We report the structural and optical properties of copper aluminium oxide (CuAlO2) thin films, which were prepared on c-plane sapphire substrates by the radio frequency magnetron sputtering method. X-ray photoelectron spectroscopy (XPS) along with X-ray diffraction (XRD) analysis confirms that the films consist of delafossite CuAlO2 phase only. The optical absorption studies show the indirect and direct bandgap is 1.8 eV and 3.45 eV, respectively. Room temperature photoluminescence (PL) measurements show three emission peaks at 360 nm (3.45 eV), 470 nm (2.63 eV) and 590 nm (2.1 eV). The first one is near band edge emission while the other two are originated from defects.  相似文献   

2.
ZnO thin films were epitaxially grown on sapphire (0 0 0 1) substrates by radio frequency magnetron sputtering. ZnO thin films were then annealed at different temperatures in air and in various atmospheres at 800 °C, respectively. The effect of the annealing temperature and annealing atmosphere on the structure and optical properties of ZnO thin films are investigated by X-ray diffraction (XRD), atomic force microscopy (AFM), photoluminescence (PL). A strong (0 0 2) diffraction peak of all ZnO thin films shows a polycrystalline hexagonal wurtzite structure and high preferential c-axis orientation. XRD and AFM results reveal that the better structural quality, relatively smaller tensile stress, smooth, uniform of ZnO thin films were obtained when annealed at 800 °C in N2. Room temperature PL spectrum can be divided into the UV emission and the Visible broad band emission. The UV emission can be attributed to the near band edge emission (NBE) and the Visible broad band emission can be ascribed to the deep level emissions (DLE). By analyzing our experimental results, we recommend that the deep-level emission correspond to oxygen vacancy (VO) and interstitial oxygen (Oi). The biggest ratio of the PL intensity of UV emission to that of visible emission (INBE/IDLE) is observed from ZnO thin films annealed at 800 °C in N2. Therefore, we suggest that annealing temperature of 800 °C and annealing atmosphere of N2 are the most suitable annealing conditions for obtaining high quality ZnO thin films with good luminescence performance.  相似文献   

3.
The development of cost-effective and low-temperature synthesis techniques for the growth of high-quality zinc oxide thin films is paramount for fabrication of ZnO-based optoelectronic devices, especially ultraviolet (UV)-light-emitting diodes, lasers and detectors. We demonstrate that the properties, especially UV emission, observed at room temperature, of electrodeposited ZnO thin films from chloride medium (at 70 °C) on fluor-doped tin oxide (FTO) substrates is strongly influenced by the post-growth thermal annealing treatments. X-ray diffraction (XRD) measurements show that the films have preferably grown along (0 0 2) direction. Thermal annealing in the temperature range of 150-400 °C in air has been carried out for these ZnO thin films. The as-grown films contain chlorine which is partially removed after annealing at 400 °C. Morphological changes upon annealing are discussed in the light of compositional changes observed in the ZnO crystals that constitute the film. The optical quality of ZnO thin films was improved after post-deposition thermal treatment at 150 °C and 400 °C in our experiments due to the reducing of defects levels and of chlorine content. The transmission and absorption spectra become steeper and the optical bandgap red shifted to the single-crystal value. These findings demonstrate that electrodeposition have potential for the growth of high-quality ZnO thin films with reduced defects for device applications.  相似文献   

4.
The effects of NaCl electrolyte concentrations in the range 6-48 mM on the galvanic deposition of ZnO in Zn(Ac)2 electrolyte is presented. Effects of thermal annealing on their structural and optical properties have been investigated by using scanning electron microscopy (SEM), X-ray diffraction (XRD) and energy-dispersive X-ray (EDX) microanalysis and photoluminescence (PL). The results show that the increase of NaCl electrolyte concentration not only results in the increase of the diameter of ZnO nanorods, but also promotes the blue-shift of UV emission of ZnO. After air annealing at 200 °C, 300 °C and 400 °C, the UV emission is first enhanced then quenched sharply, while the visible emission tends to be enhanced tremendously. It can be ascribed to the new defect states introduced in ZnO after annealing at high temperature.  相似文献   

5.
Thin gallium-doped zinc oxide (in GZO the Ga2O3 contents are approximately 3 wt%) films having different ZnO buffer layers were deposited using radio frequency (rf) magnetron sputtering. The use of a grey-based Taguchi method to determine the processing parameters of ZnO buffer layer deposition has been studied by considering multiple performance characteristics. A Taguchi method with an L9 orthogonal array, signal-to-noise (S/N) ratio, and analysis of variance (ANOVA) is employed to investigate the performance characteristics in the deposition operations. The effect and optimization of ZnO buffer deposition parameters (rf power, sputtering pressure, thickness, and annealing) on the structure, morphology, electrical resistivity, and optical transmittance of the GZO films are studied. Annealing treatment and reduction in thickness resulted in a decrease in root-mean-square (RMS) surface roughness of the ZnO buffer layer. Using the optimal ZnO buffer layer obtained by the application of the grey-based Taguchi method, the electrical resistivity of GZO films was decreased from 2.94×10−3 to 9.44×10−4 Ω cm and the optical transmittance in the visible region was slightly increased from 84.81% to 85.82%.  相似文献   

6.
In this study, the effects of the annealing duration of a zinc oxide (ZnO) buffer layer on structural and optical properties of ZnO rods grown by a hydrothermal process are discussed. A ZnO buffer layer was deposited on p-type Si (1 1 1) substrates by the metal organic chemical vapor deposition (MOCVD) method. After that, ZnO rods were grown on the ZnO-buffer/Si (1 1 1) substrate by a hydrothermal process. In order to determine the optimum annealing duration of the buffer layer for the growth of ZnO rods, durations ranging from 0.5 to 30 min were tried. The morphology and crystal structure of the ZnO/ZnO-buffer/Si (1 1 1) were measured by field emission scanning electron microscopy (FE-SEM) and x-ray diffraction (XRD). The optical properties were investigated by photoluminescence (PL) measurement.  相似文献   

7.
The surface treatment effects of sapphire substrate on the ZnO thin films grown by magnetron sputtering were studied. The sapphire substrates properties have been investigated by means of atomic force microscopy (AFM) and X-ray diffraction rocking curves (XRCs). The results show that sapphire substrate surfaces have the best quality by CMP with subsequent chemical etching. The surface treatment effects of sapphire substrate on the ZnO thin films were examined by X-ray diffraction (XRD) and photoluminescence (PL) measurements. Results show that the intensity of (0 0 2) diffraction peak of ZnO thin films on sapphire substrates treated by CMP with subsequent chemical etching was strongest, FWHM of (0 0 2) diffraction peak is the narrowest and the intensity of UV peak of PL spectrum is strongest, indicating surface treatment on sapphire substrate preparation may improve ZnO thin films crystal quality and photoluminescent property.  相似文献   

8.
P doped ZnO films were grown on quartz by radio frequency-magnetron sputtering method using a ZnO target mixed with 1.5 at% P2O5 in the atmosphere of Ar and O2 mixing gas. The as-grown P doped ZnO film showed n-type conductivity, which was converted to p-type after 800 °C annealing in Ar gas. The P doped ZnO has a resistivity of 20.5 Ω cm (p∼2.0×1017 cm−3) and a Hall mobility of 2.1 cm2 V−1 s−1. XRD measurement indicated that both the as-grown and the annealed P doped ZnO films had a preferred (0 0 2) orientation. XPS study agreed with the model that the PZn-2VZn acceptor complex was responsible for the p-type conductivity as found in the annealed P-doped ZnO. Temperature-dependent photoluminescence (PL) spectrum showed that the dominant band is located at 3.312 eV, which was attributed to the free electronic radiative transition to neutral acceptor level (FA) in ZnO. The PZn-2VZn acceptor complex level was estimated to be at EV=122 meV.  相似文献   

9.
XPS depth profiles were used to investigate the effects of rapid thermal annealing under varying conditions on the structural, magnetic and optical properties of Ni-doped ZnO thin films. Oxidization of metallic Ni from its metallic state to two-valence oxidation state occurred in the film annealed in air at 600 °C, while reduction of Ni2+ from its two-valence oxidation state to metallic state occurred in the film annealed in Ar at 600 and 800 °C. In addition, there appeared to be significant diffusion of Ni from the bottom to the top surface of the film during annealing in Ar at 800 °C. Both as-deposited and annealed thin films displayed obvious room temperature ferromagnetism (RTFM) which was from metallic Ni, Ni2+ or both with two distinct mechanisms. Furthermore, a significant improvement in saturation magnetization (Ms) in the films was observed after annealing in air (Ms = 0.036 μB/Ni) or Ar (Ms = 0.033 μB/Ni) at 600 °C compared to that in as-deposited film (Ms = 0.017 μB/Ni). An even higher Ms value was observed in the film annealed in Ar at 800 °C (Ms = 0.055 μB/Ni) compared to that at 600 °C mainly due to the diffusion of Ni. The ultraviolet emission of the Ni-doped ZnO thin film was restored during annealing in Ar at 800 °C, which was also attributed to the diffusion of Ni.  相似文献   

10.
Zinc oxide (ZnO) thin films were deposited on a polycrystalline (poly) 3C-SiC buffer layer using RF magnetron sputtering and a sol-gel method. The post-deposition annealing was performed on ZnO thin films prepared using both methods. The formation of ZnO piezoelectric thin films with less residual stress was due to a close lattice mismatch of the ZnO and SiC layers as obtained by the sputtering method. Nanocrystalline, porous ZnO film prepared using the sol-gel method showed strong ultraviolet UV emission at a wavelength of 380 nm. The 3C-SiC buffer layer improved the optical and piezoelectric properties of the ZnO film produced by the two deposition methods. Moreover, the different structures of the ZnO films on the 3C-SiC intermediate layer caused by the different deposition techniques were also considered and discussed.  相似文献   

11.
The well-like ZnO nanostructures were obtained by chemical vapor deposition method. The uniform and dense ZnO slim nano-columns were grown along the circle to form a microwell. The growth mechanisms, such as 1D linear, 2D screw dislocation and step growth are discussed. These observations provide some insight into the growth kinetics in vapor-solid growth process. The fabrication of ZnO microwell morphology provided a direct experimental evidence for explaining the 1D growth mechanism based on the axial screw dislocation. Photoluminescence (PL) microscopy showed the surface-related optical properties. The green light emission enhancement revealed that the ZnO microwells have waveguide properties. The abnormal enhancement of integrated PL intensity of deep-level emission with temperature increase showed abundant surface state existence.  相似文献   

12.
In this paper we report the effect of deposition temperature on the structural and optical properties of ZnO thin films prepared by rf magnetron sputtering. The films grown at lower deposition temperatures were in a state of large compressive stress, whereas the films grown at higher temperature (450 °C) were almost stress free. In the absorption spectra, the ZnO excitonic and the Zn surface plasmon resonance (SPR) peaks have been observed. A redshift in the optical band gap of ZnO films has also been observed with the increase in the deposition temperature. The shift in the band gap calculated from the size effect did not match with the observed shift values and the observed shift has been attributed to the compressive stress present in the films.  相似文献   

13.
Al-doped ZnO (AZO, ZnO:Al2O3 = 98:2 wt%) films are deposited on different substrates by an RF magnetron sputtering and subsequently annealed at three different conditions to investigate the microstructural, electrical, and optical properties. X-ray diffraction and scanning electron microscope results show that all the samples are polycrystalline and the samples rapid-thermal-annealed at 900 °C in an N2 ambient contain larger grains compared to the furnace-annealed samples. It is shown that the sample deposited at room temperature on the sapphire gives a resistivity of 5.57 × 10−4 Ω cm when furnace-annealed at 500 °C in a mixture of N2:H2 (9:1). It is also shown that the Hall mobility vs. carrier concentration (μ-n) relation is divided into two groups, depending on the annealing conditions, namely, either rapid-thermal annealing or furnace annealing. The relations are described in terms of either grain boundary scattering or ionized impurity scattering mechanism. In addition, the samples produce fairly high transmittance of 91-96.99% across the wavelength region of 400-1100 nm. The optical bandgaps of the samples increase with increasing carrier concentration.  相似文献   

14.
Zinc oxide (ZnO) thin film has been epitaxially grown on (1 1 1) Mg0.4Al2.4O4 substrate by RF-magnetron sputtering. In resonant Raman scattering, higher-order longitudinal optical phonon modes were clearly observed, revealing high optical quality of the ZnO film. Optical absorption indicated a visible exciton absorption at room temperature. The near band edge emission showed a red shift due to the shrinkage of the band gap with increasing the temperature.  相似文献   

15.
The structural and photoluminescence analyses were performed on un-doped and Mn doped ZnO thin films grown on Si (1 0 0) substrate by pulsed laser deposition (PLD) and annealed at different post-deposition temperatures (500-800 °C). X-ray diffraction (XRD), employed to study the structural properties, showed an improved crystallinity at elevated temperatures with a consistent decrease in the lattice parameter ‘c’. The peak broadening in XRD spectra and the presence of Mn 2p3/2 peak at ∼640 eV in X-ray Photoelectron Spectroscopic (XPS) spectra of the doped thin films confirmed the successful incorporation of Mn in ZnO host matrix. Extended near band edge emission (NBE) spectra indicated the reduction in the concentration of the intrinsic surface traps in comparison to the doped ones resulting in improved optical transparency. Reduced deep level emission (DLE) spectra in doped thin films with declined PL ratio validated the quenching of the intrinsic surface traps thereby improving the optical transparency and the band gap, essential for optoelectronic and spintronic applications. Furthermore, the formation and uniform distribution of nano-sized grains with improved surface features of Mn-doped ZnO thin films were observed in Field Emission Scanning Electron Microscopy (FESEM) images.  相似文献   

16.
Nanocolumnar ZnO films were prepared by electrodeposition (ED) on a glass substrate covered with a conductive layer of thin oxide doped with fluorine (FTO). After deposition the samples were annealed in oxidizing or reducing atmosphere, at temperatures between 100 to 500 C, in order to follow the evolution of optical properties and morphology. The optical properties of these films were studied by means of photoluminescence spectroscopy (PL) and the morphology by scanning electron microscopy (SEM). Films annealed at 300 C exhibit a higher ultraviolet emission peak, originating from exciton transitions. A green band related to deep-level emission centered at 500 nm, shows a drastic increase at 500 C. These results are independent of the annealing atmosphere. An increase of coalescence is also observed after annealing at 500 C. These results are explained taking into account the contribution of different point defects.  相似文献   

17.
The optical properties of ZnO grown on (1 0 0) GaAs substrate using metalorganic chemical vapor deposition are investigated by photoluminescence (PL) spectroscopy. Postgrowth annealing in nitrogen and oxygen was performed for different times and temperatures in order to incorporate As from the substrate into the ZnO thin films. The PL spectra of the samples annealed in different ambients reveal that the effect of As diffusion into the ZnO thin films is more pronounced when the annealing is performed in oxygen at 550 °C. The 11 K PL spectra show the appearance of a transition at ∼3.35 eV after annealing in oxygen at 550 °C for 1 h. A further increase in the annealing temperature leads to the disappearance of this line, while for annealing times longer than 2 h at 550 °C, it is no longer prominent. The increase in intensity of this new transition is also accompanied by the enhancement of radiative centers related to structural defects, such as the stacking fault-related transition at 3.31 eV and the Y-line. Temperature dependent PL illustrates the excitonic nature of the new transition at ∼3.35 eV, which is therefore assigned to (A0, X) transition, where the acceptor is possibly the 2VZn-AsZn complex, with an activation energy EA in the range of 160-240 meV. Furthermore, the enhancement of the radiative centers related to structural defects is regarded as evidence that As atoms tend to segregate in the vicinity of structural defects to relieve local strain.  相似文献   

18.
Transparent conducting thin films of ZnO:Al (Al-doped ZnO, AZO) were prepared via pulsed DC magnetron sputtering with good transparency and relatively lower resistivity. The AZO films with 800 nm in thickness were deposited on soda-lime glass substrates keeping at 473 K under 0.4 Pa working pressure, 150 W power, 100 μs duty time, 5 μs pulse reverse time, 10 kHz pulse frequency and 95% duty cycle. The as-deposited AZO thin films has resistivity of 6.39 × 10−4 Ω cm measured at room temperature with average visible optical transmittance, Ttotal of 81.9% under which the carrier concentration and mobility were 1.95 × 1021 cm−3 and 5.02 cm2 V−1 s−1, respectively. The films were further etched in different aqueous solutions, 0.5% HCl, 5% oxalic acid, 33% KOH, to conform light scattering properties. The resultant films etched in 0.5% HCl solution for 30 s exhibited high Ttotal = 78.4% with haze value, HT = 0.1 and good electrical properties, ρ = 8.5 × 10−4 Ω cm while those etched in 5% oxalic acid for 150 s had desirable HT = 0.2 and relatively low electrical resistivity, ρ = 7.9 × 10−4 Ω cm. However, the visible transmittance, Ttotal was declined to 72.1%.  相似文献   

19.
Highly orientated polycrystalline ZnO films were deposited on sapphire, silicon and quartz substrates at room temperature by r.f. magnetron sputtering. Different photoluminescence (PL) spectra were observed when excited with different wavelength light. A UV emission peak (356 nm) and a blue peak (446 nm) were generated for the films on sapphire, silicon and quartz substrates, and only the 446 nm blue emission appeared for the films on glass substrates when the wavelength of the excitation light was 270 nm. With increasing the wavelength of the excitation light up to 300 and 320 nm, the UV emission disappeared for films on various substrates and the wavelength of the PL peaks increased up to 488 and 516 nm, respectively. When the wavelength of the excitation light increased to 398 nm, the PL spectrum becomes a wide band that is consistent with three emission peaks.  相似文献   

20.
Optical properties of ZnO thin films with/without MgO-buffer annealing were investigated by low and room temperature photoluminescence measurements. The ZnO films were grown on c-sapphire substrates by plasma-assisted molecular-beam epitaxy employing a thin MgO-buffer layer. Dislocation density of ZnO layer was reduced from 5.3 × 109 to 1.9 × 109 cm−2 by annealing MgO-buffer prior to the growth of ZnO. The intensity of free exciton emission from the sample with MgO-buffer annealing was almost twice of that from the sample without annealing, while the deep level emission from the sample with MgO-buffer annealing was about 1/3 of that without annealing. The MgO-buffer annealing improves optical quality of overgrown ZnO films.  相似文献   