) have been achieved. The CMR value reaches nearly 99% in the temperature ranges of 90 K to 140 K and 90 K to 170 K for 20 kOe and 40 kOe magnetic fields in the cooling mode, respectively. The observed unusual behavior is attributed to the co-existence of La-rich and Nd-rich domains assumed to be distributed randomly in the compound.  相似文献   

13.
通过实验研究了La0.67-xGdxSr0.33CoO3、La0.67-xGdxSr0.33MnO3(x=0.00、0.05、0.10、0.20、0.30、0.40、0.50、0.60、0.67)体系的磁化强度与温度的关系(M~T)曲线、磁化强度与磁场强度的关系(M~H)曲线.实验结果表明,随Gd掺杂浓度增高,La0.67-xGdxSr0.33CoO3体系的磁结构表现为团簇玻璃态,x>0.10样品的M~T曲线出现了低温区M值急剧上升的奇特现象;La0.67-xGdxSr0.33MnO3体系的磁结构从长程铁磁有序向团簇玻璃态、反铁磁状态转变,x≥0.50样品的M~T曲线在低温区急剧下降.两种体系呈现的不同现象,来源于Gd与Co、Mn不同的耦合作用和Co的自旋态的转变.  相似文献   

14.
The dependence of magnetization on the variation of temperature for La0.67Ca0.33MnO3 and La0.67Sr0.33MnO3 perovskite-type ceramic materials under an external magnetic field was modelled. Application of phenomenological model was performed, showing a good agreement with the experimental data. Temperature dependence of change of both magnetic entropy and specific heat under magnetic field 0.05?T was predicted for La0.67Ca0.33MnO3 and La0.67Sr0.33MnO3. Predicted values of maximum magnetic entropy change, full-width at half-maximum, relative cooling power and maximum specific heat under 0.05 T were evaluated.  相似文献   

15.
Annealing dependence of the lattice parameter, resistivity, magnetoresistance and thermopower have been studied on Nd0.7-Sr0.33MnO3 thin films deposited on LaAlO3 and alumina substrates by pulsed laser ablation. Upon annealing at 800°C and 1000°C the lattice constant of the LaAlO3 film tends toward that of the bulk target due to reduction in oxygen vacancies. This results in a metal-insulator transition at temperatures which increase with progressive annealing along with a decrease in the observed low temperature MR. Using a magnon scattering model we estimate the e g bandwidth of the film annealed at 1000°C and show that the magnon contribution to the resistivity is suppressed in a highly oxygen deficient film and gains prominence only upon subsequent annealing. We also show that upon annealing, the polaron concentration and the spin cluster size increases in the paramagnetic phase, using an adiabatic polaron hopping model which takes into account an exchange dependent activation energy above the resistivity peak.  相似文献   

16.
本文通过固相反应方法制备了具有钙钛矿结构的稀土掺杂锰氧化物La0.875Sr0.125MnO3(LSMO)块材,并用磁控溅射方法在LaAlO3衬底上生长了厚度为50nm的单晶薄膜.X射线衍射仪分别对LSMO块材和薄膜材料进行分析,表明薄膜和衬底具有相同的钙钛矿结构;通过研究该薄膜光诱导效应和磁场下输运行为,发现其输运性质明显改变,表明外场改变体系的电子自旋输运特性,引起双交换作用减弱和增强,分别导致电阻率的增加和减小.  相似文献   

17.
《Current Applied Physics》2018,18(11):1320-1326
High crystalline quality CrN thin films have been grown on La0.67Sr0.33MnO3 (LSMO) templates by molecular beam epitaxy. The structure and magnetic properties of CrN/LSMO heterojunctions are investigated combining with the experiments and the first-principles simulation. The Nėel temperature of the CrN/LSMO samples is found to be 281 K and the saturation magnetization of CrN/LSMO increases compared to that of LSMO templates. The magnetic property of CrN/LSMO heterostructures mainly comes from Cr atoms of (001) CrN and Mn atoms of (001) LSMO. The (001) LSMO induces and couples the spin of the CrN sublattice at CrN/LSMO interface.  相似文献   

18.
La0.67Ba0.33MnO3 (LBMO) thin film is deposited on a 36.7°C SrTiO3 bicrystal substrate using laser ablation technique. A microbridge is created across bicrystal grain boundary and its characteristics are compared with a microbridge on the LBMO film having no grain boundary. Presence of grain boundary exhibits substantial magnetoresistance ratio (MRR) in the low field and low temperature region. Bicrystal grain boundary contribution in MRR disappears at temperature T>175 K. At low temperature, I-V characteristic of the microbridge across bicrystal grain boundary is nonlinear. Analysis of temperature dependence of dynamic conductance-voltage characteristics of the bicrystal grain boundary indicates that at low temperatures (T<175 K) carrier transport across the grain boundary in LBMO film is dominated by inelastic tunneling via pairs of manganese atoms and tunneling through disordered oxides. At higher temperatures (T>175 K), magnetic scattering process is dominating. Decrease of bicrystal grain boundary contribution in magnetoresistance with the increase in temperature is due to enhanced spin-flip scattering process.  相似文献   

19.
Although Cd and Ca ions have the same valence and cation size, their incorporation into vacancy-doped La manganites induce different properties. While the incorporation of Ca leads to high Tc up to 250 K and induces a metallic-like behaviour, the incorporation of Cd severely reduces Tc and promotes insulator-like behaviour. In this work, the Cd hyperfine fields have been measured with the Perturbed Angular Correlations (PAC) technique after implantation and annealing of 111m Cd in La–Cd–MnO3 samples. The PAC results are compared with measurements of the resistivity and magnetization performed on the same samples. The mixed La and Mn site Cd occupancy is suggested as a possibility to explain the properties of the La–Cd–MnO3 system.  相似文献   