This study investigated and discovered a new miscible ternary blend system comprising three amorphous polymers: poly(vinyl acetate) (PVAc), poly(vinyl p‐phenol) (PVPh), and poly(methyl methacrylate) (PMMA) using thermal analysis and optical and scanning electron microscopies. The ternary compositions are largely miscible except for a small region of borderline ternary miscibility near the side, where the binary blends of PVAc/PMMA are originally of a borderline miscibility with broad Tg. In addition to the discovering miscibility in a new ternary blend, another objective of this study was to investigate whether the introduction of a third polymer component (PVPh) with hydrogen bonding capacity might disrupt or enhance the metastable miscibility between PVAc and PMMA. The PVPh component does not seem to exert any “bridging effect” to bring the mixture of PVAc and PMMA to a better state of miscibility; neither does the Δχ effect seem to disrupt the borderline miscible PVAc/PMMA blend into a phase‐separated system by introducing PVPh. Apparently, the ternary is able to remain in as a miscible state as the binary systems owing to the fact that PVPh is capable of maintaining roughly equal H‐bonding interactions with either PVAc or PMMA in the ternary mixtures to maintain balanced interactions among the ternary mixtures. © 2006 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 44: 1147–1160, 2006  相似文献   

2.
Polymer blends of poly(vinylphenol) (PVPh) and poly(styrene‐co‐vinylphenol) with poly(p‐acetoxystyrene) (PAS) were prepared by solution casting from tetrahydrofuran solution. The thermal properties and hydrogen bonding of the blends were investigated by differential scanning calorimetry (DSC) and Fourier transform infrared spectroscopy. Although hydrogen bonding existed between the PVPh and PAS segments, the experimental results indicated that PVPh is immiscible with PAS as shown by the existence of two glass‐transition temperatures over the entire composition range by DSC. This phenomenon is attributed to the strong self‐association of PVPh, intramolecular screening, and functional group accessibility effects of the PVPh/PAS blend system. However, the incorporation of an inert diluent moiety such as styrene into the PVPh chain renders the modified polymer to be miscible with PAS. Copolymers containing between 16 and 51 mol % vinylphenol were fully miscible with PAS according to DSC studies. These observed results were caused by the reduction of the strong self‐association of PVPh and the increase of the interassociation between PVPh and PAS segments with the incorporation of styrene on the PVPh chain. According to the Painter‐Coleman association model, the interassociation equilibrium constant of PVPh/PAS blends was determined by a model compound and polymer blend. Good correlation between these two methods was obtained after considering the intramolecular screening and functional group accessibility effect in the polymer blend. © 2002 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 40: 1661–1672, 2002  相似文献   

3.
Thermal analysis and Fourier transform infrared spectroscopy characterizations were performed on three ternary blend systems that comprise poly(4‐vinyl phenol) (PVPh) and any two of the three homologous aryl polyesters [poly(ethylene terephthalate) (PET), poly(trimethylene terephthalate) (PTT), and poly(butylene terephthalate) (PBT)]. Although PVPh is miscible with any one of the polyesters in forming a binary blend system, miscibility in ternary systems by introducing one more polymer of different structures to the blend system is not always expected. However, this study concludes that miscibility does exist in all these three ternary blends of all compositions investigated. Reasons and factors for such behavior were probed. Quantitative interactions in the ternary blend system were also estimated. The overall interaction energy density (B) by analysis of melting point depression for the PBT/PVPh/PET ternary blend system led to a negative value (B = −5.74 cal/cm3). Similarly, Tg‐composition analyses were performed on two other ternary blend systems, PET/PVPh/PTT and PTT/PVPh/PBT. Comparison of the qualitative results showed that the interaction energy densities in the other two ternary blend systems are similarly negative and comparable to the PBT/PVPh/PET ternary blend system. The Fourier transform infrared spectroscopy results also support the qualitative findings among these three ternary blend systems. © 2006 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 44: 1339–1350, 2006  相似文献   

4.
Poly (methyl methacrylate) (PMMA) was known to be miscible with poly (vinyl phenol) (PVPh). According to literature, poly (vinyl cinnamate) (PVCN) was also miscible with PVPh. The miscibility between PMMA and PVCN was corroborated on the basis of preliminary experiments. Is a ternary blend consisting of PMMA, PVPh and PVCN miscible in all the blend compositions? To answer this question, the miscibility of this ternary was examined in different blend compositions mainly based on calorimetry data in this investigation. The results using two different molecular weights of PVPh demonstrated an interestingly closed-loop behavior of immiscibility. The reason is likely because of the “Δχ effect”.  相似文献   

5.
Miscibility with a linear T g–composition relationship was proven for blend of poly(butylene adipate-co-butylene terephthalate) [P(BA-co-BT)] with poly(4-vinyl phenol) (PVPh). In comparison to the blends of PBA/PVPh and poly(butylene terephthalate) (PBT)/PVPh, the Kwei’s T g model fitting on data for the P(BA-co-BT)/PVPh blend yields a q value between those for the PBA/PVPh and PBT/PVPh blends. The q values suggest that the interaction strength in the P(BA-co-BT)/PVPh blend is not as strong as that in the PBT/PVPh blend. Upon mixing the PVPh into the immiscible blend of PBA and PBT, the ternary PBA/PBT/PVPh blends only exhibits partial miscibility. Full-scale ternary miscibility in whole compositions is not possible owing to the significant ∆χ effect (χ ij  – χ ik ). The wavenumber shifts of the hydroxyl IR absorbance band indicates that the H-bonding strength is in decreasing order—PBT/PVPh > P(BA-co-BT)/PVPh > PBA/PVPh—and shows that the BA segment in the copolymer tends to defray interactions between P(BA-co-BT) and PVPh in blends.  相似文献   

6.
Spherulite ring-band patterns and growth regimes in neat poly(?-caprolactone) (PCL) and its miscible blends were analyzed using polarized-light optical microscopy and differential scanning calorimetry (DSC). Spherulite growth in thin-film forms and transformation of spherulite patterns in different regimes were investigated by comparing neat PCL with its miscible blends. Three miscible diluents in PCL were probed: poly(p-vinyl phenol) (PVPh), poly(benzyl methacrylate) (PBzMA), and poly(phenyl methacrylate) (PPhMA), which represent strong H-bonding and weak polar interactions, respectively. Blending of PCL with miscible amorphous polymers changes the spherulite patterns significantly. The effect of different diluent polymers varies. Inclusion of different amorphous polymers in PCL leads to different extents of suppression in growth rates and induces different spherulitic patterns. The H-bonding interaction leads to that the PCL/PVPh blend shows dendritic crystals and no ring bands. Although PPhMA differs from PBZMA only by a methylene in the chemical structure of repeat unit, the coil-like textures of ring bands in the PCL/PPhMA blend are widely different from the zig-zag ring bands in the PCL/PBzMA blend. Regime plots show that the growth of neat PCL behaves quite differently from any of its blends with amorphous polymers (PVPh, PPhMA, or PBzMA). Regime plots for PCL/PBzMA blend also differ from those for the PCL/PPhMA blend, which correlates with the crystal patterns seen in these two blend systems.  相似文献   

7.
Blends of poly(N‐methyldodecano‐12‐lactam) PMDL with poly(4‐vinyphenol) PVPh have been studied by the DSC and ATR FTIR methods. The difference in glass transition temperature Tg between the components is 206 °C. A single composition‐dependent Tg suggests miscibility of the system, that is, homogeneity on the scale of about 10 nm. Fitting of the equation of Brostow et al. to the Tg data indicates relatively strong specific interactions and high complexity of the system. The Schneider's equation applied separately to low‐ and high‐PVPh regions provides good agreement with experiment; the calculated curves cross at the point of PVPh weight fraction 0.27. In the low‐PVPh region, the analysis indicates weak interactions with predominance of segment homocontacts and strong involvement of conformational entropy. In the high‐PVPh region, strong specific interactions predominate and entropic effects are suppressed. Composition dependences of the heat capacity difference at Tg and the width of glass transition indicate strong interactions in the system and existence of certain heterogeneities on segmental level, respectively. According to ATR FTIR, hydrogen bonds between PVPh as proton donor and PMDL as proton acceptor induce miscibility in blends of higher PVPh content (above about 0.28 weight fraction). In low‐PVPh blends, it is conformational entropy that enables intimate intermolecular mixing. Hydrogen bonds adopt several (distorted) geometries and are on average stronger than average hydrogen bonds formed in self‐associating PVPh. © 2011 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys, 2011  相似文献   

8.
Effects of a strong‐interacting amorphous polymer, poly(4‐vinyl phenol) (PVPh), and an alkali metal salt, lithium perchlorate (LiClO4), on the amorphous and crystalline domains in poly(ethylene oxide) (PEO) were probed by differential scanning calorimetry (DSC), optical microscopy (OM), and Fourier transform infrared spectroscopy (FTIR). Addition of lithium perchlorate (LiClO4, up to 10% of the total mass) led to enhanced Tg's, but did not disturb the miscibility state in the amorphous phase of PEO/PVPh blends, where the salt in the form of lithium cation and ClO anion was well dispersed in the matrix. Competitive interactions between PEO, PVPh, and Li+ and ClO ions were evidenced by the elevation of glass transition temperatures and shifting of IR peaks observed for LiClO4‐doped PEO/PVPh blend system. However, the doping distinctly influenced the crystalline domains of LiClO4‐doped PEO or LiClO4‐doped PEO/PVPh blend system. LiClO4 doping in PEO exerted significant retardation on PEO crystal growth. The growth rates for LiClO4‐doped PEO were order‐of‐magnitude slower than those for the salt‐free neat PEO. Dramatic changes in spherulitic patterns were also seen, in that feather‐like dendritic spherulites are resulted, indicating strong interactions. Introduction of both miscible amorphous PVPh polymer and LiClO4 salt in PEO can potentially be a new approach of designing PEO as matrix materials for electrolytes. © 2006 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 44: 3357–3368, 2006  相似文献   

9.
The fully amorphous films of highly syndiotactic poly[(R,S)‐3‐hydroxybutyrate] (s‐PHB)/atactic poly(4‐vinylphenol) (PVPh) blends show reversible thinning/thickening phenomena at 37 °C in aqueous medium. On the other hand, isotactic poly[(R)‐3‐hydroxybutyrate] (i‐PHB)/PVPh blend film, in which i‐PHB blend component was partially crystalline, did not show any thinning/thickening phenomena under the same conditions. To elucidate the factors influencing these phenomena, the structure and molecular interaction in these blends were characterized by Fourier transform infrared spectroscopy (FTIR), differential scanning calorimetry, and wide‐angle X‐ray diffraction. The FTIR spectra indicated that the ester carbonyl of PHB and the phenolic hydroxyl of PVPh formed hydrogen bonds in both the thinned and thickened s‐PHB/PVPh blend films. The blend composition, intermolecular hydrogen‐bonding interaction, crystallization behavior, miscibility, and the glass‐transition temperature of the blends affected the thinning/thickening phenomena. Some other polyesters such as poly(?‐caprolactone), poly (L‐lactic acid), atactic poly(D,L‐lactic acid), and poly(ethylene terephthalate) had no ability to exhibit thinning/thickening phenomena in water at 37 °C when they were blended with PVPh. This result implies that s‐PHB/PVPh is the rare example with the ability to show reversible thinning/thickening phenomena. © 2002 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 40: 2736–2743, 2002  相似文献   

10.
A vinyl‐terminated benzoxazine (VB‐a), which could be polymerized through ring‐opening polymerization, was synthesized through the Mannich condensation of bisphenol A, formaldehyde, and allylamine. This VB‐a monomer was then subjected to blending with poly(ethylene oxide) (PEO), followed by thermal curing, to form poly(VB‐a)/PEO blends. The specific interactions, miscibility, morphology, and thermal properties of these blends were investigated with Fourier transform infrared (FTIR) spectroscopy, differential scanning calorimetry, dynamic mechanical analysis (DMA), and scanning electron microscopy (SEM). Before curing, we found that PEO was miscible with VB‐a, as evidenced by the existence of a single composition‐dependent glass transition temperature (Tg) for each composition. The FTIR spectra revealed the presence of hydrogen‐bonding interactions between the hydroxyl groups of poly(VB‐a) and the ether groups of PEO. Indeed, the ring‐opening reaction and subsequent polymerization of the benzoxazine were facilitated significantly by the presence of PEO. After curing, DMA results indicated that the 50/50 poly(VB‐a)/PEO blend exhibited two values of Tg: one broad peak appeared in the lower temperature region, whereas the other (at ca. 327 °C, in the higher temperature region) was higher than that of pristine poly(VB‐a) (301 °C). The presence of two glass transitions in the blend suggested that this blend system was only partially miscible. Moreover, SEM micrographs indicated that the poly(VB‐a)/PEO blends were heterogeneous. The volume fraction of PEO in the blends had a strong effect on the morphology. © 2007 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 45: 644–653, 2007  相似文献   

11.
In this article we determine the miscibility of azobenzene derivative (poly(4‐(N‐(2‐methacryloyloxyethyl)‐N‐ethylamino)‐4′‐nitroazobenzene)90‐co‐(methyl methacrylate)10)/poly(vinyl acetate) (PVAc) and azobenzene derivative/poly(vinyl chloride) (PVC) blends using Fourier Transform infrared (FT‐IR) spectroscopy. With this method we can clearly identify the exact interactions responsible for miscibility. In the azobenzene derivative 50:50PVAc blend new peaks were evident at 2960, 2890, 1237 and 959 cm?1, these peaks depict miscible interactions. These wavenumbers indicate that the miscible interactions occurring are from the C? H stretching band, the vinyl acetate C?O, conjugated to the ester carbonyl, the cis‐transformation N?N stretch frequency and the acetate ester weak doublet. The azobenzene derivative 80:20PVC blend display peaks identical in profile to the blend homopolymers, indicating no miscible interactions. However, this could be due to overlapping of peaks within the same wavenumber region, making resolution difficult. This research demonstrates FT‐IR can deduce favorable interactions for miscibility and therefore numerous miscible blends can successfully be calculated if possessing the same groups responsible for miscibility. This paves the way for a new generation of designer optical materials with the desired properties. Copyright © 2003 John Wiley & Sons, Ltd.  相似文献   

12.
The solid-state NMR isotropic line shape of the carbonyl 13C resonance is useful as a qualitative diagnostic probe of the polyester component′s morphology and molecular mobility in partially miscible blends with poly(vinylphenol), PVPh. The main-chain polyesters chosen for investigation in this study are poly(ethylene succinate), poly(ethylene adipate), poly(butylene adipate), and poly(caprolactone). A crystalline phase exists for polyester-rich mixtures in all cases. Verification of this claim is provided by DSC endothermic tran-sitions that map out melting point depression in the temperature-composition phase dia-grams. The carbonyl 13C-NMR signal in the crystalline domains exhibits a full width at half height of 1–2 ppm when the glass transition temperature of the blends is below the temperature of the NMR experiment. In all cases, a single concentration-dependent glass-transition temperature is measured by DSC, which increases monotonically from below ambient for polyester-rich blends to well above ambient for blends that are rich in poly(vinylphenol). When the concentration of the amorphous proton donor PVPh is suf-ficient to thwart crystallization of the polyester and increase the glass transition temperature of the blends above the temperature of the NMR experiment, the line width of the carbonyl resonance increases three- to fourfold to ca. 5–6 ppm. When the blends are completely amorphous and Tg is above ambient, the polyester carbonyl 13C line shape reveals at least two morphologically inequivalent microenvironments. A partially resolved carbonyl signal in rigid amorphous blends is (a) identified at higher chemical shift relative to the crystalline component, and (b) attributed to hydrogen bonding in the amorphous phase. This inter-action-sensitive hydrogen-bonded carbonyl signal accounts for an increasing fraction of the overall NMR absorption envelope of the carbonyl carbon site when the polyester is saturated with PVPh. The main-chain polyesters were chosen to probe the effect of chemical structure of the proton acceptor on the potential for hydrogen-bond formation. Aliphatic CH2 spacers between the carbonyl groups dilute the concentration of interacting sites, and the dependence of the carbonyl 13C-NMR line shape on blend concentration reveals unique spectroscopic behavior in each of the four blend systems investigated. © 1993 John Wiley & Sons, Inc.  相似文献   

13.
Poly(l-lactide) (PLLA) was melt-blended with poly(p-vinyl phenol) (PVPh) using a two-roll mill, and the miscibility between PLLA and PVPh and degradation of the blend films were investigated. It was found that PLLA/PVPh blend has miscibility in the amorphous state because only single Tg was observed in the DSC and DMA measurements. The Tg of the PLLA/PVPh blend could be controlled in the temperature range from 55 °C to 117 °C by changing the PVPh weight fraction. In alkaline solution, degradation rate of PLLA/PVPh blends was faster than that of neat PLLA because PVPh could dissolve in alkaline solution. The surface morphology of degraded PLLA and PLLA/PVPh blend were observed by SEM. The surface morphology of degraded PLLA/PVPh blend was finer than that of PLLA. Young's modulus of PLLA/PVPh blend increased with increasing PVPh content. Yield stress of PLLA/PVPh blends whose PVPh content was less than 30 wt% kept the level of about 55 MPa and that of PLLA/PVPh blend whose PVPh content was 40 wt% is much lower than that of neat PLLA.  相似文献   

14.
A truly miscible ternary miscible blend consisting of poly(?‐caprolactone) (PCL), poly(phenyl methacrylate), and poly(benzyl methacrylate) (PBzMA) was discovered. The three‐polymer blend system was completely miscible within the entire composition range at ambient temperature up to about 150 °C, and ternary phase diagrams at increasing temperatures were characterized and interpreted. A ternary‐interaction model based on the modified Flory–Huggins expression was used to describe the phase diagrams with the individual binary interaction strengths. The model fitted well with the experimental‐phase diagram for the ternary blend system at T = 250 °C, where the binary PCL‐PBzMA blend system is on the critical points of phase separation. Interpretation of discrepancy between the model and experimental at other temperatures was handled with an empirical approach. © 2002 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 40: 747–754, 2002  相似文献   

15.
采用差热扫描分析、红外光谱、固体核磁、小角X光散射等方法研究了聚(β-羟基丁酸酯-co-β-羟基戊酸酯(P(HB-co-HV))/聚(对-羟基苯乙烯)(简称PVPh)共混物的相容性和形态。结果表明两组分间形成较强的分子间氢键,形成完全相容的共混体系。固体核磁结果表明P(HB-co-HV)/PVPh(50/50)在3.4nm尺寸上是完全均相的。小角X光散射结果表明,在等温结晶的共混物中无定形的PVPh分子分散在P(HB-co-HV)片晶之间与非晶的P(HB-co-HV)分子形成非晶区,从而使非晶区加宽,长周期增加。  相似文献   

16.
In a first step of this contribution, the observed glass transition temperature‐composition behavior of miscible blends of poly(styrene‐coN,N‐dimethylacrylamide) (SAD17) containing 17 mol % of N,N‐dimethylacrylamide and poly(styrene‐co‐acrylic acid) (SAA18, SAA27, and SAA32) containing increasing acrylic acid content, are analyzed according to theoretical approaches. Both Kwei and Brostow equations describe well the experimental data though better fits were obtained with the Brostow's approach. The specific interactions involved in these systems are a combination of intra and interassociation hydrogen bonding. The positive deviation from the linear mixing rule of Tg‐composition observed within the SAA18+SAD17 blend system, indicates that interassociation interactions are prevailing. More pronounced intra‐association interactions within the SAA32+SAD17 blend system led to a large negative deviation while a fine balance is established between these two types of interactions within the SAA27+SAD17 blend. A thermodynamic analysis was carried out according to the Painter‐Coleman association model. The miscibility and phase behavior of SAD17+SAA18 and SAD17+SAA27 blends are well predicted. However, this model predicts a partial miscibility of SAD17+SAA32 system. Finally, the fitting parameter free method developed by Coleman to predict the Tg‐composition behavior is applied. This method predicts fairly well the evolution trend of experimental Tgs of the SAA18+SAD17 and SAA27+SAD17 blend systems. However, the compositional dependence of SAA32+SAD17 blend Tg was not predictable by this method. © 2009 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 47:2074–2082, 2009  相似文献   

17.
The miscibility of nylon‐6 with poly(4‐vinylphenol) (PVPh) or poly(1‐hydroxy‐2,6‐methylphenylene) (p‐Cl‐novolac) was studied with differential scanning calorimetry and small‐angle X‐ray scattering techniques. Both PVPh and p‐Cl‐novolac are miscible with nylon‐6 at the molecular level. The presence of the phenolic polymers affects the crystallization of nylon‐6 and suppresses its melting point. PVPh increases the long space order in crystalline nylon‐6 because it increases the thickness of the amorphous layers. In contrast, a small quantity of p‐Cl‐novolac tends to decrease the long space order. It seems that p‐Cl‐novolac distributed in the amorphous regions introduces more order in these regions and makes the amorphous layers thinner. © 2001 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 39: 841–850, 2001  相似文献   

18.
The miscibility and hydrogen‐bonding interactions of carbon dioxide and epoxy propane copolymer to poly(propylene carbonate) (PPC)/poly(p‐vinylphenol) (PVPh) blends were investigated with differential scanning calorimetry (DSC), Fourier transform infrared (FTIR) spectroscopy and X‐ray photoelectron spectroscopy (XPS). The single glass‐transition temperature for each composition showed miscibility over the entire composition range. FTIR indicates the presence of strong hydrogen‐bonding interassociation between the hydroxyl groups of PVPh and the oxygen functional groups of PPC as a function of composition and temperature. XPS results testify to intermolecular hydrogen‐bonding interactions between the oxygen atoms of carbon–oxygen single bonds and carbon–oxygen double bonds in carbonate groups of PPC and the hydroxyl groups of PVPh by the shift of C1s peaks and the evolution of three novel O1s peaks in the blends, which supports the suggestion from FTIR analyses. © 2002 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 40: 1957–1964, 2002  相似文献   

19.
Previously, poly(methyl methacrylate) (PMMA) was found to be almost immiscible with poly(vinyl acetate) (PVAc) regardless of tacticity of PMMA and casting solvent. Poly(vinyl phenol) (PVPh) was found successful previously in making immiscible atactic PMMA/PVAc miscible. In this investigation, tacticity effect of PMMA on a ternary composed of PMMA, PVAc and PVPh was studied. Isotactic PMMA ternary was shown to be miscible in all the studied compositions on the basis of single Tg observation. However, syndiotactic PMMA ternary demonstrated immiscibility at ca. 25% PVPh and miscibility was observed at higher PVPh concentrations. A modified Kwei equation based on the binary interaction parameters was proposed to describe the experimental Tg of the miscible ternary almost quantitatively.  相似文献   

20.
《先进技术聚合物》2018,29(8):2287-2299
There is a huge demand especially for polyvinylidene fluoride (PVDF) and its copolymers to provide high performance solid polymer electrolytes for use as an electrolyte in energy supply systems. In this regard, the blending approach was used to prepare PVDF‐based proton exchange membranes and focused on the study of factor affecting the ir proton conductivity behavior. Thus, a series of copolymers consisting of poly (methyl methacrylate) (PMMA), polyacrylonitrile (PAN), and poly(2‐acrylamido‐2‐methyl‐l‐propanesulfonic acid) (PAMPS) as sulfonated segments were synthesized and blended with PVDF matrix in order to create proton transport sites in PVDF matrix. It was found that addition of PMMA‐co‐PAMPS and PAN‐co‐PAMPS copolymers resulted in a significant increase in porosity, which favored the water uptake and proton transport at ambient temperature. Furthermore, crystallinity degree of the PVDF‐based blend membranes was increased by addition of the related copolymers, which is mainly attributed to formation of hydrogen bonding interaction between PVDF matrix and the synthesized copolymers, and led to a slight decrease in proton conductivity behavior of blend membranes. From impedance data, the proton conductivity of the PVDF/PMMA‐co‐PAMPS and PVDF/PAN‐co‐PAMPS blend membranes increases to 10 and 8.4 mS cm−1 by adding only 50% of the related copolymer (at 25°C), respectively. Also, the blend membranes containing 30% sulfonated copolymers showed a power density as high as 34.30 and 30.10 mW cm−2 at peak current density of 140 and 79.45 mA cm−2 for the PVDF/PMMA‐co‐PAMPS and PVDF/PAN‐co‐PAMPS blend membranes, respectively. A reduction in the tensile strength was observed by the addition of amphiphilic copolymer, whereas the elongation at break of all blend membranes was raised.  相似文献   