As20S80 thin films with different thicknesses (49.4-763.1 nm) were deposited on glass substrates using a thermal evaporation technique. Spectrophotometric measurements of the films' transmittance were taken in the wavelength range of 190-2500 nm. The transmission spectra were simulated with a computer model based on dielectric modelling to determine the optical constants and thicknesses of the films. The O'Leary-Johnson-Lim (OJL) models implemented in the commercial software programme SCOUT were used. Thicknesses obtained by the simulated method were correlated to the results obtained from a surface profiler technique. Optical parameters, such as the refractive index n, the absorption coefficient k, the optical band gap Eg, the high-frequency dielectric constant ε, the Urbach energy EU, the single-oscillator energy and the dispersion energy, were determined. The results indicated that the thickness effect can be separated into two distinct groups for films of thicknesses either less than or greater than 312 nm.  相似文献   

2.
A high-quality ZnNb2O6 single-crystal grown by optical floating zone method has been used as a research prototype to analyze the optoelectronic parameters by measuring the absorption coefficient and transmittance spectra along the b-axis from 200 nm to 1000 nm at room temperature. The optical interband transitions of ZnNb2O6 have been determined as a direct transition with a band gap of 3.84 eV. The refractive index, extinction coefficient, and real and imaginary parts of the complex dielectric constants as functions of the wavelength for ZnNb2O6 crystal are obtained from the measured absorption coefficients and transmittance spectra. In the Urbach tail of 3.16–3.60 eV, the validity of the Cauchy–Sellmeier equation has also been evaluated. Using the single effective oscillator model, the oscillator energy Eo is found to be 4.77 eV. The dispersion energy Ed is 26.88 eV and ZnNb2O6 crystal takes an ionic value.  相似文献   

3.
In this work, GaMnAs alloy materials were deposited on 7059 Corning glass and GaAs (1 0 0) substrates via RF magnetron sputtering technique. A concentration of Mn about 0.28 was obtained by Energy Dispersive X-ray spectroscopy. The substrate temperature was changed from 440 to 520 °C and layer thicknesses between 172 and 514 nm were obtained. Characterization by atomic force microscopy and X-ray diffraction were performed to determinate surface morphology and crystal structure, respectively. From transmittance spectral measurements we were able to determine optical constants: band gap energy (Eg), absorption coefficient (α), and refraction index (n). A correlation between morphological properties and substrate type was also studied. Diluted magnetic semiconductors like GaMnAs are considered among promising materials for the development of new spin-electronic devices.  相似文献   

4.
Daeil Kim 《Optics Communications》2010,283(9):1792-1794
Au-intermediate TiO2/Au/TiO2 (TAT) multilayer films were deposited by RF magnetron sputtering onto glass substrates. Changes in the optical and electrical properties of the films were investigated with respect to the thickness of the Au interlayer.The observed optical and electrical properties were dependent on the thickness of the Au interlayer. The resistivity decreased to 3.3 × 10−4 Ω cm for TiO2 films with a 20 nm-thick Au interlayer and the optical transmittance was also influenced by the Au interlayer. Although optical transmittance deteriorated as Au thickness increased, TiO2 films with a 5 nm-thick Au interlayer showed a relatively high optical transmittance of 80% at a wavelength of 550 nm. In addition, since a TAT film with a 5 nm-thick Au interlayer showed a relatively high work function value, it is an alternative candidate for use as a transparent anode in OLEDs and flat panel displays.  相似文献   

5.
Bi4Ti3O12 (BTO) and Bi3.25In0.75Ti3O12 (BTO:In) thin films were prepared on fused quartz and LaNiO3/Si (LNO) substrates by chemical solution deposition (CSD). Their microstructures, ferroelectric and optical properties were investigated by X-ray diffraction, scanning electron microscope, ferroelectric tester and UV-visible-NIR spectrophotometer, respectively. The optical band-gaps of the films were found to be 3.64 and 3.45 eV for the BTO and BTO:In films, respectively. Optical constants (refractive indexes and extinction coefficients) were determined from the optical transmittance spectra using the envelope method. Following the single electronic oscillator model, the single oscillator energy E0, the dispersion energy Ed, the average interband oscillator wavelength λ0, the average oscillator strength S0, the refractive index dispersion parameter (E0/S0), the chemical bonding quantity β, and the long wavelength refractive index n were obtained and analyzed. Both the refractive index and extinction coefficient of the BTO:In films are smaller than those of the BTO films. Furthermore, the refractive index dispersion parameter (E0/S0) increases and the chemical bonding quantity β decreases in the BTO and BTO:In films compared with those of bulk.  相似文献   

6.
采用金属有机分解法(MOD)在石英衬底上沉积了SrTiO3薄膜。所制备的薄膜是晶格常数为a=b=c=3.90?的多晶结构。通过测量190—1100nm波段内的透射光谱,采用包络方法计算了薄膜的光学常数(折射率n和消光系数k)。结果表明,采用MOD方法制备的薄膜的折射率大于采用射频磁控溅射、溶胶—凝胶和化学气相沉积方法制备的薄膜的折射率;薄膜的折射率色散关系满足单振子模型,其中振子强度S0为0.88′1014m-2,振子能量E0为6.40eV;薄膜的禁带宽度为3.68eV。  相似文献   

7.
Thin films of SnO2 were deposited by RF-magnetron sputtering on quartz substrates at room temperature in an environment of Ar and O2. The XRD pattern shows amorphous nature of the as-deposited films. The optical properties were studied using the reflectance and transmittance spectra. The estimated optical band gap (Eg) values increase from 4.15 to 4.3 eV as the Ar gas content decreases in the process gas environment. The refractive index exhibits an oscillatory behavior that is strongly dependent on the sputtering gas environment. The Urbach energy is found to decrease with increase in band gap. The band gap is found to decrease on annealing the film. The role of oxygen defects is explored in explaining the variation of optical parameters.  相似文献   

8.
Thin films of indium oxide, In2O3, were deposited by chemical spray pyrolysis technique, using aqueous alcoholic solutions of indium acetylacetonate (In-acac) precursor, on glass substrates kept at temperatures between 300 and 500 °C. The structural, optical, and electrical properties have been investigated as a function of deposition temperature, precursor concentration, carrier gas pressure, and substrate-to-nozzle distance. X-ray diffraction studies showed that the formation of nanocrystalline In2O3 films is preferentially oriented along (2 2 2) plane. The surface morphological modifications with substrate temperature were observed using scanning electron and atomic force microscopic studies. Optical transmittance behavior of the films in the visible and IR region was strongly affected by the deposition parameters. The optical band gap values observed are between 3.53 and 3.68 eV. The long wavelength limit of refractive index is 1.83. The Hall mobility is found to vary from 23 to 37 cm2/V s and carrier density is found nearly constant at about 1020 cm−3.  相似文献   

9.
Electron beam evaporation technique was used to prepare TiO2 and Ti2O3 thin films onto glass substrates of thicknesses 50, 500 and 1000 nm for each sample. The structural investigations revealed that the as-deposited films are amorphous in nature. Transmittance measurements in the wavelength range (350-2000 nm) were used to calculate the refractive index n and the absorption index k using Swanepoel's method. The optical constants such as optical band gap , optical conductivity σopt, complex dielectric constant, relaxation time τ and dissipation factor tan δ were determined. The analysis of the optical absorption data revealed that the optical band gap Eg was indirect transitions. The optical dispersion parameters Eo and Ed were determined according to Wemple and Didomenico method.  相似文献   

10.
11.
The results of gadolinium (Gd)-doped barium titanate (BaTiO3) thin films prepared by laser ablation on glass and silicon substrates are reported. Rutherford backscattering (RBS) analyses carried out on glass samples indicated the substitution of barium (Ba) by gadolinium (Gd) after annealing, leading to a film with composition Ba0.76TiGd0.01O2.5. There is a reduction in the thickness from 2.21 to 2.02 microns for as-deposited and annealed films. The films on silicon showed a higher degree of crystallinity compared to that of glass substrates due to increased annealing temperature. The average grain size calculated using the X-ray diffraction (XRD) pattern from silicon substrates was 30 nm. The film has a tetragonal structure with a “c/a” ratio of 1.03 signifying that the incorporation of Gd in BaTiO3 led to the elongation of the c-axis. The percentage transmittance reduced from 80 to 50% due to annealing and this is probably due to structural changes in the film. Swanepoel envelope method employed on the interference fringes of the transmittance pattern led to the determination of the variation of the refractive index with wavelength. Sellmier single oscillator model was applied to determine the optical constants of the films on glass substrates. Bandgap analyses carried out showed the reduction in bandgap with annealing and also the possibility that Gd incorporation has modified the film chemistry leading to the existence of direct (4.35 eV) and indirect (3.88 eV) allowed transitions in the annealed films. Dielectric property measurement carried out under ambient conditions gave a relaxation time τ of 1.6×10−4 s and conduction by small polaron with the onset of polaron conduction set at about 7 kHz. It is conjectured that these properties, especially the high refractive index and the high bandgaps, can make Gd-doped BaTiO3 a good candidate for optoelectronic applications.  相似文献   

12.
Nearly stoichiometric thin films of In49Se48Sn3 were deposited at room temperature, by conventional thermal evaporation of the presynthesized materials, onto precleaned glass substrates. The microstructural studies on the as-deposited and annealed films, using transmission electron microscopy and diffraction (TEMD), revealed that the as-deposited films are amorphous in nature, while those annealed at 498 K are crystalline. The optical properties of the investigated films were determined from the transmittance and reflectance data, in the spectral range 650-2500 nm. An analysis of the optical absorption spectra revealed a non-direct energy gap characterizing the amorphous films, while both allowed and forbidden direct energy gaps characterized the crystalline films. The electrical resistance of the deposited films was carried out during heating and cooling cycles in the temperature range 300-600 K. The results show an irreproducible behavior, while after crystallization the results become reproducible. The analysis of the temperature dependence of the resistance (ln(R) vs. 1000/T) for crystalline films shows two straight lines corresponding to both extrinsic and intrinsic conduction. The room temperature I-V characteristics of the as-deposited films sandwiched between similar Ag metal electrodes shows an ohmic behavior, while non-ohmic behavior attributed to space charge limited conduction has been observed when the films are sandwiched between dissimilar Ag/Al metal electrodes.  相似文献   

13.
In this paper, the effect of annealing temperature on optical constants was studied. The ZnO films were deposited on microscopic glass substrates using the sol-gel method for various annealing temperatures. The deposited zinc oxide (ZnO) films were characterized by an X-ray diffractometer (XRD), a spectrophotometer and scanning electron microscopy (SEM). The transmittance spectra recorded through the spectrophotometer exhibits 90% transmittance. The XRD spectra showed polycrystalline nature of ZnO film. Optical constants were determined through transmittance spectra using an envelope method. It was found that there was a significant effect of annealing temperature on the refractive index and extinction coefficient of deposited ZnO films. In this experiment, the optimum refractive index value of 1.97 was obtained at 350 °C annealing temperature at visible (vis) wavelength. The optical energy gap was found to be of ∼3.2 eV for all the samples. The top view of SEM showed the ZnO grain growth on the glass substrates.  相似文献   

14.
Electron beam gun technique was used to prepare Ta2O5 thin films onto infrasil substrates of thicknesses 333 and 666 nm. The structure characterization was investigated using X-ray diffraction patterns. Transmittance measurements in the wavelength range (240-2000 nm) were used to calculate the refractive index n and the absorption index k depending on Swanepole's method. The dispersion curve of the refractive index shows an anomalous dispersion in the absorption region and a normal one in the transparent region. The analysis of the optical absorption data revealed that the optical band gap Eg was indirect transition. It was found that the refractive index dispersion data obeyed the single oscillator of the Wemple-DiDomenico model, from which the dispersion parameters (Eo and Ed) and the high frequency dielectric constant were determined. The electric free carrier susceptibility and the carrier concentration to the effective mass ratio were estimated according to the model of Spitzer and Fan. Graphical representation of the relaxation time as a function of photon energy was also presented.  相似文献   

15.
This paper focuses the influence of porous morphology on the microstructure and optical properties of TiO2 films prepared by different sol concentration and calcination temperatures. Mesoporous TiO2 thin films were prepared on the glass substrates by sol-gel dip coating technique using titanium (IV) isopropoxide. Porous morphology of the films can be regulated by chemical kinetics and is studied by scanning electron microscopy. The optical dispersion parameters such as refractive index (n), oscillator energy (Ed), and particle co-ordination number (Nc) of the mesoporous TiO2 films were studied using Swanepoel and Wemple-DiDomenico single oscillator models. The higher precursor concentration (0.06 M), films exhibit high porosity and refractive index, which are modified under calcination treatment. Calcinated films of low metal precursor concentration (0.03 M) possess higher particle co-ordination number (Nc = 5.05) than that of 0.06 M films (Nc = 4.90) due to calcination at 400 °C. The lattice dielectric constant (E) of mesoporous TiO2 films was determined by using Spintzer model. Urbach energy of the mesoporous films has been estimated for both concentration and the analysis revealed the strong dependence of Urbach energy on porous morphology. The influence of porous morphology on the optical dispersion properties also has been explained briefly in this paper.  相似文献   

16.
Chalcogenide glasses are interesting materials due to their infrared transmitting properties and photo induced effects exhibited by them. Thin films with thickness of 3000 Å of the glasses Se75S25−xCdx with x=6, 8 and 10 at% prepared by melt quench technique were evaporated by thermal evaporation onto glass substrates under a vacuum of 10−6 Torr. The optical constants (absorption coefficient, refractive index and extinction coefficient) of as-prepared and annealed films have been studied as a function of photon energy in the wave length region 400-1000 nm. Analysis of the optical absorption data shows that the rule of non-direct transitions predominates. It has been found that the absorption coefficient and optical band gap increase with increasing annealing temperatures. The refractive index (n) and the extinction coefficient (k) were observed to decrease with increasing annealing temperature.  相似文献   

17.
Se90Te10−xAgx (0 ≤ x ≤ 6) compositions were prepared by quenching technique. Thin films with different thicknesses of the obtained compositions were deposited on dry clean glass substrates by thermal evaporation technique. Energy dispersive X-ray spectroscopy (EDX) indicates that samples are nearly stoichiometric. X-ray diffraction patterns indicate that they are in the amorphous state. The optical constants, the refractive index n and the absorption index k, have been calculated from transmittance T and reflectance R through the spectral range of 400-2500 nm for the studied films with different thicknesses (165-711 nm). From the analysis of refractive index n data, high frequency dielectric constant ? was determined. Both ? and n are found to decrease with the increase of Ag content. The optical band gap is calculated for all compositions from the absorption coefficient analysis. The effect of the Ag addition on the obtained optical parameters has been discussed. The analysis of absorption index k data, revealed the existence of allowed indirect transitions for all compositions. It is indicated also that increase with increasing Ag content.  相似文献   

18.
TiO2 doped WO3 thin films were deposited onto glass substrates and fluorine doped tin oxide (FTO) coated conducting glass substrates, maintained at 500 °C by pyrolytic decomposition of adequate precursor solution. Equimolar ammonium tungstate ((NH4)2WO4) and titanyl acetyl acetonate (TiAcAc) solutions were mixed together at pH 9 in volume proportions and used as a precursor solution for the deposition of TiO2 doped WO3 thin films. Doping concentrations were varied between 4 and 38%. The effect of TiO2 doping concentration on structural, electrical and optical properties of TiO2 doped WO3 thin films were studied. Values of room temperature electrical resistivity, thermoelectric power and band gap energy (Eg) were estimated. The films with 38% TiO2 doping in WO3 exhibited lowest resistivity, n-type electrical conductivity and improved electrochromic performance among all the samples. The values of thermoelectric power (TEP) were in the range of 23-56 μV/K and the direct band gap energy varied between 2.72 and 2.86 eV.  相似文献   

19.
TiO2 thin films were deposited on the glass substrates by dc reactive magnetron sputtering technique at different sputtering pressures (2 × 10−3 to 2 × 10−2 mbar). The films prepared at low pressures have an anatase phase, and the films prepared at high pressures have an amorphous phase. The optical properties were studied by measuring the transmittance and the ellipsometric spectra. The optical constants of the films in the visible range were obtained by fitting the transmittance combined with the ellipsometry measurements using the classical model with one oscillator. The refractive index of the films decreases from 2.5 until 2.1 as the sputtering pressure increases from 2 × 10−3 to 2 × 10−2 mbar. The films prepared at the pressure higher than 6 × 10−3 mbar show a volume inhomogeneity. This volume inhomogeneity has been calculated by fitting the transmittance and the ellipsometric spectra. The volume inhomogeneity of the film prepared at the highest sputtering pressure is about 10%. Although the films prepared at high pressures show a large volume inhomogeneity, they have low extinction coefficients. It is suggested that the anatase phase results in more light scattering than amorphous phase does, and then a high extinction coefficient.  相似文献   

20.
Thin films of In-doped Ge-S in the form of Ge35In8S57 with different film thickness were deposited using an evaporation method. The X-ray diffraction studies demonstrate that the as-prepared films are amorphous in nature for these films. Some optical constants were calculated at a thickness of 150, 300, 450 and 900?nm and annealing temperature of 373, 413, 437 and 513?K. Our optical observations show that the mechanism of the optical transition obeys the indirect transition. It was found that the energy gap, Eg, decreases from 2.44 to 2.20?eV with expanding the thickness of the film from 150 to 900?nm. On the other hand, it was found that Eg increases with annealing temperature from 373 to 513?K. The increment in the band gap can be attributed to the gradual annealing out of the unsaturated bonds delivering a decreasing the density of localized states in the band structure. Using the single oscillator model, the dispersion of the refractive index is described. The dispersion constants of these films were calculated with different both thickness and annealing temperatures. Additionally, both of nonlinear susceptibility, χ(3) and nonlinear refractive index, n2 were calculated.  相似文献   