首页 | 本学科首页   官方微博 | 高级检索  
相似文献
 共查询到20条相似文献,搜索用时 31 毫秒
1.
2.
考虑三轴约束时孔洞的聚合机理及有效能量准则   总被引:10,自引:0,他引:10  
李振环  匡震邦 《力学学报》2000,32(4):428-438
通过体胞分析方法,对不同状孔洞在从光滑试样到裂纹试样的三轴应力场中的聚合机理进行了较精解的有限元分析,计算结果表明:(1)孔洞的相互靠近和横向扩展是导致相邻孔洞发生内颈缩聚合的两种基本机制,在应力三维度Rσ等于1.25附近,这两种机制发生较明显的变化。(2)单纯以孔洞体积分数fC概念为基础的材料破坏参数一般敏感于应力三维度,不能很好地预报不同三轴应力场中材料的破坏,在此基础上,提出了描述孔洞聚合的  相似文献   

3.
Finite element (FE) calculations of a cylindrical cell containing a spherical hole have been performed under large strain conditions for varying triaxiality with three different constitutive models for the matrix material, i.e. rate independent plastic material with isotropic hardening, visco-plastic material under both isothermal and adiabatic conditions, and porous plastic material with a second population of voids nucleating strain controlled. The “mesoscopic” stress-strain and void growth responses of the cell are compared with predictions of the modified Gurson model in order to study the effects of varying triaxiality and strain rate on the critical void volume fraction. The interaction of two different sizes of voids was modelled by changing the strain level for nucleation and the stress triaxiality. The study confirms that the void volume fraction at void coalescence does not depend significantly on the triaxiality if the initial volume fraction of the primary voids is small and if there are no secondary voids. The strain rate does not affect fc either. The results also indicate that a single internal variable, f, is not sufficient to characterize the fracture processes in materials containing two different size-scales of void nucleating particles.  相似文献   

4.
三轴应力场中不同形状孔洞的长大及其新模型   总被引:2,自引:0,他引:2  
对不同形状孔洞在从光滑试样到裂纹试样这样广泛三轴应力场中的长大规律,本文通过控制体胞宏观应力三维度的方法进行了精确的有限元分析,计算结果表明:(1)孔洞的体积改变和形状变化是孔洞演化的两种基本机制,在不同的三轴应力场中,这两种机制的作用不同;(2)现有模型对孔洞长大规律的描述是不准确的,由它们得到的临界孔洞扩张比参数HGC与临界孔洞体积分数fc不具备一一对应关系,因此不以很好地反映也洞的实际扩张。在此基础上,提出了一个描述孔洞长大的新模型,与四种常用的现有模型相比,该模型不仅能更好地描述不同三轴应力场中孔洞的长大,而且能反映不同应力三维度水平下材料破坏模式的变化。  相似文献   

5.
Void growth and coalescence in single crystals are investigated using crystal plasticity based 3D finite element calculations. A unit cell involving a single spherical void and fully periodic boundary conditions is deformed under constant macroscopic stress triaxiality. Simulations are performed for different values of the stress triaxiality, for different crystal orientations, and for low and high work-hardening capacity. Under low stress triaxiality, the void shape evolution, void growth, and strain at the onset of coalescence are strongly dependent on the crystal orientation, while under high stress triaxiality, only the void growth rate is affected by the crystal orientation. These effects lead to significant variations in the ductility defined as the strain at the onset of coalescence. An attempt is made to predict the onset of coalescence using two different versions of the Thomason void coalescence criterion, initially developed in the framework of isotropic perfect plasticity. The first version is based on a mean effective yield stress of the matrix and involves a fitting parameter to properly take into account material strain hardening. The second version of the Thomason criterion is based on a local value of the effective yield stress in the ligament between the voids, with no fitting parameter. The first version is accurate to within 20% relative error for most cases, and often more accurate. The second version provides the same level of accuracy except for one crystal orientation. Such a predictive coalescence criterion constitutes an important ingredient towards the development of a full constitutive model for porous single crystals.  相似文献   

6.
One of the low-temperature failure mechanisms in ductile metallic alloys is the growth of voids and their coalescence. In the present work we attempt to obtain atomistic insights into the mechanisms underpinning cavitation in a representative metal, namely Aluminum. Often the pre-existing voids in metallic alloys such as Al have complex shapes (e.g. corrosion pits) and the defromation/damage mechanisms exhibit a rich size-dependent behavior across various material length scales. We focus on these two issues in this paper through large-scale calculations on specimens of sizes ranging from 18 thousand to 1.08 million atoms. In addition to the elucidation of the dislocation propagation based void growth mechanism we highlight the observed length scale effect reflected in the effective stress-strain response, stress triaxiality and void fraction evolution. Furthermore, as expected, the conventionally used Gurson's model fails to capture the observed size-effects calling for a mechanistic modification that incorporates the mechanisms observed in our (and other researchers') simulation. Finally, in our multi-void simulations, we find that, the splitting of a big void into a distribution of small ones increases the load-carrying capacity of specimens. However, no obvious dependence of the void fraction evolution on void coalescence is observed.  相似文献   

7.
Recent experimental evidence points to limitations in characterizing the critical strain in ductile fracture solely on the basis of stress triaxiality. A second measure of stress state, such as the Lode parameter, is required to discriminate between axisymmetric and shear-dominated stress states. This is brought into the sharpest relief by the fact that many structural metals have a fracture strain in shear, at zero stress triaxiality, that can be well below fracture strains under axisymmetric stressing at significantly higher triaxiality. Moreover, recent theoretical studies of void growth reveal that triaxiality alone is insufficient to characterize important growth and coalescence features. As currently formulated, the Gurson Model of metal plasticity predicts no damage change with strain under zero mean stress, except when voids are nucleated. Consequently, the model excludes shear softening due to void distortion and inter-void linking. As it stands, the model effectively excludes the possibility of shear localization and fracture under conditions of low triaxiality if void nucleation is not invoked. In this paper, an extension of the Gurson model is proposed that incorporates damage growth under low triaxiality straining for shear-dominated states. The extension retains the isotropy of the original Gurson Model by making use of the third invariant of stress to distinguish shear dominated states. The importance of the extension is illustrated by a study of shear localization over the complete range of applied stress states, clarifying recently reported experimental trends. The extension opens the possibility for computational fracture approaches based on the Gurson Model to be extended to shear-dominated failures such as projectile penetration and shear-off phenomena under impulsive loadings.  相似文献   

8.
9.
A phenomenological anisotropic damage progression formulation for porous ductile metals with second phases is described through mechanisms of void nucleation, growth and coalescence. The model is motivated from fracture mechanisms and microscale physical observations. To describe the creation of new pores, the decohesion at the particle–matrix interface and the fragmentation of second phase particles, the void-crack nucleation equation is related to several microstructural parameters (fracture toughness, length scale parameter, particle size, volume and fraction of second phase), the plastic strain level, and the stress state. Nucleation is represented by a general symmetric second rank tensor, and its components are proportional to the absolute value of the plastic strain rate components. Based on the Rice and Tracey model, void growth is a scalar function of the trace of damage tensor and the positive triaxiality. Like nucleation, coalescence is a second rank tensor governed by the plastic strain rate tensor and the stress state. The coalescence threshold is related to the void length scale for void impingement and void sheet mechanisms. The coupling of damage with the Bammann–Chiesa–Johnson (BCJ) plasticity model is written in the thermodynamic framework and derives from the concept of effective stress assuming the hypothesis of energy equivalence. A full-implicit algorithm is used for the stress integration and the determination of the consistent tangent operator. Finally, macroscale correlations to cast A356 AL alloy and wrought 6061-T6 AL alloy experimental data are completed with predictive void-crack evolution to illustrate the applicability of the anisotropic damage model.  相似文献   

10.
Micromechanics of coalescence in ductile fracture   总被引:2,自引:0,他引:2  
Significant progress has been recently made in modelling the onset of void coalescence by internal necking in ductile materials. The aim of this paper is to develop a micro-mechanical framework for the whole coalescence regime, suitable for finite-element implementation. The model is defined by a set of constitutive equations including a closed form of the yield surface along with appropriate evolution laws for void shape and ligament size. Normality is still obeyed during coalescence. The derivation of the evolution laws is carefully guided by coalescence phenomenology inferred from micromechanical unit-cell calculations. The major implication of the model is that the stress carrying capacity of the elementary volume vanishes as a natural outcome of ligament size reduction. Moreover, the drop in the macroscopic stress accompanying coalescence can be quantified for many initial microstructures provided that the microstructure state is known at incipient coalescence. The second part of the paper addresses a more practical issue, that is the prediction of the acceleration rate δ in the Tvergaard-Needleman phenomenological approach to coalescence. For that purpose, a Gurson-like model including void shape effects is used. Results are presented and discussed in the limiting case of a non-hardening material for different initial microstructures and various stress states. Predicted values of δ are extremely sensitive to stress triaxiality and initial spacing ratio. The effect of initial porosity is significant at low triaxiality whereas the effect of initial void shape is emphasized at high triaxiality.  相似文献   

11.
12.
A micromechanics model based on the theoretical framework of plastic localization into a band introduced by Rice is developed. The model consists of a planar band with a square array of equally sized cells, with a spherical void located in the centre of each cell. The periodic arrangement of the cells allows the study of a single unit cell for which fully periodic boundary conditions are applied. The micromechanics model is applied to analyze failure by ductile rupture in experiments on double notched tube specimens subjected to combined tension and torsion carried out by the present authors. The stress state is characterized in terms of the stress triaxiality and the Lode parameter. Two rupture mechanisms can be identified, void coalescence by internal necking at high triaxiality and void coalescence by internal shearing at low triaxiality. For the internal necking mechanism, failure is assumed to occur when the deformation localizes into a planar band and is closely associated with extensive void growth until impingement of voids. For the internal shearing mechanism, a simple criterion based on the attainment of a critical value of shear deformation is utilized. The two failure criteria capture the transition between the two rupture mechanisms successfully and are in good agreement with the experimental result.  相似文献   

13.
One of the major drawbacks of the Gurson-type of porous plasticity models is the inability of these models to predict material failure under low stress triaxiality, shear dominated conditions. This study addresses this issue by combining the damage mechanics concept with the porous plasticity model that accounts for void nucleation, growth and coalescence. In particular, the widely adopted Gurson–Tvergaard–Needleman (GTN) model is extended by coupling two damage parameters, representing the volumetric damage (void volume fraction) and the shear damage, respectively, into the yield function and flow potential. The effectiveness of the new model is illustrated through a series of numerical tests comparing its performance with existing models. The current model not only is capable of predicting damage and fracture under low (even negative) triaxiality conditions but also suppresses spurious damage that has been shown to develop in earlier modifications of the GTN model for moderate to high triaxiality regimes. Finally the modified GTN model is applied to predict the ductile fracture behavior of a beta-treated Zircaloy-4 by coupling the proposed damage modeling framework with a recently developed J2J3 plasticity model for the matrix material. Model parameters are calibrated using experimental data, and the calibrated model predicts failure initiation and propagation in various specimens experiencing a wide range of triaxiality and Lode parameter combinations.  相似文献   

14.
The GTN model proposed by Gurson, Tvergaard and Needleman has been widely applied to predict ductile fracture. However, the evaluation of the GTN model under high stress triaxiality has only been reported in a few studies. In this paper, a series of tensile tests on round notched specimens were performed to evaluate the applicability of the GTN model parameters under high stress triaxiality. The evaluation was carried out by comparing the predicted load-displacement curves with experimental results. It was observed the GTN model parameters only depend on the material except the critical void volume fraction. The influence of stress triaxiality on the critical void volume fraction was discussed. A further discussion about the construction of a new void coalescence criterion for the GTN model was also presented in this paper.  相似文献   

15.
张毅  薛世峰  韩丽美  周博  刘建林  贾朋 《力学学报》2021,53(6):1671-1683
损伤本构模型对研究材料的断裂失效行为有重要意义, 但聚合物材料损伤演化的定量表征实验研究相对匮乏. 通过4种高密度聚乙烯(high density polythylene, HDPE)缺口圆棒试样的单轴拉伸实验获得了各类试样的载荷-位移曲线和真应力-应变曲线, 采用实验和有限元模拟相结合的方法确定了HDPE材料不同应力状态下的本构关系, 并建立了缺口半径与应力三轴度之间的关系;采用两阶段实验法定量描述了4种HDPE试样单轴拉伸过程中的弹性模量变化, 并建立了基于弹性模量衰减的损伤演化方程, 结合中断实验和扫描电子显微镜分析了应力状态对HDPE材料微观结构演化的影响. 结果表明缺口半径越小, 应力三轴度越大, 损伤起始越早、演化越快; 微观表现为: 高应力三轴度促进孔洞的萌生和发展, 但抑制纤维状结构的产生;基于实验和有限元模拟获得的断裂应变、应力三轴度、损伤演化方程等信息提出了一种适用于聚合物的损伤模型参数确定方法, 最后将本文获得的本构关系和损伤模型用于HDPE平板的冲压成形模拟, 模拟结果与实验结果吻合良好.   相似文献   

16.
用碳化硅强化金属基复合材料制作的不同切口的拉伸试样进行了拉伸试验并使用三维电子扫描显微镜对拉伸延性断面进行了微小空穴的三维形状测试,分析了在不同应力三维度下空穴聚合时空穴几何形状的变化,为准确模拟金属基复合材料在多向外载荷下的损伤过程,判断延性损伤机理提供了科学依据。  相似文献   

17.
Hydrostatic stress can affect the non-elastic deformation and flow stress of polymeric materials and certain metallic alloys. This sensitivity to hydrostatic stress can also influence the fracture toughness of ductile materials, which fail by void growth and coalescence. These materials typically contain a non-uniform distribution of voids of varying size-scales and void shapes. In this work, the effects of void shape and microvoid interaction in pressure-sensitive materials are examined via a two-prong approach: (i) an axisymmetric unit-cell containing a single ellipsoidal void and (ii) a plane-strain unit-cell consisting of a single large void and a population of discrete microvoids. The representative material volume in both cases is subjected to physical stress states similar to highly stressed regions ahead of a crack. Results show that oblate voids and microvoid cavitation can severely reduce the critical stress of the material. These effects can be compounded under high levels of pressure-sensitivity. In some cases, the critical stress responsible for rapid void growth is reduced to levels comparable to the yield strength of the material. The contribution of void shape and pressure-sensitivity to the thermal- and moisture-induced voiding phenomenon in IC packages is also discussed.  相似文献   

18.
Void closing from a spherical shape to a crack is investigated quantitatively in the present study. The constitutive relation of the Void-free matrix is assumed to obey the Norton power law. A representative volume element (RVE) which includes matrix and void is employed and a Rayleigh-Ritz procedure is developed to study the deformation-rates of a spherical void and a penny-shaped crack. Based on an approximate interpolation scheme, an analytical model for void closure in nonlinear plastic materials is established. It is found that the local plastic flows of the matrix material are the main mechanism of void deformation. It is also shown that the relative void volume during the deformation depends on the Norton exponent, on the far-field stress triaxiality, as well as on the far-field effective strain. The predictions of void closure using the present model are compared with the corresponding results in the literature, showing good agreement. The model for void closure provides a novel way for process design and optimization in terms of elimination of voids in billets because the model for void closure can easily be applied in the CAE analysis.  相似文献   

19.
本文对含不同形状孔洞的幂硬化材料的圆柱体胞模型,运用控制宏观应力三维工的方法进行了有限元分析。计算结果表明:1.孔洞初始形状,应力三维度对孔洞的长大有重要影响;2.Guson模型对孔洞长大规律的描述是不准确的,不准确度与孔洞初始形状,应力三维度有关,修正后的Gurson模型与有限元结果吻合较好;3.在低应力三维度区,孔洞以及形状改变为主,在高应力三维度区,孔洞以扩张为主;  相似文献   

20.
State of the art ductile fracture models often rely on simple power laws to describe the strain hardening of the matrix material. Power laws do not distinguish between the two main stages of hardening observed in polycrystals, referred to as stage III and stage IV hardening, and which emerge from the evolution of the dislocation substructure. The aim of this study is to couple a physics based strain hardening law including these two stages to a micromechanics based ductile damage model. One of the main motivations is that, the stage IV constant hardening rate stage, occurring only at large strain, will be attained in most ductile failure problems if not at the overall level of deformation, at least locally around the growing voids. Furthermore, proper modelling of the stage III involving dislocation storage and recovery terms and the transition to stage IV provides a link with the underlying physical mechanisms of deformation and with the microstructure. First, in order to evaluate the effects of the stage III and stage IV hardening on void growth and coalescence, an extensive parametric study is performed on two-dimensional (2D) axisymmetric finite element (FE) unit cell calculations, using a Kocks-Mecking type hardening law. The cell calculations demonstrate that accounting for the stage IV hardening can have a profound effect on delaying void coalescence and increasing the ductility. The magnitude of the recovery term during stage III has also a significant effect on the void growth rate. Then, the Kocks-Mecking law is incorporated into the Gologanu-Leblond-Devaux (GLD) porous plasticity model supplemented by two different versions of the Thomason void coalescence criterion. The predictions of the damage model are in good agreement with the results of the FE calculations in terms of the stress-strain curves, the evolution of void shape and porosity, as well as the strain value at the onset of void coalescence.  相似文献   

设为首页 | 免责声明 | 关于勤云 | 加入收藏