1.
YF(3) and YF(3):Eu(3+) mesoporous hexagonal nanocrystals were successfully synthesized via a simple hydrothermal process based on the in situ assembly of the as-synthesized YF(3) and YF(3):Eu(3+) nanoparticles. The well defined mesoporous nanostructures are formed by phenanthroline assisted assembly of ~20 nm nanoparticles, and 2-4 nm pores are contained as indicated by N(2) adsorption-desorption studies. The obtained YF(3):Eu(3+) mesoporous hexagonal nanoplates show a significant photoluminescence intensity enhancement compared with other shaped YF(3):Eu(3+) nanocrystals.  相似文献   

2.
This work explores the sensitization of luminescent lanthanide Tb(3+) and Eu(3+) cations by the electronic structure of zinc sulfide (ZnS) semiconductor nanoparticles. Excitation spectra collected while monitoring the lanthanide emission bands reveal that the ZnS nanoparticles act as an antenna for the sensitization of Tb(3+) and Eu(3+). The mechanism of lanthanide ion luminescence sensitization is rationalized in terms of an energy and charge transfer between trap sites and is based on a semiempirical model, proposed by Dorenbos and co-workers (Dorenbos, P. J. Phys.: Condens. Matter 2003, 15, 8417-8434; J. Lumin. 2004, 108, 301-305; J. Lumin. 2005, 111, 89-104. Dorenbos, P.; van der Kolk, E. Appl. Phys. Lett. 2006, 89, 061122-1-061122-3; Opt. Mater. 2008, 30, 1052-1057. Dorenbos, P. J. Alloys Compd. 2009, 488, 568-573; references 1-6.) to describe the energy level scheme. This model implies that the mechanisms of luminescence sensitization of Tb(3+) and Eu(3+) in ZnS nanoparticles are different; namely, Tb(3+) acts as a hole trap, whereas Eu(3+) acts as an electron trap. Further testing of this model is made by extending the studies from ZnS nanoparticles to other II-VI semiconductor materials; namely, CdSe, CdS, and ZnSe.  相似文献   

3.
YPO(4) nanoparticles codoped with Eu(3+) (5 at. %) and Bi(3+) (2-10 at. %) have been synthesized by a simple coprecipitation method using a polyethylene glycol-glycerol mixture, which acts as capping agent. It has been found that the incorporation of Bi(3+) ions into the YPO(4):Eu(3+) lattice induces a phase transformation from tetragonal to hexagonal, and also a significant decrease in Eu(3+) luminescence intensity was observed. This is related to the association of the water molecules in the hexagonal phase of YPO(4) in which the nonradiative process from the surrounding water molecules around Eu(3+) is dominating over the radiative process. On annealing above 800 °C, luminescence intensity recovers due to significant removal of water. 900 °C annealed Bi(3+) codoped YPO(4):Eu(3+) shows enhanced luminescence (2-3 times) as compared to that of YPO(4):Eu(3+). When sample was prepared in D(2)O (instead of H(2)O), 4-fold enhancement in luminescence was observed, suggesting the extent of reduction of multiphonon relaxation in D(2)O. This study illustrates the stability of water molecules even at a very high temperature up to 800 °C in Eu(3+) and Bi(3+) codoped YPO(4) nanoparticles.  相似文献   

4.
A variety of redispersible Eu(3+)-doped LaPO(4) nanoparticles have been prepared in a high-boiling coordinating solvent mixture, and the Eu(3+) lattice sites of these materials have been investigated by luminescence line-narrowing measurements. In this spectroscopic method, Eu(3+) ions occupying different lattice sites are selectively excited with a tunable narrow-bandwidth laser system and distinguished by their luminescence spectra ("site-selective spectroscopy"). Depending on the concentration of the dopant, up to three different lattice sites could be identified in the interior of the LaPO(4) nanoparticles. These sites correspond to those known from bulk LaPO(4). In addition, a variety of surface sites is observed, which could be converted completely into bulk sites by overgrowing the nanoparticles with a shell of pure LaPO(4). The surface sites are identical to those obtained by reacting Eu(3+) with the surface of pure LaPO(4) nanoparticles. The spectroscopic properties of Eu(3+)-doped LaPO(4) nanoparticles differ from those of pure EuPO(4) nanoparticles, which were also investigated. Remarkably, the core/shell synthesis investigated in this paper allows one to prepare doped nanoparticles that contain no other dopant sites than those known from the corresponding bulk material.  相似文献   

5.
This work explores the size-induced lattice modification and its relevance to photoluminescence properties of tetragonal zircon-type GdVO(4):Eu(3+) nanostructures. GdVO(4):Eu(3+) nanoparticles with crystallite sizes ranging from 14.4 to 24.7 nm were synthesized by a hydrothermal method using sodium citrate as a capping agent. Regardless of the reaction temperatures, all samples retained an ellipsoidal-like morphology. Nevertheless, as the crystallite size reduces, there appears a tensile strain and lattice distortion, which is accompanied by a lattice expansion and a decreased symmetry of structural units. These lattice modifications could be associated with the changes in the interior chemical bonding due to the interactions of surface defect dipoles that have imposed an increased negative pressure with crystallite size reduction. Furthermore, crystallite size reduction also led to a significant increase in the amounts of surface hydroxyl groups and citric species, as well as the concentration of the surface Eu(3+) ions. When Eu(3+) was taken as a structural probe, it was found that the asymmetric ratio (I(02)/I(01)) of Eu(3+) gradually declined to show a remarkable decrease in color chromaticity as crystallite size reduces, which could be interpreted as due to the change of local environments of Eu(3+) ions from the interior to the surface of the nanoparticles.  相似文献   

6.
A series of doped CeF(3): RE(3+) (RE(3+): Tb(3+), Eu(3+) and Dy(3+)) nanoparticles were synthesized, with the aim of obtaining a white light emitting composition, by a simple polyol route at 160°C and characterized by X-ray diffraction (XRD), high resolution transmission electron microscopy (HR-TEM), Fourier transform infrared spectroscopy (FT-IR) and photoluminescence. Uniformly distributed and highly water-dispersible rectangular nanoparticles (length ~15-20 nm, breadth ~5-10 nm) were obtained. The steady state and time resolved luminescence studies confirmed efficient energy transfer from the host to activator ions. Lifetime studies revealed that optimum luminescence is observed for 2.5 mol% Dy(3+) and 7.5 mol% Tb(3+). The energy transfer efficiencies (Ce(3+) to activators) were found to be 89% for CeF(3): Tb(3+) (7.5 mol%) nanoparticles and 60% for CeF(3): Dy(3+) (2.5 mol%) nanoparticles. Different concentrations of Tb(3+), Eu(3+) and Dy(3+) were doped to achieve a white light emitting phosphor for UV-based LEDs (light emitting diodes). Finally CeF(3), triply doped with 2.0 mol%Tb(3+), 4.5 mol% Eu(3+) and 3.5 mol% Dy(3+), was found to have impressive chromaticity co-ordinates, close to broad day light. The colloidal solutions of doped CeF(3) nanoparticles emitted bright green (Tb(3+)), blue (Dy(3+)) and white (triply doped) luminescence upon host excitation. Composites of poly methyl methacrylate (PMMA) and poly vinyl alcohol (PVA) were made with CeF(3): 5.0 mol%Tb(3+), CeF(3): 5.0 mol% Dy(3+) and triply doped white light emitting composition. The CeF(3)/PMMA (PVA) nanocomposite films, so obtained, are highly transparent (in the visible spectral range) and exhibit strong photoluminescence upon UV excitation.  相似文献   

7.
The preparation of nearly monodisperse (40 nm), silica-coated LaF(3):Ln(3+) nanoparticles and their bioconjugation to FITC-avidin (FITC=fluorescein isothiocyanate) is described in this report. Doping of the LaF(3) core with selected luminescent Ln(3+) ions allows the particles to display a range of emission lines from the visible to the near-infrared region (lambda=450-1650 nm). First, the use of Tb(3+) and Eu(3+) ions resulted in green (lambda=541 nm) and red (lambda=591 and 612 nm) emissions, respectively, by energy downconversion processes. Second, the use of Nd(3+) gave emission lines at lambda=870, 1070 and 1350 nm and Er(3+) gave an emission line at lambda=1540 nm by energy downconversion processes. Additionally, the Er(3+) ions gave green and red emissions and Tm(3+) ions gave an emission at lambda=800 nm by upconversion processes when codoped with Yb(3+) (lambda(ex)=980 nm). Bioconjugation of avidin, which has a bound fluorophore (FITC) as the reporter, was carried out by means of surface modification of the silica particles with 3-aminopropyltrimethoxysilane, followed by reaction with the biotin-N-hydroxysuccinimide activated ester to form an amide bond, imparting biological activity to the particles. A 25-fold or better increase in the FITC signal relative to the non-biotinylated silica particles indicated that there is minimal nonspecific binding of FITC-avidin to the silica particles.  相似文献   

8.
Luminescence and power-gated spectral holeburning studies have been performed on Eu-doped MgS nanoparticles. These particles are atomically tailored to produce and control the relative concentration of Eu(2+) and Eu(3+), which is necessary for power-gated holeburning. The spectral holes are permanent at low temperatures. Optical studies show that the electron-phonon coupling is stronger in nanoparticles than in thin films or microparticles of the same material. This is the reason for inherently broader spectral holes in nanoparticles as compared to microparticle or thin-film samples. Temperature broadening of spectral holes in nanoparticles follows a T(2.4) behavior, a faster rate than thin films or microparticles. This behavior can be attributed to the glassy nature of the particles produced.  相似文献   

9.
Ligand-capped gold nanoparticles were synthesized by capping monothiol derivatives of 2,2'-dipyridyl onto the surface of Au nanoparticles (Au-BT). The average size of the metal core is around 4 nm, with a shell of approximately 340 bipyridine ligands around the Au nanoparticle. The high local concentration of the chelating ligands ( approximately 5 M) around the Au nanoparticle makes these particles excellent ion sponges, and their complexation with Eu(III)/Tb(III) ions yields phosphorescent nanomaterials. Absorption spectral studies confirm a 1:3 complexation between Eu(III)/Tb(III) ions and bipyridines, functionalized on the surface of Au nanoparticles. The red-emitting Au-BT:Eu(III) complex exhibits a long lifetime of 0.36 ms with six line-like emission peaks, whereas the green-emitting Au-BT:Tb(III) complex exhibits a lifetime of 0.7 ms with four line-like emission peaks. These phosphorescent nanomaterials, designed by linking BT:Eu(III) complexes to Au nanoparticles, were further utilized as sensors for metal cations. A dramatic decrease in the luminescence was observed upon addition of alkaline earth metal ions (Ca(2+), Mg(2+)) and transition metal ions (Cu(2+), Zn(2+), Ni(2+)), resulting from an isomorphous substitution of Eu(III) ions, whereas the luminescence intensity was not influenced by the addition of Na(+) and K(+) ions. Direct interaction of bipyridine-capped Au nanoparticles with Cu(2+) ions brings the nanohybrid systems closer, leading to the formation of three-dimensional superstructures. Strong interparticle plasmon interactions were observed in these closely spaced Au nanoparticles.  相似文献   

10.
Time-resolved laser fluorescence spectroscopy (TRLFS) is an effective speciation technique for fluorescent metal ions and can be further extended by the parallel factor analysis (PARAFAC). The adsorption of Eu(3+) on kaolinite as well as gibbsite as a reference mineral was investigated by TRLFS together with batch adsorption measurements. The PAFAFAC modeling provided the fluorescence spectra, decay lifetimes, and relative intensity profiles of three Eu(3+) surface complexes with kaolinite; an outer-sphere (factor A) complex and two inner-sphere (factors B and C) complexes. Their intensity profiles qualitatively explained the measured adsorption of Eu(3+). Based on the TRLFS results in varied H(2)O/D(2)O media, it was shown that the outer-sphere complex exhibited more rapid fluorescence decay than Eu(3+) aquo ion, because of the energy transfer to the surface. Factor B was an inner-sphere complex, which became dominant at relatively high pH, high salt concentration and low Eu(3+) concentration. Its spectrum and lifetime were similar to those of Eu(3+) adsorbed on gibbsite, suggesting its occurrence on the edge face of the gibbsite layer of kaolinite. From the comparison with the spectra and lifetimes of crystalline or aqueous Eu(OH)(3), factor C was considered as a poly-nuclear surface complex of Eu(3+) formed at relatively high Eu(3+) concentration.  相似文献   

11.
A novel europium (III) ternary complex, Eu(TPBDTFA)(3)Phen, was designed and synthesized. Photoluminescence measurements show that the energy absorbed by the organic ligands was efficiently transferred to the central Eu(3+) ions, and the complex exhibits strongly red emission due to the (5)D(0)-(7)F(j) transitions of Eu(3+) ions with appropriate CIE (Commission Internationale de l'Eclairage, International Commission on Illumination) chromaticity coordinates (x=0.66, y=0.33) under 310-420 nm light excitation. The luminescence quantum yield for the Eu(3+) complex is 0.18. Thermogravimetric analysis (TGA) confirms a high thermal stability of the complex with a decomposition temperature of 341 degrees C. All the characteristics indicate that the Eu(3+) complex is a highly efficient red phosphor suitable to be excited by near UV light. An intense red-emitting LED was fabricated by combining the mono-phosphor Eu(TPBDTFA)(3)Phen with a approximately 395 nm emitting InGaN chip.  相似文献   

12.
Solvent-driven room-temperature synthesis of nanoparticles BiPO4:Eu3+   总被引:1,自引:0,他引:1  
Fu C  Li G  Zhao M  Yang L  Zheng J  Li L 《Inorganic chemistry》2012,51(10):5869-5880
In this work, a novel solvent-driven room-temperature synthesis of BiPO(4):Eu(3+) nanoparticles was presented. By virtue of 11 solvents with different properties and function groups, phase structure and composition of BiPO(4):Eu(3+) can be systematically tailored. Hexagonal phase (HP) of BiPO(4):Eu(3+) was obtained in water and hydrophobic organic solvents such as arenes and cyclohexane, while low-temperature monoclinic phase (LTMP) was prepared in hydrophilic alcohols. In other solvents (i.e., hydrophilic ethers, aldehydes, ketones, and carboxylic acids), a mixture of HP and LTMP was formed, in which the relative content of LTMP gradually increased following the above solvent sequence. It is also found that particle sizes of BiPO(4):Eu(3+) nanoparticles were closely related to the phase structure: HP exhibited a comparatively larger particle size. The phase evolution processes for both polymorphs with varying solvents were investigated in details. Photoluminescence (PL) properties were sensitive to the phase structure and compositions of the final products. With increasing the phase content of LTMP, the lifetimes and quantum yields both increased. The methodology reported here is fundamentally important, which may give a novel insight into the polymorph-controlled synthesis for further optimized materials performance.  相似文献   

13.
White light was generated from a single silica thin film made with Yb0.75La0.2Eu0.05F3, La0.45Yb0.5Er0.05F3, and La0.75Yb0.2Tm0.05F3 nanoparticles by exciting with a single source near-infrared light (980 nm CW diode laser). Eu3+ and Tm3+ ions are responsible for red and blue emission, respectively. Er3+ ion is responsible for green as well as red emission. The Commission Internationale de l'Eclairage (CIE) coordinates of the resulting light were easily adjusted by controlling the concentration of Ln3+ (Eu3+, Er3+, Tm3+) ions in the nanoparticles as well as the concentration of Ln3+-doped nanoparticles in the sol-gel thin layer.  相似文献   

14.
A comprehensive survey of electronic structure and optical properties of rare-earth ions-doped semiconductor is of vital importance for their potential applications. In this work, Eu(3+)-doped β-Ga(2)O(3) nanocrystals were synthesized via a combustion method. The evolution of the optical properties of nanophosphors with increasing the annealing temperature was investigated in detail by means of excitation and emission spectra at room temperature and 10 K. Eu(3+) ions were proved to be incorporated into the crystal lattice of the β-Ga(2)O(3) phase after annealing the as-prepared nanoparticles at 1100 °C. It was observed that the substitution of Eu(3+) for Ga(3+) occurred at merely single site, in spite of two crystallographically nonequivalent sites of Ga(3+) in β-Ga(2)O(3). Spectroscopic evidence corroborated and clarified the local symmetry of C(s) for Eu(3+) at this single site. From the high-resolution excitation and emission spectra, 71 crystal-field levels of Eu(3+) in β-Ga(2)O(3) were identified and analyzed in terms of 19 freely varied free-ions and crystal-field parameters based on C(s) symmetry. The standard deviation of the final fitting is as low as 12.9 cm(-1), indicating an excellent agreement between experimental and calculated energy levels. The temperature-dependent luminescence dynamics of the (5)D(0) multiplet for Eu(3+) in β-Ga(2)O(3) phosphors has also been revealed for the first time from 10 to 300 K.  相似文献   

15.
Detection of chelatable zinc (Zn(2+)) in biological studies has attracted much attention recently, because chelatable Zn(2+) plays important roles in many biological systems. Lanthanide complexes (Eu(3+), Tb(3+), etc.) have excellent spectroscopic properties for biological applications, such as long luminescence lifetimes of the order of milliseconds, a large Stoke's shift of >200 nm, and high water solubility. Herein, we present the design and synthesis of a novel lanthanide sensor molecule, [Eu-7], for detecting Zn(2+). This europium (Eu(3+)) complex employs a quinolyl ligand as both a chromophore and an acceptor for Zn(2+). Upon addition of Zn(2+) to a solution of [Eu-7], the luminescence of Eu(3+) is strongly enhanced, with high selectivity for Zn(2+) over other biologically relevant metal cations. One of the important advantages of [Eu-7] is that this complex can be excited with longer excitation wavelengths (around 340 nm) as compared with previously reported Zn(2+)-sensitive luminescent lamthanide sensors, whose excitation wavelength is at too high an energy level for biological applications. The usefulness of [Eu-7] for monitoring Zn(2+) changes in living HeLa cells was confirmed. This novel Zn(2+)-selective luminescent lanthanide chemosensor [Eu-7]should be an excellent lead compound for the development of a range of novel luminescent lanthanide chemosensors for biological applications.  相似文献   

16.
Nordén M  Ephraim JH  Allard B 《Talanta》1997,44(5):781-786
Effects of competing ions, Fe (2+)Fe (3+) and Al(3+), on Eu(3+) complexation with an aquatic fulvic acid (FA), have been investigated using an ion exchange technique. The influence of different concentrations (10(-6), 10(-4) M) of the competing ions on the distribution coefficient for Eu was measured, and the overall complex formation function, beta(ov), was resolved for the Eu systems with Fe and Al. All systems showed pH-dependent beta(ov)-functions. The presence of 10(-4) M concentration of competing ion reduced the resolved complex formation function (logbeta(ov)) for Eu complexation with fulvic acid by 0.6 and 0.4 log units at pH 5 for Fe and Al, respectively. this indicates that Fe has a more perturbing effect on Eu-FA complexation than Al. In similar competition studies Sr and Eu were found not to perturb each others complexation with fulvic acid, suggesting therefore that the two metals probably bind to different sites on the fulvic acid molecule.  相似文献   

17.
In(2)O(3) sol-gel thin films made with LaF(3):Ln(3+) (Ln=Er, Nd, and Eu) nanoparticles were prepared and showed sensitized emission of the lanthanide ions after In(2)O(3) matrix excitation. The excitation spectra showed an In(2)O(3) absorption band in addition to the excitation peaks of the lanthanide ions, clearly demonstrating that there is energy transfer from the In(2)O(3) matrix to Ln(3+) (Er(3+), Nd(3+), and Eu(3+)). Similarly, HfO(2) and ZrO(2) sol-gel thin films made with LaF(3):Ln(3+) nanoparticles also showed energy transfer from the semiconductor matrix to the lanthanide ions.  相似文献   

18.
Grimes TS  Tian G  Rao L  Nash KL 《Inorganic chemistry》2012,51(11):6299-6307
Time-resolved fluorescence spectroscopy and Fourier transform IR spectroscopy have been applied to characterize the coordination environment of lipophilic complexes of Eu(3+) with bis(2-ethylhexyl)phosphoric acid (HDEHP) and (2-ethylhexyl)phosphonic acid mono(2-ethylhexyl) ester (HEH[EHP]) in 1,4-diisopropylbenzene (DIPB). The primary focus is on understanding the role of lactate (HL) in lanthanide partitioning into DIPB solutions of HDEHP or HEH[EHP] as it is employed in the TALSPEAK solvent extraction process for lanthanide separations from trivalent actinides. The broader purpose of this study is to characterize the changes that can occur in the coordination environment of lanthanide ions as metal-ion concentrations increase in nonpolar media. The optical spectroscopy studies reported here complement an earlier investigation of similar solutions using NMR spectroscopy and electrospray ionization mass spectrometry. Emission spectra of Eu(3+) complexes with HDEHP/HEH[EHP] demonstrate that, as long as the Eu(3+) concentration is maintained well below saturation of the organic extractant solution, the Eu(3+) coordination environment remains constant as both [HL](org) and [H(2)O](org) are increased. If the total organic-phase lanthanide concentration is increased (by extraction of moderate amounts of La(3+)), the (5)D(0) → (7)F(1) transition singlet splits into a doublet with a notable increase in the intensity of both (5)D(0) → (7)F(1) and (5)D(0) → (7)F(2) electronic transitions. The increased multiplicity in the emission spectra indicates that Eu(3+) ions are present in multiple coordination environments. The increased emission intensity of the 614 nm band implies an overall reduction in symmetry of the extracted Eu(3+) complex in the presence of macroscopic La(3+). Although [H(2)O](org) increases to above 1 M at high [HL](tot), this water is not associated with the Eu(3+) metal center. IR spectroscopy results confirm a direct Ln(3+)-lactate interaction at high concentrations of lanthanide and lactate in the extractant phase. At low organic-phase lanthanide concentrations, the predominant complex is almost certainly the well-known Ln(DEHP·HDEHP)(3). As lanthanide concentrations in the organic phase increase, mixed-ligand complexes with the general stoichiometry Ln(L)(n)(DEHP)(3-n) or Ln(L)(n)(DEHP·HDEHP)(3-n) become the dominant species.  相似文献   

19.
Attapulgite, an extremely stable fibrillar mineral present in nature, is a promising new carrier of luminescent lanthanide complexes for further applications. A europium complex Eu(DBM)(3)(H(2)O)(2) (HDBM = dibenzoylmethane) was covalently coupled onto modified attapulgites (or silica nanoparticles) via a ligand exchange reaction, generating attapulgite-based ternary europium complexes. The composites were characterized by CHN elemental analysis, inductively coupled plasma-atomic emission spectroscopy (ICP-AES) for Eu(3+) content, powder X-ray diffraction (XRD), thermogravimetry (TG) and UV-vis absorption spectra. The results indicate that the Eu(3+) complex was grafted covalently to the outer surfaces of attapulgites (or silica nanoparticles) and modifications by coupling agents containing different alkoxide groups (aminopropyltriethoxysilane (APTES) or aminopropylmethyldiethoxysilane (APMDES)) led to different grafting ratios. The structures of these composites were further evidenced by the determination of photophysical behaviours and coordinated water molecules of the complexes linked to matrices. Attapulgite-based lanthanide composites linked by APTES can be excited by visible light, with a wide excitation wavelength range from UV to visible light (a maximum at 398 nm), long luminescence lifetime (503 μs), high quantum yield (48%) and improved exposure durability. When incubated with HeLa cells at 37 °C, the fluorescence of matrix-APTES-cpa-Eu(DBM)(3) is observed on the cell membrane. Moreover, the low cytotoxicity of our present system results in potential applications for cell imaging in biological systems.  相似文献   

20.
One-dimensional La(9.33)(SiO(4))(6)O(2): Ln(3+) (Ln = Ce, Eu, Tb) microfibers were fabricated by a simple and cost-effective electrospinning method. X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), scanning electron microscopy (SEM), transmission electron microscopy (TEM), high-resolution transmission electron microscopy (HRTEM), photoluminescence (PL) and low voltage cathodoluminescence (CL) as well as kinetic decay were used to characterize the resulting samples. SEM and TEM results indicated that the diameter of the microfibers annealed at 1000 °C for 3 h was 200-245 nm. The microfibers were further composed of fine and closely linked nanoparticles. La(9.33)(SiO(4))(6)O(2): Ln(3+) (Ln = Ce, Eu, Tb) phosphors showed the characteristic emission of Ce(3+) (5d → 4f), Eu(3+) ((5)D(0)→(7)F(J)) and Tb(3+) ((5)D(3,4)→(7)F(J)) under ultraviolet excitation and low-voltage electron beams (3-5 kV) excitation. An energy transfer from Ce(3+) to Tb(3+) was observed in the La(9.33)(SiO(4))(6)O(2): Ce(3+), Tb(3+) phosphor under ultraviolet excitation and low-voltage electron beam excitation. Luminescence mechanisms were proposed to explain the observed phenomena. Blue, red and green emission can be realized in La(9.33)(SiO(4))(6)O(2): Ln(3+) (Ln = Ce, Eu, Tb) microfibers by changing the doping ions. So the La(9.33)(SiO(4))(6)O(2): Ln(3+) (Ln = Ce, Eu, Tb) phosphors have potential applications in full-color field emission displays.  相似文献   