Bulk Ge20Se80−xTlx (x ranging from 0 to 15 at%) chalcogenide glasses were prepared by conventional melt quenching technique. Thin films of these compositions were prepared by thermal evaporation, on glass and Si wafer substrates at a base pressure of 10−6 Torr. X-ray diffraction studies were performed to investigate the structure of the thin films. The absence of any sharp peaks in the X-ray diffractogram confirms that the films are amorphous in nature. The optical constants (absorption coefficient, optical band gap, extinction coefficient and refractive index) of Ge20Se80−xTlx thin films are determined by absorption and reflectance measurements in a wavelength range of 400-900 nm. In order to determine the optical gap, the absorption spectra of films with different Tl contents were analyzed. The absorption data revealed the existence of allowed indirect transitions. The optical band gap showed a sharp decrease from 2.06 to 1.79 eV as the Tl content increased from 0% to 15%. It has been found that the values of absorption coefficient and refractive index increase while the extinction coefficient decreases with increase in Tl content in the Ge-Se system. These results are interpreted in terms of the change in concentration of localized states due to the shift in Fermi level. DC electrical conductivity of Ge20Se80−xTlx thin films was carried out in a temperature range 293-393 K. The electrical activation energy of these films was determined by investigating the temperature dependence of dc conductivity. A decrease in the electrical activation energy from 0.91 to 0.55 eV was observed as the Tl content was increased up to 15 at% in Ge20Se80−xTlx system. On the basis of pre-exponential factor, it is suggested that the conduction is due to thermally assisted tunneling of the carriers in the localized states near the band edges.  相似文献   

2.
Polycrystalline InxGa1−xN thin films were prepared by mixed source modified activated reactive evaporation (MARE) technique. The films were deposited at room temperature on glass substrates without any buffer layer. All the films crystallize in the hexagonal wurtzite structure. The indium concentration calculated from XRD peak shift using Vegard's law was found to be varying from 2% to 92%. The band gap varies from 1.72 eV to 3.2 eV for different indium compositions. The indium rich films have higher refractive indices as compared to the gallium rich films. The near infra-red absorption decreases with gallium incorporation into InN lattice which is mainly due to decrease in the free carrier concentration in the alloy system. This fact is further supported from Hall effect measurements. MARE turns out to be a promising technique to grow InxGa1−xN films over the entire composition range at room temperature.  相似文献   

3.
CuIn1−xAlxSe2 (CIASe) thin films with x=0.25, 0.5 and 0.65 were prepared by four-source elemental evaporation. The structural and optical properties were investigated by X-ray diffraction, scanning electron microscopy, energy dispersive analysis, and optical transmission. The results showed that these films contain chalcopyrite structure with preferred orientation along (112) direction. The morphology, grain distribution and composition of CIASe films were studied and compared for different Al content. The optical studies revealed that the films were highly absorbing and the energy band gap calculated from transmission spectra for x=0.25, 0.5 and 0.65 were 1.2, 1.51 and 1.73 eV, respectively. The variation of Al content in the CIASe composition offered a very effective change in the optical band gap.  相似文献   

4.
The optical absorption of the as-prepared and thermally annealed Se85−xTe15Sbx (0≤x≤9) thin films was measured. The mechanism of the optical absorption follows the rule of non-direct transition. The optical energy gap (E0) decreased from 1.12 to 0.84 eV with increasing Sb content of the as-prepared films from 0 to 9 at.%. The as-prepared Se76Te15Sb9 films showed an increase in (E0) with increasing the temperature of annealing in the range above Tg (363 K). The electrical conductivity of the as-prepared and annealed films was found to be of Arrhenius type with temperature in the range 300-360 K. The activation energy for conduction was found to decrease with increasing both the Sb content and temperature of annealing. The results were discussed on the basis of the lone-pair electron effect and of amorphous crystalline transformation.  相似文献   

5.
Thin films of samples of the glassy SxSe100−x system with 0 ≤ x ≤ 7.28 have been prepared by thermal evaporation technique at room temperature (300 K). X-ray investigations show that the structure of pure selenium (Se) does change seriously by the addition of small amount of sulphur S ≤7.28%. The lattice parameters were determined as a function of sulphur content. Results of differential thermal analysis (DTA) of the glassy compositions of the system SxSe100−x were discussed. The characteristic temperatures (Tg, Tc and Tm) were evaluated. Dark electrical resistivities, ρ, of SxSe100−x thin films with different thicknesses from 100 to 500 nm, were measured in the temperature range from 300 to 423 K. Two distinct linear parts with different activation energies were observed. The variation of electrical resistivity of examined compositions has been discussed as a function of the film thickness, temperature and the sulphur content. The application of Mott model for the phonon assisted hopping of small polarons gave the same two activation energies obtained from the resistivity temperature calculations.  相似文献   

6.
The electrical conductivity σ, Hall effect RH, and thermoelectric power Q of CuGa0.25In0.75Se2 thin films with different growth conditions have been measured at temperature 300-520 K. These properties were also measured at room temperature for different composition of CuGaxIn1−xSe2 (0.75≥x≥0) deposited at the same evaporation conditions. All investigated films are p-type over the whole temperature range. Electrical conduction was studied in order to establish its mechanism.The room temperature photoelectric response of those films were measured as a function of wavelength (2.5≥λ≥0.3) μm. It is found that the energy gap values follow a second order equation in x giving a downward bowing parameter of about 0.31 eV.  相似文献   

7.
Ternary alloyed CdS1−xSex thin films of variable composition ‘x’ were grown by the simple and economical chemical bath deposition technique. The as-grown thin films were characterized for structural, compositional, surface morphological, optical and electrical studies. The X-ray diffraction (XRD) patterns of the sample indicated that all the samples were polycrystalline in nature with hexagonal structure. Scanning electron microscopy (SEM) micrographs showed uniform morphology with spherical shaped grains distributed over entire glass substrate. EDAX studies confirmed that the CdS1−xSex films were having approximately same stoichiometry initially as well as finally. Room temperature optical measurements showed that band gap engineering could be realized in CdS1−xSex thin films via modulation in composition ‘x’. Electrical resistivity of CdS1−xSex thin films for various compositions was found to be low. The broad and fine tunable band gap properties of ternary CdS1−xSex thin films have potential applications in opto-electronic devices.  相似文献   

8.
Physical properties of In35Sb45Se20−xTex thin films with different compositions (x=2.5, 5, 7.5, 10, 12.5 and 15 at %) prepared by electron beam evaporation method are studied. X-ray diffraction results indicate that the as-evaporated films depend on the Te content and the crystallized compounds consist mainly of Sb2Se3 with small amount of Sb2SeTe2. Transmittance and reflectance of the films are found to be thickness dependent. Optical-absorption data indicate that the absorption mechanism is direct transition. Optical band gap values decrease with increase in Te content as well as with increase in film thickness.  相似文献   

9.
Ga2(1−x)In2xO3 thin films with different indium content x [In/(Ga + In) atomic ratio] were prepared on α-Al2O3 (0 0 0 1) substrates by the metal organic chemical vapor deposition (MOCVD). The structural and optical properties of the Ga2(1−x)In2xO3 films were investigated in detail. Microstructure analysis revealed that the film deposited with composition x = 0.2 was polycrystalline structure and the sample prepared with x up to 0.8 exhibited single crystalline structure of In2O3. The optical band gap of the films varied with increasing Ga content from 3.72 to 4.58 eV. The average transmittance for the films in the visible range was over 90%.  相似文献   

10.
Glasses in the system Ge-Se-S were prepared with different Se/S ratios in order to investigate the compositional dependence of selected physical properties. We report the results of a systematic study examining the UV-vis transmission, dc electrical conductivity and X-ray diffraction of the system Ge(SxSe1−x)2 with x=0, 0.1, 0.4 and 1.0 where replacement of S by Se was made. The changes in the optical energy gap, Eg, (from 1.95 to 2.43 eV) and band tail width, Ee, (from 103 to 243 meV) behave contrarily to the change in refractive index, n, (from 2.3 to 2) with the progressive replacement of S by Se. This behavior was discussed and interpreted with the changes in cohesive energy. The analysis of defects in the prepared films was carried out by the examination of activation energies obtained from dc electrical conductivity. The analysis of the X-ray diffraction pattern revealed a remarkable reduction in the intensity of the first and second diffraction peaks with the progressive replacement of S content, which confirms a change in the intermediate range order structure: reorganization of the structural properties.  相似文献   

11.
Optical absorption at room temperature and electrical conductivity at temperatures between 283 and 333 K of vacuum evaporated GexFexSe100−2x (0≤x≤15) amorphous thin films have been studied as a function of composition and film thickness. It was found that the optical absorption is due to indirect transition and the energy gap increases with increasing both Ge and Fe content; on the other hand, the width of the band tail exhibits the opposite behavior. The optical band gap Eopt was found to be almost thickness independent. The electrical conductivity show two types of conduction, at higher temperature the conduction is due to extended states, while the conduction at low temperature is due to variable range hopping in the localized states near Fermi level. Increasing Ge and Fe contents were found to decrease the localized state density N(EF), electrical conductivity and increase the activation energy for conduction, which is nearly thickness independent. Variation of the atomic densities ρ, molar volume V, glass transition temperature Tg cohesive energy C.E and number of constraints NCo with average coordination number Z was investigated. The relationship between the optical gap and chemical composition is discussed in terms of the cohesive energy C.E, average heat of atomization and coordination numbers.  相似文献   

12.
A series of ZnO1−xSx alloy films (0 ≤ x ≤ 1) were grown on quartz substrates by radio-frequency (rf) magnetron sputtering of ZnS ceramic target, using oxygen and argon as working gas. X-ray diffraction measurement shows that the ZnO1−xSx films have wurtzite structure with (0 0 2) preferential orientation in O-rich side (0 ≤ x ≤ 0.23) and zinc blende structure with (1 1 1) preferential orientation in S-rich side (0.77 ≤ x ≤ 1). However, when the S content is in the range of 0.23 < x < 0.77, the ZnO1−xSx film consists of two phases of wurtzite and zinc blende or amorphous ZnO1−xSx phase. The band gap energy of the films shows non-linear dependence on the S content, with an optical bowing parameter of about 2.9 eV. The photoluminescence (PL) measurement reveals that the PL spectrum of the wurtzite ZnO1−xSx is dominated by visible band and its PL intensity and intensity ratio of UV to visible band decrease greatly compared with undoped ZnO. All as-grown ZnO1−xSx films behave insulating, but show n-type conductivity for w-ZnO1−xSx and maintain insulating properties for β-ZnO1−xSx after annealed. Mechanisms of effects of S on optical and electrical properties of the ZnO1−xSx alloy are discussed in the present work.  相似文献   

13.
Bulk InxSe1−x (with x=5-25 at%) glasses were prepared using the melt-quench technique. Short range order(SRO) was examined by the X-ray diffraction using Cu(kα) radiation in the wave vector interval 0.28≤k≤6.5 A0−1.The SRO parameters have been obtained from the radial distribution function. The inter-atomic distance obtained from the first and second peak are r1=0.263 and r2=0.460 nm, which is equivalent In-Se and Se-Se bond length. The fundamental structural unit for the studied glasses is In2Se3 pyramid. Using the differential scanning calorimetry (DSC), the crystallization mechanism of InxSe1−x chalcogenide glass has been studied. The glass transition activation energy (Eg) is 289±0.3 kj/mol.There is a correlation amongst the glass forming ability, bond strength and the number of lone pair electrons. The utility of the Gibbs-Di Marzio relation was achieved by estimating Tg theoretically.  相似文献   

14.
R. Ghosh 《Applied Surface Science》2009,255(16):7238-7242
MgxZn1−xO (x = 0.0-0.20) thin films have been deposited by sol-gel technique on glass substrates and the effect of growth ambient (air and oxygen) on the structural, and optical properties have been investigated. The films synthesized in both ambient have hexagonal wurtzite structure. The c-axis lattice constant decreases linearly with the Mg content (x) up to x = 0.05, and 0.10 respectively for air- and oxygen-treated films, above which up to x = 0.20, the values vary irregularly with x. The change in the optical band gap values and the ultraviolet (UV) peak positions of MgxZn1−xO films show the similar change with x. These results suggest that the formation of solid solution and thus the structural and optical properties of MgxZn1−xO thin films are affected by the growth ambient.  相似文献   

15.
Thin film binary alloys of InxSe1−x (0.05?x?0.30) have been prepared by the thermal evaporation technique. The optical transmission and reflection spectrum of these films were measured in the range 300-1100 nm. Both refractive index, n and extinction coefficient k have been determined from transmission and reflection measurements in terms of Murmann's equations. The dispersion of the refractive index is discussed in terms of the single-oscillator Wemple-DiDomenico model. The width of band tail is determined and the optical absorption edge is described using the ‘non-direct transition’ model proposed by Tauc. Finally, the relationship between the optical gap and chemical composition in InxSe1−x amorphous system is discussed in terms of the average heat of atomization Hs and average coordination number Nc. The results of these calculations can be used rationalize the observed optical properties of these materials. Finally, the chemical bond approach has been also applied to interpret the decrease of the glass optical gap with increasing In content.  相似文献   

16.
Chalcogenide glasses are interesting materials due to their infrared transmitting properties and photo induced effects exhibited by them. Thin films with thickness of 3000 Å of the glasses Se75S25−xCdx with x=6, 8 and 10 at% prepared by melt quench technique were evaporated by thermal evaporation onto glass substrates under a vacuum of 10−6 Torr. The optical constants (absorption coefficient, refractive index and extinction coefficient) of as-prepared and annealed films have been studied as a function of photon energy in the wave length region 400-1000 nm. Analysis of the optical absorption data shows that the rule of non-direct transitions predominates. It has been found that the absorption coefficient and optical band gap increase with increasing annealing temperatures. The refractive index (n) and the extinction coefficient (k) were observed to decrease with increasing annealing temperature.  相似文献   

17.
Silver doped indium oxide (In2−x Agx O3−y) thin films have been prepared on glass and silicon substrates at room temperature (300 K) by reactive DC magnetron sputtering technique using an alloy target of pure indium and silver (80: 20 atomic %. The magnetron power (and hence the metal atom sputter flux) is varied in the range 40-80 W. The energy dispersive analysis of X-ray (EDAX) results show that the silver content in the film decreases with increasing magnetron power. The grain size of these films is of the order of 100 nm. The resistivity of these films is in the range 10−2-10−3 Ω cm. The work function of the silver-indium oxide films (by Kelvin Probe) are in the range: 4.64-4.55 eV. The refractive index of these films (at 632.8 nm) varies in the range: 1.141-1.195. The optical band gap of indium oxide (3.75 eV) shrinks with silver doping. Calculations of the partial ionic charge (by Sanderson's theory) show that silver doping in indium oxide thin films enhance the ionicity.  相似文献   

18.
The crystal structure, band gap energy and bowing parameter of In-rich InxAl1−xN (0.7 < x < 1.0) films grown by magnetron sputtering were investigated. Band gap energies of InxAl1−xN films were obtained from absorption spectra. Band gap tailing due to compositional fluctuation in the films was observed. The band gap of the as-grown InN measured by optical absorption method is 1.34 eV, which is larger than the reported 0.7 eV for pure InN prepared by molecular beam epitaxy (MBE) method. This could be explained by the Burstein-Moss effect under carrier concentration of 1020 cm−3 of our sputtered films. The bowing parameter of 3.68 eV is obtained for our InxAl1−xN film which is consistent with the previous experimental reports and theoretical calculations.  相似文献   

19.
Herein is a report of a study on a Cd1−xZnxS thin film grown on an ITO substrate using a chemical bath deposition technique. The as-deposited films were annealed in air at 400 °C for 30 min. The composition, surface morphology and structural properties of the as-deposited and annealed Cd1−xZnxS thin films were studied using EDX, SEM and X-ray diffraction techniques. The annealed films have been observed to possess a crystalline nature with a hexagonal structure. The optical absorption spectra were recorded within the range of 350-800 nm. The band gap of the as-deposited thin films varied from 2.46 to 2.62 eV, whereas in the annealed film these varied from 2.42 to 2.59 eV. The decreased band gap of the films after annealing was due to the improved crystalline nature of the material.  相似文献   

20.
Mixed thin films of (CdO)1−x(PbO)x and (CdS)1−x(PbS)x (x=0.25) were prepared on glass substrates by spray pyrolysis technique for various substrate temperatures 300, 320 and 340 °C. Structural and optical properties were studied. XRD studies reveal the formation of mixed films. The substrate temperature of 340 °C seems to be critical for the formation of CdO-PbO mixed films. It is observed that (CdS)1−x(PbS)x mixed films were formed at all the three substrate temperatures. The direct band gap value of (CdO)1−x(PbO)x and (CdS)1−x(PbS)x mixed films is about 2.6 and 2.37 eV, respectively.  相似文献   