采用传统水热法合成SSZ-13分子筛,铜离子交换法制备Cu-SSZ-13分子筛催化剂,用于氨选择性催化还原(NH3-SCR)脱硝,研究了有机模板剂(OSDA)用量、硅源、铝源、水硅比、硅铝比以及老化时间等制备参数对Cu-SSZ-13分子筛形貌、晶粒大小、酸性、Cu2+位点以及NH3-SCR催化性能的影响。结果表明,在一定范围内,SSZ-13分子筛的硅铝比越高,其晶粒越大,所负载的活性铜含量越低,NH3-SCR催化活性也越差。以硅溶胶为硅源、硫酸铝为铝源所合成的SSZ-13分子筛晶粒较小,结晶度最高,所得到的Cu-SSZ-13催化剂的NH3-SCR活性也最好。较高的水硅比所合成的分子筛晶粒较大,而增加模板剂的用量有利于提高SSZ-13分子筛的结晶度,降低其晶粒尺寸。适当延长老化时间,能降低SSZ-13分子筛晶粒尺寸,提升Cu-SSZ-13的NH3-SCR催化活性。其中,Si/Al比为10、硅溶胶为硅源、硫酸铝为铝源、OSDA/Si比为0.4、水硅比为88、老...  相似文献   

2.
以聚乙烯醇(PVA)或拟薄水铝石(SB粉)为涂覆助剂,采用超声波辅助分散法将Cu-SSZ-13分子筛涂覆于蜂窝状堇青石(Cordierite)上,制备了整体式堇青石负载的Cu-SSZ-13分子筛催化剂(Cu-SSZ-13/Cordierite),用于氨选择性催化还原(NH3-SCR)脱硝,并结合XRD、氮气吸附、SEM及H2-TPR等表征手段,研究了涂覆助剂对该催化剂的Cu-SSZ-13涂层稳定性、NH3-SCR脱硝活性、水热稳定性和抗SO2毒化能力的影响。结果表明,以PVA为涂覆助剂制备的整体式Cu-SSZ-13(PVA)/Cordierite催化剂,其Cu-SSZ-13涂层稳定、脱落率低,选择性催化还原脱硝活性与Cu-SSZ-13原粉基本相当;同时,该Cu-SSZ-13(PVA)/Cordierite催化剂也具有较好的耐高温水热稳定性和抗硫中毒能力,在移动源和固定源脱硝方面有较好应用前景。  相似文献   

3.
谢利娟  石晓燕  刘福东  阮文权 《化学进展》2016,28(12):1860-1869
柴油车尾气NOx控制是目前大气污染控制领域的重要研究内容,对改善城市大气污染现状有着极其重要的作用。NH3选择性催化还原NOx(NH3-SCR)是应用于该领域的主流技术之一。近年来,以具有菱沸石(chabazite,CHA)结构的分子筛为载体负载Cu制备的Cu-CHA(Cu-SSZ-13和Cu-SAPO-34)系列催化剂,因其优秀的NH3-SCR活性和良好的水热稳定性,成为学者们关注的热点。本文首先从制备方法及反应条件对Cu-CHA催化性能的影响和NH3-SCR反应机理这几个方面系统阐述Cu基菱沸石在柴油车尾气NOx催化净化领域的研究进展;然后总结了负载其他过渡金属和稀土金属制备的M-CHA分子筛催化剂在NH3-SCR反应中的应用,指出双活性中心菱沸石催化剂在NH3-SCR领域表现出的优势;在此基础上对菱沸石NH3-SCR催化剂的进一步改良做出展望。  相似文献   

4.
采用铜胺配合物(Cu2+-四乙烯五胺,Cu-TEPA)作为结构导向剂,通过一步水热法合成不同铜铝比(nCu/nAl)和硅铝比(nSi/nAl)的Cu-SSZ-13分子筛催化剂,研究其在贫燃条件下丙烯选择性催化还原NO(C3H6-SCR)的性能。当nCu/nAl=2、nSi/nAl=6时2.0Cu-SSZ-13(6)催化剂具有最好的低温脱硝活性,200℃时NO转化率超过80%,在250~300℃可实现100%脱硝效率和~100%N2选择性,同时具有较强的抗水、抗硫性能。为研究不同nCu/nAl和nSi/nAl对催化剂物理化学特性的影响,通过X射线衍射(XRD)、扫描电子显微镜(SEM)、N2吸附-脱附测试、H2程序升温还原(H2-TPR)、氨气程序升温脱附(NH3-TPD)、紫外可见光谱(UV-Vis)等手段对样品进行表征。结果表明,2.0Cu-SSZ-13(6)具有最佳的脱硝性能,这是因为其具有最大的比表面积、最强的表面酸性和分布最多的孤立态Cu2+离子。Cu-SSZ-13上丰富的酸性位可以有效促进C3H6和NO的吸附和活化,SSZ-13分子筛八元环中孤立的Cu2+离子具有良好的氧化还原性能,是C3H6-SCR反应的主要活性位。随着nCu/nAl的增加,孤立的Cu2+离子会在分子筛表面迁移、集聚形成CuO物种,从而导致C3H6-SCR活性下降。  相似文献   

5.
近年来,氧化锰基催化剂由于在低温氨选择性催化还原(NH3-SCR)NOx反应中表现出优良的催化活性得到了广泛的关注。本文综述了氧化锰基催化剂低温NH3-SCR反应的研究进展,分别分析了氧化锰的氧化态、晶体结构和表面结构以及掺杂离子和载体类型等因素对其催化性能的影响:高的氧化态的锰和高比表面积的催化剂有利于低温NH3-SCR反应;金属离子如铈、铬、铁、铜和锡等的掺杂可以提高NOx的转化率和/或N2选择性;具有独特性能的载体如TiO2或硅铝分子筛等可以进一步提高氧化锰基催化剂的抗湿和抗硫性能等。本文同时分别对活化NH3、NO或同时活化NO和NH3的低温NH3-SCR反应机理进行了详细总结, 根据不同的反应条件,在氧化锰基催化剂上很多低温NH3-SCR反应,Eley-Rideal、Langmuir-Hinshelwood以及Mars-van Krevelen 机理可能是同时存在的。本文最后论证和指出了氧化锰基催化剂低温NH3-SCR反应研究的主要发展方向。  相似文献   

6.
使用四乙基氢氧化铵作为有机模板剂, 利用常规铝源和硅源而不需要高硅Y沸石作为起始原料, 同时加入适量的沸石晶种直接合成了SSZ-13沸石分子筛. 所合成的沸石产物结晶度好, 具有良好的水热稳定性, 并在氨选择性催化还原(NH3-SCR)反应中显示出优异的催化性能, 为其在工业上广泛应用提供了可能.  相似文献   

7.
NOx控制是目前大气污染控制领域的重要研究内容,NH3选择性催化还原技术(NH3-SCR)是消除NOx最有效的技术之一,其核心是高性能催化剂的开发。本研究综述了金属负载型分子筛催化剂(Cu基和Fe基分子筛催化剂)的NH3-SCR活性、水热稳定性以及水热老化失活机制,并对影响催化剂水热稳定性的因素(包括Si/Al比、分子筛拓扑结构、活性金属负载量、粒径和合成方法等)进行了系统阐述,总结了一些有效提高催化剂水热稳定性的改性方法,比如磷改性、第二活性金属改性、碱金属改性和外表面改性等。最后,对进一步提高金属负载型分子筛催化剂在NH3-SCR反应中的水热稳定性进行了展望。  相似文献   

8.
针对生物酶在固相载体负载后存在的催化活性与稳定性之间“此消彼长”的问题, 本工作采用“自牺牲模板”策略以铝基金属有机骨架材料(Al-MOF)为前驱体设计制备多级孔Al2O3 (MHAl2O3)材料, 再以“聚多巴胺(PDA)”仿生膜对材料表面进行功能化修饰后用以固载辣根过氧化物酶(HRP). 通过调节前驱体的煅烧温度来实现载体孔径大小的调控, 探讨了载体的孔道限域效应对固定化酶反应器催化活性的影响, 所得固定化酶反应器的热稳定性和重复使用性显著提高. 为了解析固定化酶反应器的构效关系, 采用酶动力学和热动力学参数研究了固定化酶反应器催化过程中酶与底物的相互作用, 结果表明固载后酶分子对底物的亲和性和专一性得到提升. 将固定化酶反应器用于模拟废水中苯胺黑药的催化降解时, 表现出非常高效的催化效率.  相似文献   

9.
采用共沉淀法制备TiO2-SnO2固溶体,浸渍法负载CeO2得到一系列xCeO2/TiO2-SnO2负载型催化剂,在模拟NH3选择性催化还原NOx(NH3-SCR)反应条件下考察催化剂低温脱硝活性。通过X射线衍射(XRD)、比表面积测定(BET)、程序升温还原(H2-TPR)、程序升温脱附(NH3-TPD)、高分辨率透射电子显微镜(HRTEM)、原位漫反射傅里叶变换红外光谱(in situ DRIFTS)等表征技术,研究了氧化铈负载后催化剂的微观结构、表面物种的存在状态、表面酸位等表面性质及NH3吸附特性。结果表明,Ce:Ti物质的量比为0.1时,催化剂催化脱硝反应活性最高,同时具有较宽的温度窗口(250~300℃)和热稳定性;铈的过量负载会导致催化剂比表面积减小、活性窗口变窄,同时其氧化还原能力和NH3吸附能力也减弱。NH3-TPD结果显示,CeO2的负载导致催化剂NH3在弱酸及中等酸位的吸附显著增强,与催化剂NH3-SCR最佳反应物温度降低有关。in situ DRIFTS表明,xCeO2/TiO2-SnO2催化剂的Lewis酸位和Brønsted酸位强度均明显增强,同时,在1657~1666cm-1处出现新的Brønsted酸位,参与SCR反应的主要物质是NH4+分子。  相似文献   

10.
采用水热合成技术, 在堇青石蜂窝陶瓷载体上原位合成了SSZ-13分子筛, 并借助X射线衍射(XRD)和场发射扫描电子显微镜(FESEM)等手段对其进行表征. 在此基础上, 研究了合成时间对催化剂结构和机械性能的影响. 另外, 使用固定床反应器测试了离子交换度为50%的Cu-SSZ-13/堇青石催化剂和Cu-SSZ-13催化剂水热老化前后的氨气选择性催化还原(NH3-SCR) NO性能. 结果表明, 通过原位合成法制备的Cu-SSZ-13/堇青石催化剂在200-500 ℃ 的窗口温度内能达到80%以上的转化率, 并在300 ℃ 时达到96.4%的转化率. 在850 ℃水热老化12 h后, Cu-SSZ-13催化剂完全丧失了催化性能, 而Cu-SSZ-13/堇青石催化剂在300 ℃时仍然保持91%的转化率. 使用XRD和固体27Al 核磁共振(27Al NMR)的方法, 研究了水热老化前后两种催化剂结构的变化, 结果表明, 当水热老化12 h 后, Cu-SSZ-13 基本丧失了SSZ-13 结构特征峰, 而Cu-SSZ-13/堇青石仍然保持了一定的SSZ-13 骨架结构. 证明了通过原位合成法制备的Cu-SSZ-13/堇青石催化剂具有较好的抗水热老化性能.  相似文献   

11.
用溶胶-凝胶法以磷钼酸(MPA)的镍盐溶液水解钛酸四丁酯制备了NiPMo/TiO2催化剂.使用ICP、 XRD、 TG-DTA、 IR、 TPD-MS和微反应技术研究了催化剂的化学组成、热稳定性、化学吸附性质和催化反应性能.杂多钼酸盐与TiO2通过O2-在TiO2表面发生了键合.在623 K下,杂多阴离子仍保持原有的Keggin结构.CO2在Lewis酸位Ni(Ⅱ)和Lewis碱位Ni-O-Mo的桥氧协同作用下生成CO2卧式吸附态Ni(Ⅱ)←O-(CO)←(O--Ni).丙烯有多种吸附态在催化剂上吸附.在563 K、 1 MPa和空速1500 h-1的反应条件下,丙烯的摩尔转化率为3.2%,产物MAA选择性为95%.  相似文献   

12.
In the context of the preparation of camptothecin and luotonin A analogs, the synthesis of some key keto-precursors and their use in Friedländer condensation are described. This paper also focuses on the stability of these keto intermediates and emphasizes the major differences between indolizinones and pyrroloquinazolinones series. Noteworthy is also the report of some original structures isolated as by-products of some experiments.  相似文献   

13.
The Langevin paramagnetic theory can’t describe the relation between magnetization of ferrofluids and applied magnetic field. The structuralization of ferrofluids, which is considered the main influence factor of the magnetization, is regarded. The part of magnetization works is deposited when the structure is forming. This action influences the magnetization of ferrofluids directly or indirectly. On the base of the “compressing” model, the Langevin function that usually describes the magnetization of ferrofluid is modified, and a well-fitted curve is obtained. An equation of the relation between the equivalent volume fraction after being “compressed” and the intensity of magnetic field is discovered, which approximately describes the process of magnetization. The relation between the approximate initial susceptibility and the volume fraction can be obtained from modified formula.  相似文献   

14.
The highly regioselective Buchwald–Hartwig amination at C-2 of the cheap and readily accessible reagent, 2,4-dichloropyridine with a range of anilines and heterocyclic amines is described. This new methodology is robust and provides a facile access to 4-chloro-N-phenylpyridin-2-amines on 0.25 mol scale. These intermediates undergo a further Buchwald–Hartwig amination at higher temperature to enable rapid exploration of the chemical space at C-4 and to provide a library of 2,4-bisaminopyridines.  相似文献   

15.
KMnO4-mediated oxidative CN bond cleavage of tertiary amines producing secondary amine was introduced, which was trapped by electrophiles (acyl chloride and sulfonyl chloride) to form amides and sulfonamides. The reaction could take place at mild condition, tolerating a wide range of function groups and affording products in moderate to excellent yields.  相似文献   

16.
The review contains a concise historical account and information on the most significant researches undertaken by the staff at the A. E. Favorsky Irkutsk Institute of Chemistry, Siberian Branch of the Russian Academy of Sciences on the Chemistry of Heterocyclic Compounds. Dedicated to Academician of the Russian Academy of Sciences B. A. Trofimov on his 70th jubilee. Translated from Khimiya Geterotsiklicheskikh Soedinenii, No. 10, pp. 1443–1502, October, 2008.  相似文献   

17.
Zhanhui Yang  Shiyi Yang  Jiaxi Xu 《Tetrahedron》2017,73(23):3240-3248
Regiospecific and direct imidation of the methyl C(sp3)–H bond of thioanisoles is realized under mild and metal-free conditions with N-fluorobis(benzenesulfonyl)imide as an oxidant and nitrogen source. Proposed mechanism suggests that thionium ion intermediates and a Pummerer-type reaction are involved. The imidation has advantages such as high step-economy, excellent functionality tolerance, and regiospecificity, giving structurally diverse imidation products.  相似文献   

18.
19.
《Tetrahedron》2014,70(21):3377-3384
The Rh(II)-catalyzed reaction of 2-carbonyl-substituted 2H-azirines with ethyl 2-cyano-2-diazoacetate or 2-diazo-3,3,3-trifluoropropionate provides an easy access to 2H-1,3-oxazines and 1H-pyrrol-3(2H)-ones. These compounds can be selectively prepared from the same starting material using temperature as the only varied parameter. The 2-azabuta-1,3-diene intermediate, a common precursor for both heterocyclic products, isomerizes into 2H-1,3-oxazine under kinetic control, while 1H-pyrrol-3(2H)-one is the sole product of the reaction at elevated temperatures. According to DFT-calculations a one-atom oxazine ring contraction involving ring-opening to a 2-azabuta-1,3-diene intermediate, followed by a 1,5- and 1,2-prototropic shift leads to the consecutive formation of imidoylketene and azomethine ylide, which then further undergo cyclization to the pyrrole derivative.  相似文献   

20.
Different approaches for the synthesis of 1-benzyloxypyrazin-2(1H)-one derivatives from simple amino acids have been investigated. A library of 33 precursors for the preparation of N-hydroxy pyrazinones was obtained in moderate to good yields.  相似文献   

设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号