1.
S. Ramesh  Lim Jing Yi 《Ionics》2009,15(6):725-730
Poly(vinylchloride) (PVC) is an insulator and acts as a host in polymer electrolyte systems where addition of inorganic salt lithium trifluoromethanesulfonate (LiCF3SO3) and dibutyl phthalate (DBP) converts the system to become conductor. The conductivity of polymer electrolytes is explained on the basis of ionic mobility. Thirty-five weight percent DBP plasticized polymer electrolyte has the highest conductivity value (3.30?×?10?9 S cm?1) at 303 K. Temperature dependence of the conductivity of polymer films obeys the Arrhenius rule. X-ray diffraction (XRD) proves that addition of DBP will increase the amorphous nature of the system and lead to enhancement in ionic conductivity. Complexation between high molecular weight PVC, LiCF3SO3, and DBP is confirmed by the shifting of peaks, decreasing of peaks intensity, and broadening of peaks in XRD. Thermogravimetric analysis reveals that addition of DBP to PVC–LiCF3SO3 system reduces the stability of the film. Subsequently, thermal stability decreases with the increase in DBP content in the polymer electrolytes.  相似文献   

2.
In the present work, ionic transport and interfacial stability of dedoped (insulating) polyaniline (PAni) nanofibers dispersed P(VdF-HFP) based nanocomposite gel polymer electrolytes have been investigated. Samples of P(VdF-HFP)-(PC+DEC)-LiClO4-x wt. % dedoped PAni nanofibers (x = 0, 2, 4, 6, 8, 10) are prepared by conventional solution casting technique. By analysis of SEM, XRD and impedance spectroscopy results it has been demonstrated that the incorporation of up to 6 wt. % of dedoped PAni nanofibers to P(VdF-HFP)-(PC+DEC)-LiClO4 polymer electrolyte system significantly enhances the ionic conductivity and interfacial stability of the electrolyte system. Above that concentration phase separation of PAni nanofibers is observed leading to decrease in ionic conductivity. The aggregated phase decreases the porosity, which results in lower ionic conductivity as confirmed by SEM. Experiments on the interfacial stability reveals that the stability of polymer electrolytes containing nanofibers is better than that of nanofiber free polymer electrolytes.  相似文献   

3.
PEO-based solid polymer electrolyte films with various concentrations of nanochitosan as filler and LiCF3SO3 as salt were prepared by membrane hot-press technique. Nanochitosan was prepared from chitosan by conventional chemical cure method. The prepared composite membranes were characterized by FT-IR, XRD, thermal, SEM, AFM analyses, electrochemical impedance spectroscopy, cyclic voltammetry and compatibility studies. The ionic conductivity and thermal stability of the polymer membranes were enhanced significantly by addition of nanofiller. The compatibility studies reveal that filler incorporated membrane is better compatible with lithium interface than filler free electrolyte.  相似文献   

4.
Hybrid solid polymer electrolyte films comprising of poly(vinyl acetate) (PVAc), poly(methyl methacrylate) (PMMA), LiClO4, and propylene carbonate are prepared by solution casting technique by varying the salt concentration. In this study, PVAc/PMMA polymer blend ratio is fixed as 25:75 on the basis of conductivity and mechanical stability of the film. X-ray diffraction, Fourier transform infrared impedance, thermogravimetry/differential thermal analysis and scanning electron microscopy studies are carried out for the polymer electrolytes. The maximum ionic conductivity is found to be 4.511 × 10−4 S cm−1 at 303 K for the plasticized polymer electrolyte with 8 wt.% of LiClO4. The ionic conductivity is found to decrease with an increase of LiClO4 concentration.  相似文献   

5.
Plasticized nanocomposite polymer electrolytes (PNCPEs) based on poly(vinyl alcohol) (PVA)–MI (M=Na, K, Ag) dispersed with nanofillers Al2O3 and plasticized with poly(ethylene glycol) (PEG) have been prepared by solution cast technique. The structural properties of the samples have been characterized using various experimental techniques such as XRD, DSC, FTIR and B-G spectroscopy. The ionic conductivity and dielectric constant of the samples have been estimated using a LCZ meter in a wide temperature range, i.e. from 30 to 170 °C. It has been observed that the presence of water molecules in polymer electrolytes significantly affects the mobility of ionic species. The temperature dependent ionic conductivity shows the Arrhenius type behavior separated in three distinct regions. The ionic transference number for all PNCPE samples is found to be ≈1, which strongly suggests their ionic nature.  相似文献   

6.
Development and characterisation of polyethylene oxide (PEO)-based nanocomposite polymer electrolytes comprising of (PEO-SiO2): NH4SCN is reported. For synthesis of the said electrolyte, polyethylene oxide has been taken as polymer host and NH4SCN as an ionic charge supplier. Sol–gel-derived silica powder of nano dimension has been used as ceramic filler for development of nanocomposite electrolytes. The maximum conductivity of electrolyte ∼2.0 × 10−6 S/cm is observed for samples containing 30 wt.% silica. The temperature dependence of conductivity seems to follow an Arrhenius-type, thermally activated process over a limited temperature range.  相似文献   

7.
《Current Applied Physics》2015,15(2):135-143
Solid polymer electrolytes consisted of poly(ethylene oxide) (PEO) and poly(methyl methacrylate) (PMMA) blend (50:50 wt/wt%) with lithium triflate (LiCF3SO3) as a dopant ionic salt at stoichiometric ratio [EO + (CO)]:Li+ = 9:1, poly(ethylene glycol) (PEG) as plasticizer (10 wt%) and montmorillonite (MMT) clay as nanofiller (3 wt%) have been prepared by solution cast followed by melt–pressing method. The X–ray diffraction study infers that the (PEO–PMMA)–LiCF3SO3 electrolyte is predominantly amorphous, but (PEO–PMMA)–LiCF3SO3–10 wt% PEG electrolyte has some PEO crystalline cluster, whereas (PEO–PMMA)–LiCF3SO3–10 wt% PEG–3 wt% MMT electrolyte is an amorphous with intercalated and exfoliated MMT structures. The complex dielectric function, ac electrical conductivity, electric modulus and impedance spectra of these electrolytes have been investigated over the frequency range 20 Hz to 1 MHz. These spectra have been analysed in terms of the contribution of electrode polarization phenomenon in the low frequency region and the dynamics of cations coordinated polymer chain segments in the high frequency region, and also their variation on the addition of PEG and MMT in the electrolytes. The temperature dependent dc ionic conductivity, dielectric relaxation time and dielectric strength of the plasticized nanocomposite electrolyte obey the Arrhenius behaviour. The mechanism of ions transportation and the dependence of ionic conductivity on the segmental motion of polymer chain, dielectric strength, and amorphicity of these electrolytes have been explored. The room temperature ionic conductivity values of the electrolytes are found ∼10−5 S cm−1, confirming their use in preparation of all-solid-state ion conducting devices.  相似文献   

8.
The development of magnesium electrolytes for battery applications has been the demand for electrochemical devices. To meet such demand, in this work solid blend polymer electrolytes were prepared using polyvinyl alcohol (PVA) and polyacrylonitrile (PAN) (92.5PVA:7.5PAN) as host polymer, magnesium chloride (MgCl2) of different molar mass percentage (m.m.%) (0.1, 0.2, 0.3, 0.4, 0.5, and 0.6%) as salt and dimethylformamide (DMF) as solvent. Structural, vibrational, thermal, electrical, and electrochemical properties of the prepared electrolytes were investigated using different techniques such as X-ray diffraction pattern, FTIR spectroscopy analysis, differential scanning calorimetry (DSC), AC impedance measurement, and transference number measurement. X-ray diffraction studies confirm the minimum volume fraction of crystalline phase for the polymer electrolyte with 0.5 m.m.% of MgCl2. FTIR confirms the complex formation between host polymer and salt. DSC analysis proves the thermal transition of the prepared films are affected by salt concentration. The optimized material with 0.5 m.m.% of MgCl2 offers a maximum electrical conductivity of 1.01 × 10?3 S cm?1 at room temperature. The Mg2+ ion conduction in the blend polymer electrolyte is confirmed from transference number measurement. Electrochemical analysis demonstrates the promising characteristic of these polymer films suitable as electrolytes for primary magnesium batteries. Output potential and discharge characteristics have been analyzed for primary magnesium battery which is constructed using optimized conducting electrolyte.  相似文献   

9.
S. Ramesh  Liew Chiam Wen 《Ionics》2010,16(3):255-262
Composite polymer electrolyte systems composed of poly(methyl methacrylate) (PMMA) as the host polymer, lithium trifluoromethanesulphonate (also known as lithium triflate; LiCF3SO3) as dopant salt, and a variety of different concentrations of nano-sized fumed silica (SiO2) as inorganic filler were studied. The effect upon addition of SiO2 on the ionic conductivity of the composite polymer electrolytes was investigated, and it was proven that the ionic conductivity had been enhanced. In addition, the interfacial stability also showed improvement. Maximum conductivity was obtained upon addition of 2 wt.% SiO2. The complexation of PMMA and LiCF3SO3 was verified through Fourier transform infrared studies. The thermal stability of the polymer electrolytes was also found to improve after dispersion of inorganic filler. This was proven in the thermogravimetric studies.  相似文献   

10.
Polymer electrolyte based on PVA doped with different concentrations of NH4Br has been prepared by solution casting technique. The complexation of the prepared polymer electrolytes has been studied using X-ray diffraction (XRD) and Fourier transform infra red (FTIR) spectroscopy. The maximum ionic conductivity (5.7×10−4 S cm−1) has been obtained for 25 mol% NH4Br-doped PVA polymer electrolyte. The temperature dependence of ionic conductivity of the prepared polymer electrolytes obeys Arrhenius law. The ionic transference number of mobile ions has been estimated by dc polarization method and the results reveal that the conducting species are predominantly ions. The dielectric behavior of the polymer electrolytes has been analyzed using dielectric permittivity and electric modulus spectra.  相似文献   

11.
Li-ion rechargeable batteries based on polymer electrolytes are of great interest for solid state electrochemical devices nowadays. Many studies have been carried out to improve the ionic conductivity of polymer electrolytes, which include polymer blending, incorporating plasticizers and filler additives in the electrolyte systems. This paper describes the effects of incorporating nano-sized MnO2 filler on the ionic conductivity enhancement of a plasticized polymer blend PMMA–PEO–LiClO4–EC electrolyte system. The maximum conductivity achieved is within the range of 10−3 S cm−1 by optimizing the composition of the polymers, salts, plasticizer, and filler. The temperature dependence of the polymer conductivity obeys the VTF relationship. DSC and XRD studies are carried out to clarify the complex formation between the polymers, salts, and plasticizer.  相似文献   

12.
Thin film of poly (vinylchloride) and poly (methylmethacrylate) blend polymer electrolytes plasticized with a combination of DBP and Li2SO4 salts have been prepared by solution casting technique. The prepared films were subjected to a.c. impedance measurements as a function of temperature ranging from 304–373 K. The maximum conductivity at 304 K was found to be 1.24 × 10−8 S·cm−1 for PVC-PMMA-Li2SO4-DBP (7.5-17.5-5-70 mole-%). Temperature dependence studies on the ionic conductivity in the PVC-PMMA-Li2SO4-DBP system suggest that the ion conduction follows the Williams-Landel-Ferry (WLF) mechanism, which is further confirmed by Vogel-Tamman-Fulcher (VTF) plots. XRD, FTIR, SEM and thermal studies revealed complex formation in.  相似文献   

13.
The polyethylene oxide (PEO) based lithium ion conducting polymer electrolytes complexed with lithium trifluoromethanesulfonate (LiCF3SO3 or LiTf) plasticized with an ionic liquid 1-ethyl 3-methyl imidazolium trifluoromethanesulfonate (EMITf) have been reported. Morphological, spectroscopic, thermal and electrochemical investigations demonstrate promising characteristics of the polymer films, suitable as electrolyte in various energy storage/conversion devices. Significant structural changes have been observed in the polymer electrolyte due to the ionic liquid addition, investigated by X-ray diffraction (XRD) and optical microscopy. The ion-polymer interaction, particularly the interaction of imidazolium cation with PEO chains, has been evidenced by IR and Raman spectroscopic studies. The optimized composition of the polymer electrolyte i.e. PEO25.LiTf + 40 wt.% EMITf offer room temperature ionic conductivity of ~ 3 × 10− 4 S cm− 1 with wide electrochemical stability window and excellent thermal stability. The ‘σ versus 1/T’ curves show apparent Arrhenius behavior below and above melting temperature. The ionic conductivity has been observed due to Li+ ions, as confirmed from 7Li-NMR studies, though the component ions of ionic liquid and anions also contribute significantly to the overall conductivity.  相似文献   

14.
Solid polymer electrolytes have attracted considerable attention due to their wide variety of electrochemical device applications. The present paper is focused on the effect of plasticizer to study the structural, electrical and dielectric properties of PVA-H3PO4 complex polymer electrolytes. XRD results show that the crystallinity decreases due to addition of plasticizer up to particular amount of polyethylene glycol (PEG) and thereafter it increases. Consequently, there is an enhancement in the amorphicity of the samples responsible for process of ion transport. This characteristic behavior can be verified by the analysis of the differential scanning calorimetry results. FTIR spectroscopy has been used to characterize the structure of polymer and confirms the complexation of plasticizer with host polymeric matrix. Electrical and dielectric properties have been studied for different wt% of plasticizer and their variations have been observed. The addition of PEG has significantly improved the ionic conductivity. The optimum ionic conductivity value of the plasticized polymer electrolyte film of 30 wt% PEG has been achieved to be of the order of 10−4 S cm−1 at room temperature and corresponding ionic transference number is 0.98. The minimum activation energy is found to be 0.25 eV for optimum conductivity condition.  相似文献   

15.
The ionic conductivity and dielectric properties of the solid nanocomposite polymer electrolytes formed by dispersing a low particle-sized TiO2 ceramic filler in a poly (ethylene oxide) (PEO)-AgNO3 matrix are presented and discussed. The solid nanocomposite polymer electrolytes are prepared by hot press method. The optimum conducting solid polymer electrolyte of polymer PEO and salt AgNO3 is used as host matrix and TiO2 as filler. From the filler concentration-dependent conductivity study, the maximum ionic conductivity at room temperature is obtained for 10 wt% of TiO2. The real part of impedance (Z′) and imaginary part of impedance (Z″) are analyzed using an LCR meter. The dielectric properties of the highest conducting solid polymer electrolyte are analyzed using dielectric permittivity (ε′), dielectric loss (ε″), loss tangent (tan δ), real part of the electric modulus (M′), and imaginary part of the electric modulus (M″). It is observed that the dielectric constant (ε′) increases sharply towards the lower frequencies due to the electrode polarization effect. The maxima of the loss tangent (tan δ) shift towards higher frequencies with increasing temperature. The peaks observed in the imaginary part of the electric modulus (M″) due to conductivity relaxation shows that the material is ionic conductor. The enhancement in ionic conductivity is observed when nanosized TiO2 is added into the solid polymer electrolyte.  相似文献   

16.
Nanocomposite polymer electrolytes (NCPEs) composed of poly(vinylidenefluoride-co-hexafluoropropylene) (PVdF-co-HFP) as a host polymer, Poly(vinyl acetate) (PVAc) as an additive, Ethylene Carbonate (EC) as a plasticizer, Lithium Perchlorate as dopant salt and Barium Titanate (BaTiO3) as a filler were prepared for various concentrations of BaTiO3 using solvent casting technique. Thermal stability of the sample having maximum ionic conductivity was found using TG/DTA analysis. Nano composite polymer electrolytes were subjected to ac impedance analysis spectra for acquiring the ionic conductivity values at different temperature. Surface structure of the sample was analysed using scanning electron microscope and the complexations of samples were analysed using X-ray diffraction analysis. It was noted that the polymer electrolyte contains 8 wt. % of BaTiO3 showed maximum ionic conductivity than the other ratios of BaTiO3.  相似文献   

17.
Poly(ethylene oxide) (PEO)-based composite polymer electrolytes (CPEs), comprising various concentrations of lithium hexafluorophosphate and magnesium aluminium silicate, were prepared by hot-press technique. The membranes were characterised by scanning electron microscopy, tensile and thermal analyses. It has been demonstrated that the incorporation of the ceramic filler in the polymeric matrix has significantly enhanced the ionic conductivity, thermal stability and mechanical integrity of the membrane. It also improved the interfacial properties with lithium electrode. Finally, an all-solid-state lithium cell composed of Li/CPE/LiFePO4 has been assembled and its cycling performance was analysed at 70 °C. The cell delivered a discharge capacity of 115 mAh g?1 at 1 °C rate and is found to be higher than previous reports.  相似文献   

18.
Polycarbonates (4a–d) with various side chain lengths were synthesized by the reaction of 1,4-bis(hydroxyethoxy)benzene derivatives and triphosgene in the presence of pyridine. The polymer electrolytes composed of 4a–d with lithium bis(trifluoromethanesulfonyl)imide (LiN(SO2CF3)2, LiTFSI) were prepared, and their ionic conductivities and thermal and electrochemical properties were investigated. 4d-Based polymer electrolyte showed the highest ionic conductivity values of 1.0?×?10?4?S/cm at 80 °C and 1.5?×?10?6?S/cm at 30 °C, respectively, at the [LiTFSI]/[repeating unit] ratio of 1/2. Ionic conductivities of these polycarbonate-based polymer electrolytes showed the tendency of increase with increasing the chain length of oxyethylene moieties as side chains, suggestive of increased steric hindrance by side chains. Unique properties were observed for the 4a(n?=?0)-based polymer electrolyte without an oxyethylene moiety. All of polycarbonate-based polymer electrolytes showed good electrochemical and thermal stabilities as polymer electrolytes for battery application.  相似文献   

19.
Structural, thermal, electrical and electrochemical behaviour of polymer blend electrolytes comprising polyvinyl alcohol (PVA) and polyvinyl pyrrolidone (PVP) as host polymers and Mg(ClO4)2 as dopant salt have been investigated. The changes in the structural properties on the incorporation of dopant in the blends were investigated by XRD and FTIR analyses. Thermal properties of pure PVA–PVP blend and their complexes were examined by DSC to measure how the thermal transitions of the prepared films were affected by different concentration of Mg(ClO4)2. The ionic conductivity and dielectric behaviour were explored using A.C. impedance spectroscopy. The trend of ionic conductivity increases almost proportionally to the content of magnesium salt and can be related to an increase of amorphous phase at high level of dopant salt. The electrochemical stability of the optimum conducting blend polymer electrolyte is found to be ~3.5 V. The Mg2+ transference number for the sample with optimized conductivity was found to be 0.31.  相似文献   

20.
Proton-conducting polymer electrolytes based on biopolymer, agar-agar as the polymer host, ammonium bromide (NH4Br) as the salt and ethylene carbonate (EC) as the plasticizer have been prepared by solution casting technique with dimethylformamide as solvent. Addition of NH4Br and EC with the biopolymer resulted in an increase in the ionic conductivity of polymer electrolyte. EC was added to increase the degree of salt dissociation and also ionic mobility. The highest ionic conductivity achieved at room temperature was for 50 wt% agar/50 wt% NH4Br/0.3% EC with the conductivity 3.73?×?10?4 S cm?1. The conductivity of the polymer electrolyte increases with the increase in amount of plasticizer. The frequency-dependent conductivity, dielectric permittivity (ε′) and modulus (M′) studies were carried out.  相似文献   