Structural and optical properties of Sc-doped ZnO films grown by RF magnetron sputtering at different substrate temperatures were investigated. All the ZnO:Sc films are polycrystalline with the hexagonal wurtzite structure. X-ray diffraction patterns of the films showed that the doped-films have (0 0 2) as preferred orientation when the deposition temperature was increased from 250 °C to 300 °C. All the films are in a state of compressive stress, whereas the stress decreases gradually with increasing substrate temperature. The average transmittance of these films was above 90% in the wavelength range from 400 nm to 800 nm. The optical band gap of these films was determined. The optical constants of these films were determined using transmittance and reflectance spectra.  相似文献   

2.
Zinc oxide thin films have been deposited on glass substrates at a substrate temperature of 673 K by spray pyrolysis. The samples are annealed in ambient atmosphere at various temperatures. The effect of annealing on structural, electrical, and optical properties of ZnO films has been investigated. X-ray diffraction patterns show that crystallinity of the ZnO films has been improved after annealing. The morphology of ZnO thin films is studied by atomic force microscopy. The tensile strain (compressive stress) is found to decrease with increase in annealing temperature which indicates the relaxation of tensile strain in ZnO thin films. A decrease in energy band gap is observed with increase of annealing temperature. The mechanism of blue-green luminescence of ZnO thin film has been analyzed. The resistivity is found to decrease with annealing temperature.  相似文献   

3.
Zinc oxide (ZnO) thin film has been epitaxially grown on (1 1 1) Mg0.4Al2.4O4 substrate by RF-magnetron sputtering. In resonant Raman scattering, higher-order longitudinal optical phonon modes were clearly observed, revealing high optical quality of the ZnO film. Optical absorption indicated a visible exciton absorption at room temperature. The near band edge emission showed a red shift due to the shrinkage of the band gap with increasing the temperature.  相似文献   

4.
The structural and luminescence related optical behaviours of Au ion implanted ZnO films grown by magnetic sputtering and their post implantation annealing behaviours in the temperature range of 100-700 °C have been investigated. Optical absorption and transmittance spectra of the films indicate that band edge of Au-implanted ZnO has shifted to high energy range and optical band gap has increased, because the sharp difference of thermal expansion induces the lattice mismatch between ZnO and SiO2. PL spectra reveal that UV and visible luminescence bands of ZnO films can be improved after thermal annealing due to recovery of defects and Au ions incorporation. Importantly, green luminescence band of 530 nm has been only observed in the Au-implanted and subsequently annealed ZnO films and it enhances with the increasing annealing temperature, which can be related to Au atoms or clusters in ZnO films. Furthermore, X-ray photoelectron spectroscopy measurements reveal that the Au0 is dominant state in Au implanted and annealed ZnO films. Possible mechanisms, such as optical transitions of Au atoms or clusters and deep level luminescence of ZnO, have been proposed for green emission.  相似文献   

5.
ZnO films were deposited by RF magnetron sputtering at the substrate temperature of 120∼420°C. XRD measurements revealed the improvement of crystalline quality and grain size of the films with substrate temperature. The dielectric function of the films was determined by fitting the experimental transmission spectra with Tauc–Lorentz (TL) model and a single Lorentzian oscillator (SLO) dispersion function in the energy range of 1∼5 eV. The optical properties of the ZnO films strongly depended on the substrate temperature. The optical band gap and the Penn gap of the ZnO films increased with the substrate temperature. The band gap of the ZnO films indicated a direct interband transition between the valence and conduction band, and the change of the in-plane film stress promoted the enhancement of the band gap. These results of the optical properties of the ZnO films might be very meaningful to the application in the window design in solar cells.  相似文献   

6.
High quality self-assemble ZnO quantum dots (QDs) have been successfully grown on the Si(111) substrates by metalorganic chemical vapor deposition (MOCVD). The diameter of ZnO QDs is about 10 nm in average, and the densities and the sizes of ZnO QDs can be well controlled by adjusting the growth temperature, which were evident in the SEM images. The properties and stress involved in ZnO QDs are studied by X-ray diffraction. In addition, room temperature photoluminescence spectra reveal that the ZnO QDs exhibit a band gap blue shift because of the quantum confinement effects.  相似文献   

7.
Undoped and cesium‐doped zinc oxide (ZnO) thin films have been deposited on sapphire substrate (0001) using the sol–gel method. Films were preheated at 300 °C for 10 min and annealed at 600 and 800 °C for 1 h. The grown thin films were confirmed to be of wurtzite structure using X‐ray diffraction. Surface morphology of the films was analyzed using scanning electron microscopy. The photoluminescence (PL) spectra of ZnO showed a strong ultraviolet (UV) emission band located at 3.263 eV and a very weak visible emission associated with deep‐level defects. Cesium incorporation induced a blue shift of the optical band gap and quenching of the near‐band‐edge PL for nanocrystalline thin film at room temperatures because of the band‐filling effect of free carriers. A shift of about 10–15 cm−1 is observed for the first‐order longitudinal‐optical (LO) phonon Raman peak of the nanocrystals when compared to the LO phonon peak of bulk ZnO. The UV resonant Raman excitation at RT shows multiphonon LO modes up to fifth order. Copyright © 2010 John Wiley & Sons, Ltd.  相似文献   

8.
To extend the applicability of ZnO, with the bulk band gap of about 3.3 eV, into deep UV region, we have grown a multilayer of alumina capped ZnO quantum dots of mean in-plane sizes in the range of ∼1.8-3.6 nm at room temperature using alternate Pulsed Laser Deposition. Size dependent blue shift of the band gap of these dots up to ∼4.5 eV is observed in the optical absorbance spectra. The observed blue shift can be understood using the effective mass approximation in weak and strong confinement regimes.  相似文献   

9.
In this paper we investigate the band gap renormalization in heavily Ga-doped ZnO thin films deposited by pulsed laser deposition on CC-plane sapphire and mica substrates. Thin films were studied by ultraviolet photoelectron spectroscopy and also by optical measurements under high pressure. The Fermi-level shift, as obtained from ultraviolet photoelectron experiments, exhibits a relatively small and positive shift (about 0.3 eV) with respect to the valence band for increasing electron concentrations up to 1021 cm−3. The optical gap exhibits a much larger increase (0.6 eV) for the same concentration range. Absorption measurements under pressure show that the pressure coefficient of the optical gap is correlated to the electron concentration in films, decreasing with increasing electron concentration. As a consequence, the contributions of band filling and band renormalization to the optical gap shift can be separated on the basis of the different pressure behavior of the physical parameters involved in each effect.  相似文献   

10.
Zinc oxide films of 40 nm thickness have been deposited on glass substrates by pulsed laser deposition using an excimer XeCl laser (308 nm) at different substrate temperatures ranging from room temperature to 650 °C. Surface investigations carried out by using atomic force microscopy have shown a strong influence of temperature on the films surface topography. UV-VIS transmittance measurements have shown that our ZnO films are highly transparent in the visible wavelength region, having an average transmittance of ∼90%. The optical band gap of the films was found to be 3.26 eV, which is lower than the theoretical value of 3.37 eV. Besides the normal absorption edge related to the transition between the valence and the conduction band, an additional absorption band was also recorded in the wavelength region around 364 nm (∼3.4 eV). This additional absorption band may be due to excitonic, impurity, and/or quantum size effects. Photoreduction/oxidation in ozone of the ZnO films lead to larger conductivity changes for higher deposition temperature. In conclusion, the ozone sensing characteristics as well as the optical properties of the ZnO thin films deposited by pulsed laser deposition are strongly influenced by the substrate temperature during growth. The sensitivity of the films towards ozone might be enhanced significantly by the control of the films deposition parameters and surface characteristics.  相似文献   

11.
ZnO and ZnO:Al films were deposited onto glass substrates by the sol gel method using spin coating technique. The effects of aluminum dopant on the crystalline structure and orientation of the ZnO films have been investigated by X-ray diffraction (XRD) study. Surface morphology of the films has also been analyzed by a field emission scanning electron microscope (FESEM) and atomic force microscope (AFM). The average optical transmittance values of all the films is over >83% in the visible region. The optical band gap and Urbach energy values of these films were determined. The absorption edge shifted to the lower energy depending on the Al doping level. The shift of absorption edge is associated with shrinkage effect. The electrical conductivity of the ZnO film enhanced with the Al dopant. From the temperature dependence of conductivity measurements, the activation energy of the films was also calculated.  相似文献   

12.
In this work, the pulsed electron beam deposition method (PED) is evaluated by studying the properties of ZnO thin films grown on c-cut sapphire substrates. The film composition, structure and surface morphology were investigated by means of Rutherford backscattering spectrometry, X-ray diffraction and atomic force microscopy. Optical absorption, resistivity and Hall effect measurements were performed in order to obtain the optical and electronic properties of the ZnO films. By a fine tuning of the deposition conditions, smooth, dense, stoichiometric and textured hexagonal ZnO films were epitaxially grown on (0001) sapphire at 700 °C with a 30° rotation of the ZnO basal plane with respect to the sapphire substrate. The average transmittance of the films reaches 90% in the visible range with an optical band gap of 3.28 eV. Electrical characterization reveals a high density of charge carrier of 3.4 × 1019 cm?3 along with a mobility of 11.53 cm²/Vs. The electrical and optical properties are discussed and compared to ZnO thin films prepared by the similar and most well-known pulsed laser deposition method.  相似文献   

13.
High quality transparent conductive gallium-doped zinc oxide (GZO) thin films were deposited on glass substrates using rf-magnetron sputtering system at the temperature ranging from room temperature (RT) to 500 °C. The temperature-dependence of Ga doping effect on the structural, optical and electrical properties in ZnO has been investigated. For the GZO thin films deposited at over 200 °C, (103) orientation was strongly observed by X-ray diffraction analysis, which is attributed to the substitution of Ga elements into Zn site. X-ray photoelectron spectroscopy measurements have confirmed that oxygen vacancies were generated at the temperature higher than 300 °C. This might be due to the effective substitution of Ga3+ for Zn site at higher temperature. It was also found that the optical band gap increases with deposition temperature. The optical transmittance of GZO thin films was above 87% in the visible region. The GZO thin films grown at 500 °C showed a low electrical resistivity of 4.50 × 10?4 Ω cm, a carrier concentration of 6.38 × 1020 cm?3 and a carrier mobility of 21.69 cm2/V.  相似文献   

14.
ZnO thin films were fabricated using zinc chloride and zinc acetate precursors by the spray pyrolysis technique on FTO coated glass substrates. The ZnO films were grown in different deposition temperature ranges varying from 400 to 550 °C. Influences of substrate temperature and zinc precursors on crystal structure, morphology and optical property of the ZnO thin films were investigated. XRD patterns of the films deposited using chloride precursor indicate that (1 0 1) is dominant at low temperatures, while those deposited using acetate precursor show that (1 0 1) is dominant at high temperatures. SEM images show that deposition temperature and type of precursor have a strong effect on the surface morphology. Optical measurements show that ZnO films are obviously influenced by the substrate temperatures and different types of precursor solutions. It is observed that as temperature increases, transmittance decreases for ZnO films obtained using zinc chloride precursor, but the optical transmittance of ZnO films obtained using zinc acetate precursor increases as temperature increases.  相似文献   

15.
Amorphous thin films of InGaZnO4 (a-IGZO) doped with Cr have been fabricated by using pulsed-laser deposition (PLD). The electrical, optical and magnetic properties of Cr-doped a-IGZO films grown at 25 °C and 150 °C were investigated. The conductivity, optical transmission and band gap of films are remarkably enhanced by increasing the growth temperature. Conductivity, carrier concentration and mobility decrease with increasing the Cr content. However, the optical transmission and band gap are not significantly affected by Cr doping. Moreover, all Cr-doped films exhibit room-temperature ferromagnetism.  相似文献   

16.
Titanium-doped cadmium oxide thin films were deposited on quartz substrate by pulsed laser deposition technique. The effect of substrate temperature on structural, optical and electrical properties was studied. The films grown at high temperature show (2 0 0) preferred orientation, while films grown at low temperature have both (1 1 1) and (2 0 0) orientation. These films are highly transparent (63-79%) in visible region, and transmittance of the films depends on growth temperature. The band gap of the films varies from 2.70 eV to 2.84 eV for various temperatures. It is observed that resistivity increases with growth temperature after attaining minimum at 150 °C, while carrier concentration continuously decreases with temperature. The low resistivity, high transmittance and wide band gap titanium-doped CdO films could be an excellent candidate for future optoelectronic and photovoltaic applications.  相似文献   

17.
Eu-doped ZnO (EZO) thin films were prepared on glass substrates at various growth temperatures by radio-frequency magnetron sputtering. The properties of deposited thin films showed a significant dependence on the growth temperature. The preferential growth orientation of all the thin films was occurred along the ZnO (002) plane. The maximum crystallite size and the minimum average transmittance in the wavelength range of 450–1100 nm were observed for the EZO thin film deposited at 25 °C. A red shift of the optical band gap was observed in the growth temperature range of 25–300 °C. The highest figure of merit, an index for evaluating the performance of transparent conducting thin films, was obtained at 200 °C of growth temperature. These results indicated that the high-quality EZO film was obtained at a growth temperature of 200 °C.  相似文献   

18.
The effect of multi-step deposition process on the crystalline quality and surface smoothness of ZnO film was investigated. ZnO films were composed of multi-layers, in which each layer was deposited at different temperatures. The maximum intensity and the smallest FWHM of (0 0 2) diffraction peak in XRD spectrum were observed for the multi-layered ZnO film of which each layer was deposited at progressively higher temperatures. In addition, the smoothest film surface was also observed for the ZnO film deposited through multi-step process in which deposition temperatures gradually increase. On the other hand, the large difference between the deposition temperatures in multi-step process did not result in the significant improvement of the crystalline quality of ZnO film. The ZnO film prepared by using multi-step process had high transmittance over 70% in visible region and the optical band gap of 3.22 eV.  相似文献   

19.
The effects of biaxial stress in ZnO:Ga thin films on different substrates, e.g., sapphire(0001), quartz, Si(001), and glass have been investigated by X-ray diffraction, atomic force microscopy, and electrical transport and ellipsometric measurements. A strong dependence of orientation, crystallite size, transport, and electronic properties upon the substrate-induced stress has been found. The structural properties indicate that a tensile stress exists in epitaxial ZnO:Ga films grown on sapphire, Si, and quartz, while a compressive stress appears in films grown on glass. The resistivity of the films decreased with increasing biaxial stress, which is inversely proportional to the product of the carrier concentration and Hall mobility. The refractive index n was found to decrease with increasing biaxial stress, while the optical band gap E0 increased with stress. These behaviors are attributed to lattice contraction and the increase in the carrier concentration that is induced by the stress. Our experimental data suggest that the mechanism of substrate-induced stress is important for understanding the properties of ZnO:Ga thin films and for the fabrication of devices which use these materials.  相似文献   

20.
ZnO:Ag films were grown on Si (1 0 0) substrates by ultrasonic spray pyrolysis at various substrate temperatures. The effect of deposition temperature on the structural and the room temperature photoluminescence (RT-PL) properties of ZnO:Ag films was studied. With the deposition temperature rising to 550 °C, the intensity of the near-band edge (NBE) emission at 378 nm decreased and a new emission peak at 399 nm was observed. On the basis of the X-ray diffraction pattern (XRD), the X-ray photoelectron (XPS) spectra of ZnO:Ag films, and the effects of annealing on the PL, we suggest that the 399 nm emission should be attributed to the electron transition from the conduction band to AgZn-related complexes defects radiative centers above the valence band.  相似文献   