2.
Segmental dynamics around Tg in the 4- and 6-arm fullerene (C60) core star-like polystyrenes with different preset arm lengths was studied by DSC as compared to that in the linear PS and PS/C60 blend. The anomalies in glass transition behavior were found for the stars including both suppression and facilitation of segmental motion, and pronounced dynamic heterogeneity within a transition range. The results are interpreted in terms of breakdown of intermolecular cooperativity of segmental motions and PS-C60 interactions.This revised version was published online in November 2005 with corrections to the Cover Date.  相似文献   

3.
Existing studies in the research literature showing conflicting changes in physical aging rates with decreasing film thickness in nanoconfined polymer films highlight the need for a single experimental technique to efficiently characterize physical aging rates in thin polymer films of varying chemical structure. To that end, we have developed a streamlined ellipsometry procedure to measure the structural relaxation of thin glassy polymer films. We evaluate different methods of calculating a physical aging rate β from the measured thickness h(t) and index of refraction n(t) data. We present extensive measurements of β as a function of aging temperature and aging time for polystyrene (PS) films supported on silicon, and determine that the physical aging rate β can be easily and reliably determined from β = −1/h0 dh/d(log t), where h0 is the initial measure of the film thickness at an aging time of 10 min. We have also carried out oxygen permeation studies on poly(methyl methacrylate) (PMMA) films from 800 μm down to 190 nm in thickness, and find no change in the permeability with film thickness or physical aging at room temperature for up to 65 days, which suggests that gas permeation may be insensitive to physical aging in such low free volume polymers. © 2009 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 47: 2509–2519, 2009  相似文献   

4.
A photobleaching technique was used to measure the rotational dynamics of rubrene dispersed in thermoset resins. The matrices were polymerized from mixtures of two monomers with five different compositions. At temperatures below the glass‐transition temperature, probe rotational correlation times were shorter and showed a much weaker temperature dependence than those observed in glassy homopolymers. The probe correlation functions became increasingly nonexponential as the amount of the minor component in the matrix increased, presumably because a more heterogeneous set of environments resulted. Dynamics in the single‐component sample were quite homogeneous at room temperature. In contrast to homopolymer systems, a bimodal distribution of local relaxation times developed with the addition of the second component. At a given polymer composition, this bimodal distribution changed shape with temperature in a reversible manner. © 2000 John Wiley & Sons, Inc. J Polym Sci B: Polym Phys 38: 2232–2239, 2000  相似文献   

5.
In previous work we observed two simultaneous transitions in high molecular weight (MW) free‐standing polystyrene films that were interpreted as two thickness‐dependent reduced glass transition temperatures (Tgs). The weaker lower transition agreed well with the MW‐dependent Tg(h) previously reported, while the much stronger upper transition matched the MW‐independent Tg(h) previously observed in low‐MW free‐standing films. Here, we investigate the nature of these two transitions by inspecting the temperature dependence of the films' thermal coefficient of expansion (TCE) and present physical aging measurements using ellipsometry both below and in‐between the two transitions. TCE values indicate approximately 80 to 90% of the film solidifies at the upper transition, while only 10 to 20% remains mobile to lower temperatures, freezing out at the lower transition. Physical aging is observed at a temperature below the upper transition, but above the lower transition, indicative of the upper transition being an actual glass transition associated with the α‐relaxation. © 2014 Wiley Periodicals, Inc. J. Polym. Sci., Part B: Polym. Phys. 2015 , 53, 64–75  相似文献   

6.
The effect of the annealing few degrees above the glass transition temperature (Tda = 62 °C) on the physical aging (Tpa = 51 °C) of amorphous quenched poly(l ‐lactide) is investigated by an implementation of variable temperature Fourier transform infrared (FTIR). By using a temperature program composed of a linear heating ramp superimposed to a temperature modulation (modulated temperature FTIR), the reversing and nonreversing intensity variation of selected bands, related to high‐energy gg and low‐energy gt conformers, is investigated. It is observed that the annealing above T g changes irreversibly the conformation distribution of the liquid polymer. The glasses obtained from annealed and nonannealed liquids behave differently, evolving in the physical aging toward their own liquid state and retaining the memory of their original condition before the vitrification. The recovery through T g of the relaxation occurred in the physical aging depends not only from aging conditions but also by the thermal history of the sample above the Tg. © 2018 Wiley Periodicals, Inc. J. Polym. Sci., Part B: Polym. Phys. 2019 , 57, 174–181  相似文献   

7.
This article presents experimental results and model predictions of the mechanical response of polymers during nonisothermal physical aging. The nonisothermal temperature history leads to a complex evolution in the aging behavior of the material. To characterize this response, sequential creep tests of polyether‐ether‐ketone (PEEK) and polyphenylene sulfide (PPS) films are performed at various aging times using a dynamic mechanical analyzer. The resulting strain histories are analyzed to determine discrete aging shift factors (ate) for each of the creep tests. The nonisothermal aging response is then predicted using the KAHR‐ate model, which combines the KAHR model of volume recovery with a suitable linear relationship between aging shift factors and specific volume. The KAHR‐ate model can be utilized to both predict aging response or to determine necessary model parameters from a set of aging shift factor data. For the PEEK and PPS materials considered in the current study, predictions of mechanical response are demonstrated to be in good agreement with the experimental results for several thermal histories. © 2008 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 47: 340–352, 2009  相似文献   

8.
The effects of confinement on glass transition temperature (Tg) and physical aging are measured in polystyrene (PS), poly(methyl methacrylate) (PMMA), and poly(2-vinyl pyridine) (P2VP) nanocomposites containing 10- to 15-nm-diameter silica nanospheres or 47-nm-diameter alumina nanospheres. Nanocomposites are made by spin coating films from sonicated solutions of polymer, nanofiller, and dye. The Tgs and physical aging rates are measured by fluorescence of trace levels of dye in the films. At 0.1–10 vol % nanofiller, Tg values can be enhanced or depressed relative to neat, bulk Tg (Tg,bulk) or invariant with nanofiller content. For alumina nanocomposites, Tg increases relative to Tg,bulk by as much as 16 K in P2VP, decreases by as much as 5 K in PMMA, and is invariant in PS. By analogy with thin polymer films, these results are explained by wetted P2VP–nanofiller interfaces with attractive interactions, nonwetted PMMA–nanofiller interfaces (free space at the interface), and wetted PS–nanofiller interfaces lacking attractive interactions, respectively. The presence of wetted or nonwetted interfaces is controlled by choice of solvent. For example, 0.1–0.6 vol % silica/PMMA nanocomposites exhibit Tg enhancements as large as 5 K or Tg reductions as large as 17 K relative to Tg,bulk when films are made from methyl ethyl ketone or acetic acid solutions, respectively. A factor of 17 reduction of physical aging rate relative to that of neat, bulk P2VP is demonstrated in a 4 vol % alumina/P2VP nanocomposite. This suggests that a strategy for achieving nonequilibrium, glassy polymeric systems that are stable or nearly stable to physical aging is to incorporate well-dispersed nanoparticles possessing attractive interfacial interactions with the polymer. © 2006 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 44: 2935–2943, 2006  相似文献   

9.
Understanding and controlling physical aging below the glass transition temperature (Tg) is very important for the long‐term performance of plastic parts. In this article, the effect of grafted silica nanoparticles on the physical aging of polycarbonate (PC) below the Tg is studied by using the evolution of the enthalpy relaxation and the yield stress. The nanocomposites were found to reach a thermodynamic equilibrium faster than unfilled PC, implying that physical aging is accelerated in presence of grafted nanosilica particles. The Tool‐Narayanaswamy‐Moynihan model shows that the aging is accelerated by the grafted silica nanoparticles, but the molecular mechanism responsible for physical aging remains unaltered. Furthermore, dynamic mechanical analysis shows that the kinetics of physical aging can be related to a free volume distribution or a local attraction‐energy distribution as a result of the change in mobility of the polymer chain. Finally, a qualitative equivalence is observed in the physical aging followed by both the enthalpy relaxation and yield stress. © 2016 Wiley Periodicals, Inc. J. Polym. Sci., Part B: Polym. Phys. 2016 , 54, 2069–2081  相似文献   